At least 109 records · Page 6

Aluminum-induced dreierketten chain cross-links increase the mechanical properties of nanocrystalline calcium aluminosilicate hydrate

The incorporation of Al and increased curing temperature promotes the crystallization and cross-linking of calcium (alumino)silicate hydrate (C-(A-)S-H), which is the primary binding phase in most contemporary concrete materials. However, the influence of Al-induced structural changes on the mechanical properties at atomistic scale is not well understood. Herein, synchrotron radiation-based high-pressure X-ray diffraction is used to quantify the influence of dreierketten chain cross-linking on the anisotropic mechanical behavior of C-(A-)S-H. We show that the ab-planar stiffness is independent of dreierketten chain defects, e.g. vacancies in bridging tetrahedra sites and Al for Si substitution. The c-axis of non-cross-linked C-(A-)S-H is more deformable due to the softer interlayer opening but stiffens with decreased spacing and/or increased zeolitic water and Ca 2+ of the interlayer. Dreierketten chain cross-links act as ‘columns’ to resist compression, thus increasing the bulk modulus of C-(A-)S-H. We provide the first experimental evidence on the influence of the Al-induced atomistic configurational change on the mechanical properties of C-(A-)S-H. Our work advances the fundamental knowledge of C-(A-)S-H on the lowest level of its hierarchical structure, and thus can impact the way that innovative C-(A-)S-H-based cementitious materials are developed using a ‘bottom-up’ approach.

36 MATERIALS SCIENCE↗

A Fresnel collector process heat experiment at Capitol Concrete Products

An experiment is planned, conducted and evaluated to determine the feasibility of using a Power Kinetics' Fresnel concentrator to provide process heat in an industrial environment. The plant provides process steam at 50 to 60 psig to two autoclaves for curing masonry blocks. When steam is not required, the plant preheats hot water for later use. A second system is installed at the Jet Propulsion Laboratory parabolic dish test site for hardware validation and experiment control. Experiment design allows for the extrapolation of results to varying demands for steam and hot water, and includes a consideration of some socio-technical factors such as the impact on production scheduling of diurnal variations in energy availability.

Hauger, J. S.↗

SaltStone Wastewater Cement Study Using Isothermal Calorimetry, Standard Concrete Characterization Techniques, and CemGEMS - 25169

Cementitious reagents are used to solidify/stabilize aqueous radioactive, hazardous, and mixed salt solutions, and sludges to meet low-level radioactive waste (LLW) and Resource Conservation and Recovery Act (RCRA) requirements for disposal at Department of Energy (DOE). It is flexible enough to solidify radioactive wastewater saturated in complex species that include but are not limited to radioactive isotopes from the bombardment of neutrons in reactor operation, corrosion products from metallic components, and a variety of soluble organic compounds. [1,2]. Waste form testing typically includes processing or fresh properties, cured properties, compressive strength and hydraulic properties, porosity, density, saturated and unsaturated moisture transport, and leachability of contaminants in the waste form pore solution. Properties are collected over a relatively limited time, typically 28 to 365 days [3]. In addition, changes in the waste form as the result of time and changing conditions are important for concrete engineers to predict overall performance of the forms and potential release of contaminants in the disposal process via unintended filtration into the environment [4]. These predictions are determined/calculated characterizing young waste forms (relative to the standard age of concrete) and are based on transport through soluble ions in pore solutions. Characterization methods include X-ray, SEM, and isothermal calorimetry among other methods used to define the composition, amorphous vs. crystalline nature of the components, and the energetic formation mechanisms for multi-phase mineral systems. [5–7] Isothermal calorimetry is a well standardized technique for cements and concretes and can be used to predict the timing and nature of the hydration reactions.[8] The technique can measure long term energetic

