Search NASA⌕ Search

SEARCH · Search NASA

Results for “Grain refinement”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Shear-based deformation processing of age-hardened aluminum alloy for single-step sheet production

Shear-based deformation processing by hybrid cutting-extrusion and free machining are used to make continuous strip, of thickness up to one millimeter, from low-workability AA6013-T6 in a single deformation step. The intense shear can impose effective strains as large as 2 in the strip without pre-heating of the workpiece. The creation of strip in a single step is facilitated by three factors inherent to the cutting deformation zone: highly confined shear deformation, in situ plastic deformation-induced heating and high hydrostatic pressure. The hybrid cutting-extrusion, which employs a second die located across from the primary cutting tool to constrain the chip geometry, is found to produce strip with smooth surfaces (S a < 0.4 μm) that is similar to cold-rolled strip. The strips show an elongated grain microstructure that is inclined to the strip surfaces – a shear texture – that is quite different from rolled sheet. Furthermore, this shear texture (inclination) angle is determined by the deformation path. Through control of the deformation parameters such as strain and temperature, a range of microstructures and strengths could be achieved in the strip. When the cutting-based deformation was done at room temperature, without workpiece pre-heating, the starting T6 material was further strengthened by as much as 30% in a single step. In elevated-temperature cutting-extrusion, dynamic recrystallization was observed, resulting in a refined grain size in the strip. Implications for deformation processing of age-hardenable Al alloys into sheet form, and microstructure control therein, are discussed.

36 MATERIALS SCIENCE↗

Microstructural evolution and intermetallic formation in Zn-3Mg (wt%) powder mixture processed by high-pressure torsion

Severe plastic deformation (SPD) techniques have been used extensively over the past 40 years for producing strong metals and alloys. High-pressure torsion (HPT) is one of the most promising SPD techniques for achieving high strength through nanoscale grain refinement and phase transformation. In this research, a mixture of pure zinc (Zn) and magnesium (Mg) powders, Zn-3Mg (wt%), was HPT-processed under a pressure of 6 GPa for 1, 5, 10, 20, and 30 turns at room temperature to achieve a high strength biodegradable material. In order to understand the effects of pre-consolidation on the resulting microstructure and hardness, HPT processing was performed on loose powders placed in the die and also on a pre-compacted powder mixture and the resulting HPT disks were characterized by X-ray diffraction, scanning electron microscopy, atom probe tomography, and Vickers microhardness. In both cases, the HPT disk microstructures contained nanoscale grains, and stable and metastable strain-induced intermetallics, but an unusual softening appeared at large shear strains. Grain size, grain morphology, and the formation of different intermetallics were analyzed to explain the unusual hardness distribution, and it was found that an inverse Hall-Petch relationship between hardness and grain size exists. It is suggested that thermally-activated phenomena such as grain boundary sliding contributed to the strain-induced softening of this nano-structured biomaterial due to its low melting point. Finally, the current results are compared with those for HPT-processed cast alloys and hybrids of the same composition.

36 MATERIALS SCIENCE↗

Mitigate Stress Corrosion Cracking (SCC) in High-strength Al Castings (CRADA 508)

