Evaluation of Tritium Content and Release from Surry-2 Fuel Cladding (Milestone Report)

To design and operate future reprocessing plants in a safe and environmentally compliant manner, the amount and form of tritium in the used nuclear fuel (UNF) must be understood and quantified. To gain a better understanding of how tritium in cladding will behave during processing, scoping tests are being performed to determine the tritium content in the cladding pre- and post-tritium pretreatment. A sample of Surry-2 pressurized water reactor (PWR) cladding was heated to 1100–1200°C to oxidize the zirconium and release all of the tritium in the cladding sample. The tritium content was measured to be ~240 µCi/g. Cladding samples were heated to 500ºC, which is within the temperature range (480 - 600ºC) expected for standard air tritium pretreatment systems, and to a slightly higher temperature (700ºC) to determine the impact of tritium pretreatment on tritium release from the cladding. Heating at 500°C for 24 hr removes ~0.2% of the tritium from the cladding, and heating at 700°C for 24 hr removes ~9%. Thus, a significant fraction of the tritium remains bound in the cladding and must be considered in operations involving cladding recycle.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fatigue Testing and Characterization of Pre-hydrided Zircaloy-4 Cladding Tubes

The solubility of hydrogen in Zircaloy-4 (Zry-4) at the cladding operating temperature is near 100 wt. ppm. Above this solubility limit, excess hydrogen precipitates as δ-hydride platelets in the cladding material. Because of the effect of the thermal gradient across the cladding thickness on the migration and precipitation of hydrogen, hydride rims are often observed at the cladding outer surface; under excessive corrosion conditions hydride blisters are possible. It is well known that the fatigue of metal alloys, especially high cycle fatigue, is sensitive to the status of surface including the microstructure, roughness, and residual stress. Thus, the question considered herein, is whether excessive hydrogen pickup modifies the microstructure such that it has a degradation effect on the fatigue performance of cladding during operation. This report describes the evaluation of fatigue performance of a pre-hydrided Zry-4 cladding. A commercial Zry-4 was polished and pre-hydrided to 800 ppm and 1300 ppm H contents. The fatigue testing was conducted under strain control at 5 Hz with fully-reversed bending by using a cyclic integrated reversible bending fatigue tester (CIRFT). Six specimens with 1300 ppm and one specimen with 800 ppm were tested. Significant variation in test results were observed. While two of the 1300 ppm specimens failed with less than 1 ×10 5 cycles (at 0.32% and 0.41%), the four other samples did not fail over the strain amplitude range of 0.25% to 0.38%. Interestingly, the fracture initiation site of the failed samples was on the outside diameter (OD) surface rather than on the inside diameter (ID) surface as is typical for the as-polished cladding. This suggested a degrading effect of the hydriding process. Subsequently, three of the unfailed specimens were then further tested at ~0.43% to observe where failure initiation occurred. Significant variation was also observed in these three specimens. One specimen failed at ~9000 cycles while the two others failed at 43000 and 1.06 ×10 5 cycles. The performance here correlated to the location of failure initiation; failure initiated on the OD in the sample that failed after 9000 cycles while it initiated on the ID in the sample that failed after 43000 and 1.06 ×10 5 cycles. Flat features at the OD initiation sites suggest a brittle hydride feature on the surface of those samples was the cause of the degradation in fatigue performance, though the overall hydrogen levels in all samples was similar. A summary of all the observations is provided below: • The un-failed specimens with 1300 ppm H were cycled to failure with a higher amplitude near 0.43%. In addition, the fatigue-treated specimen tended to have a longer fatigue at the same induced amplitude. • Fractography revealed a mixed failure mode for the pre-hydrided specimen. Particularly, the specimen with fracture initiation site (FIS) located on the outer diameter surface of tube tended to have a shorter fatigue life than that of FIS on the inner diameter surface. • Etched cross section was shown to have hydride platelets aligned with tube longitudinal axis as expected, and the density of hydrides is at the similar level as in literature data. Meanwhile, a LECO procedure was applied for hydrogen concentration measurement, which showed the measured hydrogen contents are close to the nominal value. • With the polished cladding tube as baseline, O’Donnell-Lager (O-L) analysis showed that a decrease of about 50% in reduction-of-area (RA) would be needed for the O-L fitting to the fatigue data of 1300 ppm cladding. The suggestion for the next steps is provided.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Transmission of laser pulses with high output beam quality using step-index fibers having large cladding