Bustamante, Michael E. [Savannah River National La↗

Cementitious Grout for Closing SRS High Level Waste Tanks - 12315

In 1997, the first two United States Department of Energy (US DOE) high level waste tanks (Tanks 17-F and 20-F: Type IV, single shell tanks) were taken out of service (permanently closed) at the Savannah River Site (SRS). In 2012, the DOE plans to remove from service two additional Savannah River Site (SRS) Type IV high-level waste tanks, Tanks 18-F and 19-F. These tanks were constructed in the late 1950's and received low-heat waste and do not contain cooling coils. Operational closure of Tanks 18-F and 19-F is intended to be consistent with the applicable requirements of the Resource Conservation and Recovery Act (RCRA) and the Comprehensive Environmental Response, Compensation, and Liability Act (CERCLA) and will be performed in accordance with South Carolina Department of Health and Environmental Control (SCDHEC). The closure will physically stabilize two 4.92E+04 cubic meter (1.3 E+06 gallon) carbon steel tanks and isolate and stabilize any residual contaminants left in the tanks. Ancillary equipment abandoned in the tanks will also be filled to the extent practical. A Performance Assessment (PA) has been developed to assess the long-term fate and transport of residual contamination in the environment resulting from the operational closure of the F-Area Tank Farm (FTF) waste tanks. Next generation flowable, zero-bleed cementitious grouts were designed, tested, and specified for closing Tanks 18-F and 19-F and for filling the abandoned equipment. Fill requirements were developed for both the tank and equipment grouts. All grout formulations were required to be alkaline with a pH of 12.4 and to be chemically reducing with a reduction potential (Eh) of -200 to -400. Grouts with this chemistry stabilize potential contaminants of concern. This was achieved by including Portland cement and Grade 100 slag in the mixes, respectively. Ingredients and proportions of cementitious reagents were selected and adjusted to support the mass placement strategy developed by Savannah River Remediation (SRR) Closure Operations. Subsequent down selection was based on compressive strength and saturated hydraulic conductivity results. Fresh slurry property results were used as the first level of screening. A high range water reducing admixture and a viscosity modifying admixture were used to adjust slurry properties to achieve flowable grouts. Adiabatic calorimeter results were used as the second level screening. The third level of screening was used to design mixes that were consistent with the fill material parameters used in the F-Tank Farm Performance Assessment which was developed to assess the long-term fate and transport of residual contamination in the environment resulting from the operational closures. The cement and slag contents of a mix selected for filling Tanks 18-F and 19-F should be limited to no more than 125 and 210 lbs/cyd, respectively, to limit the heat generated as the result of hydration reaction during curing and thereby enable mass pour placement. Trial mixes with water to total cementitious materials ratios of 0.550 to 0.580 and 125 lbs/cyd of cement and 210 lbs/cyd of slag met the strength and permeability requirements. Mix LP no.8-16 was selected for closing SRS Tanks 18-F and 19-F because it meets or exceeds the design requirements with the least amount of Portland cement and blast furnace slag. This grout is expected to flow at least 45 feet. A single point of discharge should be sufficient for unrestricted flow conditions. However, additional entry points should be identified as back-up in case restrictions in the tank impede flow. The LP no.8 series of trial mixes had surprisingly high design compressive strengths (2000 to 4000/5000 psi) which were achieved at extended curing times (28 to 90 days, respectively) given the small amount of Portland cement in the mixes (100 to 185 lbs/cyd). The grouts were flowable structural fills containing 3/8 inch gravel and concrete sand aggregate. These grouts did not segregate and require no compaction. They have low permeabilities (≤ 10{sup -9} cm/s) and are consequently expected to be very durable. This series of trial mixes contained by-product materials, i.e., slag and Class F fly ash, and an admixture system initially specified for the grouts used to close Tanks 17-F and 20-F at SRS. The mix designs have low CO{sub 2} footprints because Portland cement contents are very low and can be considered environmentally friendly. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Low-velocity impact resistance and failure characteristics of all thermoplastic woven polymer-fiber-reinforced plastic composites

This study addresses the impact performances of recyclable composites made of all thermoplastic polymer-fiber-reinforced plastics (PFRPs), where the reinforcing fibers and matrix are made of thermoplastic polymers. Three woven PFRPs systems were evaluated, including polypropylene fibers, polypropylene matrix, and high-density polyethylene matrix. In low-velocity impact scenario with an impactor speed of less than 6 m/s, our results demonstrate the energy absorption capabilities of the flat laminate PFRPs compared to woven carbon fiber-reinforced plastics (CFRPs) and aluminum alloy 5052. For the systems studied, the PFRPs can reach the specific energy absorption 89% to 115% of the CFRPs. Even compared with the aluminum alloy 5052, the PFRPs can reach up to 97%. We investigate the failure morphologies of the PFRPs using X-ray µCT scans. They reveal the PFRPs’ unique ductile failure morphologies compared to common CFRPs. In addition, we heal the perforated region in the PFRPs by applying the manufacturing process identical to the initial curing process. The healed panels are perforated again, and they recovered 30% to 38% of their original specific energy absorption, a recovery not achievable with CFRPs. This study provides valuable experimental results, and concrete insights into the potential applications of recyclable PFRPs in various engineering fields. It emphasizes their excellent energy-absorbing capability and repairability.