Development of high strength, corrosion resistant, aluminum alloys is important to a number of industries, including automotive, aerospace, power, etc. Understanding how processing methods such as casting, chemistry, additives and recycle content affect an alloy’s microstructure and performance in real world environments is crucial to their implementation. One major concern is how the repeated exposure to saline solutions can be detrimental to the structural integrity of aluminum alloy components. This study was undertaken as a collaboration between Eck Industries and PNNL to investigate the stress corrosion cracking (SCC) and corrosion behavior of aluminum alloys. This work examines the SCC response of three different materials set. First is cast A206 Al alloy produced by three different casting techniques (i.e., permanent mold, and sand casting with and without chill) and with or without nano forming additives as potential grain refiners. The second materials set comprises Al alloy tubes extruded by PNNL’s ShAPE process and produced using raw material with three different ratios of twitch and pre-consumer Al 6061 scrap. Finally, the third materials set comprises two Al-Si-Mg-Fe alloys with controlled Si% and Fe% to mimic recycle grade Al alloys. The corrosion behavior of these materials was characterized using SCC testing and scanning electrochemical cell microscopy (SECCM) technique; mechanical behavior was characterized using tensile testing, and microstructure was characterized using optical and electron microscopy techniques. Of the A206 Al alloys, the samples with nano forming additives performed poorly compared to those without. The best SCC performance (i.e. least degradation in mechanical properties) was demonstrated by A206 alloy sand cast with chill while the permanent mold sample showed the worst SCC performance. The SECCM was performed on A206 alloy sand cast with chill to understand the effect of microstructure and determine the location-dependent corrosion properties on grain boundaries (GB) and inside grains (IG) on the sample. The corrosion potential and current measured on GB and IG at various points on the sample established that the GB locations are more cathodic and corrosive than the IG locations. Further work needs to be conducted to investigate the mechanisms behind the observed dependence of SCC on casting technique and nano forming additives. Among the ShAPE extruded tubes, SECCM data suggests the decreasing order of tendency to corrode as follows: 100% twitch > 75% twitch > 50% twitch. Finally, both variants of the Al-Si-Mg-Fe alloys showed a large volume fraction of Fe- and Si-containing intermetallics and additional work is needed to discern differences in their respective corrosion responses. In summary, correlating local electrochemical behavior (e.g. via SECCM) with micro/nanostructure, in conjunction with bulk mechanical behavior, can help identify the right fabrication method and alloy chemistry to minimize SCC issues in Al alloys.

36 MATERIALS SCIENCE↗

Synergy of tensile strength and high cycle fatigue properties in a novel additively manufactured Al-Ni-Ti-Zr alloy with a heterogeneous microstructure

Alloy design strategies in additive manufacturing (AM) to achieve grain refinement and terminal eutectic solidification have been introduced to engineer Al alloys having microstructural hierarchy and heterogeneity. Such alloy design strategies enable crack-free builds with an expanded AM processing window and pushed the strength limit in Al alloys. However, fatigue performance of Al alloys made by AM is restricted by the presence of process induced defects and its stochasticity. In this work, tensile and high cycle fatigue (HCF) behavior of a novel Al-Ni-Ti-Zr alloy with a heterogeneous microstructure is studied in the as-built condition, supplemented by detailed microstructural and mechanical characterization. Excellent strength-ductility synergy of 342 MPa and 16% failure strain achieved in the alloy was associated with the microstructural attributes that pertain to the novel alloy. Additionally, the alloy showed excellent HCF performance with a fatigue endurance limit to ultimate tensile strength ratio of 0.29 in flexural fatigue mode. The study revealed the existence of multiple crack retardation mechanisms and favorable crack propagation pathways through the fine-grained regions which enabled good fatigue performance to the alloy. Further, a probabilistic model has been used to estimate the fatigue life of the alloy as a function of the stochastic microstructure by utilizing the statistical distribution of pores, solid-state inclusions, and grains in the AM Al alloy. Finally, the model parametric trends are consistent with the experimental observations.

36 MATERIALS SCIENCE↗

Plasticity and Damage Modeling of Stress Asymmetry and Dynamic Behavior of AFS Additive Manufactured Aluminum Alloy 2219

