Development of aluminum alloy compounds for electroluminescent light sources
Aluminum alloy compounds as wide band gap semiconductors for electroluminescent light sources
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Aluminum alloy compounds as wide band gap semiconductors for electroluminescent light sources
Dip-brazing process joins aluminum castings to aluminum sheet made from different aluminum alloy. Process includes careful cleaning, surface preparation, and temperature control. It causes minimum distortion of parts.
The fracture behavior for structural aluminum alloys (2024, 6061, 7075, and 7178) was examined in selected heat treatments. The investigation included tensile, shear, and precracked notch-bend specimens fractured at ambient temperature under monotonic loading. Specimens were obtained from thin sheets and thick plates and were tested in longitudinal and transverse orientations at different strain rates. Microstructures of alloys were examined using the optical microscope and the scanning electron microscope with associated energy dispersive X ray chemical analysis. Several different types of second phase particles, some not reported by other investigators, were identified in the alloys. Fracture morphology was related to microstructural variables, test variables, and type of commercial product. Specimen orientation examined in the present investigation had little effect on fracture morphology. Test strain rate changes resulted in some change in shear fracture morphology, but not in fracture morphology of tensile specimens.
The available sources of data on the mechanical properties of aluminum alloys at low temperatures are listed and a summary of the material to be found in each source is given. There is included a discussion of the results of recent tests of aluminum alloys at low temperatures made at the Aluminum Research Laboratories.
Shear assisted processing and extrusion has been used to fabricate multi-metallic tubing that incorporates regions with clad and butt-joined structures. In this work, aluminum alloys 6061, 7075, and 1100 are combined to create a monolithic extruded tubing with weldable ends (6061), a high strength center (7075), and a corrosion-resistant cladding (1100). Optical microscopy shows a gradual, defect-free, transition between alloys at the butt-joint interfaces and a sharp transition between alloys at the clad interface. Tensile testing proved the mechanical coherency of the joint, with failure occurring outside the tri-metallic structure. In conclusion, smoothed particle hydrodynamic simulations identified a spiral pattern of the cladding alloy that leads to inconsistent cladding thickness, and identified a simplified 2-alloy combination of aluminum alloys 6082 and 2014 that accomplished the design objectives of the tri-metallic structure.
Explore the source record for details and available documents.
The present disclosure concerns embodiments of aluminum alloy compositions exhibiting microstructural stability and strength at high temperatures. The disclosed aluminum alloy compositions comprise particular combinations of components that contribute the ability of the compositions to exhibit improved microstructural stability and hot tearing resistance as compared to conventional alloys. Also disclosed herein are embodiments of methods of making and using the alloys.
The present disclosure concerns embodiments of aluminum alloy compositions exhibiting superior microstructural stability and strength at high temperatures. The disclosed aluminum alloy compositions comprise particular combinations of components that contribute the ability of the alloys to exhibit improved microstructural stability and hot tearing resistance as compared to conventional alloys. Also disclosed herein are embodiments of methods of making and using the alloys.
High strength aluminum casting alloy for cryogenic applications in aerospace engineering
The United States government currently manages nearly 13 metric tons of aluminum-clad spent nuclear fuel (SNF) without a long-term storage solution, so a fundamental understanding of corrosion processes occurring on aluminum alloy surfaces is of utmost importance to plan for extended (>50 years) interim dry storage of aluminum-clad SNF. While thermal and chemical corrosion processes are well characterized for aluminum, radiation effects are not. To help understand the impacts of radiation on aluminum-clad SNF, here the radiation-induced molecular hydrogen gas (H 2 ) generation from pristine and pre-corroded aluminum alloy 1100 (Al-1100) coupons have been studied. Corrosion of coupons was achieved by submerging coupons in water at 95 °C for 29 days, yielding a ~5 μm boehmite/bayerite oxide film. Pre-corroded coupons were exposed to cobalt-60 gamma radiation to absorbed doses of up to 1.0 MGy under a variety of conditions: cover-gas composition (argon, nitrogen, or air), relative humidity (0, 50, and 100%), and temperature (ambient, 100, and 200 °C). Post-irradiation measurements demonstrated that the yield of H 2 was directly attributable to the presence of the Al-1100 coupons and their physisorbed water with dependence on absorbed gamma dose, relative humidity, and cover-gas composition. No H 2 was quantified in the presence of air, while both nitrogen and argon environments afforded higher H 2 yields with increasing relative humidities. This was attributed to the greater availability of adsorbed water for radiolytic processes. Irradiation of pre-corroded Al-1100 coupons at different temperatures under 0% relative humidity argon conditions yielded statistically equivalent H 2 yields for ambient temperatures and 100 °C. However, irradiation at 200 °C promoted a 3 to 4-fold increase in the yield of H 2 , possibly due to the transformation of bayerite to boehmite and/or improved efficiency of H • and H 2 release from oxide surfaces.
