Search NASA⌕ Search

SEARCH · Search NASA

Results for “Alumina”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Packed Alumina Absorbs Hypergolic Vapors

Beds of activated alumina effective as filters to remove hypergolic vapors from gas streams. Beds absorb such substances as nitrogen oxides and hydrazines and may also absorb acetylene, ethylene, hydrogen sulfide, benzene, butadiene, butene, styrene, toluene, and xoylene. Bed has no moving parts such as pumps, blowers and mixers. Reliable and energy-conservative. Bed readily adapted to any size from small portable units for use where little vapor release is expected to large stationary units for extensive transfer operations.

Thomas, J. J.↗

Rhombohedral twinning in alumina

Alumina single crystals were deformed in compression along the c axes at temperatures of 625 to 1373 K. Large scale deformation by rhombohedral twinning was observed at a constant resolved shear stress of only 12.6 MPa between about 900 and 1373 K. Below 900 K, the twinning stress for specimens with ground surfaces rose rapidly to 227 MPa at 625 K. A model for twin growth in the absence of dislocation slip is proposed.

Scott, W. D.↗

Structure and grain coarsening during the sintering of alumina

The pore surface area (Sp) and grain-boundary area (Sgb) were measured during the sintering of undoped and doped (100 ppm MgO) alumina compacts. Since the presence of the additive affects only Sgb (raising it at a given value of the density), pinning of the boundaries by solid-solution drag is the only additive function evidenced by the results. The importance of such pinning even at densities as low as 75 percent of theoretical is linked to the existence of microstructural inhomogeneities.

Shaw, N. J.↗

The effect of texture on the crack growth resistance of alumina

The crack growth resistance of a textured, extruded alumina body was compared with that of an isotropic, isopressed body of similar grain size, density, and chemistry. R-curve levels reflected the preferred orientation; however, R-curve slopes (dK sub IR/d Delta a) were the same in all instances, implying a similar crack growth resistive mechanism. Three orthogonal orientations of crack growth in the two structures exhibited similar forms of K sub IR versus Delta-a curves, for which a schematic diagram for polycrystalline ceramics is proposed.

Salem, Jonathan A.↗

Tribological properties of alumina-boria-silicate fabric from 25 to 850 C

Demanding tribological properties are required of the materials used for the sliding seal between the sidewalls and the lower wall of the variable area hypersonic engine. Temperatures range from room temperature and below to operating temperatures of 1000 C in an environment of air, hydrogen, and water vapor. Candidate sealing materials for this application are an alumina-boria-silicate, ceramic, fabric rope sliding against the engine walls which may be made from copper- or nickel-based alloys. Using a pin-on-disk tribometer, the friction and wear properties of some of these potential materials and possible lubrication methods are evaluated. The ceramic fabric rope displayed unacceptably high friction coefficients (0.6 to 1.3) and, thus, requires lubrication. Sputtered thin films of gold, silver, and CaF2 reduced the friction by a factor of two. Sprayed coatings of boride nitride did not effectively lubricate the fabric. Static heat treatment tests at 950 C indicate that the fabric is chemically attacked by large quantities of silver, CaF2, and boron nitride. Sputtered films or powder impregnation of the fabric with gold may provide adequate lubrication up to 1000 C without showing any chemical attack.

Dellacorte, Christopher↗

Synthesis and characterization of high-T(sub c) screen-printed Y-Ba-Cu-O films on alumina

Thick films of YBa2Cu3O(sub 7-x) have been deposited on highly polished alumina substrates by the screen printing technique. To optimize the post-printing heat treatment, the films were baked at various temperatures for different lengths of time and oxygen-annealed at a lower temperature. The resulting films were characterized by electrical resistivity measurements, x-ray diffraction, and optical and scanning electron microscopy. Properties of the films were found to be highly sensitive to the post-printing thermal treatment. Films baked for 15 min at 1000 C in oxygen were hard, adherent, near single phase, and superconducting with T(sub c)(onset) approx 96 K, T(sub c)(zero) approx 66 K and Delta T sub c (10 to 90 percent) approx 10 K.