The Solid State Additive Manufacturing (AM) process referred as MELD that fabricated the samples in this study, provides a new path for repairing, coating, joining and additive manufacturing metals and metal matrix composites. This research will be the first application of a physics-based microstructure dependent internal state variable (ISV) plasticity and damage material model to capture the mechanical response of an AM Aluminum Alloy (AA) 2219 via the MELD process. In this research, a microstructure-based internal state variable (ISV) plasticity-damage model was used to capture the mechanical behavior of AFS 2219 aluminum alloy. Aeroprobe Corporation, creator and patent holder for the MELD process, fabricated the material by pushing a solid filler rod of AA2219-T861 material through a hollow rotating tool onto an AA2219 T851 plate substrate. As feedstock, solid or powder precursor metals are pushed through a nonconsumable rotating cylindrical tool. Herein, added layers are deposited and metallurgically bonded to substrate material or previously deposited layers by the heat generated from the rotating tool through plastic deformation of the filler material. Once a layer has been added, the tool height increases, and starts the deposition of the next layer. This process results in beneficial properties such as grain refinement, homogenization and reduced porosity (fully dense). This process will experience temperatures similar to those in the weld nugget zone (WNZ) in friction stir welding (FSW), ranging from 0.6-0.9 Tm, with Tm being the melting point of the material. MELD is highly scalable with AA deposition rates reaching over 1000 cm3/hr, which allows for MELD being used for repairs, coatings, and building components. A motivating factor driving the research for physics-based history dependent material modeling of MELD components is the ability to accurately capture the stress-state and strain rate dependence in the material caused by variations in material microstructure from the MELD processing of new or repaired components. The ISV model incorporates microstructural content and is consistent with continuum level kinematics, kinetics, and thermodynamics. These features allow the ISV model to capture large deformations at the structural scale using the kinematic and isotropic hardening, while microscale damage is obtained from the microstructural features. The benefits of the ISV model arise from the inclusion of structure-property relationships identified from microstructural characterization and experimentation. The Bauschinger effect (BE) is an important concept, vital in the accurate prediction of cyclic stress-strain response of ductile materials such as metals. The ISV model has been successfully used to capture the behavior and damage, and the BE of different aluminum alloys and steels. The ISV model uses kinematic and isotropic hardening to help capture deformations of the material at the macro scale. To understand this hardening relationship, calculating the kinematic and isotropic hardening relationship in the material is warranted for a high-fidelity model. Electron Backscattered Diffraction (EBSD) was used to characterize the as-fabricated microstructure, where a fully-dense equiaxed grain morphology with average grain size of 2.5 μm was observed. Microhardness mapping of the as-built structures, monotonic tension and compression experiments at both quasi-static (0.001/s) strain rates, tension-followed-by-compression and compression-followed-by-tension experiments were performed to obtain the set of plasticity and damage constants necessary to capture strain rate and stress state behavior of this additive material. To calibrate the plasticity-damage model, a single set of constants were determined to capture the different stress states the MELD AA2219. One set of the constants was determined from experimental true stress-strain curves for the tension and compression data. Additionally, microstructural information and data from the open literature were used as the other model constants. This research is a first of its kind for AFS AA2219, includes correlating the ISV model to the monotonic experimental results that capture the isotropic and kinematic plasticity mechanical response.

Rivera, O. G.↗

Mechanical Milling – Induced Microstructure Changes in Argyrodite LPSCl Solid-State Electrolyte Critically Affect Electrochemical Stability

Microstructure of argyrodite solid-state electrolyte (SSE) critically affects lithium metal electrodeposition/dissolution. While the stability of unmodified SSE is mediocre, once optimized state-of-the-art electrochemical performance is achieved (symmetric cells, full cells with NMC811) without secondary interlayers or functionalized current collectors. Planetary mechanical milling in wet media (m-xylene) is employed to alter commercial Li 6 PS 5 Cl (LPSCl) powder. Quantitative stereology demonstrates how milling progressively refines grain and pore size/distribution in the SSE compact, increases its density, and geometrically smoothens the SSE-Li interface. Mechanical indentation demonstrates that these changes lead to reduced site-to-site variation in the compact's hardness. Milled microstructures promote uniform early-stage electrodeposition on foil collectors and stabilize solid electrolyte interphase (SEI) reactivity. Analysis of half-cells with bilayer electrolytes demonstrates the importance of microstructure directly contacting current collector, with interface roughness due to pore and grain size distribution being key. For the first time, short-circuiting Li metal dendrite is directly identified, employing 1.5 mm diameter “mini” symmetrical cell and cryogenic focused ion beam (cryo-FIB) electron microscopy. The branching sheet-like dendrite traverses intergranularly, filling the interparticle voids and forming an SEI around it. Importantly, mesoscale modeling reveals the relationship between Li-SSE interface morphology and the onset of electrochemical instability, based on underlying reaction current distribution.

