Search NASA⌕ Search

SEARCH · Search NASA

Results for “Ion Irradiation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Investigation of ion irradiation effects on mineral analogues of concrete aggregates

Irradiation can cause prominent damage to reactor concrete aggregates leading to amorphization, strength and modulus decrease, radiation induced volume expansion (RIVE) and micro-cracking, which limits their long-term performance. Here, to develop an improved understanding of irradiation effects in concrete, three mineral analogues of concrete aggregates (limestone, marble and quartzite) were irradiated by 5.5 MeV He ions and 13 MeV Ni ions to surface doses of 0.011 displacements per atom (dpa) and 0.23 dpa, respectively, at room temperature. The two different ion species allow irradiation spectrum effects (ionizing and displacive) to be examined. Irradiation induced cracks were observed in He irradiated limestone and marble, and Ni irradiated quartzite. Full amorphization was observed in Ni irradiated quartzite with 14.3 % RIVE, and ∼25 % hardness and modulus decrease, while almost no change was observed in He irradiated quartzite except 4.35 % RIVE, revealing a possible ionization enhanced diffusion effect for high energy light ions. Furthermore, partial amorphization was observed in Ni irradiated marble and limestone matrix with a 12 % hardness decrease in marble while no amorphization was observed for He irradiation with a 20 % hardness increase in limestone matrix. The role of knock-on damage and irradiation spectrum on amorphization, volumetric expansion and mechanical property changes are discussed. Moreover, the onset and critical doses for amorphization and RIVE in quartz are obtained for ion irradiations at room temperature. The dose dependence of RIVE exhibits a delay compared to the amorphization behavior. The superior irradiation resistance of calcite phase compared to quartz phase implies there could be advantages to using calcareous aggregates and lowering the usage of siliceous aggregates for concrete in nuclear power plants for extended operation beyond 60 years. However, other effects such as corrosion, aging and reactions during severe accidents should also be considered, and further investigations are needed.

Amorphous↗

In situ microstructural evolution in face-centered and body-centered cubic complex concentrated solid-solution alloys under heavy ion irradiation

This study characterizes the microstructural evolution of single-phase complex concentrated solid-solution alloy (CSA) compositions under heavy ion irradiation with the goal of evaluating mechanisms for CSA radiation tolerance in advanced fission systems. Three such alloys, Cr 18 Fe 27 Mn 27 Ni 28 , Cr 15 Fe 35 Mn 15 Ni 35 , and equimolar NbTaTiV, along with reference materials (pure Ni and E90 for the Cr-FeMnNi family and pure V for NbTaTiV) were irradiated at 50 K and 773 K with 1 MeV Kr ++ ions to various levels of displacements per atom (dpa) using in-situ transmission electron microscopy. Cryogenic irradiation resulted in small defect clusters and faulted dislocation loops as large as 12 nm in face-centered cubic (FCC) CSAs. With thermal diffusion suppressed at cryogenic temperatures, defect densities were lower in all CSAs than in their less compositionally complex reference materials indicating that point defect production is reduced during the displacement cascade stage. High temperature irradiation of the two FCC CSA resulted in the formation of interstitial dislocation loops which by 2 dpa grew to an average size of 27 nm in Cr 18 Fe 27 Mn 27 Ni 28 and 10 nm in Cr 15 Fe 35 Mn 15 Ni 35 . This difference in loop growth kinetics was attributed to the difference in Mn-content due to its effect on the nucleation rate by increasing vacancy mobility or reducing the stacking-fault energy.

36 MATERIALS SCIENCE↗

Coordinated Analysis of an Ion Irradiated Carbonaceous Chondrite Suggests Complex Space Weathering Effects

Surfaces of airless planetary bodies are exposed to micrometeorite bombardment and solar wind irradiation which alter the microstructural, compositional, and optical properties of regoliths over time. These processes are collectively known as space weathering, and they complicate the interpretation of remote sensing data and the subsequent characterization of airless surfaces. Within the next 5 years, NASA’s OSIRIS-REx (Origins, Spectral Interpretation, Resource Identification, Security, Regolith Explorer) and JAXA (Japan Aerospace Exploration Agency)’s Hayabusa2 missions will return samples from C-type asteroids Bennu and Ryugu, respectively. Compared to the Moon and S-type asteroids, our understanding of the space weathering of C-complex asteroids is limited. In order to maximize scientific return from remote sensing data and to prepare for the analysis of returned samples from these missions, we must better understand the effects of space weathering on hydrated, organic-rich materials. We can do so by simulating these processes in the laboratory. In this study, we simulate solar wind exposure through ion irradiation of the CM2 carbonaceous chondrite Murchison - a suitable analog for C-complex asteroids. Here, we present coordinated analyses of a sample before and after ion irradiation.

