Search NASA⌕ Search

SEARCH · Search NASA

Results for “Fading”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Investigating the Chemical Reactivity of Lithium Silicate Model SEI Layers

Silicon anodes suffer from an unstable solid electrolyte interphase (SEI) layer that contributes to undesirable capacity fade with cycling. A key part to addressing this unstable SEI formation is to examine how certain components of the SEI react with the electrolyte over time. One SEI component that has not been thoroughly studied in the context of the chemical reactivity against the electrolyte is lithiated silicate. Four model silicate thin films with increasing lithium content were deposited by radio frequency (RF) magnetron sputtering to study how the lithiation of the native oxide on a silicon anode affects the chemical stability of the anode surface. SiO2, Li2Si2O5, Li2SiO3, and Li3SiOx films were exposed to 1.2 M LiPF6 in the 3:7 wt% ethylene carbonate/ethyl methyl carbonate (EC/EMC) electrolyte for periods of time that are representative of the amount of time it takes to undergo cell formations. Soaked samples were rinsed, dried, and characterized by a combination of attenuated total reflectance-infrared spectroscopy (ATR-IR), focused ion beam-secondary electron microscopy (FIB-SEM), and X-ray photoelectron spectroscopy (XPS) depth profiling. It was found that the rate of the decrease in film thickness of the silicates exposed to the electrolyte over time increases as a function of the lithium content in the thin film. This reaction involves HF etching and LiPF6 salt degradation leading to silicate loss and fluorination throughout the bulk. Understanding this chemical instability is critical to determining the overall mechanism of SEI degradation over time.

ADVANCED PROPULSION SYSTEMS,ENERGY STORAGE↗

Anodic Interfacial Evolution in Extremely Fast Charged Lithium-Ion Batteries

Interfacial reaction mechanisms at the anode/separator interface play a central role in the performance and safety of lithium-ion batteries during fast charging. We report a mechanistic study on the evolution and interactions of the aging mechanisms at the anode/separator interface in lithium cobalt oxide/graphite pouch cells charged with variable charging rates (1–6C) over 10 cycles. In situ electrochemical measurements, including voltage relaxation, Coulombic efficiency, and direct current internal resistance, indicated an incremental lithium loss until the C rates were ≤5C. A substantial capacity fade is observed in the first few cycles of fast charging, but the magnitude of capacity fade progressively diminishes with the number of cycles, indicating a suppression in the lithium deposition mechanism. Post-mortem film thickness, X-ray photoelectron spectroscopy (XPS), and scanning electron microscopy (SEM) analyses were performed to elucidate the evolution of electrolyte decomposition, the solid–electrolyte interface (SEI), lithium plating, and film fracture mechanisms with C rate. XPS measurements confirmed an increasing lithium concentration in an SEI film with an increase in the C rate. SEM images showed a growth of dendritic lithium on the anode surface from 1C to 3C. Precrack formation leading to an interfacial film fracture was observed at higher C rates. Furthermore, a differential analysis of the discharge capacity indicated a possible two-phase delithiation from the anode and reduced cathodic lithiation due to lithium loss at high C rates.

36 MATERIALS SCIENCE↗

LiNi0.8Mn0.1Co0.1O2 Thin Films Prepared by Polymer-Assisted Deposition for the Study of Cathode-Electrolyte Interphases in Lithium-Ion Batteries

High-nickel layered oxide cathodes such as LiNi0.8Mn0.1Co0.1O2 (NMC811) are critical for next-generation lithium-ion batteries (LIBs) due to their superior energy density and reduced reliance on cobalt. However, many Ni-rich cathodes suffer from rapid capacity fade and structural instability originating from complex interfacial reactions at the cathode-electrolyte interface. Traditional composite electrodes exhibit degradation mechanisms that are challenging to quantitatively understand due to additives, including binders and carbon black. In this study, we demonstrate a new synthesis approach for binder- and additive-free NMC811 thin films using polymer-assisted deposition (PAD). PAD-NMC811 are model thin-film cathodes for investigating interfacial phenomena that can be obscured in composite cathodes. Structural and chemical characterization by X-ray diffraction, soft X-ray absorption spectroscopy, and atomic force microscopy show that PAD-NMC811 films possess high phase purity, crystallinity, chemical homogeneity, and morphological uniformity. Electrochemical analyses using cyclic voltammetry and galvanostatic cycling revealed electrochemical behavior consistent with that of composite electrodes, along with a moderate capacity fade indicative of cathode-electrolyte interphase (CEI) formation. Our findings illustrate the effectiveness of PAD synthesis of thin films tailored for detailed mechanistic studies, which offer critical insights into CEI evolution and cathode degradation pathways.