An apparatus and method for transmission of laser pulses with high output beam quality using large core step-index silica optical fibers having thick cladding, are described. The thick cladding suppresses diffusion of modal power to higher order modes at the core-cladding interface, thereby enabling higher beam quality, M.sup.2, than are observed for large core, thin cladding optical fibers. For a given NA and core size, the thicker the cladding, the better the output beam quality. Mode coupling coefficients, D, has been found to scale approximately as the inverse square of the cladding dimension and the inverse square root of the wavelength. Output from a 2 m long silica optical fiber having a 100 .mu.m core and a 660 .mu.m cladding was found to be close to single mode, with an M.sup.2=1.6. Another thick cladding fiber (400 .mu.m core and 720 .mu.m clad) was used to transmit 1064 nm pulses of nanosecond duration with high beam quality to form gas sparks at the focused output (focused intensity of >100 GW/cm.sup.2), wherein the energy in the core was <6 mJ, and the duration of the laser pulses was about 6 ns. Extending the pulse duration provided the ability to increase the delivered pulse energy (>20 mJ delivered for 50 ns pulses) without damaging the silica fiber.

42 ENGINEERING↗

Fuel Performance Simulation of Iron-Chrome-Aluminum Cladding during Steady-State LWR Operation

During a severe accident scenario, such as a loss-of-coolant accident, a nuclear reactor may lose its capacity to cool its fuel. The fuel rod temperatures begin to increases, quickly reaching temperatures where the coolant begins to evaporate. This lowers the coolant level in the core and eventually uncovers the fuel. Without sufficient heat transfer from the fuel rods to the coolant, the temperature of the fuel and cladding will increase dramatically. In the case of traditional zirconium-based alloys, as the temperature of the cladding reaches ∼1200 deg. C the zirconium rapidly begins to oxidize with H{sub 2}O in the coolant and steam. This oxidation reaction causes both thinning of the Zr-alloy cladding as the metal reacts and releases large amounts of H{sub 2} gas into the reactor pressure vessel. In order to increase the safety margin of LWR fuel in severe accident scenarios, several alternative cladding materials have been proposed to replace the currently used zirconium-based alloys. Of these materials, there is a particular focus on select iron-chrome-aluminum (FeCrAl) alloys because of slower oxidation Kinetics in high temperature steam than zirconium-based alloys. This increased oxidation resistance may provide additional coping time to mitigate any further damage resulting from an accident. However, by changing the cladding material, the neutronic characteristics of the core will change. FeCrAl alloys exhibit thermal neutron absorption cross sections nearly ∼12-16 x greater than Zr-alloys. This decreases the reactivity of the core, subsequently decreasing the potential cycle length for operation. To counteract this, fissile material may be added in the form of increased enrichment or increased fuel mass or the cladding thickness might be decreased, effectively reducing the neutronic penalty from using the alloy. In this study, all three changes are considered. To assess the viability of FeCrAl as an alternative cladding to Zr-alloys, engineering-scale fuel performance analysis is used to monitor the cladding and integral fuel rod behavior through its operation. Ongoing work is being performed to identify key parameters essential to modeling FeCrAl alloys for LWR applications and properly model fuel compliance and stress relief mechanisms for UO{sub 2} fuel. To improve the predictive capability of fuel performance codes for FeCrAl cladding under normal operation, high-fidelity mechanistic/physics-based material models are needed. This information can be generated and improved by access to experimental data on targeted FeCrAl alloys. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Cladding Alloys for Fluoride Salt Compatibility

This report provides an overview of several candidate technologies for cladding nickel-based corrosion protection layers onto high-temperature structural alloys. The report also provides a brief overview of the welding and weld performance issues associated with joining nickel-clad nickel-based alloys. From the available techniques, two cladding technologies were selected for initial evaluation. The first technique is a line-of-sight method that would be useful for cladding large structures such as vessel interiors or large piping. The line-of-sight method is a laser-based surface cladding technique in which a high-purity nickel powder mixed into a polymer binder is first sprayed onto the surface, baked, and then rapidly melted using a high-power laser. The second technique is a vapor phase technique based on the nickel-carbonyl process that is suitable for cladding inaccessible surfaces such as the interior surfaces of heat exchangers. An initial evaluation for performed on the quality of nickel claddings processed using the two selected cladding techniques.

alloys↗

Study on the mechanism of diametral cladding strain and mixed-oxide fuel element breaching in slow-ramp extended overpower transients

