Search NASA⌕ Search

SEARCH · Search NASA

Results for “dissolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,063 records · Page 59

The growth and nanothermite reaction of 2Al/3NiO multilayer thin films

Nanothermite NiO–Al is a promising material system for low gas emission heat sources; still, its reactive properties are highly dependent on material processing conditions. In the current study, sputter deposition is used to fabricate highly controlled nanolaminates comprised of alternating NiO and Al layers. Films having an overall stoichiometry of 2Al to 3NiO were produced with different bilayer thicknesses to investigate how ignition and self-sustained, high temperature reactions vary with changes to nanometer-scale periodicity and preheat conditions. Ignition studies were carried out with both hot plate and laser irradiation and compared to slow heating studies in hot-stage x-ray diffraction. Ignition behavior has bilayer thickness and heating rate dependencies. The 2Al/3NiO with λ ≤ 300 nm ignited via solid/solid diffusion mixing (activation energy, E a = 49 ± 3 kJ/mole). Multilayers having λ ≥ 500 nm required a more favorable mixing kinetics of solid/liquid dissolution into molten Al (E a = 30 ± 4 kJ/mole). This solid/liquid dissolution E a is a factor of 5 lower than that of the previously reported powder compacts due to the elimination of a passivating Al oxide layer present on the powder. The reactant mixing mechanism between 300 and 500 nm bilayer thicknesses was dependent on the ignition source's heating rate. The self-propagating reaction velocities of 2Al/3NiO multilayers varied from 0.4 to 2.5 m/s. Pre-heating nanolaminates to temperatures below the onset reaction temperatures associated with forming intermediate nickel aluminides at multilayer interfaces led to increased propagation velocities, whereas pre-heating samples above the onset temperatures inhibited subsequent attempts at laser ignition.

36 MATERIALS SCIENCE↗

Large-scale molecular dynamics simulations of bubble collapse in water: Effects of system size, water model, and nitrogen

Molecular dynamics simulations in the microcanonical ensemble are performed to study the collapse of a bubble in liquid water using the single-site mW and the four-site TIP4P/2005 water models. To study system size effects, simulations for pure water systems are performed using periodically replicated simulation boxes with linear dimensions, L, ranging from 32 to 512 nm with the largest systems containing 8.7 × 10 6 and 4.5 × 10 9 molecules for the TIP4P/2005 and mW water models, respectively. The computationally more efficient mW water model allows us to reach converging behavior when the bubble dynamics results are plotted in reduced units, and the limiting behavior can be obtained through linear extrapolation in L –1 . Qualitative differences are observed between simulations with the mW and TIP4P/2005 water models, but they can be explained by the models’ differences in predicted viscosity and surface tension. Although bubble collapse occurs on time scales of only hundreds of picoseconds, the system sizes used here are sufficiently large to obtain bubble dynamics consistent with the Rayleigh–Plesset equation when using the models’ thermophysical properties as input. For the conditions explored here, extreme heating of the interfacial water molecules near the time of collapse is observed for the larger mW water systems (but the model underpredicts the viscosity), whereas heating is less pronounced for the TIP4P/2005 water systems because its larger viscosity contribution slows the collapse dynamics. The presence of nitrogen within the bubble only starts to affect bubble dynamics near the very end of the initial collapse, leading to an incomplete collapse and strong rebound for the mW water model. Although nitrogen is non-condensable at 300 K, it becomes highly compressed and reaches a liquid-like density near the collapse point. We find that the dissolution of nitrogen is much slower than the movement of the collapsing water front, and the re-expansion of the dense nitrogen droplet gives rise to bubble rebound. The incompatibility of the collapse and dissolution time scales should be considered for continuum-scale modeling of bubble dynamics. Finally, we also confirm that the diffusion coefficient for dissolved nitrogen is insensitive to pressure as the liquid transitions from a compressed to a stretched state.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Lithium metal stripping beneath the solid electrolyte interphase

Lithium stripping is a crucial process coupled with lithium deposition during the cycling of Li metal batteries. Lithium deposition has been widely studied, whereas stripping as a subsurface process has rarely been investigated. Here we reveal the fundamental mechanism of stripping on lithium by visualizing the interface between stripped lithium and the solid electrolyte interphase (SEI). We observed nanovoids formed between lithium and the SEI layer after stripping, which are attributed to the accumulation of lithium metal vacancies. High-rate dissolution of lithium causes vigorous growth and subsequent aggregation of voids, followed by the collapse of the SEI layer, i.e., pitting. We systematically measured the lithium polarization behavior during stripping and find that the lithium cation diffusion through the SEI layer is the rate-determining step. Nonuniform sites on typical lithium surfaces, such as grain boundaries and slip lines, greatly accelerated the local dissolution of lithium. As a result, the deeper understanding of this buried interface stripping process provides beneficial clues for future lithium anode and electrolyte design.