25 ENERGY STORAGE↗

Prelithiated SiO x /Graphite-NMC811 Cells: Capacity Loss, Impedance Rise and Hidden Degradation Pathways Revealed Using Three-Electrode Diagnostics

Electrodes containing SiO x /graphite (Gr) materials are attractive as anodes for high-energy lithium-ion batteries. However, their mechanical deformation, electrochemical response, and impedance evolution during long-term cycling are strongly coupled, complicating accurate diagnosis of performance fade mechanisms. In this work, the behavior of electrochemically prelithiated SiO x /Gr anodes paired with NMC811 cathodes is systematically investigated using techniques that include in-situ dilatometry, three-electrode electrochemistry, and multiscale post-cycling microscopy. The SiO x /Gr electrode exhibits a maximum expansion of 49% upon lithiation to 10 mV vs Li + /Li, with 84% of the expansion and 91% of the capacity being reversible. In full cells, relatively stable cycling with only 12% capacity fade over 500 cycles is observed. Three-electrode experiments reveal cell-level impedance growth, which is dominated by the NMC811 cathode: the SiO x /Gr anode exhibits minimal net impedance rise and an initial impedance decrease at low potentials. Despite this apparent electrochemical stability, cross-sectional SEM, PFIB tomography, and cryo-STEM reveal irreversible anode thickening caused by the accumulation of an inorganic-rich solid electrolyte interphase (SEI) permeating the anode bulk. Electrode potential-shift analysis further demonstrates that Li + ions released from lithium reservoirs in the prelithiated anode mask true lithium inventory loss during aging. These results demonstrate that low-expansion SiO x /Gr anodes can simultaneously exhibit favorable cycling and impedance metrics while undergoing substantial, hidden degradation, underscoring the importance of electrode-resolved diagnostics for evaluating prelithiated silicon-based anodes.

25 ENERGY STORAGE↗

Formation of LiF Surface Layer During Direct Fluorination of High-Capacity Co-Free Disordered Rocksalt Cathodes

Disordered rocksalt (DRX) cathodes have attracted interest due to their high capacity and compositional flexibility (e.g., Co-free chemistries). However, the sloping voltage profile and gradual capacity fade during cycling have hindered widespread adoption of these materials. Simulations predict that fluorine substitution in DRX cathodes will improve their capacity, rate performance and cyclability. In this study we use a fluidized bed reactor to fluorinate a model Lirich DRX composition (Li1.15Ni0.375Ti0.375Mo0.1O2, NTMO) to investigate how fluorine content impacts the cathode’s structure and electrochemical performance. Instead of substituting O with F to form oxyfluoride phases, direct fluorination of DRX cathodes leads to formation of LiF surface films which improves the specific energy and capacity retention. This study demonstrates the feasibility of direct fluorination to improve the electrochemical performance of high voltage cathodes by tuning the material’s surface chemistry.

Co-free disordered rock-salt cathode, direct fluor↗

Influence of Calendering on the Electrochemical Performance of LiNi 0.9 Mn 0.05 Al 0.05 O 2 Cathodes in Lithium-Ion Cells

Electrode calendering is a necessary process used in industry to improve the volumetric capacity of lithium-ion batteries. However, calendering high-nickel cathodes leads to electrode particle pulverization, raising concerns of a reduced cycle life due to parasitic side reactions. We present here an investigation of the impact of calendering on the morphology and electrochemical performance of the cobalt-free layered oxide cathode LiNi 0.9 Mn 0.05 Al 0.05 O 2 (NMA-90). We find that secondary particle pulverization and fusion simultaneously occur at sufficiently high pressures. The initial surface area of the cathode is shown to increase with the degree of calendering, despite the higher likelihood of secondary particle fusion. Long-term cycling of full coin cells assembled with the NMA-90 cathode and the graphite anode indicates that cells with higher degrees of cathode calendering exhibit lower capacity fade compared to uncalendered cathodes. Hybrid pulse-power tests demonstrate that the usable capacity range of cells with calendered cathodes far exceeds those with uncalendered cells after long-term cycling. The improved capacity retention and pulse-power performance are attributed to the enhanced mechanical properties of the electrode after calendering that prevents loss of the primary particle contact during long-term cycling. As a result, we find that calendering high-nickel NMA-90 to industrially relevant densities does not have a detrimental effect on capacity fade, marking an important step toward commercial adoption.