CFRPs↗

Evaluation of Environmental Conditions on the Curing Of Commercial Fixative and Intumescent Coatings

Performance metrics for evaluating commercial fixatives are often not readily available for important parameters that must be considered per the facility safety basis and the facility Basis for Interim Operations (BIO). One such parameter is the behavior of such materials in varied, “non-ideal” conditions where ideal is defined as 75 °F, 40% RH. Coupled with the inherent flammable nature of the fixative materials that can act to propagate flame along surfaces that are otherwise fireproof (concrete, sheet metal), much is left unknown when considering the safety basis implications for introducing these materials into nuclear facilities. Through SRNL’s efforts, three (3) fixatives, one (1) decontamination gel, and six (6) intumescent coatings were examined for their responses to environmental conditions to determine whether these materials were impervious to non-nominal temperatures and humidities that may be found in nuclear facilities. Characteristics that were examined included set-to-touch time, dust free time, and adhesion testing of the fully cured compounds. Of these ten materials, three were two-part epoxy materials while the other seven consisted of only one constituent. The results show that the epoxies tested are unable to cure in sub-freezing temperatures, with the low temperatures inhibiting crosslinking to a very significant degree. These efforts show significant inhibiting of performance for non-nominal environmental conditions, something that must be addressed both in the decision process for a fixative material to apply and per the safety basis to ensure the accurate flammability and material at risk is calculated.

36 MATERIALS SCIENCE↗

Evaluation of Environmental Conditions on the Curing Of Commercial Fixative and Intumescent Coatings

Performance metrics for evaluating commercial fixatives are often not readily available for important parameters that must be considered per the facility safety basis and the facility Basis for Interim Operations (BIO). One such parameter is the behavior of such materials in varied, “non-ideal” conditions where ideal is defined as 75 °F, 40% RH. Coupled with the inherent flammable nature of the fixative materials that can act to propagate flame along surfaces that are otherwise fireproof (concrete, sheet metal), much is left unknown when considering the safety basis implications for introducing these materials into nuclear facilities. Through SRNL’s efforts, three (3) fixatives, one (1) decontamination gel, and six (6) intumescent coatings were examined for their responses to environmental conditions to determine whether these materials were impervious to non-nominal temperatures and humidities that may be found in nuclear facilities. Characteristics that were examined included set-to-touch time, dust free time, and adhesion testing of the fully cured compounds. Of these ten materials, three were two-part epoxy materials while the other seven consisted of only one constituent. The results show that the epoxies tested are unable to cure in sub-freezing temperatures, with the low temperatures inhibiting crosslinking to a very significant degree. These efforts show significant inhibiting of performance for non-nominal environmental conditions, something that must be addressed both in the decision process for a fixative material to apply and per the safety basis to ensure the accurate flammability and material at risk is calculated.

