At least 1,063 records · Page 59

Interface characteristics of Ti6Al4V-TiAl metal-intermetallic laminate (MIL) composites prepared by a novel hot-pack rolling

Highlights: • The Ti6Al4V/high Nb-TiAl metal-intermetallic (MIL) composite was fabricated. • The formation of γ and α{sub 2} phase at interface is diffusion controlled. • The formation of O phase at interface is due to the segregation of Nb atoms. • The Vickers hardness from Ti6Al4V to TiAl alloy shows a trend of a decrease then an increase and finally a decrease. - Abstract: Ti6Al4V (wt%)/Ti-44Al-8Nb-0.2W-0.2B-0.03Y (at.%) (high Nb-TiAl) metal–intermetallic laminate (MIL) composite with a defect-free interface was successfully prepared by hot-pack rolling and the interface microstructure was characterized by XRD, SEM, EBSD, and TEM techniques. The results showed that the interface was about 260 μm thick and consisted of four different microstructure regions. The thickness of each region was about 60–80 μm and the microstructure of the four regions consisted of acicular O, α{sub 2}, and β/B2 phases; acicular α{sub 2} phase; acicular α{sub 2} and β/B2 phases; and acicular γ, α{sub 2}, and β/B2 phases respectively. The resulting microstructure of the interface region was attributed to the interdiffusion of Ti atoms from the starting Ti6Al4V alloy layer to the high Nb-TiAl alloy layer and Al and Nb atoms from the high Nb-TiAl alloy layer to the Ti6Al4V alloy layer. The formation of acicular α{sub 2} and γ phases was diffusion-controlled and the Nb segregation at the interface caused the formation of O phase which had specific relationships with α{sub 2} and β/B2 phases. The detailed interface microstructural evolution of the Ti6Al4V/high Nb-TiAl MIL composite and the Vickers hardness of the composite are also discussed in this paper.

36 MATERIALS SCIENCE↗

Microstructure and texture evolution of deformed Mg-Zn alloy during recrystallization

Highlights: • The texture intensity in the Mg-Zn alloy relied on the microstructure. • Fine DRXed grains showed a fiber texture distributing between <10.0> and <11.0>. • Coarse DRXed grains mainly exhibited <11.0> fiber texture. • The preferred growth of <11.0> oriented grains resulted in texture evolution. - Abstract: The microstructure and texture evolution of Mg-Zn alloy during recrystallization was investigated by EBSD in the present study. Deformed region, fine DRXed region and coarse DRXed region were obtained in Mg-Zn alloy during deformation. It was found that the texture intensity in DRXed region was weaker compared with the deformed region. The second phase at grain boundaries resulted in the formation of fine DRXed grains with weaker texture compared with the coarse DRXed region. Additionally, a remarkable grain-size driven textural transition from <10.0>–<11.0> texture to <11.0> texture were detected with the growth of DRXed grains. The recrystallized grains with small grain size showed a fiber texture distributing homogeneously between <10.0> and <11.0>, while <11.0> fiber texture was predominant for the large recrystallized grains. It is suggested that <11.0> oriented grains grew faster than other oriented grains, which was ascribed to larger misorientation between <11.0> oriented grains and their neighboring grains.

36 MATERIALS SCIENCE↗

Structure, Morphology, and Optical Properties of Amorphous and Nanocrystalline Gallium Oxide Thin Films

Ga2O3 thin films were produced by sputter deposition by varying the substrate temperature (Ts) in a wide range (Ts=25-800 oC). The structural characteristics and optical properties of Ga2O3 films were evaluated using X-ray diffraction (XRD), scanning electron microscopy (SEM), energy-dispersive X-ray spectrometry (EDS), Rutherford backscattering spectrometry (RBS) and spectrophotometric measurements. The effect of growth temperature is significant on the chemistry, crystal structure and morphology of Ga2O3 films. XRD and SEM analyses indicate that the Ga2O3 films grown at lower temperatures were amorphous while those grown at Ts≥500 oC were nanocrystalline. RBS measurements indicate the well-maintained stoichiometry of Ga2O3 films at Ts=300-700 oC. The spectral transmission of the films increased with increasing temperature. The band gap of the films varied from 4.96 eV to 5.17 eV for a variation in Ts in the range 25-800 oC. A relationship between microstructure and optical property is discussed.