Handbook has been published which integrates results of 19 research programs involving welding of high-strength aluminum alloys. Book introduces metallurgy and properties of aluminum alloys by discussing commercial alloys and heat treatments. Several current welding processes are reviewed such as gas tungsten-arc welding and gas metal-arc welding.
A series of fracture tests on large-scale, pre-cracked, aluminum alloy panels is being carried out to examine and to characterize the process by which cracks propagate and link up in this material. Extended grips and test fixtures were specially designed to enable the panel specimens to be loaded in tension, in a 1780-kN-capacity universal testing machine. Twelve panel specimens, each consisting of a single sheet of bare 2024-T3 aluminum alloy, 3988 mm high, 2286 mm wide, and 1.016 mm thick are being fabricated with simulated through-cracks oriented horizontally at mid-height. Using existing information, a test matrix has been set up that explores regions of failure that are controlled by fracture mechanics, with additional tests near the boundary between plastic collapse and fracture. In addition, a variety of multiple site damage (MSD) configurations have been included to distinguish between various proposed linkage mechanisms. All tests but one use anti-buckling guides. At this writing seven specimens have been tested. Three were fabricated with a single central crack, three others had multiple cracks on each side of the central crack, and one had a single crack but no anti-buckling guides. Each fracture event was recorded on film, video, computer, magnetic tape, and occasionally optical microscopy. The visual showed the crack tip with a load meter in the field of view, using motion picture film for one tip and SVHS video tape for the other. The computer recorded the output of the testing machine load cell, the stroke, and twelve strain gages at 1.5 second intervals. A wideband FM magnetic tape recorder was used to record data from the same sources. The data were analyzed by two different procedures: (1) the plastic zone model based on the residual strength diagram; and (2) the R-curve. The first three tests were used to determine the basic material properties, and these results were then used in the analysis of the two subsequent tests with MSD cracks. There is good agreement between measured values and results obtained from the model.
Results are presented of a series of fatigue tests to study crack propagation and the resulting stress distributions in tension panels. The panels were all of the same general design, and configurations varied mainly in the relative amount of cross-sectional area in the skin, stiffeners, and flanges. The panels were constructed of 2024-T3 and 7075-T6 aluminum alloys. It was found that the average rate of crack growth was slower in panels made of 2024-T3 aluminum alloy than in panels made of 7075-T6 aluminum alloy. All cracks initiated in the skin, and the slowest crack growth was measured in configurations where the highest percentage of cross-sectional area was in the stiffeners. Strain-gage surveys were made to determine the redistribution of stress as the crack grew across the panels. As a crack approached a given point in the skin, the stress at that point increased rapidly. The stress in the stiffeners also increased as the crack approached the stiffeners. During the propagation of the crack the stress was not distributed uniformly in the remaining area.
In this paper the effect of nanoparticles A12O3 and A13-X compounds (X= Ti, V, Zr) on the improvement of mechanical properties of aluminum alloys for elevated temperature applications is presented. These nanoparticles were selected based on their chemical stability and low diffusions rates in aluminum matrix at high temperatures. The strengthening mechanism for aluminum alloy is based on the mechanical blocking of dislocation movements by these nanoparticles. Samples were prepared from A12O3 nanoparticle preforms, which were produced using ceramic injection molding process and pressure infiltrated by molten aluminum. A12O3 nanoparticles can also be homogeneously mixed with aluminum powder and consolidated into samples through hot pressing and sintering. On the other hand, the Al3-X nanoparticles are produced as precipitates via in situ reactions with molten aluminum alloys using conventional casting techniques. The degree of alloy strengthening using nanoparticles will depend on the materials, particle size, shape, volume fraction, and mean inter-particle spacing.