Cladding strain caused by fuel/cladding mechanical interaction (FCMI) was evaluated for mixed-oxide fuel elements subjected to 70–90% slow-ramp extended overpower transient tests in the experimental breeder reactor II. Calculated transient-induced cladding strains were correlated with cumulative damage fractions (CDFs) using cladding strength correlations. In a breached high-smeared density solid fuel element with low strength cladding, cladding thermal creep strain was significantly increased to approximately half the transient-induced cladding strain that was considered to be caused by the tertiary creep when the CDF was close to the breach criterion (=1.0), with the remaining strain due to instantaneous plastic deformation. In low-smeared density annular fuel elements, FCMI load was significantly mitigated and resulted in little cladding strain. The CDFs of the annular fuel elements were lower than 0.01 at the end of the overpower transient, indicating a substantial margin to breach. A substantial margin to breach was also maintained in a high-smeared density fuel element with high strength cladding.

99 GENERAL AND MISCELLANEOUS↗

Development and preliminary validation of a mechanistic multiscale model for fuel-cladding chemical interaction in metallic nuclear fuels

Despite decades of fuel rod material and design improvements, fuel-cladding chemical interaction (FCCI) remains the single-most lifetime-limiting behavior for modern metallic fuel rods. Constraining fuel lifetime increases operating costs, limiting the economic viability of commercializing metallic nuclear fuel technology. A mechanistic multiscale model utilizing the finite element method-based MARMOT and BISON codes was developed to more confidently predict cladding-side FCCI and its impact on fuel performance. The new BISON model incorporates mesoscale models for the effects of fuel microstructure evolution on the transport of wastage-inducing lanthanides through the fuel and for the kinetics of cladding wastage layer growth. The mesoscale models, in turn, build on lanthanide transport property data obtained from the atomistic scale. Preliminary validation studies using wastage thickness and cladding profilometry data from four fuel rods irradiated in Experimental Breeder Reactor II experiment X447 and one fuel rod from Fast Flux Test Facility experiment IFR1 show that the new model predicts cladding wastage and its effects on cladding deformation as well as existing empirical FCCI correlations. The new model is expected to aid in the design of new metallic fuel concepts, including fuel additives, cladding liners, and sodium-free annular fuel geometries. In conclusion, future work will focus on broader validation and refinement of the model’s treatment of different fuel alloys and cladding materials.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Assessment of wear coefficients of nuclear zirconium claddings without and with pre-oxidation

In the cores of pressurized water nuclear reactors, water-flow induced vibration is known to cause claddings on the fuel rods to rub against their supporting grids. Such grid-to-rod-fretting (GTRF) may lead to fretting wear-through and the leakage of radioactive species. The surfaces of actual zirconium alloy claddings in a reactor are inevitably oxidized in the high-temperature pressurized water, and some claddings are even pre-oxidized. As a result, the wear process of the surface oxide film is expected to be quite different from the zirconium alloy substrate. In this paper, we attempt to measure the wear coefficients of zirconium claddings without and with pre-oxidation rubbing against grid samples using a bench-scale fretting tribometer. Results suggest that the volumetric wear coefficient of the pre-oxidized cladding is 50 to 200 times lower than that of the untreated cladding. In terms of the linear rate of wear depth, the pre-oxidized alloy wears about 15 times more slowly than the untreated cladding. Finally, fitted with the experimentally-determined wear rates, a stage-wise GTRF engineering wear model demonstrates good agreement with in-reactor experience in predicting the trend of cladding lives.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Influence Of The Laser Cladding Strategies On The Mechanical Properties Of Inconel 718

This work presents different experimental results of the mechanical properties of Inconel registered 718 test parts built-up by laser cladding. Recently, turbine manufacturers for aeronautical sector have presented high interest on laser cladding processes. This process allows building fully functional structures on superalloys, such as Inconel registered 718, with high flexibility on complex shapes. However, there is limited data on mechanical properties of the laser cladding structures. Moreover, the available data do not include the influence of process parameters and laser cladding strategies. Therefore, a complete study of the influence of the laser cladding parameters and mainly, the variation of the tensile strength with the laser cladding strategy is presented. The results show that there is a high directionality of mechanical properties, depending on the strategies of laser cladding process. In other words, the test parts show a fiber -like structure that should be considered on the laser cladding strategy selection.