Laczniak, D. L.↗

Heavy ion irradiation response of an additively manufactured 316LN stainless steel

Additive manufacturing has become an appealing technique to fabricate three-dimensional metallic materials and components for nuclear reactors. However, response of additively manufactured alloys to high-dose heavy ion irradiations at elevated temperatures is still not well understood. Here, an additively manufactured 316LN austenitic stainless steel with high-density solidification cells was irradiated using 3.5 MeV Fe ion to a peak dose of 220 dpa at 450 °C. Microscopy studies show a lower Frank loop density and smaller size in the additively manufactured sample compared with its cold worked counterpart, and the cellular structures may largely suppress the formation of perfect loops and dislocation networks and reduce the magnitude of solute segregations comparing with high angle grain boundaries. In conclusion, the present work advances the understanding on the high-temperature irradiation response of additively manufactured steels for nuclear reactor applications.

36 MATERIALS SCIENCE↗

Heavy ion irradiation induced failure of gallium nitride high electron mobility transistors: effects of in-situ biasing

Abstract While radiation is known to degrade AlGaN/GaN high-electron-mobility transistors (HEMTs), the question remains on the extent of damage governed by the presence of an electrical field in the device. In this study, we induced displacement damage in HEMTs in both ON and OFF states by irradiating with 2.8 MeV Au 4+ ion to fluence levels ranging from 1.72 × 10 10 to 3.745 × 10 13 ions cm −2 , or 0.001–2 displacement per atom (dpa). Electrical measurement is done in situ , and high-resolution transmission electron microscopy (HRTEM), energy dispersive x-ray (EDX), geometrical phase analysis (GPA), and micro-Raman are performed on the highest fluence of Au 4+ irradiated devices. The selected heavy ion irradiation causes cascade damage in the passivation, AlGaN, and GaN layers and at all associated interfaces. After just 0.1 dpa, the current density in the ON-mode device deteriorates by two orders of magnitude, whereas the OFF-mode device totally ceases to operate. Moreover, six orders of magnitude increase in leakage current and loss of gate control over the 2-dimensional electron gas channel are observed. GPA and Raman analysis reveal strain relaxation after a 2 dpa damage level in devices. Significant defects and intermixing of atoms near AlGaN/GaN interfaces and GaN layer are found from HRTEM and EDX analyses, which can substantially alter device characteristics and result in complete failure.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Temperature effects on damage evolution in ion-irradiated NiCoCr concentrated solid-solution alloy

In this work, the damage evolution in equiatomic NiCoCr single crystals irradiated at 138 and 500 K with 1.5 MeV Ni+ ions has been investigated using ion channeling analysis and compared with previous results obtained at 300 K under identical irradiation conditions. As expected, irradiation temperature has a major influence on damage evolution and long-range effects in ion-irradiated NiCoCr. A change in relative irradiation resistance as a function of temperature is revealed when the ion channeling data are compared with previous ion channeling results from Ni-irradiated NiFe at 150, 300 and 500 K. Additionally, NiCoCr has superior irradiation resistance than NiFe under ion irradiation at ≤ 300 K; surprisingly, the relative irradiation resistance is reversed under ion irradiation performed at > 300 K (i.e., 500 K), which may be attributed to local chemical ordering. These observations indicate that the NiFe alloy exhibits a more favorable chemical environment for suppressing deleterious microstructural degradation under high temperature irradiation than the NiCoCr alloy.