25 ENERGY STORAGE↗

Physicochemical Heterogeneity in Silicon Anodes from Cycled Lithium-Ion Cells

The severe capacity fade of lithium-ion cells with silicon-dominant anodes has hindered their widescale commercialization. In this work, we link cell capacity fade to the heterogeneous physicochemical evolution of silicon anodes during battery cycling. Through a multi-length scale characterization approach, we demonstrate that silicon particles near the anode surface react differently than those near the copper current collector. In particular, near the anode surface we find an amorphized wispy silicon encased in a highly fluorinated matrix of electrolyte-reduction products. In contrast, closer to the current collector, the silicon retains more of its initial morphology and structure, suggesting the presence of isolated particles. Here, the results show that accessibility of active silicon to lithium-ions varies across the anode matrix. Material and cell designs, which minimize electrode expansion resulting from the in-filling of pores with the solid electrolyte interphase (SEI), are needed to enhance anode homogeneity during the electrochemical cycling.

25 ENERGY STORAGE↗

A Quasi-Ordered Mn-Rich Cathode with Highly Reversible Oxygen Anion Redox Chemistry

Anionic oxygen redox chemistry in Li-rich Mn-based layer oxide cathodes represents a transformative approach for boosting the energy density of next-generation lithium-ion batteries. However, conventional oxygen redox reactions often induce oxygen dimerization at high voltages, leading to irreversible lattice oxygen loss and a rapid voltage fade. Herein, we achieve highly reversible oxygen redox chemistry through a new quasi-ordered structural design that incorporates both intra- and interlayer cation disorder configurations. This unique structure significantly enhances lattice oxygen stability, effectively stabilizes oxidized oxygen, and inhibits the formation of peroxo- or superoxol-like species, thereby enabling anionic redox reactions to proceed reversibly even at deep delithiation states. The quasi-ordered design mitigates irreversible phase transitions and preserves the structural integrity throughout extended cycling. Consequently, the proposed cathode demonstrates exceptional cyclability with negligible capacity and voltage fade, retaining 99% capacity and 98% average voltage after long-term cycling. Finally this work provides fresh insights into addressing issues related to lattice oxygen instabilities and reforming strategies for developing long-life, high-energy-density anionic redox cathode materials for advanced batteries.

chemical structure↗

Generation of Subauroral Longitudinally Extended Emissions Following Intensifications of the Poleward Boundary of the Substorm Bulge and Streamer Production

Observations showing the development of Subauroral Longitudinally Extended Emigerssions on a global scale are presented. It is demonstrated that they occur as a separation of an east-west arc-like band of luminosity that detaches away from the equatorward edge of the auroral distribution following episodes of auroral streamer production. They persist for time intervals on the order of ~30 min and devolve into patchy disjointed segments before they fade. Emissions are seen in both 557.7 nm OI and 391.4 nm N + 2 1NG lines, and 630.0 nm emissions are often observed equatorward. The 391.4 nm emissions are typically weaker and fade away more quickly than the 557.7 nm emissions, suggesting that an auroral precipitation source is initially present but is rapidly depleted as the forms age. All cases are associated with enhanced Subauroral Polarization Stream (SAPS) flows, and one event shows clear association with large-scale Giant Undulations (GUs) and the formation of spur-like forms that fold equatorward under the main oval. A model is proposed for the production of subauroral longitudinally extended forms in which nonlinear growth of SAPS-induced surface waves on the plasmapause results in a disruption of the boundary. It is suggested that hot plasma of plasma sheet origin becomes entrained in the plasmasphere to produce transient precipitation-associated auroral emissions that may decay into STEVE emissions and that cold dense plasma from the plasmasphere becomes entrained onto open drift paths to feed long-lived drainage plumes. This process may occur quasi periodically during intense substorms and storm-time conditions.

79 ASTRONOMY AND ASTROPHYSICS↗

Structural evolution at the oxidative and reductive limits in the first electrochemical cycle of Li 1.2 Ni 0.13 Mn 0.54 Co 0.13 O 2

High-energy-density lithium-rich materials are of significant interest for advanced lithium-ion batteries, provided that several roadblocks, such as voltage fade and poor energy efficiency are removed. However, this remains challenging as their functioning mechanisms during first cycle are not fully understood. Here we enlarge the cycling potential window for Li 1.2 Ni 0.13 Mn 0.54 Co 0.13 O 2 electrode, identifying novel structural evolution mechanism involving a structurally-densified single-phase A’ formed under harsh oxidizing conditions throughout the crystallites and not only at the surface, in contrast to previous beliefs. We also recover a majority of first-cycle capacity loss by applying a constant-voltage step on discharge. Using highly reducing conditions we obtain additional capacity via a new low-potential P” phase, which is involved into triggering oxygen redox on charge. Altogether, these results provide deeper insights into the structural-composition evolution of Li 1.2 Ni 0.13 Mn 0.54 Co 0.13 O 2 and will help to find measures to cure voltage fade and improve energy efficiency in this class of material.

