Search NASA⌕ Search

SEARCH · Search NASA

Results for “Graphite specimens”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Effects of matrix toughness on fatigue response of graphite fiber composite laminates

The effect of the matrix toughness on the fatigue response of graphite-fiber-composite laminates was investigated by comparing the fatigue-response results, obtained using the test method of Bakis et al. (1989), for two graphite-epoxy specimens subjected to constant-amplitude fully-reversed loading, namely, (0/ +45/90/ -45)s4 AS4/PEEK samples with drilled center holes and T300-5208 samples. It was found that, although similar matrix damage modes were observed in the two materials, several significant differences occurred in the S-N data and in stiffness data taken over the lives of the two materials, especially at high cyclic stresses.

Simonds, Robert A.↗

Strain energy release rate distributions for double cantilever beam specimens

A 24-ply composite double cantilever-beam specimen under mode I (opening) loading has been analyzed by a 3D FEM code that calculated along a straight delamination starter for several different specimen materials. An isotropic specimen was found to have a strain-energy release rate distribution which varied along its delamination front due to the boundary-layer effect and another effect associated with the anticlastic curvature of the bent specimen arms. A 0-deg graphite-reinforced epoxy specimen had a nearly-uniform strain-energy release rate distribution which dropped only near the edge, due to the boundary-layer effect, and a +/- 45-deg graphite/epoxy specimen exhibited a pronounced strain-energy release rate variation across the specimen width.

Crews, J. H., Jr.↗

New acousto-ultrasonic techniques applied to aerospace materials

The use of an NdYAG pulsed laser for generating ultrasonic waves for NDE in resin matrix composites was investigated. A study was conducted of the use of the 1.064 micron wavelength NdYAG pulsed laser with the neat, unreinforced resin as well as graphite fiber/polymer composite specimens. In the case of the neat resins it was found that, at normal incidence, about 25 percent of the laser pulse energy was reflected at the incident surface. An attenuation coefficient for the polyimide resin, PMR-15 was determined to be approximately 5.8 np/cm. It was found in energy balance studies that graphite fiber/polymer specimens attenuate the laser beam more than do neat resins. The increase absorption is in the graphite fibers. The occurrence of laser induced surface damage was also studied. For the polymer neat resin, damage appears as pit formation over a small fraction of the pulse impact area and discoloration over a larger part of the area. A damage threshold was inferred from observed damage as a function of pulse energy. The 600 F cured PMR-15 and PMR-11 exhibit about the same amount of damage for a given laser pulse energy. The damage threshold is between 0.06 and 0.07 J/sq cm.

Kautz, Harold E.↗

Status of Initial Assessment of Physical and Mechanical Properties of Graphite Grades for NGNP Appkications

Current candidate graphite grades for the core structures of NGNP include grades NBG-17, NBG-18, PCEA and IG-430. Both NBG-17 and NBG-18 are manufactured using pitch coke, and are vibrationally molded. These medium grain products are produced by SGL Carbon SAS (France). Tayo Tanso (Japan) produces IG-430 which is a petroleum coke, isostatically molded, nuclear grade graphite. And PCEA is a medium grain, extruded graphite produced by UCAR Carbon Co. (USA) from petroleum coke. An experimental program has been initiated to develop physical and mechanical properties data for these current candidate graphites. The results will be judged against the requirements for nuclear grade graphites set forth in ASTM standard D 7219-05 "Standard Specification for Isotropic and Near-isotropic Nuclear Graphites". Physical properties data including thermal conductivity and coefficient of thermal expansion, and mechanical properties data including tensile, compressive and flexural strengths will be obtained using the established test methods covered in D-7219 and ASTM C 781-02 "Standard Practice for Testing Graphite and Boronated Graphite Components for High-Temperature Gas-Cooled Nuclear Reactors". Various factors known to effect the properties of graphites will be investigated. These include specimen size, spatial location within a graphite billet, specimen orientation (ag and wg) within a billet, and billet-to-billet variations. The current status of the materials characterization program is reported herein. To date billets of the four graphite grades have been procured, and detailed cut up plans for obtaining the various specimens have been prepared. Particular attention has been given to the traceability of each specimen to its spatial location and orientation within a billet.