36 MATERIALS SCIENCE↗

Printable Fiber Reinforced Cement Composites – Feasibility Study

Additive manufacturing is enabling the manufacturability of structures with previously unattainable complexity or functionality, and there is growing interest in additive manufacturing of “printed” concrete structures. The focus of this Phase 1 Technical Collaboration (TC) project was to evaluate feasibility of printing hybrid cement composite structures reinforced with textile carbon fibers (tCF). This project leverages other (non-IACMI) projects on cement formulation and printing process development, as well as on the production process for tCF. This project’s primary focus was to explore cement composite mix design with textile carbon fibers to be manufactured by MonteFibre (TC partner) and evaluate suitable fiber-matrix interface or sizing for cement composites working with Michelman (TC Partner). This project supports IACMI’s goal of reducing the cost and embodied energy of carbon fiber composites. Cost is one of the fundamental challenges to carbon fiber reinforced cement composites. Cement is an extremely inexpensive material (approximately $\$$0.05/lb). Adding 1 wt% of conventional carbon fiber to cement quadruples its cost. Therefore, the need to use low-cost carbon fiber and ensure that the additional cost of the carbon fiber has a greater cost benefit to the final product. This was the first preliminary evaluation to integrate tCF reinforcement in cement composites, and such potential tCF utilization should significantly reduce materials cost. Cement composite production is energy and emissions intensive, thus by strengthening it less material will be required. Hence, the embodied energy and production time of the resulting structures will be reduced. Additionally, integrating these new materials into additive processes can enable selective use of the material in high load or stress areas. It is noteworthy that past work in this field of fiber reinforced cement composites did not consider the optimization of fiber-matrix interface using suitable sizing. Carbon fiber reinforcement offers potential added benefits of thermal conductivity (which affects cure rate) and flow behavior that could provide opportunities for site specific utilization of carbon fiber on hybrid cement structures (e.g. use the fiber reinforcement on outer surfaces to enhance strength and modulus and then infiltrating the internal structures with conventional concrete). MonteFibre was the industry lead and planned on supplying the tCF for this project. However, during the short Phase-1 duration of this project, MonteFibre was unable to produce tCF for this project due to manufacturing plant being off-line throughout the course of the project. The project team decided to pursue an alternate option which involved demonstrating printable concrete with steel fibers by the ORNL lead, Dr. Brian Post. The University of Tennessee collaboration team focused on evaluating the suitable chemical sizing for carbon fibers working with Michelman and also developed methods for material characterization of cement-based composites to evaluate the material response for compression, shear, flexure, and tension. The two milestones for University of Tennessee, Knoxville were realized related to identification of one sizing suitable for carbon fiber reinforced cement composite and developing data associated with mechanical behavior of unreinforced (neat) and carbon fiber reinforced cement composites. ORNL could not complete the task of carbon fiber reinforced printed cement composites due to the reasons mentioned earlier, but was able to replace tCF with steel fibers to demonstrate the feasibility of printing with fiber reinforced cement composites. The Project team reviewed possible sizing chemistry available in collaboration with Michelman for use on carbon fiber reinforcement in cement composites and concrete applications. Our initial goal was to identify a sizing most promising for formulation with textile carbon fibers (tCF) to deliver excellent mechanical properties in composite material state. Since tCF was not available for this project as originally envisioned, the team continued this task to identify a suitable sizing for carbon fiber applications by applying such sizing to lower cost carbon fibers currently available commercially from Zoltek called Panex fibers. At a future time this can be optimized for textile carbon fibers from Montefibre. The bulk of previous work on carbon fiber reinforced cement has neglected the importance of fiber-matrix adhesion on mechanical properties of the cement composite and identifying this missing link was an important accomplishment for future research. Tensile behavior of fiber reinforced concrete is important to evaluate in order to realize the dream of concrete products that do not need reinforcing steel. Important sample preparation and testing procedures were addressed in this study and it was concluded that substantial improvements in tensile behavior, without compromising compressive strength, and improved ductility can result from the use of carbon fiber reinforcement.

36 MATERIALS SCIENCE↗

Low Temperature Regolith Bricks for In-Situ Structural Material

Current technology for producing in-situ structural materials on future missions to Mars or the moon relies heavily on energy-intensive sintering processes to produce solid bricks from regolith. This process requires heating the material up to temperatures in excess of 1000 C and results in solid regolith pieces with compressive strengths in the range of 14000 to 28000 psi, but are heavily dependent on the porosity of the final material and are brittle. This method is currently preferred over a low temperature cementation process to prevent consumption of precious water and other non-renewable materials. A high strength structural material with low energy requirements is still needed for future colonization of other planets. To fulfill these requirements, a nano-functionalization process has been developed to produce structural bricks from regolith simulant and shows promising mechanical strength results. Functionalization of granular silicate particles into alkoxides using a simple low temperature chemical process produces a high surface area zeolite particles that are held together via inter-particle oxygen bonding. Addition of water in the resulting zeolite particles produces a sol-gel reaction called "inorganic polymerization" which gives a strong solid material after a curing process at 60 C. The aqueous solution by-product of the reaction is currently being investigated for its reusability; an essential component of any ISRU technology. For this study, two batches of regolith bricks are synthesized from JSC-1A; the first batch from fresh solvents and chemicals, the second batch made from the water solution by-product of the first batch. This is done to determine the feasibility of recycling necessary components of the synthesis process, mainly water. Characterization including BET surface area, SEM, and EDS has been done on the regolith bricks as well as the constituent particles,. The specific surface area of 17.53 sq m/g (average) of the granular regolith material was obtained from nitrogen adsorption isotherm measurement. The size, shape and textures of regolith from SEM shows that the particles are 25-50 micrometers in size and mostly irregular in shape (Figure 1a). The elemental composition of regolith was identified from EDS analysis showed the presence of Si, Al, Fe, Na, Mg, Ca, Ti, O and C (see figure 1b). Each set of cylindrical brick samples were prepared by low energy process, and cured for 21 and 28 days, respectively to compare their compressive strength. Figure 1c, and d shows the JSC-1A brick and the compressive strength measurements. The results from the 21 day cured bricks (2 bricks) have been done and yielded an aver-age strength of 3050 psi, considerably higher than Portland cement mortars (Type IV and V). This promising technology provides the benefits of construction material similar to concrete, with a low complexity, low energy synthesis process and the likelihood of complete reusability of precious resources. Compressive strength using this method can be improved by increasing the surface area of the particles, using bi-modal particle size distribution, and adding certain additives to increase inter-particle forces.