Environmental Molecular Sciences Laboratory↗

Plastic strain arrangement in copper single crystals in sliding

Deformation of tribologically loaded contact zone is one of the wear mechanisms in spite of the fact that no mass loss may occur during this process. Generation of optimal crystallographic orientations of the grains in a polycrystalline materials (texturing) may cause hardening and reducing the deformation wear. To reveal the orientation dependence of an individual gain and simplify the task we use copper single crystals with the orientations of the compression axis along [111] and [110]. The plastic deformation was investigated by means of optical, scanning electron microscopy and EBSD techniques. It was established that at least four different zones were generated in the course of sliding test, such as non-deformed base metal, plastic deformation layer sliding, crystalline lattice reorientation layer and subsurface grain structure layer. The maximum plastic strain penetration depth was observed on [110]-single crystals. The minimum stability of [111]-crystals with respect to rotation deformation mode as well as activation of shear in the sliding contact plane provide for rotation deformation localization below the worn surface. The high-rate accumulation of misorientations and less strain penetration depth was observed on [111]-crystals as compared to those of [110]-oriented ones.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of the Laser Irradiation on Graphene Oxide Foils in Vacuum and Air

A Nd:YAG laser operating at 1064 nm was used to irradiate, at different intensities, graphene oxide foils placed in vacuum and in air. The laser irradiated GO foils were analysed successively by using different techniques such as 2.0 MeV alpha particle Rutherford backscattering spectrometry, X-ray photoemission spectroscopy and SEM-EDX. In particular, in vacuum irradiated graphene oxide samples the oxygen reduction has been observed with increment of the carbon content. In air irradiated GO samples an increase in oxygen has instead been highlighted. Furthermore thermal and chemical effects are induced by the photon irradiation. Results will be presented and discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Gallium Oxide Nanostructures for High Temperature Sensors

Gallium oxide (Ga 2 O 3 ) thin films were produced by sputter deposition by varying the substrate temperature (T s ) in a wide range (T s =25-800 °C). The structural characteristics and electronic properties of Ga 2 O 3 films were evaluated using X-ray diffraction (XRD), scanning electron microscopy (SEM), energy-dispersive X-ray spectrometry (EDS), Rutherford backscattering spectrometry (RBS) and spectrophotometric measurements. The effect of growth temperature is significant on the chemistry, crystal structure and morphology of Ga 2 O 3 films. XRD and SEM analyses indicate that the Ga 2 O 3 films grown at lower temperatures were amorphous while those grown at T s ≥500 oC were nanocrystalline. RBS measurements indicate the well-maintained stoichiometry of Ga 2 O 3 films at T s =300-800 °C. The electronic structure determination indicated that the nanocrystalline Ga 2 O 3 films exhibit a band gap of ~5 eV. Tungsten (W) incorporated Ga 2 O 3 films were produced by co-sputter deposition. W-concentration was varied by the applied sputtering-power. No secondary phase formation was observed in W-incorporated Ga 2 O 3 films. W-induced effects were significant on the structure and electronic properties of Ga2O3 films. The band gap of Ga 2 O 3 films without W-incorporation was ~5 eV. Oxygen sensor characteristics evaluated using optical and electrical methods indicate a faster response in W-doped Ga 2 O 3 films compared to intrinsic Ga 2 O 3 films. The results demonstrate the applicability of both intrinsic and W-doped Ga-oxide films for oxygen sensor application at temperatures ≥700 °C.

