Search NASA⌕ Search

SEARCH · Search NASA

Results for “Dilatometry”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Crystal structure and phase transitions of Sr{sub 2}Ni{sub 1–y}Mg{sub y}MoO{sub 6} solid solutions

Sr{sub 2}Ni{sub 1–y}Mg{sub y}MoO{sub 6} mixed oxides with a double perovskite structure have been synthesized via the pyrolysis of glycerol–salt mixtures. The phase composition and structure of the samples have been determined using X-ray diffraction and Raman spectroscopy. The temperatures of phase transitions in Sr{sub 2}Ni{sub 1–y}Mg{sub y}MoO{sub 6} with y = 0.25, 0.5, and 0.75 have been determined by high-temperature X-ray diffraction and dilatometry.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Formation of voids and secondary-phase precipitates in the Fe-16Cr-15Ni-2Mo-1Mn-Ti-Si steel under high-doze neutron irradiation and during post-irradiation annealing

The effect of high-dose neutron irradiation on the structural changes in Fe-16Cr-15Ni-2Mo-1Mn-Ti-Si austenitic steel have been investigated. Samples irradiated at temperatures of 390, 500, and 600{sup o} to damage doses of 46, 86, and 46 dpa, respectively, were analyzed by electron microscopy and dilatometry. The quantitative characteristics of radiation voids and secondary-phase precipitates formed under neutron irradiation are obtained. Their behavior upon heating to 700{sup o}C and annealing at this temperature for 2 h is studied. It is shown that annealing leads to the dissociation of small voids, which is accompanied by the growth of large ones. The secondary-phase precipitates are partially dissolved upon annealing, and their volume fraction decreases.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Single crystals of (FeIn{sub 2}S{sub 4}){sub x} · (CuIn{sub 5}S{sub 8}){sub 1–x} alloys: Crystal structure, nuclear gamma resonance spectra, and thermal expansion

FeIn{sub 2}S{sub 4} and CuIn{sub 5}S{sub 8} compounds and (FeIn{sub 2}S{sub 4}){sub x} · (CuIn{sub 5}S{sub 8}){sub 1–x} alloy single crystals are grown by planar crystallization. It is shown that both of the initial FeIn{sub 2}S{sub 4} and CuIn{sub 5}S{sub 8} compounds and alloys on their basis crystallize with the formation of the cubic spinel structure. It is established that the unit-cell parameter a linearly varies with the composition parameter x. By means of nuclear gamma resonance spectroscopy in the transmission mode of measurements, the local states of iron ions in the alloys are studied. For the single crystals grown in the study, thermal expansion is explored using the dilatometry technique, the thermal-expansion coefficients are determined, and the Debye temperature and rms (root-mean-square) dynamic displacements are calculated.

36 MATERIALS SCIENCE↗

The Thermal Expansion of Ag{sub x}Pb{sub 1 –} {sub x}S Limited Semiconductor Solid Solutions

One-phase powders of Ag{sub x}Pb{sub 1 –} {sub x}S cubic solid solutions with a maximum relative silver content to x = 0.12 were synthesized via the chemical codeposition from lead acetate and silver nitrate aqueous solutions in the presence of sulphidizer, as well as complexing and stabilizing agents. The thermal expansion of produced semiconductor solid solutions was first measured via the dilatometry in a temperature range of 295–580 K. As shown, substituting silver atoms for lead in Ag{sub x}Pb{sub 1 –} {sub x}S results in a slight decrease in thermal expansion value, because of alterations in unharmonism of atomic vibrations.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Temperature Dependent Tensile Fracture Stress of n- and p-Type Filled-Skutterudite Materials

