At least 109 records · Page 6

An EBIC study of HEM polycrystalline silicon

Low-cost silicon for solar cells grown by the heat exchanger method (HEM) was studied in the electron beam induced current (EBIC) mode of a scanning electron microscope (SEM). Comparisons were made between the defects observed optically and the recombination centers visible in EBIC. Much of the HEM material was single crystalline, but structural defects were found from areas near the corners of the grown material. Most of these defects consisted of linear twin boundaries and grain boundaries. The electrical activity of these boundaries was dependent on symmetry of the boundaries. Symmetric twin boundaries did not exhibit recombination activity while unsymmetric twin boundaries were electrically active.

Koch, T.↗

Creep and fracture of dispersion-strengthened materials

The creep and fracture of dispersion strengthened materials is reviewed. A compilation of creep data on several alloys showed that the reported values of the stress exponent for creep varied between 3.5 and 100. The activation energy for creep exceeded that for lattice self diffusion in the matrix in the case of some materials and a threshold stress behavior was generally reported in these instances. The threshold stress is shown to be dependent on the interparticle spacing and it is significantly affected by the initial microstructure. The effect of particle size and the nature of the dispersoid on the threshold stress is not well understood at the present time. In general, most studies indicate that the microstructure after creep is similar to that before testing and very few dislocations are usually observed. It is shown that the stress acting on a dispersoid due to a rapidly moving dislocation can exceed the particle yield strength of the G sub p/1000, where G sub p is the shear modulus of the dispersoid. The case when the particle deforms is examined and it is suggested that the dislocation creep threshold stress of the alloy is equal to the yield strength of the dispersoid under these conditions. These results indicate that the possibility that the dispersoid creep threshold stress is determined by either the particle yield strength or the stress required to detach a dislocation from the dispersoid matrix interface. The conditions under which the threshold stress is influenced by one or the other mechanism are discussed and it is shown that the particle yield strength is important until the extent of dislocation core relaxation at the dispersoid matrix interface exceeds about 25 pct. depending on the nature of the particle matrix combination. Finally, the effect of grain boundaries and grain morphology on the creep and fracture behavior of dispersoid strengthened alloys is examined.

Raj, Sai V.↗

Grain size control of rhenium strip

Ensuring the desired grain size in the pure Re strip employed by the SP-100 space nuclear reactor design entails the establishment of an initial grain size in the as-received strip and the avoidance of excessive grain growth during subsequent fabrication. Pure Re tapered tensile specimens have been fabricated and tested in order to quantify the effects of grain-boundary migration. Grain size could be rendered fine and uniform by means of a rolling procedure that uses rather large reductions between short intermediate anneals. The critical strain regime varies inversely with annealing temperature.

Schuster, Gary B.↗

Fatigue Behavior and Deformation Mechanisms in Inconel 718 Superalloy Investigated

The nickel-base superalloy Inconel 718 (IN 718) is used as a structural material for a variety of components in the space shuttle main engine (SSME) and accounts for more than half of the total weight of this engine. IN 718 is the bill-of-material for the pressure vessels of nickel-hydrogen batteries for the space station. In the case of the space shuttle main engine, structural components are typically subjected to startup and shutdown load transients and occasional overloads in addition to high-frequency vibratory loads from routine operation. The nickel-hydrogen battery cells are prooftested before service and are subjected to fluctuating pressure loads during operation. In both of these applications, the structural material is subjected to a monotonic load initially, which is subsequently followed by fatigue. To assess the life of these structural components, it is necessary to determine the influence of a prior monotonic load on the subsequent fatigue life of the superalloy. An insight into the underlying deformation and damage mechanisms is also required to properly account for the interaction between the prior monotonic load and the subsequent fatigue loading. An experimental investigation was conducted to establish the effect of prior monotonic straining on the subsequent fatigue behavior of wrought, double-aged, IN 718 at room temperature. First, monotonic strain tests and fully-reversed, strain-controlled fatigue tests were conducted on uniform-gage-section IN 718 specimens. Next, fully reversed fatigue tests were conducted under strain control on specimens that were monotonically strained in tension. Results from this investigation indicated that prior monotonic straining reduced the fatigue resistance of the superalloy particularly at the lowest strain range. Some of the tested specimens were sectioned and examined by transmission electron microscopy to reveal typical microstructures as well as the active deformation and damage mechanisms under each of the loading conditions. In monotonically strained specimens, deformation during the subsequent fatigue loading was mainly confined to the deformation bands initiated during the prior monotonic straining. This can cause dislocations to move more readily along the previously activated deformation bands and to pile up near grain boundaries, eventually making the grain boundaries susceptible to fatigue crack initiation. The mechanisms inferred from the microstructural investigation were extremely valuable in interpreting the influence of prior monotonic straining on the subsequent fatigue life of Inconel 718 superalloy.