25 ENERGY STORAGE↗

Exploring the Microstructure-Property Relationship of Mg-Al-Mn alloys enhanced via Friction Stir Processing

Friction Stir Processing (FSP) is a solid-state thermomechanical processing technique that enables local grain refinement, densification, and homogenization of microstructure in metallic components. Here, FSP is applied to thin sheets of high-pressure die cast AM60 to address the porosity and heterogeneities inherent to the casting process. In this work, microstructure characterization is correlated to improvements in the static mechanical properties of the Mg-Al-Mn alloy system at various FSP processing conditions. Notably, there is a significant increase in the ductility and ultimate tensile stress of system following FSP. The dominant deformation mechanisms for the as-cast material and the FSP material are investigated. Finally, the fatigue life improvement is correlated to microstructure modifications that may lead to distinct behavior in crack initiation and crack propagation for the as-cast and FSP material.

Garcia, David↗

Solid Phase Processing of Mg-Al-Mn-Ca for High Strength and Ductility

While rare-earth Mg alloys have remarkable properties for high strength applications, lower cost alternatives are necessary for the widespread industry use of Mg. Ca added Mg alloys have shown promise as an alternative to rare-earth alloys. Ca-based precipitates can reduce basal texture, reduce casting porosity, and increase mechanical strength. However, the accumulation of Ca-based precipitates along inter-dendritic regions can severely limit ductility. Here, we apply two solid phase processing techniques, friction stir processing and shear assisted processing and extrusion, to produce wrought microstructure sheet and extruded tubes from a cast Mg-Al-Mn-Ca alloy. Ductility of the alloy is enhanced by densification under applied force and elevated temperature, grain refinement, and refinement of (Al,Mg)-Ca based precipitate.

Garcia, David↗

Meshfree Process Modeling and Experimental Validation of Friction Riveting of Aluminum 5052 to Aluminum 6061

Friction riveting (Fric-riveting) is an innovative, fast, and energy-efficient process for spot-joining metal-metal structures. Although fric-riveting has been studied experimentally in recent years, its process modeling is rarely found in the literature primarily because of the associated large material deformation, extreme thermomechanical conditions, and complex contact conditions. In this work, a mesh-free smoothed particle hydrodynamics (SPH) framework that can well handle the abovementioned numerical challenges is used to simulate the fric-riveting of AA5052 to AA6061. Predicted material morphology, multi-point temperatures, and plunge force are thoroughly validated by experimental observations. The material severe plastic deformation zone in the vicinity of the riveting zone is further predicted by the SPH model, which indicates the material mixing and potential grain refinement zone. Based on the validated model, process parameters can be optimized which yields better performance over the baseline case.