47 OTHER INSTRUMENTATION↗

High quality transmission Kikuchi diffraction analysis of deformed alloys - Case study

Modern scanning electron microscopes (SEM) equipped with thermally assisted field emission guns (Schottky FEG) are capable of imaging with a resolution in the range of several nanometers or better. Simultaneously, the high electron beam current can be used, which enables fast chemical and crystallographic analysis with a higher resolution than is normally offered by SEM with a tungsten cathode. The current resolution that limits the EDS and EBSD analysis is related to materials' physics, particularly to the electron-specimen interaction volume. The application of thin, electron-transparent specimens, instead of bulk samples, improves the resolution and allows for the detailed analysis of very fine microstructural features. Beside the typical imaging mode, it is possible to use a standard EBSD camera in such a configuration that only transmitted and scattered electrons are detected. This modern approach was successfully applied to various materials giving rise to significant resolution improvement, especially for the light element magnesium based alloys. This paper presents an insight into the application of the transmission Kikuchi diffraction (TKD) technique applied to the most troublesome, heavily-deformed materials. In particular, the values of the highest possible acquisition rates for high resolution and high quality mapping were estimated within typical imaging conditions of stainless steel and magnesium-yttrium alloy. - Highlights: •Monte Carlo simulations were used to simulate EBSD camera intensity for various measuring conditions. •Transmission Kikuchi diffraction parameters were evaluated for highly deformed, light and heavy elements based alloys. •High quality maps with 20 nm spatial resolution were acquired for Mg and Fe based alloys. •High speed TKD measurements were performed at acquisition rates comparable to the reflection EBSD.

36 MATERIALS SCIENCE↗

Nucleation and growth of ZnO on PMMA by low-temperature atomic layer deposition

ZnO films were grown by atomic layer deposition at 35 °C on poly(methyl methacrylate) substrates using diethylzinc and water precursors. The film growth, morphology, and crystallinity were studied using Rutherford backscattering spectrometry, time-of-flight elastic recoil detection analysis, atomic force microscopy, scanning electron microscopy, and x-ray diffraction. The uniform film growth was reached after several hundreds of deposition cycles, preceded by the precursor penetration into the porous bulk and island-type growth. After the full surface coverage, the ZnO films were stoichiometric, and consisted of large grains (diameter 30 nm) with a film surface roughness up to 6 nm (RMS). The introduction of Al{sub 2}O{sub 3} seed layer enhanced the initial ZnO growth substantially and changed the surface morphology as well as the crystallinity of the deposited ZnO films. Furthermore, the water contact angles of the ZnO films were measured, and upon ultraviolet illumination, the ZnO films on all the substrates became hydrophilic, independent of the film crystallinity.

36 MATERIALS SCIENCE↗

The influence of power spinning and annealing temperature on microstructures and properties of Cu-Sn alloy

Highlights: • The strengthening effect of power spinning is mainly achieved by strengthening fine grains and dislocations. • Twins formed by the aggregation and overlapping of stacking faults grow and widen • In power spinning of Cu-Sn alloy, plastic deformation is primarily powered by dislocation sliding. - Abstract: Electron back scatter diffraction pattern (EBSD), metallographic microscope (OM) and transmission electron microscope (TEM) are used to analyze the microstructural state of the Cu-Sn alloy before and after power spinning and annealing. The results show that after power spinning, the α phase grains are refined and gradually evolve into small and fine α{sub II} and deformed α{sub III} crystal grains, with an average grain size of about 2.2 μm. Work hardening results in massive network-like subgrain boundaries distributed in power spinning microstructure. Annealing at 400 °C contributes to the formation of dislocation cells and stacking faults, and high-angle grain boundaries (HABS) start to migrate and slide. After the formation of less defective equiaxed grains at 500 °C, twins continue to grow and widen based through continuous accumulation of stacking faults. Further testing of mechanical properties reveals that power spinning is conducive to the improvement of mechanical properties of Cu-Sn alloy.