36 MATERIALS SCIENCE↗

Interpretation of Ion Irradiation and Neutron Irradiation Damage in Additively Manufactured 316 Stainless Steel using Multiscale Modeling

The accelerated adoption of nuclear energy necessitates advanced manufacturing technologies, such as additive manufacturing, to meet heightened supply chain requirements and support innovative reactor technologies. Due to the unique microstructural characteristics of additively manufactured materials under distinct solidification conditions, comprehensive evaluation of their performance in reactor environments is essential. The Advanced Materials and Manufacturing Technologies program under the Department of Energy's Office of Nuclear Energy focuses on understanding the irradiation performance and damage evolution of laser powder bed fusion 316 stainless steel, with an emphasis on integrating ion and neutron irradiation data to accelerate the development and qualification of materials for advanced nuclear reactor applications. While ion irradiation is a cost- and time-effective method, modeling and simulation are required to interpret the data for the broader range of irradiation conditions encountered in advanced reactors. In fiscal year 2025, integrated multiscale modeling and simulations were conducted to assess irradiation damage in additively manufactured 316 stainless steel. Key outcomes include predictions of chromium enrichment at grain boundaries, nickel enrichment at dislocation cell walls and void surfaces, and heterogeneous void evolution under ion and neutron irradiation conditions. Cluster dynamics simulations revealed the coarsening of voids at high irradiation temperatures and the suppression of void growth by high network dislocation density, while also demonstrating significant growth and coarsening of voids and self-interstitial atom loops at low dose rates. Machine learning-accelerated atomistic simulations highlighted the impact of the local environment and chromium concentration on vacancy diffusivity, providing key insights on the influence of composition on void swelling and radiation-induced segregation. Additionally, molecular dynamics simulations demonstrated the presence of defect production bias and a significant effect of carbon content on defect cluster behavior. These combined efforts aim to predict the performance of additively manufactured materials under various reactor conditions, supporting their qualification for nuclear reactor applications by interpreting ion irradiation data. This report underscores the potential of integrated multiscale modeling to analyze ion irradiation data in the effort to accelerate the qualification of additively manufactured materials for nuclear reactor components.

316 stainless steel↗

In situ study on heavy ion irradiation induced microstructure evolution in single crystal Cu with nanovoids at elevated temperature

Understanding the response of nanovoids to irradiation damage advances our capability to design radiation tolerant materials. Recent in situ studies reveal the shrinkage of hexagon-shaped nanovoids in (110) textured Cu. However, the evolution of voids with irregular geometries under irradiation is less well understood. Here, in situ Kr ion irradiation was performed at 100 °C on single-crystal Cu (112) that possesses nanovoids with high aspect ratio. In situ studies show these elongated voids fragment into smaller voids and shrink gradually with increasing dose. Phase field simulations confirm that fragmentation of the void is governed by the competing kinetics between atoms diffusing toward and away from the elongated nanovoid. In conclusion, cost irradiation analysis reveals the formation of high-density defect clusters.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

A quantitative method to determine the region not influenced by injected interstitial and surface effects during void swelling in ion-irradiated metals

We propose and demonstrate a microstructurally-based experimental method to quantitively determine the depth regions in self-ion-irradiated metals that are affected by the injected interstitial effect and various surface effects, focusing on the choice of safe analysis zones to minimize the impact of these phenomena. The goal is to define the depth ranges where extracted data can be confidently applied to ion-neutron correlations for reactor application. Since ion energies in the range of 1–5 MeV are most frequently employed by the radiation effects community, irradiations were conducted at four energies in this range, all proceeding at 475 °C. The experiment was conducted on relatively pure single crystal iron to focus only on physical phenomena, avoiding the influence of possibly confounding chemical or segregation processes. Care was also taken to minimize the influence of other physical factors such as crystalline orientation. It was shown that, at 475 °C, ion energies of ≤1 MeV were too shallow in penetration and did not yield a safe depth range, but irradiations at 2.5 MeV and above yielded useful safe zones with predicted swelling behavior becoming independent of ion energy. The surface-affected zone width was found to be roughly twice that of the void-denuded zone width and to be independent of accumulated displacement dose. The largest injected-interstitial effect arises from the injected interstitial depression of void nucleation and growth. The interstitial-affected region starts at about one half of the projected range and does not show any “spreading” of its influence in depth as the peak damage level increases from 50 to 100 dpa. This study provides some confidence that enhances the credibility of ion simulation when applied to prediction of void swelling in neutron environments.