Source record↗

Effect of high temperature hydrogen exposure on the strength and microstructure of mullite

The corrosion of near stoichiometric mullite (3Al2O3-2SiO2) by pure dry hydrogen gas was studied at 1050 and 1250 C for times up to 500 hr. The hydrogen preferentially attacked the grain boundaries of the mullite where an aluminosilicate glass was present. Corrosion of the mullite grains was observed after 125 hr at 1250 C. The hydrogen reaction removed SiO2 from the glassy grain boundaries and the mullite grains resulting in a porous alumina rich surface. At 1250 C the strength increased after short exposure times (at least up to 125 hr) and decreased by 53 percent after 500 hr. At 1050 C, all exposure times (25 to 500 hr) decreased the strength. At 500 hr room temperature strength of mullite exposed to 1050 C was reduced by 22 percent. The strength reduction after short exposure times at 1050 C is attributed to crystallization of the grain boundary glass phase.

Herbell, Thomas P.↗

A Record of Low-Temperature Asteroidal Processes of Amoeboid Olivine Aggregates from the Kainsaz Co3.2 Chondrite

Amoeboid olivine aggregates (AOAs) from the Kainsaz CO3.2 chondrite were analyzed using transmission electron microscopy in order to gain a more complete understanding of thermal metamorphism on the parent body and the role of fluids during metamorphic heating. The Kainsaz AOAs are dominated by strongly zoned, fine-grained, olivine grains (Fa2-31) with heterogeneous Fe enrichments along the grain boundaries, which are interpreted as the result of 26Fe2+-Mg2+ interdiffusion with the matrix during thermal metamorphism. However, our diffusion calculations show that such AOA olivine zoning and compositions cannot be produced by a simple diffusional exchange during metamorphic heating, unlike chondrule olivine zoning and compositions. In addition, fine-grained ferroan olivine overgrowths occur heterogeneously in crystallographic continuity with olivines on the AOA exteriors. The overgrowths (Fa33-36) are compositionally distinct from the underlying AOA olivines and are not fully equilibrated with the matrix olivines (Fa~20-55).The ferroan olivine overgrowths likely formed by precipitation from fluids in an epitaxial relationship with forsteritic olivine on the edges of AOAs. Texturally and compositionally diverse chromite grains are also observed along olivine grain boundaries, in olivine grains, and in pore spaces between olivine grains. They share a similar crystallographic orientation relationships with adjacent olivine, suggestive of their formation by exsolution and/or epitaxial growth. Collectively, these observations provide evidence for the mobilization of Fe, Mg, Si, Cr, and Al in the presence of fluids along olivine grain boundaries and into olivine grains during thermal metamorphism. We conclude that in Kainsaz AOAs, the strong zonation development in individual olivine grains and the formation of ferroan olivine overgrowths and chromite grains were a fluid-driven process that occurred at relatively low temperatures (<500°C), during the cooling history of the CO3 chondrite parent body, following the peak of thermal metamorphism.