25 ENERGY STORAGE↗

Surface regulation enables high stability of single-crystal lithium-ion cathodes at high voltage

Abstract Single-crystal cathode materials for lithium-ion batteries have attracted increasing interest in providing greater capacity retention than their polycrystalline counterparts. However, after being cycled at high voltages, these single-crystal materials exhibit severe structural instability and capacity fade. Understanding how the surface structural changes determine the performance degradation over cycling is crucial, but remains elusive. Here, we investigate the correlation of the surface structure, internal strain, and capacity deterioration by using operando X-ray spectroscopy imaging and nano-tomography. We directly observe a close correlation between surface chemistry and phase distribution from homogeneity to heterogeneity, which induces heterogeneous internal strain within the particle and the resulting structural/performance degradation during cycling. We also discover that surface chemistry can significantly enhance the cyclic performance. Our modified process effectively regulates the performance fade issue of single-crystal cathode and provides new insights for improved design of high-capacity battery materials.

25 ENERGY STORAGE↗

Ultrastable cathodes enabled by compositional and structural dual-gradient design

Cathodes for next-generation batteries are pressed for higher voltage operation (≥4.5 V) to achieve high capacity with long cyclability and thermal tolerance. Current cathodes fail to meet these requirements owing to structural and electrochemical strains at high voltages, leading to fast capacity fading. Here, in this work, we present a cathode with a coherent architecture ranging from ordered to disordered frameworks with concentration gradient and controllable Ni oxidation activities, which can overcome voltage ceilings imposed by existing cathodes. This design enables simultaneous high-capacity and high-voltage operation at 4.5 V without capacity fading, and up to 4.7 V with negligible capacity decay. Multiscale diffraction and imaging techniques reveal the disordered surface is electrochemically and structurally indestructible, preventing surface parasitic reactions and phase transitions. Structural coherence from ordering to disordering limits lattice parameter changes, mitigating lattice strain and enhancing morphological integrity. The dual-gradient design also notably improves thermal stability, driving the advancement of high-performance cathode materials.

36 MATERIALS SCIENCE↗

Unlocking anionic redox activity in O3-type sodium 3 d layered oxides via Li substitution

Sodium ion batteries, because of their sustainability attributes, could be an attractive alternative to Li-ion technology for specific applications. However, it remains challenging to design high energy density and moisture stable Na-based positive electrodes. Here, we report an O3-type NaLi 1/3 Mn 2/3 O 2 phase showing anionic redox activity, obtained through a ceramic process by carefully adjusting synthesis conditions and stoichiometry. This phase shows a sustained reversible capacity of 190 mAh g -1 that is rooted in cumulative oxygen and manganese redox processes as deduced by combined spectroscopy techniques. Unlike many other anionic redox layered oxides so far reported, O3-NaLi 1/3 Mn 2/3 O 2 electrodes do not show discernible voltage fade on cycling. This finding, rationalized by density functional theory, sheds light on the role of inter- versus intralayer 3d cationic migration in ruling voltage fade in anionic redox electrodes. Another practical asset of this material stems from its moisture stability, hence facilitating its handling and electrode processing. Altogether, this work offers future directions towards designing highly performing sodium electrodes for advanced Na-ion batteries.

25 ENERGY STORAGE↗

Essential effect of the electrolyte on the mechanical and chemical degradation of LiNi 0.8 Co 0.15 Al 0.05 O 2 cathodes upon long-term cycling

Capacity fading during long-term cycling (>1500×) is still a critical challenge for Li-ion batteries that use Ni-rich layered oxides, e.g. LiNi 0.8 Co 0.15 Al 0.05 O 2 (NCA), as the cathode. Microcracks have been previously recognized as one of the primary reasons for the observed capacity fade. Although there exists a generally developed mechanical understanding of microcracks, the role of the electrolyte has not been clearly understood, especially after extended cycling and at the atomic scale. Here, we unveil the microstructural evolution of spherical NCA secondary particles after long-term cycling using scanning transmission electron microscopy accompanied with electron energy loss spectroscopy. In this work, we found that the microcracks initiated and grew through grain boundaries, which then serve as the pathway for electrolyte penetration into secondary NCA particles. Additionally, the rock-salt phase reconstruction is prone to occur at the (003) surfaces of the primary particles or the crack surfaces, largely due to electrolyte (LiPF 6 EC/EMC) corrosion. Crack propagation within the NCA grains is primarily a joint consequence from electrolyte corrosion and mechanical strain during lithiation/delithiation. During extended cycling, due to the distinctive surface facets, the primary grains located in the center of the secondary particles experience more intensive electrolyte corrosion, leading to a reduced contact with nearby particles, impairing the overall capacity. These results establish the initiation and growth mechanism of microcracks and voids in NCA-based cathodes during cycling and point out the role of the electrolyte in affecting the degradation of NCA-based cathodes.