36 MATERIALS SCIENCE↗

In-situ ion irradiation study of alloy 709 stainless steels with different processing histories

Alloy 709 stainless steel (A709 SS) has gained an increased interest in nuclear applications due to its advanced properties at high temperatures over the widely used Type 316 SS. However, how this alloy behaves under irradiation with concurrent environmental factors, such as mechanical deformation and/or thermal annealing, has not been studied. In this work, we used in-situ ion irradiation inside a transmission electron microscope (TEM) to investigate the effects of irradiation on the microstructures of A709 SS samples with different prior processing histories, including as-received, annealed, and creep-deformed. It was found that, compared to room temperature irradiation, 600 degrees C irradiation led to larger dislocation loop sizes and lower loop densities. Furthermore, with 600 degrees C irradiation, the creep-deformed sample, which had the highest precipitate density and the highest dislocation density, had the smallest loop size and the lowest loop density compared to others. This observation has been rationalized with quantitative evaluation of the sink strength factors in each sample. This study shows that in-service deformation can significantly affect the irradiation performance in structural materials at reactor operating conditions.

36 MATERIALS SCIENCE↗

Void swelling of conventional and composition engineered HT9 alloys after high-dose self-ion irradiation

Ferritic/martensitic (F/M) steels are being considered as potential structural materials for next generation nuclear reactors, and variants of the alloy HT9 are some of the most promising candidates. In this study, two conventional and two composition engineered HT9 alloys were irradiated using 3.5 MeV Fe 2+ up to 600 peak displacement-per-atom (dpa) at 450 °C. Void swelling and microstructure evolution were characterized for each alloy and compared. The two conventional HT9 alloys (INL and ACO3) showed similar void swelling behavior due to their similar elemental composition and processing conditions. The INL HT9 exhibited a maximum of 2.4% swelling and the ACO3 HT9 showed a maximum of 2.8% swelling at 342 and 393 average local dpa, respectively. On the other hand, the two-composition engineered HT9 alloys with varying N contents (10 ppm for low N and 440 ppm for high N) showed disparate swelling behavior. The low N HT9 exhibited a maximum of 4.6% swelling, while the high N HT9 showed a maximum of 0.7% swelling at 342 average local dpa. Changes in the N content also affected Ni/Si rich G-phase formation. The low N HT9 showed a larger size and lower density of G-phase precipitates compared with the high N HT9 after 600 peak dpa irradiation. This study compares the void swelling behavior of the ion irradiated four current HT9 alloys to extremely high doses, with the void swelling data from neutron irradiated HT9 alloys. Furthermore, the comparison lends critical insights into how well these current alloys can withstand high neutron fluxes in future reactors, especially since the low N and high N HT9 alloys have never been exposed to such high doses before.

36 MATERIALS SCIENCE↗

Microstructural Characterization of Ion Irradiated ODS MA956 Alloy

Oxide Dispersion Strengthened (ODS) alloys are considered as promising nuclear materials for the next generation advanced nuclear reactors due to their improved elevated temperature mechanical properties and radiation damage resistance. MA956 is a commercial ODS alloy with superior oxidation resistance and creep strength at elevated temperatures. The improved properties for ODS alloys can be attributed to the presence of dispersed nanosized oxide particles. These oxide particles can act as barriers to dislocation motion and provide additional sinks and sites for point defect recombination. Hence, their stability can greatly affect the properties of the irradiated ODS alloys. Besides, irradiation will induce defects into the ODS alloys, and these defects can develop further as irradiation dose increases. Furthermore, the defects propagation can significantly undermine the mechanical properties of the bulk materials, resulting in irradiation hardening and lower ductility. Therefore, it is necessary to have a good understanding of the defect’s evolution with irradiation. Hence, efforts are ongoing to understand the effect of ion irradiation on ODS MA956 with emphasis on oxide particles and evolution of defects as a function of dose (2.5, 50 and 100 dpa).