While materials with excellent thermoelectric performance are most desirable for higher heat to electrical energy conversion efficiency, thermoelectric materials must also be sufficiently mechanically robust to withstand the large number of thermal cycles and vibrational stresses likely to be encountered while in service, particularly in automotive applications. Further these TE materials should be composed of non-toxic and naturally abundant constituent elements and be available as both n- and p-type varieties. Skutterudite based thermoelectric materials seemingly fit this list of criteria. In this contribution we report on the synthesis, tensile fracture strengths, low temperature electrical and thermal transport properties, and coefficients of thermal expansion (CTE), of the n-type skutterudite La{sub 0.05({+-}0.01)}Ba{sub 0.07({+-}0.04)}Yb{sub 0.08({+-}0.02)}Co{sub 4.00({+-}0.01)}Sb{sub 12.02({+-}0.03)} and the p-type Ce{sub 0.30({+-}0.02)}Co{sub 2.57({+-}0.02)}Fe{sub 1.43({+-}0.02)}Sb{sub 11.98({+-}0.03)}. Both materials have tensile fracture strengths that are temperature independent up to 500 C, and are in the range of {approx}140 MPa as measured by a three point bend flexure test fixture described herein. The CTE's were measured by dual rod dilatometry and were determined to be 10.3 ppm/C for the n-type material and 11.5 ppm/C for p-type up to 450 C.

36 MATERIALS SCIENCE↗

Digital Manufacturing of Gradient Meshed SOFC Sealing Composites with Self-Healing Capabilities

Solid oxide fuel cells (SOFC) hold great promise for clean power generation. However, high temperature stability and long term durability of the SOFC components have presented serious problems in SOFC technological advancement and commercialization. The seals of the fuel cells are the most challenging area to address. A high temperature gas seal is highly needed which is durable against cracking and gas leakage during thermal cycling and extended operation. This project investigates a novel composite seal by integrating 3D printed shape memory alloy (SMA) wires into a glass matrix. The SMA we use is TiNiHf and the glass matrix we use is SrO-La{sub 2}O{sub 3}-Al{sub 2}O{sub 3}-B{sub 2}O{sub 3}-SiO{sub 2} (SLABS). Dilatometry shows to be an extremely useful tool in providing the CTEs. It pinpoints regions of different CTEs under simulated SOFC thermal cycles for the same glass. For the studied SLABS glass system, the region with the greatest CTE mismatch between the glass seal and the adjacent components is 40-500 C, the typical heating and cooling regions for SOFCs. Even for low temperature SOFC development, this region is still present and needs to be addressed. We have demonstrated that the proposed SLABS glass has great potential in mitigating the thermal expansion mismatch issues that are limiting the operation life of SOFCs. TiNiHf alloy has been successfully synthesized with the desired particle size for the 3DP process. The TiNiHf SMA shape memory effect very desirably overlaps with the problematic low CTE region of the glass. This supports the design intent that the gradient structure transition, phase transformation toughening, and self-healing of the SMA can be utilized to mitigate/eliminate the seal problem. For the 3DP process, a new binder has been identified to match with the specific chemistry of the SMA particles. This enables us to directly print SMA particles. Neutron diffraction shows to be an extremely useful tool in providing information regarding the austenite to martensite phase transformation, SMA alloy lattice constant change, and the corresponding thermal stress from the glass matrix. It pinpoints regions of SMA phase transformation and the thermal stress effect under simulated SOFC thermal cycles. The bilayer test shows that there is still much work to be done for the proper integration of the seal components. Large scale production should lower the cost associated with the proposed approach, especially on the raw material cost and 3D printing.

30 DIRECT ENERGY CONVERSION↗

Multi Scale Study of Self-irradiation Effects in Plutonium Alloys

Experimental measurements have shown that plutonium alloys exhibit changes of their macroscopic as well as microscopic properties. For example, a swelling of plutonium alloys was observed with aging with dilatometry and X-ray diffraction. The main idea to explain these changes rises in self irradiation undergoing by those materials. Plutonium {alpha} decay is at the origin of displacements cascades creating a large amount of structural defects. These later by annihilation and recombination give rise to larger defects such as voids and clusters. The aim of this work is to study the occurrence of such phenomena combining ab-initio, molecular dynamic and Monte Carlo methods in a coherent multi-scale approach which would help to understand long term behavior of structural defects and consequences of self irradiation. We show that plutonium does not seem to behave like other metals under ion irradiation. We discuss results obtained for high energy displacements cascade simulations. After parametric study of displacements cascade simulations combining temperature and cascade energy has been exposed, superposition of low energies displacements cascades is discussed as a method to construct realistic defect microstructures and to reach a rational use of computational time. At the end, we will present results of preliminary Monte Carlo simulations based on our molecular dynamic data which show that the spatial correlation of the stable defects populations created by the cascades seems to have a great influence on the predicted swelling. (authors)