01 COAL, LIGNITE, AND PEAT↗

The effect of impact damage and circular holes on the compressive strength of a graphite-epoxy laminate

Specimens were impacted by 1.27-cm-diameter aluminum spheres with speeds ranging from 52 to 101 m/s. Some specimens were impacted without any applied compressive load and then loaded to failure to determine their residual strength. Other specimens were loaded to a prescribed axial compressive strain and impacted while at that applied load. Loaded specimens that did not fail catastrophically on impact were subsequently loaded to failure to determine their residual strength. Low-velocity impact damage was found to degrade seriously the laminate static compressive strength. Low-strain compression-compression cyclic loading was found to degrade further the compressive strength of impact-damaged specimens. Specimens with circular holes having diameters up to a third of the specimen width were loaded to failure in compression. It was found that circular holes can also degrade the static compressive strength of the laminate. The effects of circular holes and impact damage on the compressive strength of the laminate are compared.

Starnes, J. H., Jr.↗

Chemical kinetics parameters and model validation for the gasification of PCEA nuclear graphite

A series of gasification experiments, using two right cylinder specimens (~ 12.7 x 25.4 mm and 25.4 x 25.4 mm) of PCEA nuclear graphite in ambient airflow, measured the total gasification flux at weight losses up to 41.5% and temperatures (893-1015 K) characteristics of those for in-pores gasification Mode (a) and in-pores diffusion-limited Mode (b). The chemical kinetics parameters for the gasification of PCEA graphite are determined using a multi-parameters optimization algorithm from the measurements of the total gasification rate and transient weight loss in experiments. These parameters are: (i) the pre-exponential rate coefficients and the Gaussian distributions and values of specific activation energies for adsorption of oxygen and desorption of CO gas; (ii) the specific activation energy and pre-exponential rate coefficient for the breakup of stable un-dissociated C(O2) oxygen radicals to form stable (CO) complexes; (iii) the specific activation energy and pre-exponential coefficient for desorption of CO2 gas and; (iv) the initial surface area of reactive free sites per unit mass. This area is consistently 13.5% higher than that for nuclear graphite grades of NBG-25 and IG-110 and decreases inversely proportional with the square root of the initial mass of the graphite specimens in the experiments. Experimental measurements successfully validate the chemical-reactions kinetics model that calculates continuous Arrhenius curves of the total gasification flux and the production rates of CO and CO2 gases. The model results at different total weight losses agree well with measurements and expand beyond the temperatures in the experiments to the diffusion-limited mode of gasification. Also calculated are the production rates of CO and CO2 gases and their relative contributions to the total gasification rate in the experiments as functions of temperature, for total weight losses of 5% and 10%.

kinetics↗

Fractography of unidirectional graphite-epoxy as a function of moisture, temperature and specimen quality

Optical microscopy and SEM have been used to examine the tensile failure surfaces of (0-deg)8 T300/5208 graphite-epoxy specimens, and fractography is employed to determine how moisture content and temperature, together with specimen preparation, affect failure modes. A low energy failure morphology is noted in defective specimens; specimens made from nondefective prepregs appeared to exhibit a decrease in flaw sensitivity and increasing strength with either temperature or moisture, although moisture also seemed to increase interfacial debonding between filament and matrix. The combination of temperature and moisture degraded performance by increasing interfacial debonding, and rendering the epoxy more prone to fracture.

Clements, L. L.↗

The correlation of ultrasonic attenuation and shear strength in graphite-polyimide composites

The buffer rod technique for measuring attenuation in thin specimens is modified here to apply to specimens having intermediate thicknesses and high attenuation. The described procedure, which requires only one accessible surface of the material, was used to determine the initial attenuation values of ultrasonic waves in short beam shear specimens of graphite-polyimide composite material. It is shown that there is good correlation between the initial attenuation values and the shear strengths of the specimens determined by the standard short beam shear test method. The modified ultrasonic buffer block technique offers much potential for service as a quantitative, nondestructive, quality assurance test for composite materials.

Hayford, D. T.↗

Titanium Nitride: An Oxidizable Coating for the High-Temperature Protection of Graphite

A titanium nitride coating for graphite, prepared by deposition process, protected test specimens for 60 seconds the vapors in a supersonic ceramic-heated air jet with a stagnation temperature of approximately 2,250 K. For the same test conditions, coated specimens showed no damage to the graphite body for the 60-second test, whereas uncoated specimens were very severely damaged after 20 seconds and were destroyed toward the end of the test. A discussion of the coating of these graphite specimens and of some of the conditions necessary for the utilization of oxidizable substances as oxidation-protective coatings for bodies facing high convective heat transfer in the atmosphere is presented.