36 MATERIALS SCIENCE↗

Epitaxial growth of rock salt MgZrN 2 semiconductors on MgO and GaN

Ternary nitride compound semiconductors have attracted recent attention as electronic materials since their properties can be tuned by cation stoichiometry and ordering. A recently discovered example is MgZrN 2 , a ternary analog to the rock salt semiconductor ScN. MgZrN 2 has a larger bandgap and stronger dielectric response than the binary compound. Polycrystalline thin films of MgZrN 2 have been studied, but demonstration of high-quality growth is still required to establish its suitability for technological applications. Here, we report on epitaxial growth of MgZrN 2 thin films on (100) and (111) MgO substrates and (001) GaN templates. The MgZrN 2 composition is confirmed by Rutherford backscattering spectrometry, showing no oxygen in the film except for a thin surface oxide layer. Epitaxial growth results in MgZrN 2 with x-ray diffraction rocking curves with a full-width at half-maximum in the range of 0.3–3.0°, depending on the substrate. Transmission electron microscopy analysis of the MgZrN 2 film grown on a (111) MgO substrate confirms epitaxial growth and shows a sharp film/substrate interface. In-plane temperature-dependent Hall effect measurements show that the material is an n-type semiconductor with a relatively high concentration ( n 300K ≈ 10 19 –10 20 cm -3 ) of thermally activated electrons. Room-temperature transport measurements show a conductivity of 25 S cm -1 and a Seebeck coefficient of -80 μ V K -1 . Overall, these results provide an important step toward integration of rock salt MgZrN 2 with other technological nitrides for device applications.

36 MATERIALS SCIENCE↗

Simulation Kinetics of Austenitic Phase Transformation in Ti+Nb Stabilized IF and Microalloyed Steels

In the present study, the influence of cooling rates (low to ultrafast) on diffusion controlled and displacive transformation of Ti-Nb IF and microalloyed steels has been thoroughly investigated. Mechanisms of nucleation and formation of non-equiaxed ferrite morphologies (i.e., acicular ferrite and bainitic ferrite) have been analyzed in details. The continuous cooling transformation behavior has been studied in a thermomechanical simulator (Gleeble 3800) using the cooling rates of 1-150 °C/s. On the basis of the dilatometric analysis of each cooling rate, continuous cooling transformation (CCT) diagrams have been constructed for both the steels to correlate the microstructural features at each cooling rate in different critical zones. In the case of the IF steel, massive ferrite grains along with granular bainite structures have been developed at cooling rates > 120 °C/s. On the other hand, a mixture of lath bainitic and lath martensite structures has been formed at a cooling rate of ~ 80 °C/s in the microalloyed steel. A strong dependence of the cooling rates and C content on the microstructures and mechanical properties has been established. The steel samples that were fast cooled to a mixture of bainite ferrite and martensite showed a significant improvement of impact toughness and hardness (157 J, for IF steel and 174 J for microalloyed steel) as compared to that of the as-received specimens (133 J for IF steel and 116 J for microalloyed steel). Thus, it can be concluded that the hardness and impact toughness properties are correlated well with the microstructural constituents as indicated by the CCT diagram. Transformation mechanisms and kinetics of austenitic transformation to different phase morphologies at various cooling rates have been discussed in details to correlate microstructural evolution and mechanical properties.

36 MATERIALS SCIENCE↗

Expanding the Zinc Precursor Toolbox: A Comparative Study of Precursors for Thermal ALD of ZnO Thin Films

Atomic layer deposition (ALD) of zinc oxide (ZnO) has been widely researched using diethyl zinc (DEZ)-based methods. The significant importance of thin films of ZnO as transparent conductive oxides (TCO) in optoelectronic devices and photovoltaics warrants examining alternative Zn precursors for ZnO ALD as potential replacements for the pyrophoric DEZ. In this study, we investigated three alternative Zn precursors: Zn(EEKI)2, Zn(DMP)2, ZnEt(HMDS), in the process development for high-quality ZnO thin films and compared them to DEZ. The ALD processes were studied using in situ spectroscopic ellipsometry. The properties of the ALD ZnO films were characterized using ex situ X-ray photoelectron spectroscopy (XPS), Rutherford backscattering spectrometry and nuclear reaction analysis (RBS/NRA), X-ray diffraction (XRD), atomic force microscopy (AFM), transmission electron microscopy (TEM), and ultraviolet-visible (UV/Vis) spectrophotometry. These measurements confirmed the formation of pure, stoichiometric, and polycrystalline ZnO films using all four Zn precursors. Although the selected precursors are chemically diverse Zn compounds, they all yielded saturating ALD processes and high-quality ZnO thin films at 200 °C. This study highlights the potential benefits of alternative zinc precursors in designing ALD processes for ZnO thin films.

