184 records · Page 6

SimH 2 : an integrated techno-economic modeling framework for hydrogen pipeline infrastructure and network optimization

Large-scale hydrogen (H 2 ) pipeline transport design and network optimization have seldom been reported due to the lack of a cost model accounting for the relationship between transport cost and hydrogen mass flow rate. Here, this work introduced a system-level cost model for hydrogen pipeline transport at supercritical state and integrated it with an existing CO 2 pipeline network tool, SimCCS, for hydrogen-specific pipeline design and optimization. The Intermountain West (I-West) region of the U.S., historically dependent on fossil fuel-based economies, is chosen to demonstrate the capabilities of our H 2 pipeline cost model and transport network optimization platform called SimH 2 . Two scenarios are examined: one where the pipeline is not allowed to pass through disadvantaged communities and the other where it is permitted. The results highlight that incorporating disadvantaged-community constraints lead to longer pipeline routes and increased transport costs, reflecting the trade-offs involved in equitable infrastructure development. It is demonstrated that the newly developed SimH 2 tool not only enables the efficient design of H 2 transportation pipelines but also optimizes the network by accounting for local terrain and the presence of disadvantaged areas.

08 HYDROGEN

Catalytic disproportionation on carbon superstructures enables long-life, high-loading Li–S batteries

Electrocatalysis has been widely explored as an effective strategy to accelerate polysulfide (PS) conversion and suppress the shuttle effect in lithium–sulfur (Li–S) batteries. However, the underlying mechanisms remain elusive, and electrocatalytic reactions are inactive during cell resting. In this work, we reveal and quantitatively analyze a previously unrecognized sulfur reduction route (SRR) driven by catalytic disproportionation at the carbon cathode surface—fundamentally distinct from conventional electrocatalysis. Unlike conventional stepwise pathways, this SRR enables high-order polysulfides (Sₓ²⁻, x = 5–8) to directly convert into S₈ and Li₂S₂, bypassing low-order intermediates. This sulfur-reduction shortcut is systematically elucidated through high-performance liquid chromatography, revealing the intrinsic catalytic contribution of carbon frameworks and the dynamic evolution of PS species. We demonstrate that carbon superstructures (CSS-0.5), assembled from nanosheet subunits with abundant N/O functionalities and interconnected charge-migration channels, synergistically promote this catalytic process. Benefiting from these features, CSS-0.5 delivers superior electrochemical performance under practical conditions, enabling high sulfur loading (6.0 mg cm⁻²) pouch cells with 80.5% capacity retention over 210 cycles. This study provides the first quantitative evidence of electrocatalytic disproportionation in Li–S batteries, offering mechanistic insights and design principles for advanced sulfur cathodes.

25 ENERGY STORAGE

Anode-less Solid-State Li–S Batteries Enabled by Fe-Stabilized Polysulfides

Anode-less solid-state lithium-sulfur batteries (SSLSBs) with lithium sulfide (Li 2 S) as the cathode promise a high energy density and ease of manufacturing. However, Li 2 S is plagued by poor conductivity, sluggish activation kinetics, and a poor cycle life. Here, in this study, we report an FeCl 3 -activated Li 2 S (FLS) cathode with solid-state polysulfide intermediates generated through a redox reaction between FeCl 3 and Li 2 S. This strategy is shown to boost the electrical conductivity of Li 2 S by 7 orders of magnitude and lower the activation barrier. During cycling, Fe plays a significant role in stabilizing the highly active polysulfide species, contributing to the exceptional electrochemical performance. The FLS cathode achieves 80% capacity retention over 500 cycles with >99% Li 2 S utilization. Furthermore, a Li-metal-free (anode-less) full cell retained over 80% of its initial capacity after 240 cycles. This work underscores the promise of leveraging Fe-stabilized polysulfides in enabling high-energy, long-lasting, solid-state Li-S batteries.