25 ENERGY STORAGE↗

Quantification of heterogeneous, irreversible lithium plating in extreme fast charging of lithium-ion batteries

Realization of extreme fast charging (XFC, ≤15 minutes) of lithium-ion batteries is imperative for the widespread adoption of electric vehicles. However, dramatic capacity fading is associated with XFC, limiting its implementation. To quantitatively elucidate the effects of irreversible lithium plating and other degradation mechanisms on the cell capacity, it is important to understand the links between lithium plating and cell degradation at both the local and global (over the full cell) scales. Here, we study the nature of local lithium plating after hundreds of XFC cycles (charging C-rates ranging from 4C to 9C) in industrially-relevant pouch cells using spatially resolved X-ray diffraction. Our results reveal a spatial correlation at the mm scale between irreversible lithium plating on the anode, inactive lithiated graphite phases, and local state-of-charge of the cathode. In regions of plated lithium, additional lithium is locally and irreversibly trapped as lithiated graphite, contributing to the loss of lithium inventory (LLI) and to a local loss of active anode material. The total LLI in the cell from irreversibly plated lithium is linearly correlated to the capacity loss in the batteries after XFC cycling, with a non-zero offset originating from other parasitic side reactions. Finally, at the global (cell) scale, LLI drives the capacity fade, rather than electrode degradation. We anticipate that the understanding of lithium plating and other degradation mechanisms during XFC gained in this work will help lead to new approaches towards designing high-rate batteries in which irreversible lithium plating is minimized.

25 ENERGY STORAGE↗

The influence of electrochemical cycling protocols on capacity loss in nickel-rich lithium-ion batteries

The transition towards electric vehicles and more sustainable transportation is dependent on lithium-ion battery (LIB) performance. Ni-rich layered transition metal oxides, such as NMC811 (LiNi 0.8 Mn 0.1 Co 0.1 O 2 ), are promising cathode candidates for LIBs due to their higher specific capacity and lower cost compared with lower Ni content materials. However, complex degradation mechanisms inhibit their use. In this work, tailored aging protocols are employed to decouple the effect of electrochemical stimuli on the degradation mechanisms in graphite/NMC811 full cells. Using these protocols, impedance measurements, and differential voltage analysis, the primary drivers for capacity fade and impedance rise are shown to be large state of charge changes combined with high upper cut-off voltage. Focused ion beam-scanning electron microscopy highlights that extensive microscale NMC particle cracking, caused by electrode manufacturing and calendering, is present prior to aging and not immediately detrimental to the gravimetric capacity and impedance. Scanning transmission electron microscopy electron energy loss spectroscopy reveals a correlation between impedance rise and the level of transition metal reduction at the surfaces of aged NMC811. The present study provides insight into the leading causes for LIB performance fading, and highlights the defining role played by the evolving properties of the cathode particle surface layer.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Probing how Ti- and Nb-substitution affect the stability and improve the electrochemical performance of β- and ε-LiVOPO 4

LiVOPO 4 is a promising next-generation multi-electron cathode material, boasting a theoretical capacity of 305 mA h g -1 , significantly higher than any commercially used Li-ion battery cathode material. However, the material still faces several limitations, including the difficulty in attaining the full theoretical capacity at higher rates and capacity fade over several cycles. Here, in this paper, we show that Ti- and Nb-substitution can be used to improve the thermal stability and electrochemical performance of LiVOPO 4 . We show through in situ heating with XRD and a novel gradient heating technique that both Ti- and Nb-substitution cause β-LiVOPO 4 to be stabilized relative to ε-LiVOPO 4 . This is due to transition-metal substitution, which increases the O-vacancy formation energies, pushing the β → ε transition to higher temperatures. We show that it is still possible to synthesize pure-phase ε-LiVOPO 4 through the use of high temperatures to generate these O-vacancies. We show that even 1% of Ti- or Nb-substitution can improve the initial capacity and long term cycling capability of LiVOPO 4 by improving the high-voltage capacity and reducing the capacity fade in both the high- and low-voltage regions. This is due to the overall improved Li + ion diffusion which is caused by an improved charge-transfer resistance during cycling.

25 ENERGY STORAGE↗