Friction riveting (fric-riveting), Smoothed partic↗

Methods to Observe Tribological Failures in Self-Mated Steel Contacts

Scuffing, a type of wear found in highly stressed or poorly lubricated contacts, is characterized by a rapid increase in friction and severe plastic deformation of the near-surface material. Scuffing has proven difficult to study because it initiates unpredictably, progresses rapidly, and typically develops within an inaccessible contact interface. Although there have been successful in-situ studies of scuffing in real-time, the transparent counter body needed for these studies changes the interactions between the surfaces and the lubricant, which affects the scuffing process in unknown ways. This paper describes the development of X-ray-compatible tribometry to study the scuffing of self-mated steels in-situ and in real-time. The method uses a crossed cylinders configuration with a thin (500 μm thick) stationary component and a small (≈200 μm) contact width to maximize X-ray interactions with atoms within the stress field generated by the contact. The resulting instrument and method are used to benchmark the scuffing response of self-mated 52,100 steel under tribologically challenging ‘oil-off’ lubrication conditions. The results demonstrate reliable scuffing in this configuration despite the relatively small contact areas and loads used. Following scuffing, gross plastic deformation was observed on both surfaces along with significant subsurface grain refinement and flow only on the stationary surface, which experienced constant contact. Interestingly, high friction initiated at specific locations of the migratory surface, which experienced intermittent contact, and then propagated across the track over time, suggesting that local conditions of the migratory surface dominated friction leading into the failure event.

36 MATERIALS SCIENCE↗

Effects of Solidification Cooling Rates on Microstructures and Physical Properties of Fe-6.5%Si Alloys

Compared to the widely used Fe-3.2wt%Si steel, Fe-6.5wt%Si has superior electric and magnetic properties, including higher electrical resistivity, lower iron loss, higher permeability, and near zero magnetostriction. However, Fe-6.5wt%Si sheet is difficult to produce using traditional manufacturing processes as the high silicon content favors the formation of ordered phases that embrittle the material. Fortunately, these ordered phases can be suppressed if the alloy is cooled fast enough from a high temperature kinetically trapping the disordered solid solution or amorphous state. Planar flow casting is known for its rapid solidification rate. In order to consider it as a viable method to manufacture ductile Fe-6.5wt%Si sheets, the effect of cooling rate on physical properties of Fe-6.5wt%Si alloy are systematically investigated. In this work, various cooling rates are achieved by changing melt-spin wheel speeds, which significantly affect the solidification temperature profile and have profound effects on ordering, microstructures, textures, hardness, and magnetic properties. High cooling rates result in refined grains, reduced ordering, enhanced <100> out of the plane texture, decreased hardness, and increased coercivity. This study demonstrates a critical cooling rate at ~1.7 × 10 5 K/s, corresponding to a tangential wheel speed of 5-7 m/s, below which the hardness significantly increases in agreement with the sudden increase of the ordered phases that causes the material embrittlement.

36 MATERIALS SCIENCE↗

A creep-resistant additively manufactured Al-Ce-Ni-Mn alloy

Existing additively manufactured aluminum alloys exhibit poor creep resistance due to coarsening of their strengthening phases and refined grain structures. In this paper, we report on a novel additively manufactured Al-10.5Ce-3.1Ni-1.2Mn wt.% alloy which displays excellent creep resistance relative to cast high-temperature aluminum alloys at 300–400 °C. In this work, the creep resistance of this alloy is attributed to a high volume fraction (~35%) of submicron intermetallic strengthening phases which are coarsening-resistant for hundreds of hours at 350 °C. The results herein demonstrate that additive manufacturing provides opportunities for development of creep-resistant aluminum alloys that may be used in bulk form in the 250–400 °C temperature range. Pathways for further development of such alloys are identified.

36 MATERIALS SCIENCE↗

Strain-rate hardening enhances fatigue resistance of AlSi10Mg alloy at 350°C

The high cycle fatigue behavior of laser powder bed fusion processed AlSi10Mg has been investigated at 350 °C (T/T m ∼ 0.7). The alloy exhibited a fatigue strength of 30 MPa defined by runout after 10 7 cycles at a conventional loading frequency of 20 Hz, corresponding to a notable fatigue strength to ultimate tensile strength ratio of 0.73. The surprising fatigue resistance was attributed to the strain-rate hardening effect at high fatigue loading frequency relative to tensile loading rates at 350 °C. The strain-rate hardening effect was validated by performing ultrasonic fatigue tests (20 kHz loading frequency) with three orders of magnitude higher strain-rates than those at conventional loading frequency. The higher strain-rates in ultrasonic fatigue increased the magnitude of strain-rate hardening resulting in longer AlSi10Mg fatigue lives compared to fatigue at conventional frequency, thus confirming the strain-rate hardening effect. The fatigue crack initiation mechanism was strain-rate dependent. Post-mortem microstructural examination revealed intergranular cavitation inside clusters of fine equiaxed grains. The cavities interlinked with each other to initiate near-surface fatigue cracks at conventional frequency. Cavitation occurred to a lesser extent at the ultrasonic frequency. As a result, fatigue cracks initiated at pre-existing processing defects near the surface in ultrasonic fatigue samples. Finally, this investigation underscores the role of fine grain clusters in promoting high-temperature fatigue crack initiation and indicates a possible trade-off between printability via grain refinement and high-temperature fatigue resistance of additively manufactured alloys.