25 ENERGY STORAGE

Making Plasticized Polymer Electrolytes Stable Against Sodium Metal for High‐Energy Solid‐State Sodium Batteries

Solid polymer electrolytes based on plastic crystals are promising for solid-state sodium metal (Na 0 ) batteries, yet their practicality has been hindered by the notorious Na 0 -electrolyte interface instability issue, the underlying cause of which remains poorly understood. Here, in this study, by leveraging a model plasticized polymer electrolyte based on conventional succinonitrile plastic crystals, we uncover its failure origin in Na 0 batteries is associated with the formation of a thick and non-uniform solid electrolyte interphase (SEI) and whiskery Na 0 nucleation/growth. Furthermore, we design a new additive-embedded plasticized polymer electrolyte to manipulate the Na 0 deposition and SEI formulation. For the first time, we demonstrate that introducing fluoroethylene carbonate (FEC) additive into the succinonitrile-plasticized polymer electrolyte can effectively protect Na 0 against interfacial corrosion by facilitating the growth of dome-like Na 0 with thin, amorphous, and fluorine-rich SEIs, thus enabling significantly improved performances of Na//Na symmetric cells (1,800 h at 0.5 mA cm −2 ) and Na//Na 3 V 2 (PO 4 ) 3 full cells (93.0 % capacity retention after 1,200 cycles at 1 C rate in coin cells and 93.1 % capacity retention after 250 cycles at C/3 in pouch cells at room temperature). Our work provides valuable insights into the interfacial failure of plasticized polymer electrolytes and offers a promising solution to resolving the interfacial instability issue.

25 ENERGY STORAGE

Self-Healing Lithium Dendrites through Spontaneous Passivating Layer Formation for Stable Solid-State Lithium–Metal Batteries

All-solid-state lithium–metal batteries have attracted significant attention, owing to their high energy density and superior safety. However, lithium–metal penetration through the solid electrolyte, leading to short-circuiting, remains a critical failure mode that demands comprehensive mitigation strategies. Most existing strategies are effective only prior to the initiation of lithium-dendrite formation and fail once dendrites begin to propagate through the electrolyte. In this study, we propose a self-healing mechanism in which the penetrated lithium reacts with a self-healing agent to form a passivating layer along the particle boundaries. Lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) was incorporated into a Li 6 PS 5 Cl solid electrolyte as the self-healing agent to suppress lithium-dendrite propagation even after dendrite formation initiated under high current densities. The self-healing induced by LiTFSI was verified through comprehensive experimental analyses and was further demonstrated in a full-cell configuration. Moreover, LiTFSI incorporation plays an important role in increasing the critical current density by reducing the overall electronic conductivity of the solid electrolyte and facilitating the formation of a robust LiF-containing solid-electrolyte interphase.

25 ENERGY STORAGE

Revealing the Roles of CuF 2 /NiF 2 Incorporation in the Electrochemical Performance of FeF 3 Cathodes in Solid‐State Batteries

Mixed metal fluorides have been considered as a promising candidate to lower the voltage hysteresis of conversion-type iron fluoride cathodes, but their cycling stability is limited due to transition metal dissolution and interphase growth in liquid electrolyte batteries. Here, we study the role of incorporating CuF 2 and NiF 2 in the electrochemical performance of FeF 3 cathode in halide-based solid-state batteries to test whether we can transfer the kinetic benefit of low voltage hysteresis to solid-state batteries while using solid electrolyte to eliminate transition metal dissolution and stabilize the interphase. Synchrotron X-ray absorption spectroscopy results indicated the redox reactions are attributed to Cu 0 /Cu + and Fe 0 /Fe 2+ in 25CuF 2 -75FeF 3 and Ni 0 /Ni 2+ and Fe 0 /Fe 3+ in 10NiF 2 -90FeF 3 . While no apparent improvement in electrode kinetics can be observed, the incorporation of CuF 2 and NiF 2 can largely improve the cycling stability of FeF 3 cathodes. In conclusion, the results demonstrate the advantages of using solid-state concept to improve the cycling stability of conversion-type cathodes.