Wakelyn, N. T.↗

Monitoring Fiber Stress During Curing of Single Fiber Glass- and Graphite-Epoxy Composites

The difference in thermal expansion characteristics of epoxy matrices and graphite fibers can produce significant residual stresses in the fibers during curing of composite materials. Tests on single fiber glass-epoxy and graphite-epoxy composite specimens were conducted in which the glass and graphite fibers were preloaded in tension, and the epoxy matrix was cast around the fibers. The fiber tension was monitored while the matrix was placed around the fiber and subjected to the temperature-time curing cycle. Two mechanisms responsible for producing stress in embedded fibers were identified as matrix thermal expansion and contraction and matrix cure shrinkage. A simple analysis based on the change in fiber tension during the curing cycle was conducted to estimate the produced stresses. Experimental results on single fiber glass- and graphite-epoxy composites show that the fiber was subjected to significant tensile stresses when the temperature was raised from the first to the second dwell period. When initial fiber pretension is about 60 percent of the fiber failure load, these curing-induced stresses can cause tensile fracture of the embedded fiber.

Madhukar, Madhu S.↗

Graphite Oxidation Rate Study on ET-10 and ETU-10 Grades - Task 4: QA Support and Testing for Structural Graphite Oxidation

INL performed targeted oxidation tests to measure oxidation rates for samples of ET-10 and ETU-10 graphite under CRADA No. 21CRA22 Mod. 3, Annex A, “Tritium Testing to Support Kairos Power Advanced Reactor Demonstration” (04/02/2024). All testing was conducted within INL’s Carbon Characterization Laboratory (CCL) using test standard ASTM D7542-21 "Standard Test Method for Air Oxidation of Carbon and Graphite in the Kinetic Regime" [ASTM International, 2021]. Kairos Power provided all test specimens through its graphite vendor Ibiden, Inc. to INL and ASTM specimen specified dimensions. Information within this report only provides the Arrhenius oxidation rate plots as a function of temperature for each graphite grade tested. The raw mass loss per time data will be provided on the Nuclear Data Management and Analysis System (NDMAS) portal located on the INL information system.

36 MATERIALS SCIENCE↗

Stiffness change of a graphite epoxy laminate under reverse fatigue loading

The stiffness of a flat specimen, made of graphite epoxy (T300/934), was measured during reverse fatigue loading. Laminates of basic layup, unidirectional cross-ply and angle-ply, as well as multidirectional (isotropic) layup, were tested. It was found that all the laminates exhibit rapid stiffness degradation on the last (third) fatigue stage. Except for the 0-deg unidirectional laminate, the last stage starts at about 70 to 80 percent of the fatigue life, regardless of the load level and the final mode of failure (tension or compression). It is shown that, for this material, stiffness degradation is a result of crack accumulation, mainly along the fibers, even for the fiber dominated laminates. This general phenomenon can serve to predict usable safe life of laminates under fatigue loading.

Rotem, Assa↗

Stiffness Study of Wound-Filament Pressure Vessels

Report presents theoretical and experimental study of stiffness of lightweight, jointed pressure vessels made of wound graphite fibers and epoxy. Specimens fabricated from layers of graphite fibers, wet with epoxy, on aluminum mandrel. Segment ends thickened with interspersed layers of axially oriented fibers to reduce pinhole bearing stresses and local deformations. Segments cured at 390 degrees F (199 degrees C). Report presents results of vibrational tests of one-quarter-scale models of wound-filament pressure vessels.