Additive manufacturing↗

Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing

Required microstructural attributes of an alloy vary with structural applications. The microstructural fine-tuning capability of laser-powder bed fusion (L-PBF) additive manufacturing (AM) enables application specific manufacture of the components. Such manufacture with L-PBF AM requires alloys that exhibit wide processing window and are amenable to multiple deformation mechanisms. However, high hot cracking susceptibility of Al alloys poses a barrier to such printability-performance synergy. In this work we show that an integration of, a) grain refinement through heterogeneous nucleation, and b) eutectic solidification, leads to crack-free parts at wide range of process parameters, microstructural heterogeneity, and hierarchy in the Al-Ni-Ti-Zr alloy. Such an integration targets hot cracking at multiple stages of solidification in L-PBF as opposed to the contemporary alloy design strategies that target hot-cracking at only specific stages of solidification. The Al-Ni-Ti-Zr alloy exhibits excellent printability and a high as-built tensile performance. Due to the wide processing window and amenability to multiple deformation mechanisms, the alloy microstructure and subsequently the performance, can be fine-tuned. Here, such strategy opens the gateway for application-specific manufacture of Al alloys with L-PBF AM and establishes a fundamental shift in current methodologies for design of these alloys for L-PBF AM.

36 MATERIALS SCIENCE↗

Fatigue performance of laser powder bed fusion hydride-dehydride Ti-6Al-4V powder

We report hydride-dehydride (HDH) Ti-6Al-4V alloy with particle size distribution of 50–120 µm is laser powder bed fusion (L-PBF) processed using optimum processing parameters and a near-fully dense structure with a density of 99.9 % is achieved. Microstructural observations and phase analyses indicate formation of columnar β grains with acicular α/α' phases in as-built condition. The roughness of the as-fabricated samples is significant with an average roughness of R a = 15.71 ± 3.96 µm and a root mean square roughness of R rms = 108.4 ± 24.9 µm, however, both values are reduced to R a = 0.19 ± 0.04 µm and R rms = 4.9 ± 0.6 µm after mechanical grinding. Mechanical tests are carried out on as-fabricated specimens followed by stress relief treatment. All samples are tested to failure in fatigue, under fully-reversed tension-compression conditions of R = –1. The as-built samples failed from the surface with crack initiation mainly at micro-notches, whereas after mechanically grinding, crack initiation changed to subsurface defects such as pores. Minimizing surface roughness by mechanically grinding eliminates surface micro-notches which improves fatigue strength in the high cycle fatigue region. Fatigue notch factor calculations showed that the effect of surface roughness was significantly lower when HDH powder is used compared to standard spherical powder. X-ray diffraction analysis revealed an in-plane compressive stress, micro-strain and grain refinement on the surface of the mechanically ground samples. Fractography observations (macroscale) revealed a fully brittle fracture in the first stage of crack growth with a transition to a dominantly ductile fracture in the third stage of crack growth. On the other hand, at the micro scale, even the brittle fracture regions showed evidence of ductile fracture within the α' martensite laths.