36 MATERIALS SCIENCE↗

Explosion Clad for Upstream Oil and Gas Equipment

Today's upstream oil and gas facilities frequently involve the combination of high pressures, high temperatures, and highly corrosive environments, requiring equipment that is thick wall, corrosion resistant, and cost effective. When significant concentrations of CO{sub 2} and/or H{sub 2}S and/or chlorides are present, corrosion resistant alloys (CRA) can become the material of choice for separator equipment, piping, related components, and line pipe. They can provide reliable resistance to both corrosion and hydrogen embrittlement. For these applications, the more commonly used CRA's are 316L, 317L and duplex stainless steels, alloy 825 and alloy 625, dependent upon the application and the severity of the environment. Titanium is also an exceptional choice from the technical perspective, but is less commonly used except for heat exchangers. Explosion clad offers significant savings by providing a relatively thin corrosion resistant alloy on the surface metallurgically bonded to a thick, lower cost, steel substrate for the pressure containment. Developed and industrialized in the 1960's the explosion cladding technology can be used for cladding the more commonly used nickel based and stainless steel CRA's as well as titanium. It has many years of proven experience as a reliable and highly robust clad manufacturing process. The unique cold welding characteristics of explosion cladding reduce problems of alloy sensitization and dissimilar metal incompatibility. Explosion clad materials have been used extensively in both upstream and downstream oil, gas and petrochemical facilities for well over 40 years. The explosion clad equipment has demonstrated excellent resistance to corrosion, embrittlement and disbonding. Factors critical to insure reliable clad manufacture and equipment design and fabrication are addressed.

36 MATERIALS SCIENCE↗

Preparation of Prototypic Irradiated Hydrided-Zircaloy Cladding for UFDC Programs

The DOE Used Fuel Disposition Campaign (UFDC) has tasked ORNL to investigate the behavior of light-water-reactor fuel cladding material performance related to extended storage and transportation of used fuel. Fast neutron irradiation of pre-hydrided zirconium-alloy cladding in the High Flux Isotope Reactor (HFIR) at elevated temperatures has been used to simulate the effects of high burnup on used fuel cladding for use in understanding the materials properties relevant to very long-term storage (VLTS) and subsequent transportation. The irradiated pre-hydrided metallic materials will generate baseline data to benchmark hot-cell testing of high-burnup used fuel cladding; and, more importantly, samples free of alpha contamination can be provided to the researchers who do not have hot cell facilities to handle highly contaminated high-burnup used fuel cladding to support their research projects for the UFDC. In order to accomplish this research, ORNL has produced unirradiated zirconium-based cladding tubes with a certain hydrogen concentration. Two capsules (HYCD-1 and HYCD-2) containing hydrided zirconium-based samples, 9.50 mm (0.374 in) in diameter, were inserted in HFIR for neutron irradiation. HYCD-1 was removed after Cycle 440B and HYCD-2 after Cycle 442. This paper will describe the general HYCD experiment configuration, achieved temperatures, and temperature gradients within the cladding, and current results of the PIE of the irradiated hydrided cladding samples.

prototypic irradiated zircaloy cladding unirradiat↗

Weld Development of FeCrAl Thin-Wall Cladding for LWR Accident Tolerant Fuel

The development of new cladding materials to replace Zr-based cladding for light water reactors (LWRs) has been actively pursued with improved high-temperature oxidation resistance to significantly suppress hydrogen production from an accident such as a loss of coolant event. FeCrAl alloy with a typical composition of approximately Fe-15Cr-5Al has been selected as a candidate material because of its improved high-temperature oxidation resistance over the present LWR zircaloy cladding. As a result of higher thermal neutron absorption for FeCrAl alloy, the cladding wall thickness needs to be reduced by approximately half compared to that of Zircaloy cladding to be comparable to the current LWR fuel performance under the normal operating condition. New weld techniques for joining the endplug to thin-walled cladding need to be developed. Both laser beam weld and pressure resistance weld were employed. This paper summarizes the recent progress on the laser weld development for FeCrAl cladding with 350 µm wall thickness. The results of microstructural characterization and mechanical property testing of the weld for the cladding-endplug set are discussed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Development of surface modified Zr cladding by coating technology for ATF