Verderaime, V.↗

AGC-2 Specimen Position Adjustment

This engineering calculations and analysis report (ECAR) calculates the Advanced Graphite Creep (AGC)-2 specimen position adjustments that result from (1) as-built dimension corrections of the Advanced Test Reactor (ATR) reactor, experiment, and specimens, (2) thermal growth of the capsule wall and graphite components, and (3) variable specimen elevations as the specimen stacks shrink due to radiation -induced shrinkage and axial load- induced creep. The specimen elevations listed in the experiment assembly documents do not accurately represent the actual specimen positions in relation to the reactor core mid-plane. Prior experiment insertion difficulties have shown that the distance from the reactor top head closure plate to the core is greater than the nominal elevations shown on the ATR facility drawings. Drawing 600001 lists the measured difference between the closure plate and the gearbox support beam as 0.313 in.ches greater than the facility drawings. Thus, the height of the specimens in relation to the core mid-plane is 0.313 in.ches higher than the nominal dimensions. AlsoIn addition, the overall dimension of the experiment is 0.084 in. shorter than the nominal drawing dimension on Drawing 601266 [1]. As a further adjustment, the average weld shrinkage of the three capsule welds is 0.035 each, which affects the as-built position of the lower isolation weld plate (i.e., Part #601266-9) onto which all graphite components are stacked. In addition to the as-built adjustments mentioned above, the specimens also are subject to a stack up error, which is due to their the thickness difference from nominal. This effect is most apparent in the center S-7 stack which that has a large number of specimens (i.e., 170 specimens). Per post-irradiation examination (PIE) measurements, the average S-7 specimen is about 0.0008 in. smaller than nominal. Even though this difference is small, when multiplied by the number specimens, the top specimen experiences an elevation reduction of 0.14 inches. Although dimensional changes were less pronounced in S-1 through S-6, specimen elevations were adjusted based on pre-irradiation length measurements.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Investigation of Oxidation-Resistant Coatings on Graphite and Molybdenum in Two Arc-Powered Facilities

A number of leading-edge specimens of ATJ graphite and 0.5-percent titanium-molybdenum alloy were tested in a 6-inch subsonic low-pressure arc-powered tunnel and a 1,500-kw subsonic arc jet to determine the effectiveness of several refractory coatings in preventing the oxidation of these materials. The results indicate that the siliconized coating for the ATJ graphite and the W-2 and Durak MG coatings for the titanium-molybdenum alloy provide adequate protection at temperatures up to 3,000 F for the durations of the tests in these facilities, approximately 70 seconds in the arc tunnel and approximately 10 minutes in the arc jet. Weight losses (less than one-half of 1 percent) experienced by a few of the coated specimens indicate that tests of longer duration in these environments may prove deleterious and that the stability of these coatings may be depreciated under the low-pressure environmental conditions encountered during reentry.

Peters, Roger W.↗

Baseline Test Specimen Machining Report

The Next Generation Nuclear Plant (NGNP) Project is tasked with selecting a high temperature gas reactor technology that will be capable of generating electricity and supplying large amounts of process heat. The NGNP is presently being designed as a helium-cooled high temperature gas reactor (HTGR) with a large graphite core. The graphite baseline characterization project is conducting the research and development (R&D) activities deemed necessary to fully qualify nuclear-grade graphite for use in the NGNP reactor. Establishing nonirradiated thermomechanical and thermophysical properties by characterizing lot-to-lot and billet-to-billet variations (for probabilistic baseline data needs) through extensive data collection and statistical analysis is one of the major fundamental objectives of the project. The reactor core will be made up of stacks of graphite moderator blocks. In order to gain a more comprehensive understanding of the varying characteristics in a wide range of suitable graphites, any of which can be classified as “nuclear grade,” an experimental program has been initiated to develop an extensive database of the baseline characteristics of numerous candidate graphites. Various factors known to affect the properties of graphite will be investigated, including specimen size, spatial location within a graphite billet, specimen orientation within a billet (either parallel to [P] or transverse to [T] the long axis of the as-produced billet), and billet-to-billet variations within a lot or across different production lots. Because each data point is based on a certain position within a given billet of graphite, particular attention must be paid to the traceability of each specimen and its spatial location and orientation within each billet. The evaluation of these properties is discussed in the Graphite Technology Development Plan (Windes et. al, 2007). One of the key components in the evaluation of these graphite types will be mechanical testing on specimens drawn from carefully controlled sections of each billet. To this end, this report will discuss the machining of the first set of test specimens that will be evaluated in this program through tensile, compressive, and flexural testing. Validation that the test specimens have been produced to the tolerances required by the applicable ASTM standards, and to the quality control levels required by this program, will demonstrate the viability of sending graphite to selected suppliers that will provide valuable and certifiable data to future data sets that are integral to the NGNP program and beyond.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

