Role of phonon scattering by elastic strain field in thermoelectric Sr{sub 1−x}Y{sub x}TiO{sub 3−δ}
Perovskite-type SrTiO{sub 3−δ} ceramics are multifunctional materials with significant potential as n-type thermoelectric (TE) materials. The electronic and thermal transport properties of spark plasma sintered polycrystalline Sr{sub 1−x}Y{sub x}TiO{sub 3−δ} (x = 0.05, 0.075, 0.1) ceramics are systematically investigated from (15–800) K. The Sr{sub 0.9}Y{sub 0.1}TiO{sub 3−δ} simultaneously exhibits a large Seebeck coefficient, α > −80 μV/K and moderately high electrical resistivity, ρ ∼ 0.8 mΩ-cm at a carrier concentration of ∼10{sup 21} cm{sup −3} at 300 K resulting in a high TE power factor defined herein as (α{sup 2}σT) ∼ 0.84 W/m-K at 760 K. Despite the similar atomic masses of Sr (87.6 g/mol) and Y (88.9 g/mol), the lattice thermal conductivity (κ{sub L}) of Sr{sub 1−x}Y{sub x}TiO{sub 3−δ} is significantly reduced with increased Y-doping, owing to the smaller ionic radii of Y{sup 3+} (∼1.23 Å, coordination number 12) compared to Sr{sup 2+} (∼1.44 Å, coordination number 12) ions. In order to understand the thermal conductivity reduction mechanism, the κ{sub L} in the Sr{sub 1−x}Y{sub x}TiO{sub 3−δ} series are phenomenologically modeled with a modified Callaway's equation from 30–600 K. Phonon scattering by elastic strain field due to ionic radii mismatch is found to be the prominent scattering mechanism in reducing κ{sub L} of these materials. In addition, the effect of Y-doping on the elastic moduli of Sr{sub 1−x}Y{sub x}TiO{sub 3−δ} (x = 0, 0.1) is investigated using resonant ultrasound spectroscopy, which exhibits an anomaly in x = 0.1 in the temperature range 300–600 K. As a result, the phonon mean free path is found to be further reduced in the Sr{sub 0.9}Y{sub 0.1}TiO{sub 3−δ} compared to that of SrTiO{sub 3−δ}, resulting in a considerably low thermal conductivity κ ∼ 2.7 W/m-K at 760 K. Finally, we report a thermoelectric figure of merit (ZT) ∼ 0.3 at 760 K in the Sr{sub 0.9}Y{sub 0.1}TiO{sub 3−δ}, the highest ZT value reported in the Y-doped SrTiO{sub 3} ceramics thus far.