25 ENERGY STORAGE↗

Multidimensional visualization of the dynamic evolution of Li metal via in situ/operando methods

The growing demands for high-energy density electrical energy storage devices stimulate the coupling of conversion-type cathodes and lithium (Li) metal anodes. While promising, the use of these “Li-free” cathodes brings new challenges to the Li anode interface, as Li needs to be dissolved first during cell operation. In this study, we have achieved a direct visualization and comprehensive analysis of the dynamic evolution of the Li interface. The critical metrics of the interfacial resistance, Li growth, and solid electrolyte interface (SEI) distribution during the initial dissolution/deposition processes were systematically investigated by employing multidimensional analysis methods. They include three-electrode impedance tests, in situ atomic force microscopy, scanning electrochemical microscopy, and cryogenic scanning transmission electron microscopy. The high-resolution imaging and real-time observations show that a loose, diffuse, and unevenly distributed SEI is formed during the initial dissolution process. This leads to the dramatically fast growth of Li during the subsequent deposition, deviating from Fick’s law, which exacerbates the interfacial impedance. The compactness of the interfacial structure and enrichment of electrolyte species at the surface during the initial deposition play critical roles in the long-term stability of Li anodes, as revealed by operando confocal Raman spectroscopic mapping. In conclusion, our observations relate to ion transfer, morphological and structural evolution, and Li (de)solvation at Li interfaces, revealing the underlying pathways influenced by the initial dissolution process, which promotes a reconsideration of anode investigations and effective protection strategies.

25 ENERGY STORAGE↗

Catalytic Effects of Silver in Iodine Reactors for Dissolved Used Nuclear Fuel

The dissolution of used nuclear fuel generates a variety of off-gasses including flammable hydrogen and other species that are a concern for environmental release. The H-Canyon facility at the Savannah River Site is currently dissolving aluminum-clad research reactor fuel from material test reactors and the High Flux Isotope Reactor (HFIR) using a mercury-catalyzed nitric acid flowsheet. Savannah River National Laboratory recently developed and deployed a Raman spectrometer to monitor the off-gas stream from the dissolution process. Results from these measurements indicated a lack of the expected hydrogen, nitrous oxide, and nitric oxide in the off-gas stream. It was proposed that the silver on the silver nitrate–coated berl saddles present in the reactors for iodine capture were acting as a catalytic hydrogen recombiner. Nitric oxide is readily oxidized to nitrogen dioxide under normal conditions, but it was unclear what happened to the nitrous oxide. A laboratory-scale iodine reactor was assembled and filled with silver nitrate–coated berl saddles to help ascertain the fate of nitrous oxide and hydrogen. Testing with this laboratory-scale reactor observed the recombination of hydrogen when a simulated dissolver off-gas was passed through the reactor containing silver nitrate–coated berl saddles at the approximate temperatures seen in H-Canyon. However, the nitrous oxide concentration was unchanged, suggesting a more complex process occurring within the off-gas stream before it reaches the iodine reactors at H-Canyon.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Niche Partitioning of Microbial Communities at an Ancient Vitrified Hillfort: Implications for Vitrified Radioactive Waste Disposal