36 MATERIALS SCIENCE↗

Cementitious Grouts for ILW Encapsulation - Hydration and Continuity of Supply within the UK - 16184

In the UK the preferred route to disposal for the majority of intermediate level nuclear waste (ILW) streams is encapsulation within a cementitious matrix, accounting for 83% of waste conditioned to date (NDA, 2013). The method is well-defined and produces a waste package that is both chemically and physically stable, providing a multi-layered barrier to the release of the waste species contained within. Due to the process of treatment, facilitated via remote operation, it is necessary for the grouting matrices to meet strict performance limits in terms of their flow, setting time and avoidance of the formation of bleed water or segregation. To this end, the limits on composition of the anhydrous materials (a mixture of ordinary Portland cement [OPC] and blast furnace slag [BFS]) are tight to ensure conformity. Whilst these limits on composition are well understood, their impact upon grout hydration, and hence performance, is poorly defined. This study investigates the effects of modifying the physical and chemical composition of both the OPC and the BFS components of the matrix in order to identify the sensitivity or otherwise of the system to ensure that a continuity of supply is maintained. A number of techniques, scanning electron microscopy - image analysis (SEM-IA), chemical shrinkage (measured via dilatometry), isothermal conduction calorimetry (ICC), thermogravimetric analysis (TGA) and X-ray diffraction (XRD), have been applied to assess the rate and degree of hydration (DoH) of a range of grouts prepared with OPC and BFS with a range of chemical and physical compositions. This has been coupled with subsequent engineering performance testing, with additional analysis to understand the impact of a fire scenario within a storage or disposal facility, to provide an indication towards the resilience of the waste packages to a potential catastrophic event. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

DEVELOPMENT OF AN IN-PILE TECHNIQUE FOR THERMAL CONDUCTIVITY MEASUREMENT

Thermophysical properties of advanced fuels and materials during irradiation must be known prior to their use in existing, advanced, or next generation reactors. Fuel thermal conductivity is one of the most important properties for predicting fuel performance and reactor safety. This paper discusses a joint Utah State University (USU)/Idaho National Laboratory (INL) project to investigate an in-pile fuel thermal conductivity measurement technique using a surrogate fuel rod. The method used a surrogate fuel rod with Joule heating to simulate volumetric heat generation as a proof-of-concept test in-pile application. Carbon structural foam, CFOAM®, a product of Touchtone Research Laboratory was chosen as the surrogate material because of the variable electrical and thermal properties upon fabrication. To stay within the surrogate fuel rod requirements, electrical and thermal properties were tailored by Touchtone Research Laboratory to match required values. This paper describes are the techniques used for quantifying thermal conductivity. A description of the test setup and preliminary results are presented. Two thermocouples are inserted into a 1-inch diameter, 6-inch long rod of CFOAM® at known locations. Knowing the applied volumetric heat to the rod by electrical resistance heating, the thermal conductivity can be calculated. Sensitivities of this measurement can also found by analysis and testing of different configurations of the sample setup. Verification of thermal conductivity is found by measuring the thermal properties of the CFOAM® using different methods. Thermal properties including thermal conductivity, specific heat capacity, and expansion coefficient of two types of CFOAM®, CFOAM20 and CFOAM25, were characterized using standard measurement techniques, such as laser flash, differential scanning calorimetry, and pushrod dilatometry.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Magnetostriction and thermal expansion on 1D quantum spin system azurite

Recently the natural mineral Azurite has been proposed as model substance for the distorted S = 1/2 diamond chain in the spin fluid state. Azurite has alternating doublet monomers and singlet dimers along the chains yielding plateau-like features in the magnetization curves. Although Azurite was also reported to order antiferromagnetically at 1.86 K, the detailed phase diagram and its relationship to the 1/3 plateau is largely unknown. In the present paper, we report preliminary results from a dilatometry study on Azurite carried out in the 0.05--2.30 K temperature range at magnetic fields up to 31 T. It is shown that sizable structural distortions accompany the magnetic ordering and that at 100 mK the long range order between monomers is suppressed precisely at the transition field where the 1/3 plateau sets in.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Giant Magnetostriction in Ferrimagnetic SmFe 5 As 3