25 ENERGY STORAGE

Selectivity mechanisms of ion intercalation in Prussian blue analogs

Prussian blue analogs (PBAs) are a family of materials with facile, reversible, and selective ion transport capability for various ions via electrochemical intercalation, owing to their vacancy structure. The large tunable compositional space of PBAs allows for manipulation of intercalation behavior and selectivity by controlling structural vacancy level through choice of transition metal centers and modifications to the synthesis process. However, a lack of understanding of the mechanisms of ion selectivity hinders the material’s design process. Here, for this work, we investigated the origins of ion selectivity using a model PBA, copper hexacyanoferrate, and focused on eight technologically and biologically prominent ions, for which we determined a sequence of selectivity: Rb + > K + > Na + > Ba 2+ > Sr 2+ ≈ Ca 2+ > Mg 2+ > Li + . We provide electrochemical, structural, and redox evidence of strong correlation between the ion identity, the dominant charge-compensating redox, and preferred occupancy site. Specifically, using synchrotron anomalous X-ray diffraction (AXRD), we reveal that monovalent ions exhibit significant association with the corner sites of the unit cell and iron redox, whereas divalent ions display affinity toward the center site with higher ratios of copper redox. Informed by selectivity results, we applied CuHCFe to Li purification and achieved 99.9% purity. Our findings demonstrate an approach to elucidating ion intercalation behavior in order to distinguish and manipulate material properties to optimize separation performance.

Prussian blue analog

Polycarbonate‐Based Solid‐Polymer Electrolytes for Solid‐State Sodium Batteries

Solid-polymer electrolytes comprised of polypropylene carbonate (PPC) and varied sodium bis(fluorosulfonyl)imide (NaFSI) salt concentrations are investigated for implementation as a conductive solid polymer electrolyte into solid-state cathode composites utilizing a sodium-layered oxide active material. The ionic conductivity generally increases with NaFSI salt content, reaching ≈1 mS cm −1 at 80 °C at the highest salt concentration (PPC:NaFSI = 0.5:1). Through an all-in-one slurry casting method, Na 2/3 Ni 1/3 Mn 2/3 O 2 cathode composites are fabricated in which the dispersed PPC electrolyte acts as the primary binder. Enabled by a bilayer polymer electrolyte system, cycling performance with the PPC cathode electrolyte is optimized with respect to salt concentration and anode material. The best cyclability is achieved with a moderate salt concentration electrolyte (PPC:NaFSI = 5:1), showcasing an initial capacity of 83 mA h g −1 with a remarkable 80% capacity retention after 150 cycles at C/5 rate and 60 °C. The superior performance of the lower salt concentration electrolyte is attributed to better electrochemical stability, as confirmed by linear sweep voltammetry and online electrochemical mass spectrometry measurements. In conclusion, these results underscore the potential of carbonate-based polymer electrolytes and the importance of balancing electrolyte conductivity and stability in cell design.

25 ENERGY STORAGE

Flexible and Extensive Platinum Ion Gel Condensers for Programmable Catalysis

Catalytic condensers composed of ion gels separating a metal electrode from a platinum-on-carbon active layer were fabricated and characterized to achieve more powerful, high surface area dynamic heterogeneous catalyst surfaces. Ion gels comprised of poly(vinylidene difluoride)/1-ethyl-3-methylimidazolium bis(trifluoromethylsulfonyl) imide were spin coated as a 3.8 μm film on a Au surface, after which carbon sputtering of a 1.8 nm carbon film and electron-beam evaporation of 2 nm Pt clusters created an active surface exposed to reactant gases. Electronic characterization indicated that most charge condensed within the Pt nanoclusters upon application of a potential bias, with the condenser device achieving a capacitance of ∼20 μF/cm 2 at applied frequencies of up to 120 Hz. The maximum charge of ∼10 14 |e – | cm –2 was condensed under stable device conditions at 200 °C on catalytic films with ∼10 15 sites cm –2 . Grazing incidence infrared spectroscopy measured carbon monoxide adsorption isobars, indicating a change in the CO* binding energy of ∼19 kJ mol –1 over an applied potential bias of only 1.25 V. Condensers were also fabricated on flexible, large area Kapton substrates allowing stacked or tubular form factors that facilitate high volumetric active site densities, ultimately enabling a fast and powerful catalytic condenser that can be fabricated for programmable catalysis applications.