Obenlüneschloß, Jorit↗

Dopant activation in ion implanted silicon by microwave annealing

Microwaves are used as a processing alternative for the electrical activation of ion implanted dopants and the repair of ion implant damage within silicon. Rutherford backscattering spectra demonstrate that microwave heating reduces the damage resulting from ion implantation of boron or arsenic into silicon. Cross-section transmission electron microscopy and selective area electron diffraction patterns demonstrate that the silicon lattice regains nearly all of its crystallinity after microwave processing of arsenic implanted silicon. Sheet resistance readings indicate the time required for boron or arsenic electrical activation within implanted silicon. Hall measurements demonstrate the extent of dopant activation after microwave heating of implanted silicon. Physical and electrical characterization determined that the mechanism of recrystallization in arsenic implanted silicon is solid phase epitaxial regrowth. The boron implanted silicon samples did not result in enough lattice damage to amorphize the silicon lattice and resulted in low boron activation during microwave annealing even though recrystallization of the Si lattice damage did take place. Despite low boron activation levels, the level of boron activation in this work was higher than that expected from traditional annealing techniques. The kinetics of microwave heating and its effects on implanted Si are also discussed.

36 MATERIALS SCIENCE↗

Crystal defects and related stress in Y{sub 2}O{sub 3} thin films: Origin, modeling, and consequence on the stability of the C-type structure

We study the impact that the crystal defects have on the C-type structure of rare earth sesquioxide thin films grown by ion-beam sputtering, through the example of Y{sub 2}O{sub 3}. By monitoring the energy of the argon beam used in the sputter deposition process (between 600 and 1200 eV), we show that it is possible to control the microstructure (defects concentration, stress state and phase) in the oxide layer. Two main types of defects, ascribed to the 'atomic peening effect', are evidenced by high-resolution transmission electron microscopy, Rutherford backscattering spectroscopy, and nuclear reaction analysis experiments: anti-Frenkel pairs, leading to a disorder on the oxygen-vacancy network, and oxygen-vacancy dislocations loops, to accommodate the strong nonstoichiometry. From a macroscopic measurement of the residual stresses in the as-deposited and the annealed layers, through x-ray diffraction and the sin{sup 2}{Psi} method, we have modeled the related stress state using an enhanced triaxial stress model. In the as-grown films, we evidence the coexistence of a biaxial and a hydrostatic stress, due to inclusions of atomic size defects. Quantitative information of the concentration and the nature of each type of defect (size effect) have also been determined, in good agreement with experiments. Interestingly, in the most energetic growth conditions corresponding to the highest degree of disorder on the oxygen-vacancy network and to the highest stress field in the film, we demonstrate that it is possible to stabilize an unexpected and metastable non equilibrium fluorite-like phase (X-type).

36 MATERIALS SCIENCE↗

Variation of lattice constant and cluster formation in GaAsBi

We investigate the structural properties of GaAsBi layers grown by molecular beam epitaxy on GaAs at substrate temperatures between 220–315 °C. Irrespective of the growth temperature, the structures exhibited similar Bi compositions, and good overall crystal quality as deduced from X-Ray diffraction measurements. After thermal annealing at temperatures as low as 500 °C, the GaAsBi layers grown at the lowest temperatures exhibited a significant reduction of the lattice constant. The lattice variation was significantly larger for Bi-containing samples than for Bi-free low-temperature GaAs samples grown as a reference. Rutherford backscattering spectrometry gave no evidence of Bi diffusing out of the layer during annealing. However, dark-field and Z-contrast transmission electron microscopy analyses revealed the formation of GaAsBi clusters with a Bi content higher than in the surrounding matrix, as well as the presence of metallic As clusters. The apparent reduction of the lattice constant can be explained by a two-fold process: the diffusion of the excess As incorporated within As{sub Ga} antisites to As clusters, and the reduction of the Bi content in the GaAs matrix due to diffusion of Bi to GaAsBi clusters. Diffusion of both As and Bi are believed to be assisted by the native point defects, which are present in the low-temperature as-grown material.