It is expected that the accident tolerance fuels (ATF) will provide an enhanced fuel performance of active cooling in the reactor core for a longer time period during design-basis events as well as maintain or improve the fuel performance during normal operations and operational transients. Thus, various ATF cladding concepts have being suggested and developed in many countries. Among them, the coated cladding concept is studied in this work after the considerations of various performances in both the accidents and normal operation of LWRs. In the surface coated cladding concepts, the combination of coating material and coating method is a very important factor to determine the ATF cladding performance. As a new coating material, Cr-based alloy was developed to increase the corrosion resistance under normal operation as well as the oxidation resistance during an accident. From the high temperature oxidation test at 1200 Celsius degrees, the Cr-based alloy showed a superior oxidation resistance to Zircaloy-4 cladding, and showed more improved corrosion resistance than Zircaloy-4 cladding under 360 Celsius degrees PWR simulated loop conditions. The 3D laser coating and a combination of arc ion plating and laser beam scanning were developed to obtain a good adhesion property of corrosion resistance alloy coated on a Zr substrate. The corrosion resistance alloy (Cr-based alloy and FeCrAl alloy) coated layer used by two types of coating methods was maintained without peeling off during the ring compression test at room temperature, although some cracks were formed on the coated layer. After a high-temperature oxidation test at 1200 Celsius degrees for 2000 s, a very thin oxide layer, which was a few microns, was formed on the corrosion resistance alloy layer. However, the ZrO{sub 2} phase, which was thicker than 100 μm was formed on the Zr alloy cladding surface. Thus, it is known that the high-temperature oxidation resistance of commercial Zr alloy cladding can be considerably improved by the coating of corrosion resistant alloys. In addition, the partial oxide dispersion strengthened (ODS) treatment using a laser beam scanning (LBS) method was applied to decrease the ballooning and rupture opening during accident conditions. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Behavior under LOCA conditions on enhanced accident tolerant chromium coated zircaloy-4 claddings

For enhanced accident tolerant fuels for light water reactors application, chromium coatings on zirconium based nuclear fuel claddings are developed and studied at CEA in the framework of the French CEA-EDF-AREVA collaborative program. The results obtained so far, mainly on Zircaloy-4 substrate, show very good corrosion resistance in nominal conditions and significant enhancement of the resistance of the material to oxidation in steam at high temperature (HT), up to 1300 Celsius degrees, with a drastic decrease of hydrogen release and/or pick-up. The present paper reports some new results obtained on chromium coated Zircaloy-4 claddings tested in loss-of-coolant accident (LOCA) conditions. In order to investigate the potential effect of the coating on the cladding mechanical behavior at HT and the capacity of the coating to sustain significant substrate deformation (i.e., during ballooning until burst occurrence) without generalized cracking/peeling, a preliminary limited set of internal pressure creep and temperature ramp tests have been performed in steam environment thanks to the EDGAR facility. The thermal-mechanical tests were done for testing/burst temperatures ranging from 600 C. degrees (α{sub Zr} phase domain) up to 1000 C. degrees (β{sub Zr} phase domain) on 50 cm long low-tin Zircaloy-4 cladding samples with a 15 μm thick outer chromium coating. It is shown that: -) whatever the applied temperature/pressure values, the chromium coating is still fully adherent after having experienced ballooning and burst, including at the vicinity of the burst opening where the Zircaloy-4 clad substrate is highly deformed; -) a HT strengthening effect of the coating on the overall creep clad behavior is evidenced when compared to uncoated Zircaloy-4 cladding materials tested in the same conditions; -) as a consequence, it is observed that, in the 600-750 C. degrees temperature range (α{sub Zr} phase domain) and after burst occurrence, the balloon sizes (i.e., 'uniform' and maximum hoop strains) are generally reduced when compared to uncoated materials; -) regarding the burst mechanism in the β{sub Zr} phase temperature range (1000 C. degrees), it is interesting to observe that, even if some ballooning occurred prior to the cladding failure, the actual burst openings are generally very small (in the order of 1 mm{sub 2} or less), reducing the risk of fuel fragments dispersal in the coolant.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fuel performance analysis of FeCrAl cladding during LWR operation

This work focuses on modeling the integral thermo-mechanical performance of FeCrAl cladded fuel during normal operation in light-water reactors. Preliminary analysis has been performed to assess FeCrAl alloys (namely Alkrothal 720 and APMT) as a suitable fuel cladding replacement for Zr-alloys, using the MOOSE-based, finite-element fuel performance code BISON. These simulations identify the effects of the mechanical-stress and irradiation responses of FeCrAl and provide a comparison with Zr-alloys. In comparing these clad materials, fuel rods have been simulated for normal reactor operation and simple steady-state operation. Normal reactor operating conditions target the cladding performance over the rod lifetime (∼4 cycles) for the highest-power rod in the highest-power fuel assembly under reactor power maneuvering. The power histories and axial temperature profiles input into BISON were generated from a neutronics study on full-core reactivity equivalence for FeCrAl using the 3D full core simulator NESTLE. Evolution of the FeCrAl cladding behavior over time is evaluated by using steady-state operating conditions such as a simple axial power profile, a constant cladding surface temperature, and a constant fuel power history. The fuel rod designs and operating conditions used are based off the Peach Bottom BWR and design consideration was given to minimize the neutronic penalty of the FeCrAl cladding by changing fuel enrichment and cladding thickness. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Evaluation of Irradiation Creep Effects in HT9 Cladding for FAST Experiments