AGC-1 Sister Specimen Testing Data Report

The AGC-1 irradiation capsule will provide irradiation creep design data and data for the effects of irradiation creep on key physical properties of several candidate graphites for the Next Generation Nuclear Plant (NGNP). A further objective of the AGC-1 creep capsule is to provide design data for the effects of neutron irradiation on the properties of a range of NGNP candidate graphites, Characterization, both non-destructively and destructively, of AGC-1 graphite creep “sister” specimens for the major grades, i.e., NBG-17, NBG-18, H-451, PCEA, IG-110, and IG-430 has been performed and is reported here. The properties measured were: bulk density by mensuration and Hg-immersion; tensile properties, including strength, stress-strain behavior, static Young’s modulus, and strain to failure; compressive properties, including strength, stress-strain behavior, static elastic modulus, and strain to failure; elastic constants, including dynamic Young’s modulus (fundamental frequency method), and sonic elastic constants, including Young’s modulus, shear modulus, and Poisson’s ratio; pore size distribution (by Hg-intrusion); crystal structure (by x-ray diffraction, XRD); specific heat (elevated temperature), and thermal conductivity (elevated temperature). Significant differences were noted in the physical properties between the grades examined and are attributed to factors such as density, structure (filler particle size and pore size) and the forming method. Some difficulties were encountered with mechanical testing of small (sub-standard) size specimens due to volume and grain size-section size effects. These difficulties are well understood and are an inevitable consequence of conducting property evaluations on small irradiation specimens. These data are judged to be sufficient to yield adequate fractional change in properties when combined with post-irradiation characterization data. However, the complication associated with small specimen testing reinforces the need to conduct full characterization programs to establish the baseline design properties of the NGNP candidate graphites. A sufficient body of experimental data has been acquired from the AGC-1 creep “sister” specimens to fully characterize the properties of interest for the major grades included in the AGC-1 capsule. These data, in combination with the pre-irradiation characterization data packages for the actual AGC-1 creep and control specimens, provide a sound and sufficient pre-irradiation data set for determination of the effects of irradiation induced dimensional change and creep strain on the physical properties of the nuclear graphite grades in the AGC-1 capsule.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Sub-ply level scaling approach investigated for graphite-epoxy composite beam columns

Scale model graphite-epoxy composite specimens were fabricated using the 'sub-ply level' approach and tested as beam-columns under an eccentric axial load to determine the effect of specimen size on flexural response and failure. In the current research project, although the fiber diameters are not scaled, the thickness of the pre-preg material itself has been scaled by adjusting the number of fibers through the thickness of a single ply. Three different grades of graphite-epoxy composite material (AS4/3502) were obtained from Hercules, Inc., in which the number of fibers through the thickness of a single ply was reduced (Grade 190 with 12 to 16 fibers, Grade 95 with 6 to 8 fibers, and Grade 48 with 3 to 4 fibers). Thus, using the sub-ply level approach, a baseline eight ply quasi-isotropic laminate could be fabricated using either the Grade 48 or Grade 95 material and the corresponding full-scale laminate would be constructed from Grade 95 or standard Grade 190 material, respectively. Note that in the sub-ply level approach, the number of ply interfaces is constant for the baseline and full-scale laminates. This is not true for the ply level and sublaminate level scaled specimens. The three grades of graphite-epoxy composite material were used to fabricate scale model beam-column specimens with in-plane dimensions of 0.5*n x 5.75*n, where n=1,2,4 corresponsing to 1/4, 1/2, and full-scale factors. Angle ply, cross ply, and quasi-isotropic laminate stacking sequences were chosen for the investigation and the test matrices for each laminate type are given. Specimens in each laminate family with the same in-plane dimensions but different thicknesses were tested to isolate the influence of the thickness dimension on the flexural response and failure. Also, specific lay-ups were chosen with blocked plies and dispersed plies for each laminate type. Specimens were subjected to an eccentric axial load until failure. The load offset was introduced through a set of hinges which were attached to the platens of a standard load test machine. Three sets of geometrically scaled hinges were used to ensure that scaled loading conditions were applied. This loading condition was chosen because it promotes large flexural deformations and specimens fail at the center of the beam, away from the grip supports. Five channels of data including applied vertical load, end shortening displacement, strain from gages applied back-to-back at the midspan of the beam, and rotation of the hinge from a bubble inclinometer were recorded for each specimen. The beam-column test configuration was used previously to study size effects in ply level scaled composite specimens of the same material system, sizes, and stacking sequences. Thus, a direct comparison between the two scaling approaches is possible. Ply level scaled beam-columns with angle ply, cross ply, and quasi-isotropic lay-ups exhibited no size dependencies in the flexural response, but significant size effects in strength. The reduction in strength with increasing specimen size was not predicted successfully by analysis techniques. It is anticipated that results from this investigation will lead to a better understanding of the strength scale effect in composite structures.

Jackson, Karen E.↗