36 MATERIALS SCIENCE↗

Growth of ordered silver nanoparticles in silica film mesostructured with a triblock copolymer PEO-PPO-PEO

Elaboration of mesostructured silica films with a triblock copolymer polyethylene oxide-polypropylene oxide-polyethylene oxide, (PEO-PPO-PEO) and controlled growth of silver nanoparticles in the mesostructure are described. The films are characterized using UV-visible optical absorption spectroscopy, TEM, AFM, SEM, X-ray diffraction (XRD) and Rutherford backscattering spectrometry (RBS). Organized arrays of spherical silver nanoparticles with diameter between 5 and 8 nm have been obtained by NaBH{sub 4} reduction. The size and the repartition of silver nanoparticles are controlled by the film mesostructure. The localization of silver nanoparticles exclusively in the upper-side part of the silica-block copolymer film is evidenced by RBS experiment. On the other hand, by using a thermal method, 40 nm long silver sticks can be obtained, by diffusion and coalescence of spherical particles in the silica-block copolymer layer. In this case, migration of silver particles toward the glass substrate-film interface is shown by the RBS experiment. - Graphical abstract: Growth of silver nanoparticles in a mesostructured block copolymer F127-silica film is performed either by a chemical route involving NaBH{sub 4} reduction or by a thermal method. An array of spherical silver nanoparticles with 10 nm diameter on the upper-side of the mesostructured film or silver sticks long of 40 nm with a preferential orientation are obtained according to the method used. a: TEM image of the Fag5SiNB sample illustrating the silver nanoparticles array obtained by the chemical process; b: HR-TEM image of the Fag20Sid2 sample illustrating the silver nanosticks obtained by the thermal process.

36 MATERIALS SCIENCE↗

Evaluation of the interface of thin GaN layers on c- and m-plane ZnO substrates by Rutherford backscattering

Lattice distortion at the interfaces between thin GaN layers with {approx}400 nm in thickness and ZnO substrates with non-polar m-plane (10-10) and polar c-plane (0001) is studied using Rutherford backscattering/ion channeling techniques. The interface between GaN/m-plane ZnO is aligned clearly to m-axis, indicating no lattice distortion, while between GaN/c-plane ZnO causes the lattice distortion in the GaN layer due to the piezoelectric field. The range of distortion exceeds {approx}90 nm from the interface of GaN/c-plane ZnO. These results are confirmed by x-ray diffraction and reflection high energy electron diffraction studies.

36 MATERIALS SCIENCE↗

Electron back scattered diffraction characterization of Sm(CoFeCuZr){sub z} magnets

In permanent magnets based on the Sm{sub 2}Co{sub 17} phase, the high coercivity depends on the presence of a complex microstructure, consisting of a Sm{sub 2}(Co,Fe){sub 17} cell phase, a cell boundary phase Sm(Co,Cu){sub 5}, and a Zr-rich platelet or lamellae phase. The aim of this work is to use electron back scatter diffraction (EBSD) in order to identify the different phases present in the isotropic magnets produced from cast alloys with the composition of Sm(Co{sub bal}Fe{sub 0.2}Cu{sub 0.1}Zr{sub x}){sub 8}, where x = 0, 0.02, or 0.06, and correlate them with the different phases observed in scanning electron microscopy (SEM) images. Due to the combination of careful surface preparation and high resolution microscopy, it was possible to observe the cellular structure characteristic of the 2:17 magnets in the SEM images. Until now, only transmission electron microscopy (TEM) had been used. Composition maps, energy dispersive spectroscopy (EDS), and EBSD measurements were used for doing the phase identification.

36 MATERIALS SCIENCE↗