A pre-Viking era vitrified hillfort, Broborg, provides a habitat analogue for disposed radioactive waste glass and shows strong niche partitioning among the organisms involved in glass alteration. Microbes cannot be eliminated from radioactive waste disposal facilities and the consequences of bio-colonization must be understood. We use Broborg as a model system to inform what microbial processes might influence long-term radioactive waste glass durability by examining anthropogenic glass that has been subjected to bio-colonization for over 1,500 years. Scanning electron microscopy (SEM) images reveal the surficial biofilm structure, and chemical/mineralogy analysis in combination with deoxyribonucleic acid (DNA) sequencing of samples from the vitrified substrate, the adjacent soil, and the general topsoil provide insight into niche partitioning. The ancient glass niche supports a unique microbial community of bacteria, fungi, and protists that manifests the species response to local geochemical and mineralogical conditions. Communities from the geochemical niche associated with the glass are distinct and less diverse than soil communities. The microbiome of the glass and adjacent soil are dominated by lichens, lichen-associated microorganisms, and other epilithic, endolithic, and epigeic organisms. Pseudomonads dominate the prokaryotic communities on the vitrified material, but not the adjacent soil. In contrast, the general topsoil communities are enriched in plant rhizosphere organisms. Taxa associated with vitrification have bio-corrosive properties that could be detrimental to glass durability, including silicate mineral dissolution, extraction of essential elements, secretion of geochemically reactive organic acids, and dissolution induced by improved water retention. However, these stable long-term biofilms also possess a homeostatic function that could limit glass alteration. Overall, this study demonstrates the potential impacts that microbial colonization and niche partitioning can have on glass alteration and subsequent release of radionuclides from a disposal facility for vitrified radioactive waste.

59 BASIC BIOLOGICAL SCIENCES↗

Impact of lithiated cobalt oxide and phosphate nanoparticles on rainbow trout gill epithelial cells

Metal oxide and phosphate nanoparticles (NPs) are ubiquitous in emerging applications, ranging from energy storage to catalysis. Cobalt-containing NPs are particularly important, where their widespread use raises questions about the relationship between composition, structure, and potential for environmental impacts. To address this gap, we investigated the effects of lithiated metal oxide and phosphate NPs on rainbow trout gill epithelial cells, a model for environmental exposure. Lithium cobalt oxide (LCO) NPs significantly reduced cell viability at 10 µg/mL, while a 10-fold higher concentration of lithiated cobalt hydroxyphosphate (LCP) NPs was required to significantly reduce viability. Exposure to Li+ and Co2+ alone, at concentrations relevant to ion released from the NPs, did not reduce cell viability and minimally impacted reactive oxygen species (ROS) levels. Both LCO- and LCP-NPs were found within membrane-bound organelles. However, only LCP-NPs underwent rapid and complete dissolution in artificial lysosomal fluid. Unlike LCP-NPs, LCO-NPs significantly increased intracellular ROS, could be found within abnormal multilamellar bodies, and induced formation of intracellular vacuoles. Increased p53 gene expression, measured in individual cells, was observed at sub-toxic concentrations of both LCO- and LCP-NPs, implicating both in inductions of cellular damage and stress at concentrations approaching predicted environmental levels. Our results implicate the intact NP, not the dissolved ions, in the observed adverse effects and show that LCO-NPs significantly impact cell viability accompanied by increase in intracellular ROS and formation of organelles indicative of cell stress, while LCP-NPs have minimal adverse effects, possibly due to their rapid dissolution in acidic organelles.

Melby, Eric S.↗

Biokinetics of 238 Pu oxides: Inferences from bioassay data

The bioassay data collected from several workers involved in 238 Pu inhalation incidents have been analyzed using the most recent biokinetic models described in Occupational Intakes of Radionuclides (OIR) series of publications. Although all exposures were thought to be to 238 Pu oxides, the observed urinary excretion patterns differed in different inhalation incidents. The urinary excretion from individuals involved in one of the incidents increased steadily with time peaking around 2-3 years before decreasing. This pattern is described in Part 4 of the OIR series using the ‘ 238 PuO 2 , ceramic’ model. This non-monotonic behavior, explained as being due to fragmentation and dissolution, was not specific to the incident, but was also observed in other incidents. The urinary excretion data collected from individuals involved in another incident showed dissolution behavior between Type M and Type S. Finally, the bioassay data from yet another incident showed a pattern that appears to represent behavior more insoluble than Type S, which is possibly a result of self-heating due to the decay heat from 238 Pu. The urinary excretion patterns and the corresponding dose coefficients have been calculated and compared.

238Pu↗

Morphology selection in dealloying: A phase field study of the coupling among kinetic mechanisms

A phase field model is used to investigate how the corrosion rate and morphology of a dealloying metal is controlled by the kinetic rates of bulk solid diffusion, interfacial diffusivity, and interface dissolution. A specific focus is investigating the manner by which variations in these kinetic parameters synergistically influence the onset of a morphological instability at the solid-liquid interface, which is known to precede rapid dealloying corrosion towards highly topologically complex structures such as bicontinuous porous solids. This work demonstrates that this instability can be suppressed by either an increase of interdiffusion in the solid alloy, or by a decreasing rate of dissolution at the solid-liquid interface. When the instability is suppressed, the result is a relatively planar, passivated dealloying front. Importantly, however, coupled changes in kinetic parameters can also promote the morphological instability and sustain fine-scale ligament and pore formation. Finally, the relevance of the solid-liquid interfacial diffusion for determining the rate of dealloying and ligament formation is highlighted. By elucidating the mechanistic influence of bulk and interfacial kinetic factors on the dealloyed morphology, this work helps to rationalize the contrasting morphologies observed in various dealloying systems.