Amoeboid olivine aggregates↗

Permeation of oxygen through high purity, large grain silver

The permeation of high purity, large grain Ag membranes by oxygen has been studied over the temperature range 400 to 800 C. The permeability was found to be quite linear and repeatable, but the magnitude was 3.2 times smaller than that determined by past research. Since previous investigators studied substantially less pure Ag and conducted experiments within much poorer vacuum environments (which indicates that their grain boundary density was much greater), the data presented here suggest oxygen transport through the membrane is primarily by grain boundary diffusion. The diffusivity measurements were found to exhibit two distinct linear regions, one above and one below a critical temperature of 630 C. The high-temperature data have an activation energy (11.1 kcal/mole) similar to that reported by others, but the low-temperature data have a higher activation energy (15.3 kcal/mole), which can be explained by impurity trapping in the grain boundaries. Vacuum desorption of the oxygen-saturated Ag was found to occur at a threshold of 630 C, which is consistent with the onset of increased mobility within the grain boundaries.

Outlaw, R. A.↗

A scanning defect mapping system for semiconductor characterization

We have developed an optical scanning system that generates maps of the spatial distributions of defects in single and polycrystalline silicon wafers. This instrument, called Scanning Defect Mapping System, utilizes differences in the scattering characteristics of dislocation etch pits and grain boundaries from a defect-etched sample to identify and count them. This system simultaneously operates in the dislocation mode and the grain boundary (GB) mode. In the 'dislocation mode,' the optical scattering from the etch pits is used to statistically count dislocations, while ignoring the GB's. Likewise, in the 'grain boundary mode' the system only recognizes the local scattering from the GB's to generate grain boundary distributions. The information generated by this instrument is valuable for material quality control, identifying mechanisms of defect generation and the nature of thermal stresses during the crystal growth, and the solar cell process design.

Sopori, Bushnan L.↗

Molecular-dynamics Simulation-based Cohesive Zone Representation of Intergranular Fracture Processes in Aluminum

A traction-displacement relationship that may be embedded into a cohesive zone model for microscale problems of intergranular fracture is extracted from atomistic molecular-dynamics simulations. A molecular-dynamics model for crack propagation under steady-state conditions is developed to analyze intergranular fracture along a flat 99 [1 1 0] symmetric tilt grain boundary in aluminum. Under hydrostatic tensile load, the simulation reveals asymmetric crack propagation in the two opposite directions along the grain boundary. In one direction, the crack propagates in a brittle manner by cleavage with very little or no dislocation emission, and in the other direction, the propagation is ductile through the mechanism of deformation twinning. This behavior is consistent with the Rice criterion for cleavage vs. dislocation blunting transition at the crack tip. The preference for twinning to dislocation slip is in agreement with the predictions of the Tadmor and Hai criterion. A comparison with finite element calculations shows that while the stress field around the brittle crack tip follows the expected elastic solution for the given boundary conditions of the model, the stress field around the twinning crack tip has a strong plastic contribution. Through the definition of a Cohesive-Zone-Volume-Element an atomistic analog to a continuum cohesive zone model element - the results from the molecular-dynamics simulation are recast to obtain an average continuum traction-displacement relationship to represent cohesive zone interaction along a characteristic length of the grain boundary interface for the cases of ductile and brittle decohesion. Keywords: Crack-tip plasticity; Cohesive zone model; Grain boundary decohesion; Intergranular fracture; Molecular-dynamics simulation

Yamakov, Vesselin I.↗

The effect of diffusive hydrogen segregation on fracture of polycrystalline nickel

Hydrogen embrittlement of polycrystalline nickel was studied under conditions which allowed the diffusion and segregation of hydrogen to grain boundaries to be controlled. It was shown that even at high solute concentrations of hydrogen, the fracture mode was ductile shear rupture, if transport of hydrogen to the grain boundaries was not allowed. As the amount of hydrogen segregation to the grain boundaries was increased, the fracture mode became increasingly intergranular. Analysis of the temperature dependence of this transition from ductile rupture to transgranular fracture yields a hydrogen segregation enthalpy of 11.6 kJ/mol. The transition in the fracture mode was also observed at a constant aging temperature by increasing the solute hydrogen concentration. The kinetics of this fracture transition suggest that the hydrogen segregation layer extends about 35 nm from the grain boundary. It is suggested that the fracture mechanism is a softening of the material in this segregation region due to the high hydrogen concentration.

