Selective Laser Melting Inconel 718 Restart Study
Selective Laser Melting (SLM) machines can occasionally shut down (such as in the event of a power failure), which requires the SLM build to be restarted. It has been observed that machine restarts can produce visible "restart lines" in the part, and, in at least one instance, a test specimen containing a restart line exhibited poor mechanical properties. The goal of this study is to evaluate the effect of different machine restart factors on the mechanical properties of the produced SLM material. Test specimens were produced by varying time to restart, the number of re-sinters, and whether or not the build required re-levelling. These are build variables that are typically controlled by the machine operator. Test results indicate that re-leveling and using three re-sinters produces acceptable material. Statistical analysis indicates that re-leveling and re-sintering have strong effects on the resulting material properties. Additionally, the visibility of a restart line loosely correlates with material properties such that obvious restart lines tended to indicate worse material properties.