Diffusion↗

Assessing an aqueous flow cell designed for in situ crystal growth under X-ray nanotomography and effects of radiolysis products

Nucleation and growth of minerals has broad implications in the geological, environmental and materials sciences. Recent developments in fast X-ray nanotomography have enabled imaging of crystal growth in solutions in situ with a resolution of tens of nanometres, far surpassing optical microscopy. Here, a low-cost, custom-designed aqueous flow cell dedicated to the study of heterogeneous nucleation and growth of minerals in aqueous environments is shown. To gauge the effects of radiation damage from the imaging process on growth reactions, radiation-induced morphological changes of barite crystals (hundreds of nanometres to ∼1 µm) that were pre-deposited on the wall of the flow cell were investigated. Under flowing solution, minor to major crystal dissolution was observed when the tomography scan frequency was increased from every 30 min to every 5 min (with a 1 min scan duration). The production of reactive radicals from X-ray induced water radiolysis and decrease of pH close to the surface of barite are likely responsible for the observed dissolution. The flow cell shown here can possibly be adopted to study a wide range of other chemical reactions in solutions beyond crystal nucleation and growth where the combination of fast flow and fast scan can be used to mitigate the radiation effects.

36 MATERIALS SCIENCE↗

Conversion kinetics of container glass batch melting

Abstract Understanding the batch‐to‐glass conversion process is fundamental to optimizing the performance of glass‐melting furnaces and ensuring that furnace modeling can correctly predict the observed outcome when batch materials or furnace conditions change. To investigate the kinetics of silica dissolution, gas evolution, and primary foam formation and collapse, we performed X‐ray diffraction, thermal gravimetry, feed expansion tests, and evolved gas analysis of batch samples heated at several constant heating rates. We found that gas evolving reactions, foaming, and silica dissolution depend on the thermal history of the batch in a similar manner: the kinetic parameters of each process were linear functions of the square root of the heating rate. This kinetic similarity reflects the stronger‐than‐expected interdependence of these processes. On the basis of our results, we suggest that changes in furnace operating conditions, such as firing or boosting, influence the melting rate less than what one would expect without consideration of batch conversion kinetics.

Ueda, Nanako↗

Peculiarities of CsPbBr3 perovskites melting in quasi-equilibrium conditions

The melting behavior of CsPbBr3 perovskite was studied by differential thermal analysis (DTA). It was found that melting of CsPbBr3 occurs non-isothermally in the temperature range of 561-570 °C. From the temperature dependence of the solid-phase melting rate, it was established that at 567±1 °C the change in the mechanism of the solid-phase melting goes from fragmentation to dissolution at the surface. The obtained values of the activation energy of the melting of the solid phase in CsPbBr3 show that the activation energy of the dissolution of the solid-phase fragments is 4 times greater than the energy of the fragmentation of the solid phase.

Kopach, O.↗

Chemical recycling of mixed textile waste

Globally, less than 0.5% of postconsumer textile waste is recycled, with the majority incinerated or ending up in landfills. Most postconsumer textiles are mixed fibers, complicating mechanical recycling due to material blends and contaminants. Here, we demonstrate the chemical conversion of postconsumer mixed textile waste using microwave-assisted glycolysis over a ZnO catalyst followed by solvent dissolution. This approach electrifies the process heat while allowing rapid depolymerization of polyester and spandex to their monomers in 15 minutes. A simple solvent dissolution enables the separation of cotton and nylon. We assess the quality of all components through extensive material characterization, discuss their potential for sustainable recycling, and provide a techno-economic analysis of the economic feasibility of the process.