Magnetostrictive materials are of interest not only from a fundamental perspective but also for their potential applications, spanning spintronics to energy harvesting. A new magnetostrictive material—SmFe 5 As 3 —reveals a complex interplay between magnetostriction, magnetic properties, and the crystal structure behavior. The ground state of SmFe 5 As 3 is ferrimagnetic, as evidenced by magnetic susceptibility data, band-structure calculations, and XANES measurements. At T m1 = 28 ± 4 K, part of the Fe sublattice reorients, transitioning into a ferromagnetic state. This is followed by an entrance into the paramagnetic state at T m2 = 76 ± 4 K. The effects observed in the magnetic measurements are accompanied by structural phase transitions. All three phases—below T m1 , between T m1 and T m2 , and above T m2 —are described by the same structural motif of the UCr 5 P 3 type (monoclinic space group P2 1 /m), differing only in the degree of deformation of the Fe–As framework. The new material exhibits giant magnetostriction of 2500 x 10 -6 . Dilatometry measurements on a SmFe 5 As 3 single crystal indicate strongly diverse behavior, exhibiting not only negative, but also zero, as well as positive thermo-elastic effects.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Austenite Formation and Manganese Partitioning during Double Soaking of an Ultralow Carbon Medium‐Manganese Steel

Double soaking (DS) is a thermal processing route intended to produce austenite–martensite microstructures in steels containing austenite‐stabilizing additions and consists of intercritical annealing (primary soaking), followed by heating and brief isothermal holding at an increased temperature (secondary soaking), and quenching. Herein, experimental dilatometry during DS of a medium‐manganese (Mn) steel with nominally 7 wt% Mn and an ultralow residual carbon concentration, in combination with phase‐field simulations of austenite formation during secondary soaking, is presented. The feasibility of maintaining heterogeneous Mn distributions during DS is demonstrated and insight is provided on the effects of the secondary soaking temperature and prior Mn distribution on the ferrite‐to‐austenite phase transformation during the secondary soaking portion of the DS treatment.

36 MATERIALS SCIENCE↗

Formation of the {gamma}ʹʹʹ-Ni2(Cr, Mo, W) phase during a two-step aging heat treatment in HAYNES® 244® Alloy

Precipitation hardening is the dominant method of achieving high strength in most Ni-based superalloys. The formation of nanoscale precipitates during thermal exposure is often studied to determine the optimal methods of attaining high strength. The commercial Ni-based superalloy, HAYNES® 244® alloy, is strengthened through a novel -Ni2(Cr, Mo, W) intermetallic phase that forms during a two-step aging cycle. The precipitation kinetics of this intermetallic phase are sluggish for single-step aging in comparison to the γʹ phase in precipitation-strengthened Ni-based alloys, but a two-step aging treatment has shown to reliably harden the alloy and improve high-temperature properties compared to a single-step aging heat treatment. To investigate the formation and coarsening of this phase, heat-treated samples of the 244 alloy were analyzed with high-energy in situ and ex situ X-ray techniques such as small angle X-ray scattering and wide angle X-ray scattering as well as Vickers micro-hardness, electron microscopy, and atom probe tomography. The relationship between hardness, aging parameters, and microstructure evolution is discussed. The enthalpy of formation and precipitate solvus temperature were determined with high-temperature differential scanning calorimetry and dilatometry analysis.

Ni-based Superalloys↗

Processing of crack-free high density polycrystalline LiTaO3 ceramics

Our work achieved high density (99.9%) polycrystalline LiTaO 3 . The keys to the high density without cracking were the use of LiF-assisted densification to maintain fine grain size as well as the presence of secondary lithium aluminate phases as grain growth inhibitors. The average grain size of the hot pressed polycrystalline LiTaO 3 is less than 5 μm, limiting residual stresses caused by the anisotropic thermal expansion. Dilatometry results clearly indicate liquid phase sintering via the added LiF sintering aid. Efficient liquid phase sintering allows densification during low temperature hot pressing. Electron microscopy confirmed the high-density microstructure. Furthermore, Rietveld analysis of neutron diffraction data revealed the presence of LiAlO 2 and LiAl 5 O 8 minority phases and negligible substitutional defect incorporation in LiTaO 3 .