36 MATERIALS SCIENCE↗

Surface and subsurface characterization of laser-interference structured Ti6Al4V

Ti6Al4V specimens were exposed to high-energy laser pulses of 1.24 J/cm 2 fluences per pulse using a two-beam optical configuration to attain laser-interference. In addition to the formation of periodic surface textures by laser-interference, scanning electron microscope (SEM) images demonstrated several microstructural changes on the surface processed. Moreover, the surface and subsurface of Ti6Al4V specimens were characterized for the as-received and laser-interference processed conditions using x-ray photoelectron spectroscopy (XPS) and electron energy dispersive spectroscopy (EDS). The XPS data showed that this laser technique is effective at removal of surface contaminants for Ti6Al4V. The XPS analysis also revealed the formation of an oxy-nitride layer on the laser treated material. Finally, the microstructure analysis indicates that grain refinement, dendrite and twin structures were found near the surface due to laser processing.

36 MATERIALS SCIENCE↗

Effects of secondary void-initiating particles on the steady-state crack growth resistance of high-strength steel

In this investigation, we focus on the dependence of stable crack growth resistance, as measured by the short-rod fracture toughness test, on secondary void-initiating particles such as AlN and Ti-based grain-refining precipitates in a variety of high-strength steels with tempered martensitic microstructures. The model developed by Ritchie and Thompson is modified to illustrate the significant amounts of toughening that can result from the refinement of secondary particles. Analysis of the data suggests that material strength is a predominant factor in increasing the short-rod fracture toughness relative to linear-elastic measures of initiation fracture toughness, but the extent of toughening is limited by the size and number density of secondary particles in the microstructure. The variation in estimates of secondary microvoid initiation and growth strains with precipitate size reinforce the notion that primary fracture at non-metallic inclusions and secondary fracture at smaller particles occur as sequential processes with a degree of concurrence that is dependent on the state of precipitation in both particle dispersions. Toughening in this connection is maximized by increases in microvoid growth strain that result from decreases in the size and areal number density of secondary void-initiating particles. Finally, the occurrence of transient instabilities during crack extension in short-rod specimens is explained with a phenomenological model that relates crack growth stability to natural variations in the dispersion of secondary void-initiating particles in the microstructure.

42 ENGINEERING↗

Shear assisted processing and extrusion of enhanced strength aluminum alloy tubing

Hollow extrusions are used in many industries to make strong, lightweight, and affordable structures. Shear Assisted Processing and Extrusion (ShAPE) enables the extrusion of many alloys, often with noteworthy properties. In this investigation, ShAPE was used to extrude 1 and 2 mm wall tubes of aluminum alloy 6063 measuring 12 mm in diameter at extrusion speeds up to 3.8 m/min. This speed is 10 and 15 times faster than has been reported for any alloy using ShAPE and friction stir back extrusion, respectively. Increasing the extrusion speed from 0.7 to 3.8 m/s resulted in using 68% less process energy at steady state. Microstructural analysis and tensile testing were performed on as-extruded tubes and tubes with a direct T5 heat treatment. Grain refinement from 65 µm to below 20 µm was observed. Growth of macroscale Mg 2 Si strengthening precipitates was not observed. ShAPE processing resulted in recrystallization, and extrusion speed was shown to influence final extrudate texture. Here, transmission electron microscopy analysis revealed that the as-extruded microstructure was free of nanoscale ß" strengthening precipitates. Nanoscale ß" was prominent in direct-aged (T5) ShAPE tubes, similar to a slightly over-aged conventional T6 microstructure. As-extruded tubes had ultimate tensile strengths on par with conventional T5 extrusions and approximately double the total elongation. Tubes that underwent a T5 heat treatment had yield and ultimate strengths averaging 198 and 234 MPa, respectively, with an average total elongation of 11%. The tensile test results are comparable to a conventional T6 heat treatment, but without the solutionization heat treatment step. Mechanical properties either remained flat or improved with increased extrusion speed, which suggests that ShAPE can be scaled up to an industrial process to create energy- and economically efficient high-strength extrusions.

36 MATERIALS SCIENCE↗