Catalysis

Speciation of Transition Metal Dissolution in Electrolyte from Common Cathode Materials

Significant capacity loss has been observed across extended cycling of lithium-ion batteries cycled to high potential. One of the sources of capacity fade is transition metal dissolution from the cathode active material, ion migration through the electrolyte, and deposition on the solid-electrolyte interphase on the anode. While much research has been conducted on the oxidation state of the transition metal in the cathode active material or deposited on the anode, there have been limited investigations of the oxidation state of the transition metal ions dissolved in the electrolyte. Here, in this work, X-ray absorption spectroscopy has been performed on electrolytes extracted from cells built with four different cathode active materials (LiMn 2 O 4 (LMO), LiNi 0.5 Mn 1.5 O 4 (LNMO), LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), and (x Li 2 MnO 3 *(1-x) LiNi a Mn b Co c O 2 , with a+b+c=1) (LMRNMC)) that were cycled at either high or standard potentials to determine the oxidation state of Mn and Ni in solution. Inductively coupled plasma-mass spectrometry has been performed on the anodes from these cells to determine the concentration of deposited transition metal ions. While transition metal ions were found dissolved in all electrolytes, the oxidation state(s) of Mn and Ni were determined to be dependent on the cathode material and independent of cycling potential.

25 ENERGY STORAGE

High Sulfur Loading and Capacity Retention in Bilayer Garnet Sulfurized‐Polyacrylonitrile/Lithium‐Metal Batteries with Gel Polymer Electrolytes

The cubic‐garnet (Li 7 La 3 Zr 2 O 12 , LLZO) lithium–sulfur battery shows great promise in the pursuit of achieving high energy densities. The sulfur used in the cathodes is abundant, inexpensive, and possesses high specific capacity. In addition, LLZO displays excellent chemical stability with Li metal; however, the instabilities in the sulfur cathode/LLZO interface can lead to performance degradation that limits the development of these batteries. Therefore, it is critical to resolve these interfacial challenges to achieve stable cycling. Here, an innovative gel polymer buffer layer to stabilize the sulfur cathode/LLZO interface is created. Employing a thin bilayer LLZO (dense/porous) architecture as a solid electrolyte and significantly high sulfur loading of 5.2 mg cm −2 , stable cycling is achieved with a high initial discharge capacity of 1542 mAh g −1 (discharge current density of 0.87 mA cm −2 ) and an average discharge capacity of 1218 mAh g −1 (discharge current density of 1.74 mA cm −2 ) with 80% capacity retention over 265 cycles, at room temperature (22 °C) and without applied pressure. Achieving such stability with high sulfur loading is a major step in the development of potentially commercial garnet lithium–sulfur batteries.

25 ENERGY STORAGE

Design and Synthesis of Cubic K 3−2 x Ba x SbSe 4 Solid Electrolytes for K–O 2 Batteries

Developing K-ion conducting solid-state electrolytes (SSEs) plays a critical role in the safe implementation of potassium batteries. In this work, a chalcogenide-based potassium ion SSE is reported, K 3 SbSe 4 , which adopts a trigonal structure at room temperature. Single-crystal structural analysis reveals a trigonal-to-cubic phase transition at the low temperature of 50 °C, which is the lowest among similar compounds and thus provides easy access to the cubic phase. The substitution of barium for potassium in K 3 SbSe 4 leads to the creation of potassium vacancies, expansion of lattice parameters, and a transformation from a trigonal phase to a cubic phase. As a result, the maximum conductivity of K 3−2x Ba x SbSe 4 reaches around 0.1 mS cm −1 at 40 °C for K 2.2 Ba 0.4 SbSe 4 , which is over two orders of magnitude higher than that of undoped K 3 SbSe 4 . This novel SSE is successfully employed in a K–O 2 battery operating at room temperature where a polymer-laminated K 2.2 Ba 0.4 SbSe 4 pellet serves as a separator between the oxygen cathode and the potassium metal anode. Effective protection of the K metal anode against corrosion caused by O 2 is demonstrated.