Bending tests provide a means to study plane strain fracture performance of 6000 series aluminum alloys. Metrics from bending tests have been correlated with self-pierce riveting (SPR) performance of a high strength AA6111 automotive aluminum alloy in previous works. Using the ORNL HPC resources, this project developed an innovative macro→micro←nano (MMN) multiscale microstructure-based finite element (FE) code to further understanding of the relationship between microstructure and fracture properties of high-strength 6000-series alloys. This work started with microstructural characterization in both mesoscale and nanoscale and bending performance characterization of AA6111 HS2-T6 alloy at Ford, the MMN framework was applied to this alloy to simulate 3-point VDA bending. From the results of the macro-modeling of 3-point VDA bending, the critical region of fracture was identified, and the region geometry was used to construct the micro-model. The fracture criterion of micron-scale precipitates and aluminum matrix which contains submicron and nano particles (AL-SMP-NP) in the micro-model was calibrated and validated by comparing simulated and measured bending results. With the AL-SMP-NP fracture strain obtained, the fracture strain of Al-matrix containing nano particles (ALNP) will similarly be determined by a submicron scale-model using an edge-constrained FE modeling approach developed by Hu et al. With the ALNP fracture strain obtained, the fracture strain of Al-matrix containing no particles will similarly be determined by a nano scale-model using an edge-constrained FE modeling approach. After the MMN framework is built and fracture criterion calibrated, nano-model FE simulations with virtual microstructures was performed to obtain a reduced order model (ROM) of the fracture criterion of the ALNP as a function of volume fraction, size, and distribution of the nanoparticle. This nano→submicron→micro modeling part allows exploration of the influence of different material nanostructures from different process conditions on the bending properties within the multiscale bending simulation framework and the ROM of material bendability as a function of nanoparticle size and shape was established. This obtained reduced order model (ROM) could help guide the design and selection of materials to improve existing SPR process models that could replace trial-and-error rivet/die selection and help to design new rivet/die combinations capable of robustly joining new higher strength 6000 5 series alloys in automotive body structures. This would enable lightweighting of Ford vehicles leading to greater fuel efficiency and reduce manufacturing time and energy.
Aluminum alloy, AlSi 10 Mg, prepared by selective laser melt (SLM) fabrication was anodized in 9.8% sulfuric acid (Type II) at 15 V for a total of 23 min. Experiments were performed to study the potentiostatic anodization process and its effects on the oxide coating morphology, thickness, and electrochemical properties of the alloy. Prior to anodization, the alloy microstructure is composed of aluminum cells encapsulated in a silicon network. Anodizing the abraded and polished AlSi 10 Mg surface produced a porous oxide layer with a thickness of 5μm. The oxide coating weight was 698 ± 29 mg/ft 2 . The oxide coating forms in the aluminum cells that are isolated from one another by the silicon eutectic phase. In electrochemical tests, the anodic and cathodic potentiodynamic polarization currents were suppressed by factors of 15× and 215×, respectively, as compared to the unanodized controls. The data indicate the anodic oxide coating suppresses the cathodic more than the anodic reaction rate. Linear polarization resistance (R p ) values increased by 279× after anodization. The corrosion current density values (j corr ) decreased by 133× after anodization. Taken together, the electrochemical data indicate the anodic oxide coating (unsealed) increases the corrosion resistance of the SLM alloy by two orders of magnitude.
Welding and inspection techniques for 2219-T81 aluminum alloy - bibliography and industry survey
Results are presented of tests to determine the column and plate compressive strength of extruded XB75S-T aluminum alloy, and comparative values are shown for 24S-T aluminum-alloy sheet. Stress-strain curves are also given,