Bansal, Narottam P.↗

Glass properties in the yttria-alumina-silica system

The glass formation region in the yttria-alumina-silica system was investigated. Properties of glasses containing 25 to 55 wt pct yttria were measured and the effect of the composition was determined. The density, refractive index, thermal-expansion coefficient, and microhardness increased with increasing yttria content. The dissolution rate in 1N HCl increased with increasing yttria content and temperature. These glasses were also found to have high electrical resistivity.

Hyatt, M. J.↗

Containerless laser-induced flourescence study of vaporization and optical properties for sapphire and alumina

Evaporation of aluminum oxide was studied from 1800 to 2327 K by laser-induced flourescence (LIF) detection of Al atom vapor over sapphire and alumina spheres that were levitated in an argon gas jet and heated with a continuous wave CO2 laser. Optical properties were determined from apparent specimen temperatures measured with an optical pyrometer and true temperatures deduced from the LIF intensity versus temperature measurements using the known temperature dependence of the Al atom vapor concentration in equilibrium with Al2O3. The effects of impurities and dissolved oxygen on the high-temperature optical properties of aluminum oxide were discussed.

Nordine, Paul C.↗

Alumina-Enhanced Thermal Barrier

Rigid, fibrous ceramic tile material called "alumina-enhanced thermal barrier" (AETB) extends temperature capability of insulating materials. Material has obvious potential for terrestrial use in kilns, furnaces, heat engines, and other applications in which light weight and high operating temperature are specified. Three kinds of ceramic fibers are blended, molded, and sintered to make refractory tiles.

Smith, Marnell↗

Screen-Printed YBa2Cu3O7-x Films On Alumina

Superconducting films made in relatively simple process. Thick films of YBa2Cu3O7-x superconductor deposited on highly-polished alumina substrates by screen printing. In addition to simplicity, screen-printing technique offers advantage that patterns for electronic and microwave circuits and devices printed directly, without additional etching steps.

Bansal, Narottam P.↗

Ultrasonic imaging of textured alumina

Ultrasonic images representing the bulk attenuation and velocity of a set of alumina samples were obtained by a pulse-echo contact scanning technique. The samples were taken from larger bodies that were chemically similar but were processed by extrusion or isostatic processing. The crack growth resistance and fracture toughness of the larger bodies were found to vary with processing method and test orientation. The results presented here demonstrate that differences in texture that contribute to variations in structural performance can be revealed by analytic ultrasonic techniques.

Stang, David B.↗

Crack growth resistance of textured alumina

The crack growth resistance of a textured, extruded alumina body was compared with that of anisotropic, isopressed body of similar grain size, density, and chemistry. R-curve levels reflected the preferred orientation; however, R-curve slopes were the same in all instances, implying a similar crack growth-resistive mechanism. Three orthogonal orientations of crack growth in the two structures exhibited similar forms of K(IR) versus Delta-a curves, for which a schematic diagram for polycrystalline ceramics is proposed.

Salem, Jonathan A.↗

High alumina (HA) and very high potassium (VHK) basalt clasts from Apollo 14 breccias. I - Mineralogy and Petrology - Evidence of crystallization from evolving magmas

The mineralogy and petrography of very high potassium (VHK) and high alumina (HA) basalts from the Apollo 14 site provide an insight into their magmatic evolution. Generally, their parageneses are similar, with olivine and chromite the early liquidus phases, followed by plagioclase and pyroxene, which crystallized together. Although late-stage ilmenite and FeNi metal occur in both VHK and HA samples, the VHKs also crystallize K-feldspar and Fa-rich olivine. Zoning of constituent minerals is similar for both basalt types, demonstrating that the parental magmas for both HA and VHK basalts became enriched in K, Na, Ca, Fe, and Ti and depleted in Mg and Al as crystallization proceeded. Enrichment of K in the VHK basalts is above that expected from normal fractional crystallization.

Neal, C. R.↗

High alumina (HA) and very high potassium (VHK) basalt clasts from Apollo 14 breccias. II - Whole rock geochemistry - Further evidence for combined assimilation and fractional crystallization within the lunar crust

The understanding of basalt petrogenesis at the Apollo 14 site has increased markedly due to the study of 'new' samples from breccia 'pull-apart' efforts. Whole-rock compositions of 26 new high alumina (HA) and 7 very high potassium (VHK) basalts emphasize the importance of combined assimilation and fractional crystallization in a lunar regime. Previously formulated models for HA and VHK basalt petrogenesis are modified in order to accomodate these new data, although modeling parameters are essentially the same. The required range in HA basalt compositions is generated by the assimilation of KREEP by a 'primitive' parental magma. The VHK basalts can be generated by three parental HA basalts assimilating granite. Results indicate that VHK basalt compositions are dominated by the parental magma, and only up to 8 percent granite assimilation is required. This modeling indicates that at least three VHK basalt flows must be present at the Apollo 14 site.