Lassila, D. H.↗

High-temperature effect of hydrogen on sintered alpha-silicon carbide

Sintered alpha-silicon carbide was exposed to pure, dry hydrogen at high temperatures for times up to 500 hr. Weight loss and corrosion were seen after 50 hr at temperatures as low as 1000 C. Corrosion of SiC by hydrogen produced grain boundary deterioration at 1100 C and a mixture of grain and grain boundary deterioration at 1300 C. Statistically significant strength reductions were seen in samples exposed to hydrogen for times greater than 50 hr and temperatures above 1100 C. Critical fracture origins were identified by fractography as either general grain boundary corrision at 1100 C or as corrosion pits at 1300 C. A maximum strength decrease of approximately 33 percent was seen at 1100 and 1300 C after 500 hr exposure to hydrogen. A computer assisted thermodynamic program was also used to predict possible reaction species of SiC and hydrogen.

Hallum, G. W.↗

Effect of high-temperature hydrogen exposure on sintered alpha-SiC

Sintered alpha-silicon carbide was exposed to pure, dry hydrogen at high temperatures for times up to 500 hr. Weight loss and corrosion were seen after 50 hr at temperatures as low as 1000 C. Corrosion of SiC by hydrogen produced grain boundary deterioration at 1100 C and a mixture of grain and grain boundary deterioration at 1300 C. Statistically significant strength reductions were seen in samples exposed to hydrogen for times greater than 50 hr and temperatures above 1100 C. Critical fracture origins were identified by fractography as either general grain boundary corrosion at 1100 C or as corrosion pits at 1300 C. A maximum strength decrease of approximately 33 percent was seen at 1100 and 1300 C after 500 hr exposure to hydrogen. A computer assisted thermodynamic program was also used to predict possible reaction species of SiC and hydrogen.

Hallum, Gary W.↗

Microstructure and mechanical properties of hip-consolidated Rene 95 powders

The effects of heat-treatments on the microstructure of P/M Rene 95 (a nickel-based powder metal), consolidated by the hot-isostatic pressing (HIP), were examined. The microstructure of as-HIP'd specimen was characterized by highly serrated grain boundaries. Mechanical tests and microstructural observations reveal that the serrated grain boundaries improved ductility at both room and elevated temperatures by retarding crack propagation along grain boundaries.

Shimanuki, Y.↗

Segregation Behavior of Sulfur and Other Impurities Onto the Free Surfaces of ED-Ni Deposits

Most researchers attribute grain boundary embrittlement in electro-deposited Nickel (ED-Ni) to the presence of small quantities of Sulfur as an impurity. It occurs in a highly mobile form that segregates to the grain boundaries. Evaluation of Sulfur segregation requires that a sample be fractured through the grain boundaries. However, this action may not always be possible. ED-Ni is inherently tough at ambient temperature, especially if a low level of Sulfur was intentionally maintained. A new method was developed to study Sulfur and other migrant species to the grain boundaries, which also migrate to free surfaces. A test specimen is heated by a quartz lamp within the sample preparation chamber, allowing the mobile species to migrate to polished free surfaces. There the mobile species are analyzed using X-ray photoelectron spectroscopy (XPS) also known as Electron Spectroscopy for Chemical Analysis (ESCA).

Panda, Binayak↗

Segregation Behavior of Sulfur and Other Impurities onto the Free Surfaces of ED-NI Deposits

Most researchers attribute grain boundary embrittlement in electro-deposited nickel (ED-Ni) to the presence of small quantities of sulfur as an impurity. It occurs in a highly mobile form that segregates to the grain boundaries. Evaluation of sulfur segregation requires that a sample be fractured through the grain boundaries. However, this action may not always be possible. ED-Ni is inherently tough at ambient temperature, especially if a low level of sulfur was intentionally maintained. A new method was developed to study sulfur and other migrant species to the grain boundaries, which also migrate to free surfaces. A test specimen is heated by a quartz lamp within the sample preparation chamber, allowing the mobile species to migrate to polished free surfaces. There the mobile species are analyzed using X-ray photoelectron spectroscopy (XPS) also known as Electron Spectroscopy for Chemical Analysis (ESCA).