25 ENERGY STORAGE

Fabrication of Large-Area Metal-on-Carbon Catalytic Condensers for Programmable Catalysis

Catalytic condensers stabilize charge on either side of a high-k dielectric film to modulate the electronic states of a catalytic layer for the electronic control of surface reactions. Here, carbon sputtering provided for fast, large-scale fabrication of metal–carbon catalytic condensers required for industrial application. Carbon films were sputtered on HfO 2 dielectric/p-type Si with different thicknesses (1, 3, 6, and 10 nm), and the enhancement of conductance and capacitance of carbon films was observed upon increasing the carbon thickness following thermal treatment at 400 °C. After Pt deposition on the carbon films, the Pt catalytic condenser exhibited a high capacitance of ∼210 nF/cm 2 that was maintained at a frequency ∼1000 Hz, satisfying the requirement for a dynamic catalyst to implement catalytic resonance. Temperature-programmed desorption of carbon monoxide yielded CO desorption peaks that shifted in temperature with the varying potential applied to the condenser (−6 or +6 V), indicating a shift in the binding energy of carbon monoxide on the Pt condenser surface. A substantial increase in capacitance (∼2000 nF/cm 2 ) of the Pt-on-carbon devices was observed at elevated temperatures of 400 °C that can modulate ∼10% of charge per metal atom when 10 V potential was applied. A large catalytic condenser of 42 cm 2 area Pt/C/HfO 2 /Si exhibited a high capacitance of 9393 nF with a low leakage current/capacitive current ratio (<0.1), demonstrating the practicality and versatility of the facile, large-scale fabrication method for metal–carbon catalytic condensers.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH

Nuclear Safety [Vol. 37, No. 2, April-June 1996]

Nuclear Safety is a journal that covers significant issues in the field of nuclear safety. Its primary scope is safety in the design, construction, operation, and decommissioning of nuclear power reactors worldwide and the research and analysis activities that promote this goal, but it also encompasses the safety aspects of the entire nuclear fuel cycle, including fuel fabrication, spent-fuel processing and handling, and nuclear waste disposal, the handling of fissionable materials and radioisotopes, and the environmental effects of all these activities. Table of Contents for this issue follows. GENERAL SAFETY CONSIDERATIONS: 97 The Nuclear Community and the Public: Cognitive and Cultural Influences on Thinking About Nuclear Risk, M. A. Meyer; 109 Twenty-Third Water Reactor Safety Information Meeting, D. A. Copinger; ACCIDENT ANALYSIS: 126 Analysis of a PWR LBLOCA Without SCRAM, Trevor N. Tyler, Rafael Macian-Juan and John H. Mahaffy; DESIGN FEATURES: 139 Vulnerability of Multiple-Barrier Systems, N. C. Lind; ENVIRONMENTAL EFFECTS: 149 A Study of Wet Catalytic Oxidation of Radioactive Spent Ion Exchange Resin by Hydrogen Peroxide, Xingchao Jian, Tianbao Wu, and Guichun Yun; 157 A Comparison Study and Resolution of Differences Between Emergency Response and Safety Analysis Codes Used at the Savannah River Site, A. A. Simpkins; OPERATING EXPERIENCES: 164 Reactor Shutdown Experience, Compiled by J. W. Cletcher; RECENT DEVELOPMENTS: 167 Reports, Standards, and Safety Guides, D. S. Queener; 172 Proposed Rule Changes as of Dec. 31,1995; ANNOUNCEMENTS: 178 American Nuclear Society 1997 Annual Meeting; 178 American Nuclear Society Nuclear Criticality and Safety Division Topical Meeting; 176 The Authors.

05 NUCLEAR FUELS

Tailored Solvent Treatment for Optimized Production of Upcycled Anodes from End-Of-Life Li-Ion Batteries

Recycling processes for lithium-ion batteries typically overlook graphite because of its lower market value relative to that of transition-metal-containing cathode materials. However, graphite recovered from cycled lithium-ion batteries holds additional engineered value associated with the solid-electrolyte interphase (SEI). The SEI contributes critical electronic passivation of the graphite surface but becomes highly resistive with extended cycling, yielding poor cell performance. In this work, we apply tailored solvent treatment to end-of-life (EOL) graphite anodes to selectively remove adverse SEI components while retaining beneficially passivating species. We evaluate a series of polar protic solvents to achieve targeted removal of SEI components and control selectivity through rational variation in solvent properties. The physiochemical properties of treatment solvents correlate with both the retained SEI composition and the corresponding electrochemical performance of solvent-treated “upcycled” graphite anodes. Within the initial set of solvents evaluated, top-performing candidates show capacity and Coulombic efficiency nearly equivalent to those of an analogous pristine anode, as well as promising electrochemical performance enhancement with regard to irreversible capacity-loss metrics. This study establishes critical design principles for an optimized anode upcycling method that enhances the value of recycled graphite by retaining and upgrading the SEI.