ISRU↗

Influence of the composition of cement kiln dust on its interaction with fly ash and slag

Cement kiln dust (CKD), a by-product of the cement industry, contains significant amounts of alkali, free lime, chloride and sulfate. Wide variation reported in the chemical composition of CKDs limits their potential application as a sustainable binder component in concrete. In the current study, the performance of two different CKDs as components in a novel binder is evaluated. Several binders are developed by blending CKDs with fly ash or slag. Binders with 70% CKD were prepared at a water-to-binder ratio of 0.4, and heat-cured at 75 °C to accelerate the strength development. The hydration progress was monitored using X-ray diffraction, and morphological examination was performed using scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Ettringite and calcium aluminosilicate hydrate (C-A-S-H) were identified as the main hydration products in the hardened binder system. Strength development of CKD-based binder was found to be significantly influenced by its free lime and sulfate contents. -- Highlights: •Interaction of cement kiln dust with fly ash and slag was explored. •CKD with higher free lime and sulfate content increased the strength of binder. •C-S-H like reaction gel with fibrillar morphology is observed in CKD-based binders.

36 MATERIALS SCIENCE↗

Using micro-XRF to characterize chloride ingress through cold joints in 3D printed concrete

Digital fabrication methods with concrete have been rapidly developing, with many problems related to component production and material control being solved in recent years. These processes produce inherently layered cementitious components that are anisotropic, and in many cases, produces a weak interface between layers, which are generally referred to as cold joints. While material strength at these interfaces has been well studied in recent years, durability has received less attention, even though cold joints can function as channels for aggressive agents, such as chlorides. This work presents a method using micro-X-ray fluorescence (μXRF) to image chloride ingress into layer interfaces of 3D printed fine-grained concrete specimens produced with varying layer deposition time intervals, and also compares it to neutron imaging of moisture uptake. The results show that cold joints formed after a 1 day time interval are highly susceptible to chloride ingress, and that curing conditions play a major role in how quickly interfacial transport can take place. The μXRF method is also shown to be useful for study of transport of chlorides in cold joints, due to its spatial resolution and direct analysis of an aggressive species of interest.

36 MATERIALS SCIENCE↗

Investigating the Depth of Penetration of Radionuclides in Concrete - 16292

This paper focuses on some chemical and structural aspects for mature concrete structural substrate that functions as a barrier to radioactive material migration. Exposure to radioactive material may be a consequence of surface contact, such as resulting from exposure by spills or leaks. In properly-prepared waste storage areas, undamaged paint and sealant helps to protect the structural cement. However, damaged surfaces, cracks, and relatively porous slab seams can offer a preferred migration pathway for spilled contaminates, including radionuclides. The cost of remediation of concrete structures is directly related to the amount of concrete that must be removed and subsequently disposed. A carefully implemented investigative plan can be utilized to determine how much concrete must be removed and the approximate level of volumetric radiological contamination can be used to estimate disposal costs. Normal concrete pore solution is saturated with calcium hydroxide and also contains sodium and potassium hydroxide; the pH is typically 13 to 14. Contaminants (such as uranium) that hydrolyze in alkaline media that form precipitant phases and tend to deposit at the near-surface. However, more soluble contaminants, such as Cs-137 (as Cs{sup +}) and Tc-99 (as the pertechnetate anion TcO{sub 4}{sup -}) diffuse more rapidly (and deeply) into the porous substrate. Profiling the migration of the water-soluble radionuclides into a cure (hardened) cement surface is a challenge, since water-cooled saws, borers and similar implements are often used to excise and/or slice the core. Alternately, dry mechanical fracturing for excavation of cement may introduce the possibility of material cross-contamination and uncertainty for the average sampling depth for the sample collection event, potentially yielding non-representative samples, and may preclude determination of crack formation that may have been present in the native (non-fractured) substrate. Structural concrete is comprised of cement and pozzolan paste, relatively impervious aggregate (typically stone and/or sand), and rebar (iron reinforcement). Near-surface aggregate may act as a hydrolytic barrier, causing contaminants leached into the pore water to by-pass the impervious grains, causing deeper-than expected penetration, especially if there are grain boundary cracks also present to facilitate migration. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