Neal, C. R.↗

Tribological properties of alumina-boria-silicate fabric from 25 C to 850 C

Demanding tribological properties are required of the materials used for the sliding seal between the sidewalls and the lower wall of the variable area hypersonic engine. Temperatures range from room temperature and below to operating temperatures of 1000 C in an environment of air, hydrogen, and water vapor. Candidate sealing materials for this application are an alumina-boria-silicate, ceramic, fabric rope sliding against the engine walls which may be made from copper- or nickel-based alloys. Using a pin-on-disk tribometer, the friction and wear properties of some of these potential materials and possible lubrication methods are evaluated. The ceramic fabric rope displayed unacceptably high friction coefficients (0.6 to 1.3) and, thus, requires lubrication. Sputtered thin films of gold, silver, and CaF2 reduced the friction by a factor of two. Sprayed coatings of boride nitride did not effectively lubricate the fabric. Static heat treatment tests at 950 C indicate that the fabric is chemically attacked by large quantities of silver, CaF2, and boron nitride. Sputtered films or powder impregnation of the fabric with gold may provide adequate lubrication up to 1000 C without showing any chemical attack.

Dellacorte, Christopher↗

Performance of alumina-supported Pt catalysts in an electron-beam-sustained CO2 laser amplifier

The performance of an alumina-supported Pt catalyst system used to maintain the gas purity in an electron-beam-sustained (636) isotope CO2 laser amplifier has been tested. The system characteristics using the two-zone, parallel flow reactor were determined for both continuous- and end-of-day reactor operation using on-line mass spectrometric sampling. The laser amplifier was run with an energy loading of typically 110 J-l/atm and an electron-beam current of 4 mA/sq cm. With these conditions and a pulse repetition frequency of 10 Hz for up to 10,000 shots, increases on the order of 100 ppm O2 were observed with the purifier on and 150 ppm with it off. The 1/e time recovery time was found to be approximately 75 minutes.

Cunningham, D. L.↗

Synthesis and characterization of high-T(c) screen-printed Y-Ba-Cu-O films on alumina

Thick films of YBa2Cu3O(sub 7-x) have been deposited on highly polished alumina substrates by the screen printing technique. To optimize the post-printing heat treatment, the films were baked at various temperatures for different lengths of time and oxygen-annealed at a lower temperature. The resulting films were characterized by electrical resistivity measurements, X-ray diffraction, and optical and scanning electron microscopy. Properties of the films were found to be highly sensitive to the post-printing thermal treatment. Films baked for 15 min at 1000 C in oxygen were hard, adherent, near single phase, and superconducting with T(sub c) (onset) approx 96 KK, T(sub c) (zero) approx 66 K and Delta T sub c (10 to 90 percent) approx 10 K.

Bansal, Narottam P.↗

Kinetics and transport at AMTEC electrodes. II - Temperature dependence of the interfacial impedance of Na(g)/porous Mo/Na-Beta-double prime alumina

The exchange current, transfer coefficient, mass-transport parameters, and electrode capacitance at the Na(g)/porous Mo/Na-Beta-double prime alumina solid electrolyte (BASE) phase boundary have been evaluated from 740 to 1220 K. The transfer coefficient exhibits a value close to 0.5 and the exchange current is dominated by collision frequency, with no significant activation energy. Since the porous Mp-electrode adopts a fairly regular microstructure on the BASE surface, the magnitude of the exchange current of mature electrodes directly depends on the actual contact zone of the porous metal film with the BASE ceramic, and decreases slightly as grain growth occurs. The exchange currents and the mass-transport parameters derived for very porous, thin Mo electrodes indicate that the charge-transfer reaction occurs at a small fraction of the interface. High-frequency limiting capacitance and resistance values due to the interface show potential dependence and a value on the order of 1 F/sq m and 0.1-1.0 Ohm-sq cm.

Williams, R. M.↗