25 ENERGY STORAGE

Nuclear Safety [Vol. 37, No. 1, January-March 1996]

Nuclear Safety is a journal that covers significant issues in the field of nuclear safety. Its primary scope is safety in the design, construction, operation, and decommissioning of nuclear power reactors worldwide and the research and analysis activities that promote this goal, but it also encompasses the safety aspects of the entire nuclear fuel cycle, including fuel fabrication, spent-fuel processing and handling, and nuclear waste disposal, the handling of fissionable materials and radioisotopes, and the environmental effects of all these activities. Table of Contents for this issue follows. GENERAL SAFETY CONSIDERATIONS: 1 A Decision Support System for Maintenance Management of a Boiling-Water Reactor Power Plant, J. H. Shen, A. Ray, and S. Levine; ACCIDENT ANALYSIS: 12 On Prediction of the Ignition Potential of Uranium Metal and Hydride, M. Epstein, W. Luangdilok, M. G. Plys, and H. K. Fauske; 26 An Overview of the Primary Parameters and Methods for Determining Condensation Heat Transfer to Containment Structures, J. Green and K. Almenas; DESIGN FEATURES: 49 Modem Tornado Design of Nuclear and Other Potentially Hazardous Facilities, J. D. Stevenson and Y. Zaho; U.S. NUCLEAR REGULATORY COMMISSION INFORMATION AND ANALYSES: 73 1994 Accident Sequence Precursor Program Results, R. J. Belles, J. W. Cletcher, D. A. Coplnger, B. W. Dolan, J. W. Minarick, and P. D. O'Reilly; ANNOUNCEMENTS: 93 American Institute of Chemical Engineers (AlChE) Spring 1997 National Meeting; 94 European Safety and Reliability Association International Conference on Safety and Reliability ESREL ’97; 95 Criticality Safety Challenges in the Next Decade; 96 21st International Symposium on the Scientific Basis for Nuclear Waste Management; 84 The Authors; 88 Letter to the Editor; 90 Indexes to Nuclear Safety, Volume 36.

05 NUCLEAR FUELS

Interface Design for High‐Performance All‐Solid‐State Lithium Batteries

All‐solid‐state batteries suffer from high interface resistance and lithium dendrite growth leading to low Li plating/stripping Coulombic efficiency (CE) of <90% and low critical current density at high capacity. Here, in this work, both challenges are simultaneously addressed and the Li plating/stripping CE is significantly increased to 99.6% at 0.2 mA cm −2 /0.2 mAh cm −2 , and critical current density (CCD) of > 3.0 mA cm −2 /3.0 mAh cm −2 by inserting a mixed ionic‐electronic conductive (MIEC) and lithiophobic LiF‐C‐Li 3 N‐Bi nanocomposite interlayer between Li 6 PS 5 Cl electrolyte and Li anode. The highly lithiophobic LiF‐C‐Li 3 N‐Bi interlayer with high ionic conductivity (10 −5 S cm −1 ) and low electronic conductivity (3.4×10 −7 S cm −1 ) enables Li to plate on the current collector (CC) surface rather than on Li 6 PS 5 Cl surface avoiding Li 6 PS 5 Cl electrolyte reduction. During initial Li plating on CC, Li penetrates into porous LiF‐C‐Li 3 N‐Bi interlayer and lithiates Bi nanoparticles into Li 3 Bi. The lithiophilic Li 3 Bi and Li 3 N nanoparticles in LiF‐C‐Li 3 N‐Li 3 Bi sub‐interlayer will move to CC along with plated Li, forming LiF‐C/Li 3 N‐Li 3 Bi lithiophobic/lithiophilic sublayer during the following Li stripping. This interlayer enables Co 0.1 Fe 0.9 S 2 /Li 6 PS 5 Cl/Li cell with an areal capacity of 1.4 mAh cm −2 to achieve a cycle life of >850 cycles at 150 mA g −1 . The lithiophobic/lithiophilic interlayer enables solid‐state metal batteries to simultaneously achieve high energy and long cycle life.

25 ENERGY STORAGE