MEASUREMENT OF SPECIFIC HEAT CAPACITY OF SALTSTONE

One of the goals of the Saltstone variability study is to identify (and quantify the impact of) the operational and compositional variables that control or influence the important processing and performance properties of Saltstone grout mixtures. The heat capacity of the Saltstone waste form is one of the important properties of Saltstone mixes that was last measured at SRNL in 1997. It is therefore important to develop a core competency for rapid and accurate analysis of the specific heat capacity of the Saltstone mixes in order to quantify the impact of compositional and operational variations on this property as part of the variability study. The heat capacity, coupled with the heat of hydration data obtained from isothermal calorimetry for a given Saltstone mix, can be used to predict the maximum temperature increase in the cells within the vaults of the Saltstone Disposal Facility (SDF). The temperature increase controls the processing rate and the pour schedule. The maximum temperature is also important to the performance properties of the Saltstone. For example, in mass pours of concrete or grout of which Saltstone is an example, the maximum temperature increase and the maximum temperature difference (between the surface and the hottest location) are controlled to ensure durability of the product and prevent or limit the cracking caused by the thermal gradients produced during curing. This report details the development and implementation of a method for the measurement of the heat capacities of Saltstone mixes as well as the heat capacities of the cementitious materials of the premix and the simulated salt solutions used to batch the mixes. The developed method utilizes the TAM Air isothermal calorimeter and takes advantage of the sophisticated heat flow measurement capabilities of the instrument. Standards and reference materials were identified and used to validate the procedure and ensure accuracy of testing. Heat capacities of Saltstone mixes were {approx} 55% higher than the previous measurement of specific heat capacity on a reference Saltstone mix in 1997. Values of mixes prepared using Deliquification, Dissolution and Adjustment (DDA), Modular Caustic Side Solvent Extraction Unit (MCU) and Salt Waste Processing Facility (SWPF) simulants and premix at 0.60 w/cm ratio were {approx} 1.95 J/g/{sup o}C and were equivalent within experimental error. The simple law of mixtures was used to predict the heat capacities of the Saltstone and the results were in excellent agreement with experimental data. This simple law of mixtures can therefore be used to predict the heat capacities of Saltstone mixes in those cases where measurements have not been made. The time dependence of the heat capacity is important as an input to the modeling of temperature increase in Saltstone vaults. The heat capacity of a mix of MCU and premix at 0.60 w/cm ratio was measured immediately after initial mixing and then periodically up to times greater than 100 days. Within experimental error, the heat capacity did not change with time. Therefore, the modeling is not complicated by requiring a time dependent function for specific heat capacity. The water to cementitious material (w/cm) ratio plays a key role in determining the value of the heat capacity. Both experimental and predictive values for SWPF mixes as function of the w/cm ratio were obtained and presented in this report. Predictions of the maximum temperatures of the Saltstone mixes were made using the heat of hydration data from previous isothermal measurements and the newly measured heat capacities for DDA, MCU and SWPF mixes. The maximum temperature increase ranged from 37 to 48 C for these mixes. The presence of aluminate at 0.33 M produced a temperature increase of 68 C which is close to the adiabatic temperature rise of 74 C observed by Steimke and Fowler in 1997 for a mix containing 0.35 M aluminate. Aluminum dissolution of the sludge will increase the aluminate in the DSS which in turn will result in a larger temperature increase in the Saltstone vaults during the curing period. The initial temperature of the Saltstone mixes in the Saltstone Production Facility (SPF) can be predicted using the specific heat capacities of Decontaminated Salt Solutions (DSS), the specific heat capacities of cementitious materials, and the initial temperatures of the DSS and the premix. This initial mix temperature is dominated by the DSS temperature due to its high heat capacity relative to the cementitious materials. Therefore, controlling the initial temperature of the DSS to lower temperatures will lead to lower maximum temperatures in the vault for a given batch of Saltstone.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The significance of nanoparticles on bond strength of polymer concrete to steel