The push for advanced reactor fuels for improved reactor safety and efficiency had led to a renewed interest in metallic fuel for nuclear reactor applications. Experimental investigation is necessary to ensure a robust understanding of the thermomechanical properties of new metallic fuel designs. Unfortunately, with the current experimental facilities, thoroughly investigating the responses of metallic fuel burnup would take a prohibitively long time. To alleviate this, the Fission Accelerated Steady State Test (FAST) was developed to accelerate the irradiation testing while simultaneously decreasing the sensitivity to fabrication tolerances by reducing the fuel diameter and scaling the experiment. This method successfully scales the radiation effects on the fuel, but the HT9 cladding is not exposed to prototypic radiation conditions. This raises questions on whether the FAST experiment results are truly indicative of the HT9 cladding performance due to radiation induced creep effects not being appropriately accounted for. Using BISON fuel performance code, the simulated FAST cladding strain is compared to simulated EBR-II cladding strain. This is done through a sensitivity study of input parameters and scaling of neutron fluence on the cladding. This allows a parametric comparison of physical phenomena on the effective difference between cladding strains between FAST and equivalent burnup EBR-II fuel pins. The results show that the irradiation induced deformation (creep or swelling) is insignificant compared to the thermal-mechanical deformation. Therefore, the difference between the FAST experiment cladding and the EBR-II experiment cladding is negligible and comparison of fuel system performance between the two experiments is appropriate.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Hydrogen permeation in FeCrAl alloys for LWR cladding application

FeCrAl is an advanced oxidation-resistant iron-based alloy class, is a highly prevalent candidate as an accident-tolerant fuel cladding material. Compared with traditional zirconium alloy fuel cladding, increased tritium permeation through FeCrAl fuel cladding to the primary coolant is expected, raising potential safety concerns. In our study, the hydrogen permeability of several FeCrAl alloys was obtained using a static permeation test station, which was calibrated and validated using 304 stainless steel. The high hydrogen permeability of FeCrAl alloys leads to concerns with respect to potentially significant tritium release when used for fuel cladding in LWRs. Also, the total tritium inventory inside the primary coolant of a light water reactor was quantified by applying a 1-dimensional steady state tritium diffusion model to demonstrate the dependence of tritium inventory on fuel cladding type. Furthermore, potential mitigation strategies for tritium release from FeCrAl fuel cladding were discussed and indicate the potential for application of an alumina layer on the inner clad surface to serve as a tritium barrier. More effort is required to develop a robust, economical mitigation strategy for tritium permeation in reactors using FeCrAl clad fuel assemblies.

36 MATERIALS SCIENCE↗

BISON validation of FeCrAl cladding mechanical failure during simulated reactivity-initiated accident conditions*

Here, a reactivity-initiated accident (RIA) is a postulated design basis accident in light water reactors (LWRs) in which a rapid reactivity insertion induces a fission rate increase and a fuel pellet temperature rise. During RIA, the fuel pellet thermally expands and may cause pellet-cladding mechanical interaction (PCMI). Separate effects PCMI tests were performed on C26M FeCrAl cladding tube samples, introducing biaxial stress via a well understood modified burst test (MBT) system. A high-speed camera in the MBT system captured the projections, covering a 360° view of the cladding deformation and enabling a digital image correlation (DIC) method to quantify the surface strains with high fidelity. Representative hot zero-power RIA mechanical loading conditions were applied to the sample, and the test duration ranged from 20 to 500 ms at an average temperature of 573 K. BISON finite element–based fuel performance code modeling was performed against the high-fidelity DIC data produced from the MBTs. Validation calculations were conducted with 2D models and systematically compared with test data of the burst time, burst pressure, burst hoop strains, and hoop strain rates. Based on the behaviors from the separate effects test, BISON calculations satisfactorily predicted the cladding deformation behaviors. Sensitivity analysis was conducted to identify highly influential mechanical properties responsible for the cladding failure behavior during the MBT experiments. The results highlight the significance of the cladding's mechanical strength in governing cladding strain, followed by the significance of the mechanical interactions between the pellet and the cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