Panda, B.↗

Hot Hydrogen Exposure Degradation of the Strength of Mullite

This study deals with the corrosion of near stoichiometric mullite (3Al2O3-2SiO2) by pure dry hydrogen gas. Exposure of the mullite samples was at temperatures of 1050 and 1250 C for times up to 500 hours. Preferential attack of the alumino-silicate glass present in the grain boundaries of the mullite occurred after 125 hours at 1250 C. Hydrogen scrubbing of the SiO2 from the glassy grain boundaries and the mullite grains yielded a porous alumina-rich surface. The room temperature strength increased after short exposure times at 1250 C (up to 125 hours), then decreased by 53 percent after exposure for 500 hours. At 1050 C, all exposure times (25 to 500 hours) decreased the strength. After 500 hours in hydrogen at 1050 C, the room temperature strength of mullite decreased 22 percent. We also observed a rapid 25 percent strength loss after short exposure times at 1050 C. This is attributed to the calcium/hydrogen assisted crystallization of the glassy, grain-boundary phase.

Herbell, Thomas P.↗

Microstructural effects on the room and elevated temperature low cycle fatigue behavior of Waspaloy

Longitudinal specimens of Waspaloy containing either coarse grains with small gamma or fine grains with large gamma were tested in air at a frequency of 0.33 Hz or 0.50 Hz. The coarse grained structures exhibited planar slip on (III) planes and precipitate shearing at all temperatures. Cracks initiated by a Stage 1 mechanism and propagated by a striation forming mechanism. At 700 C and 800 C, cleavage and intergranular cracking were observed. Testing at 500 C, 700 C, and 800 C caused precipitation of grain boundary carbides. At 700 C, carbides precipitated on slip bands. The fine grained structures exhibited planar slip on (111) planes. Dislocations looped the large gamma precipitates. This structure led to stress saturation and propagation was observed. Increasing temperatures resulted in increased specimen oxidation for both heat treatments. Slip band and grain boundary oxidation were observed. At 800 C, oxidized grain boundaries were cracked by intersecting slip bands which resulted in intergranular failure. The fine specimens had crack initiation later in the fatigue life, but with more rapid propagation crack propagation.

Lerch, B. A.↗

Carbonates in fractures of Martian meteorite Allan Hills 84001: petrologic evidence for impact origin

Carbonates in Martian meteorite Allan Hills 84001 occur as grains on pyroxene grain boundaries, in crushed zones, and as disks, veins, and irregularly shaped grains in healed pyroxene fractures. Some carbonate disks have tapered Mg-rich edges and are accompanied by smaller, thinner and relatively homogeneous, magnesite microdisks. Except for the microdisks, all types of carbonate grains show the same unique chemical zoning pattern on MgCO3-FeCO3-CaCO3 plots. This chemical characteristic and the close spatial association of diverse carbonate types show that all carbonates formed by a similar process. The heterogeneous distribution of carbonates in fractures, tapered shapes of some disks, and the localized occurrence of Mg-rich microdisks appear to be incompatible with growth from an externally derived CO2-rich fluid that changed in composition over time. These features suggest instead that the fractures were closed as carbonates grew from an internally derived fluid and that the microdisks formed from a residual Mg-rich fluid that was squeezed along fractures. Carbonate in pyroxene fractures is most abundant near grains of plagioclase glass that are located on pyroxene grain boundaries and commonly contain major or minor amounts of carbonate. We infer that carbonates in fractures formed from grain boundary carbonates associated with plagiociase that were melted by impact and dispersed into the surrounding fractured pyroxene. Carbonates in fractures, which include those studied by McKay et al. (1996), could not have formed at low temperatures and preserved mineralogical evidence for Martian organisms.

Carbonates/analysis↗