Here, polymer concrete (PC) is a commonly used material in construction due to its improved durability and good bond strength to steel substrate. PC has been suggested as a repair and seal material to restore the bond between the cement annulus and the steel casing in wells that penetrate formations under consideration for CO 2 sequestration. Nanoparticles including Multi-Walled Carbon Nano Tubes (MWCNTs), Aluminum Nanoparticles (ANPs) and Silica Nano particles (SNPs) were added to an epoxy-based PC to examine how the nanoparticles affect the bond strength of PC to a steel substrate. Slant shear tests were used to determine the bond strength of PC incorporating nanomaterials to steel; results reveal that PC incorporating nanomaterials has an improved bond strength to steel substrate compared with neat PC. In particular, ANPs improve the bond strength by 51% over neat PC. Local shear stresses, extracted from Finite Element (FE) analysis of the slant shear test, were found to be as much as twice the apparent/average shear/bond strength. These results suggest that the impact of nanomaterials is higher than that shown by the apparent strength. Fourier Transform Infrared (FTIR) measurements of epoxy with and without nanomaterials showed ANPs to influence curing of epoxy, which might explain the improved bond strength of PC incorporating ANPs.

36 MATERIALS SCIENCE↗

Development of a Leave-in-Place Slab Edge Insulating Form System

Concrete slabs represent the primary foundation type in residential buildings in the fast-growing markets throughout the southern and southwestern United States. Nearly 75% of the 2005 U.S. population growth occurred in these southern tier states. Virtually all of these homes have uninsulated slab perimeters that transfer a small, but steady, flow of heat from conditioned space to outdoors during the heating season. It is estimated that new home foundations constructed each year add 0.016 quads annually to U.S. national energy consumption; we project that roughly one quarter of this amount can be attributed to heat loss through the slab edge and the remaining three quarters to deep ground transfers, depending upon climate. With rising concern over national energy use and the impact of greenhouse gas emissions, it is becoming increasingly imperative that all cost-effective efforts to improve building energy efficiency be implemented. Unlike other building envelope components that have experienced efficiency improvements over the years, slab edge heat loss has largely been overlooked. From our vantage point, a marketable slab edge insulation system would offer significant benefits to homeowners, builders, and the society as a whole. Conventional slab forming involves the process of digging foundation trenches and setting forms prior to the concrete pour. Conventional wood form boards (usually 2 x 10's) are supported by vertical stakes on the outer form board surface, and by supporting 'kickers' driven diagonally from the top of the form board into soil outside the trench. Typically, 2 x 10's can be used only twice before they become waste material, contributing to an additional 400 pounds of construction waste per house. Removal of the form boards and stakes also requires a follow-up trip to the jobsite by the concrete subcontractor and handling (storage/disposal) of the used boards. In the rare cases where the slab is insulated (typically custom homes with radiant floor heating), the most practical insulation strategy is to secure rigid foam insulation, such as Dow Styrofoam{trademark}, to the inside of the wooden slab edge forms. An alternative is to clad insulation to the perimeter of the slab after the slab has been poured and cured. In either case, the foam must have a 'termite strip' that prevents termites from creating hidden tunnels through or behind the foam on their way to the wall framing above. Frequently this termite strip is a piece of sheet metal that must be fabricated for each project. The above-grade portion of the insulation also needs to be coated for appearance and to prevent damage from construction and UV degradation. All these steps add time, complexity, and expense to the insulating process.