Science & Technology - Other Topics↗

Pigment removal from reverse-printed laminated flexible films by solvent-targeted recovery and precipitation

The solvent-targeted recovery and precipitation (STRAP) process separates and recovers the constituent resins in multilayer plastic packaging films by selective polymer dissolution. In this work, the cause of coloring in the STRAP-recycled polyethylene (PE) resins from postindustrial printed films was identified as decomposed diarylide pigments. Two different approaches are needed to completely remove the dissolved colorants during the STRAP process including (i) adding an activated carbon (AC) adsorbent to the solvent after polymer dissolution and (ii) proper mechanical filtration of the polymer-solvent cake to remove as much solvent from the cake as possible. Colorless recycled PE can be produced by a combination of the proposed approaches (choosing the proper solvent, adding an AC adsorbent, and doing proper mechanical filtration) with minimal accumulation of colorants in the recycled STRAP solvents. This study demonstrated that high-quality STRAP low-density PE can be obtained from printed plastic films, enhancing the potential circularity of these packaging materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Methods of chemical and phase composition analysis of gallstones

This review presents the instrumental methods used for chemical and phase composition investigation of gallstones. A great body of data has been collected in the literature on the presence of elements and their concentrations, obtained by fluorescence microscopy, X-ray fluorescence spectroscopy, neutron activation analysis, proton (particle) induced X-ray emission, atomic absorption spectroscopy, high-resolution gamma-ray spectrometry, electron paramagnetic resonance. Structural methods—powder X-ray diffraction, infrared spectroscopy, Raman spectroscopy—provide information about organic and inorganic phases in gallstones. Stone morphology was studied at the macrolevel with optical microscopy. Results obtained by analytical scanning and transmission electron microscopy with X-ray energy dispersive spectrometry are discussed. The chemical composition and structure of gallstones determine the strategy of removing stone from the body and treatment of patients: surgery or dissolution in the body. Therefore one chapter of the review describes the potential of dissolution methods. Early diagnosis and appropriate treatment of the disease depend on the development of clinical methods for in vivo investigation, which gave grounds to present the main characteristics and potential of ultrasonography (ultrasound scanning), magnetic resonance imaging, and X-ray computed tomography.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Editors’ Choice—Necessity to Avoid Titanium Oxide as Electrocatalyst Support in PEM Fuel Cells: A Membrane Durability Study

Pt/TiO 2 as electrocatalyst was found to significantly increase the rate of the membrane chemical degradation in a polymer electrolyte membrane (PEM) fuel cell. The increased degradation was proved to be due to TiO x (TiO 2 or Ti 4 O 7 ), which is widely recognized as a promising corrosion-resistant electrocatalyst support. The membrane degradation (thinning) appears to be preferentially in the side facing anode electrode. Migrated Ti species as a result of TiO x dissolution during fuel cell operation in an acidic environment was quantified by electron probe microanalysis (EPMA). Total fluorine inventory loss of the membrane strongly depends on the quantity of migrated Ti species (likely Ti 3+ and/or Ti 4+ ). The membrane chemical degradation induced by TiO x is proposed to be due to dissolved ionic Ti species reacting with H 2 O 2 through a Fenton reaction. TiO x is determined to be inviable as electrocatalyst support for PEM fuel cells, and future research is suggested to be directed toward alternative oxides with similar corrosion-resistance.

08 HYDROGEN↗

Understanding the Degradation of La 1−x Sr x FeO 3−δ (0 ≤ x ≤ 1) Perovskite Oxides during the Oxygen Evolution Reaction in Alkaline Solution

Perovskite oxides are an emerging class of highly active catalysts for the oxygen evolution reaction (OER); however, their electrochemical stability remains poorly understood. Here, we report a systematic evaluation of the OER activity and stability of La 1−x Sr x FeO 3-δ perovskites in 1 M KOH. Their initial OER activity first increases with increasing Sr content (fromx= 0 to 0.8), and then decreases when the Sr content is increased to 1. Their stability evaluated by monitoring the element leaching from the electrodes show that La does not leach at a detectable rate, but Sr and Fe leach substantially. The leaching of Sr occurs at similar rates under open circuit potential (OCP) and OER potential, suggesting a nonelectrochemical dissolution process. The leaching of Fe is, however, strongly dependent on the electrode potential. More Fe leaching is observed under the OER potential than OCP. Additionally, the electrode with higher initial OER activity leaches more Fe. These results indicate that OER facilitates the dissolution of Fe from the electrode. The leaching of Fe, in turn, is considered responsible for the activity loss of La 1-x Sr x FeO 3−δ during OER. This study brings new insight into the degradation mechanism of La 1-x Sr x FeO 3−δ and their related perovskite oxides during electro-oxidation processes.

Electrochemistry↗