36 MATERIALS SCIENCE↗

A Limit to Accelerated Free-Sintering: Nano-Phase Separation Interferes With Organic Debinding

Nano-phase separating Ni–12 at. pct Ag powders are processed via high-energy ball milling and brought into a supersaturated state with a reduction of the grain size to the nanocrystalline scale, a combination that is designed to encourage rapid densification by phase separation upon heating. This unstable powder is then characterized by dilatometry, in-situ x-ray diffraction, thermogravimetry and microstructure analysis for sintering cycles up to 940 °C. However, these powder compacts exhibit excessive pore evolution and significant macroscopic swelling caused by removal of the organic process additives. This competition of organic removal with densification is known in nanocrystalline metals, but the present study adds an additional dimension of phase separation, which shifts the dominant swelling mechanism as the formation of the second phase traps the volatilizing organics and hinders the debinding process. The creep swelling and overall loss in relative density is then dominated by the creep deformation of the second Ag phase. The interference between organic removal and low-temperature onset of consolidation represents a new challenge to efforts aimed at rapid free sintering and should guide the design of rapidly sintering alloys; specifically, the present work emphasizes the need to select alloys that have their sintering-accelerating phase separation temperature above the range where gases are evolved.

36 MATERIALS SCIENCE↗

Main Directions of Recent Works on Al-Zn-Based Alloys for Foundry Engineering

The composition and structural modification of high-aluminum zinc alloys and high-zinc aluminum alloys influence their wear properties and structural stability. The work described has been aimed at improving properties of the sand-cast Al-Zn-based foundry alloys, particularly their ductility and dimensional stability, by melt inoculation and/or change of chemical composition. In a series of studies, high-aluminum Zn-(25-26) wt.% Al-(1-2.5) wt.% Cu and high-zinc Al-(27-30) wt.% Zn-(1.5-2.5) wt.% Cu alloys have been doped with different levels of added Ti and Mn. The alloys’ structure and mechanical properties have been studied using scanning electron microscopy (SEM), light microscopy (LM), dilatometry and pin-on-disk wear measurements. A small addition of Ti introduced with Zn-4Ti master alloy leads to significant grain refinement of the high-aluminum zinc alloys. A small addition of Ti introduced with Al-3Ti-0.15C master alloy leads to significant grain refinement of the high-zinc aluminum alloys. In the ternary alloys, partially replacing Cu with Ti and/or Mn allows dimensional changes to be reduced while preserving good wear properties.

36 MATERIALS SCIENCE↗

Evolution of the Microstructure and Hardness of Fe-8Cr-2.1Mo-Si-V Die Steel at Different Cooling Rates after Hot Deformation

In this study, the effect of microstructure evolution, especially that involving the proeutectoid carbides, on hardness distribution of ledeburite steel containing 8% chromium content was investigated at different cooling rates after hot deformation. The continuous cooling transformation was carried out using a fully automatic transformation measuring apparatus under cooling rates in the range of 0.03-80 °C/s. The transformation temperatures, Ac1, Ac3 and Ms, were measured by dilatometry. A nanoindentation test was employed to evaluate the mechanical properties of the cooled specimens. The evolution of microstructure indicated that the proportion trend of the precipitated carbides was dependent on the cooling rates. In addition, a mixture of pearlite and proeutectoid carbides was observed under slow cooling rates in the range of 0.03-0.2 °C/s, for which only a martensite transformation took place in austenite, and the proeutectoid carbides precipitated negligibly at cooling rates greater than or equal to 10 °C/s. The results also showed that the nanohardness significantly decreased and then slowly increased to a stable value with increasing cooling rates, which was similar to the content trend of the carbides that precipitated during the cooling process.

36 MATERIALS SCIENCE↗