09 BIOMASS FUELS↗

USE OF CEMENTITIOUS MATERIALS FOR SRS REACTOR FACILITY IN-SITU DECOMMISSIONING - 11620

The United States Department of Energy (US DOE) concept for facility in-situ decommissioning (ISD) is to physically stabilize and isolate in tact, structurally sound facilities that are no longer needed for their original purpose of, i.e., producing (reactor facilities), processing (isotope separation facilities) or storing radioactive materials. The Savannah River Site 105-P and 105-R Reactor Facility ISD requires about 250,000 cubic yards of grout to fill the below grade structure. The fills are designed to prevent subsidence, reduce water infiltration, and isolate contaminated materials. This work is being performed as a Comprehensive Environmental Response, Compensations and Liability Act (CERCLA) action and is part of the overall soil and groundwater completion projects for P- and R-Areas. Cementitious materials were designed for the following applications: (1) Below grade massive voids/rooms: Portland cement-based structural flowable fills for - Bulk filling, Restricted placement and Underwater placement. (2) Special below grade applications for reduced load bearing capacity needs: Cellular portland cement lightweight fill (3) Reactor vessel fills that are compatible with reactive metal (aluminum metal) components in the reactor vessels: Calcium sulfoaluminate flowable fill, and Magnesium potassium phosphate flowable fill. (4) Caps to prevent water infiltration and intrusion into areas with the highest levels of radionuclides: Portland cement based shrinkage compensating concrete. A system engineering approach was used to identify functions and requirements of the fill and capping materials. Laboratory testing was performed to identify candidate formulations and develop final design mixes. Scale-up testing was performed to verify material production and placement as well as fresh and cured properties. The 105-P and 105-R ISD projects are currently in progress and are expected to be complete in 2012. The focus of this paper is to describe the (1) grout mixes for filling the reactor vessels, and (2) a specialty grout mix to fill a selected portion of the P-Reactor Disassembly Basin. Details of the grout mixes designed for ISD of he SRS Reactor Disassembly Basins and below grade portions of the 105-Buildings was described elsewhere. Material property test results, placement strategies, full-scale production and delivery systems will also be described.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

History of the Development of Liquid-Applied Coatings for Protection of Reinforced Concrete

Corrosion of reinforcing steel in concrete is an insidious problem for structures at Kennedy Space Center (KSC). KSC is located on the coast of Florida in a highly corrosive atmosphere. Launch pads, highway bridge infrastructure, and buildings are strongly affected. To mitigate these problems, NASA initiated a development program for a Galvanic Liquid-Applied Coating System (GLACS). A breakthrough in this area would have great commercial value in transportation, marine and construction industry infrastructures. The patented NASA GLACS system has undergone considerable testing to meet the needs of commercialization. A moisture-cure coating gives excellent adhesion with ease of application compared to existing galvanic products on the market. The latest development, GalvaCori; can be sprayed or hand applied to almost any structure shape. A self-adhesive conductive tape system has been devised to simplify current collection within the coating areas. In testing programs, millivolt potential and milliamp output per square foot of anode have been closely studied at actual test sites. These two parameters are probably the most challenging items of a resin-based, room-temperature-applied, galvanic coating. Extensive re-formulation has resulted in a system that provides the needed polarization for catholic protection of reinforcing steel in concrete in a variety of structure environments. The rate of corrosion of rebar in concrete is greatly affected by the environment of the structure. In addition to this, for any given concrete structure; moisture level, carbonization, and chloride contamination influences the rate of rebar corrosion. Similarly, the cathodic protection level of galvanic systems is also dependent on the moisture level of the concrete. GalvaCorr is formulated to maintain galvanic activity as the moisture level of the structure declines. GalvaCorr is available as a three-part kit. The mixing step requires about ten minutes. The viscosity can be easily adjusted to meet the application needs. The pot or working life is four to six hours, depending on the temperature. GalvaCorr can be thought of as a spray-on coating, battery ready to provide up to -1.4 volts (relative to CSE) of cathodic protection (CP) potential.

Curran, Joseph J.↗

Strategies for Developing High-Volume Fly Ash Concrete with High Early-Age Strength for Precast Applications

Partial replacement of portland cement with supplementary cementitious materials (SCMs), such as fly ash, is an effective strategy for improving durability and reducing the CO 2 footprint of concrete. However, using high-volume fly ash (HVFA) binders in precast and prestressed concrete is currently limited; largely due to reduced early-age strength development that impedes rapid production and prestressing of precast concrete. To investigate and address this challenge, HVFA mortars with a minimum of 40% fly ash by mass of cementitious materials were developed and tested in this study. Two fresh fly ashes (an ASTM C618 Class F and a Class C) and a landfilled fly ash (Class F) were included. Various strategies for improving the early strength were evaluated, including gypsum optimization, chemical accelerators, steam curing, use of CSA cements, and adding other reactive SCMs like silica fume, calcined clay, and slag cement. Steam curing and the use of CSA cement at high dosages (40% of total binder) were found to be the most successful strategies across all three fly ashes. Additionally, significant improvements were observed with gypsum optimization (for Class C fly ash) and the use of accelerators (for Class F fly ashes), and these strategies are likely to be more feasible considering later-age strength and economic viability. Interestingly, HVFA mixtures made with the landfilled fly ash used in this study were able to achieve high early strengths with water-to-cementitious materials ratio adjustment alone. As a result, these HVFA mixtures were also found to be less responsive to accelerators when compared to the fresh Class F fly ash, highlighting an important distinction between the materials despite the similarity in chemical composition.