07 ISOTOPE AND RADIATION SOURCES↗

R-O-C(triple bond)N species produced by ion irradiation of ice mixtures: comparison with astronomical observations

We have investigated the effects induced by ion bombardment of mixtures containing nitrogen-bearing compounds at low temperatures. The results show the formation of a band at 2080 cm-1 in binary mixtures, NH3:CH4 and N2:CH4, which we attribute to HCN embedded in the organic residue formed by ion irradiation. In addition to this band, ternary mixtures containing an oxygen-bearing species (i.e., H2O) form a compound with a prominent absorption band at about 2165 cm-1 (4.62 microns). We ascribe this band to a nitrile compound containing O that is bonded to the organic residue. A detailed comparison of the laboratory results with astronomical data of the 4.62 microns absorption band in protostellar spectra shows good agreement in peak position and profile. Our experimental studies show that N2, which is a more likely interstellar ice component than NH3, can be the molecular progenitor of the carrier of the interstellar band. This is an alternative to the pathway by which UV photolysis of NH3-containing ices produces the 4.62 microns band and implies that ion bombardment may well play an important role in the evolution of interstellar ices. Here, we discuss the implications of our studies for the chemical route by which the carrier of the 4.62 microns band is formed in these laboratory experiments.

NASA Discipline Exobiology↗

Defect evolution in Ni and solid-solution alloys of NiFe and NiFeCoCr under ion irradiation at 16 and 300 K

Single-phase concentrated solid-solution alloys (SP-CSAs) have shown unique chemical complexity at the levels of electrons and atoms, and their defect evolution is expected to be different from conventional dilute alloys. Single crystals of Ni, NiFe and NiFeCoCr are chosen as model systems to understand the chemical complexity on defect formation and damage accumulation in SP-CSAs under ion irradiation. The high-quality crystals were irradiated at 16 and 300 K to different ion fluences, to form irradiated region with little to heavy damages. Additionally, the ion-induced damage was determined using Rutherford backscattering spectrometry technique along a channeling direction (RBS/C) and the level of lattice damage in irradiated Ni and SP-CSAs was quantified from Monte Carlo (MC) simulations. The results are interpreted using the Multi Step Damage Accumulation model to reveal material damage accumulation kinetics. Key findings of the study are that in case of room temperature irradiations the damage level measured for complex alloys at the highest irradiation fluence of 2 × 10 15 cm -2 (~3 dpa) is significantly higher than that obtained for pure nickel samples and suggest two-step damage accumulation process with a defect transformation taking place at a fluence of about 1.5 × 10 15 cm -2 . Furthermore, structural and damage kinetic differences clearly imply that, with increasing degree of chemical complexity and high solid-solution strengthening effects from Ni to NiFe and to NiFeCoCr, the enhanced lattice stiffness resists to randomization of atomic configurations and inhibits the growth of extended defects.

36 MATERIALS SCIENCE↗

Behavior of helium cavities in ion-irradiated W-Ni-Fe ductile-phase toughened tungsten

This study reports on the distribution of helium (He) cavities in a hot-rolled W-Ni-Fe ductile-phase toughened tungsten (DPT W) composite irradiated to a dose and a helium concentration that are comparable to those in the material after 5-year irradiation in a conceptual fusion power plant. Here, the DPT W sample consists of W particles embedded in a ductile-phase NiFeW matrix with a nominal composition of 90W-7Ni-3Fe by weight. It was hot-rolled to a thickness reduction by 87% (87R DPT W). Sequential irradiation of the material with 1.2 MeV Ni + ions to a fluence of 2.15×10 16 Ni + /cm 2 and 90 keV He + ions to 6.5×10 15 He + /cm 2 was performed at 973 K. Larger He cavities with a lower number density are observed in NiFeW than W. Helium cavities are aggregated preferentially along the NiFeW/W interphase boundary. This behavior is not observed along the W/W grain boundary under the same irradiation conditions. A similar distribution of He cavities with comparable sizes is observed in 87R DPT W irradiated with He + ions only, suggesting that the He cavity distribution is not significantly affected by pre-irradiation of Ni + ions at 973 K. The data from this study does not provide any evidence for formation of visible voids or Ni precipitates in W phase irradiated with Ni + ions only. Diffusion and clustering of He atoms and mobile vacancies during ion irradiation at 973 K are responsible for the formation and growth of the He cavities.

36 MATERIALS SCIENCE↗

In-situ microstructure observation of oxidized SiC layer in surrogate TRISO fuel particles under krypton ion irradiation

In accidental scenarios of high temperature gas-cooled reactors, both oxidation of and irradiation to the SiC layer in tri-structural-isotropic (TRISO) fuel particles can change the microstructure and integrity of the fuel elements. Here, in the present study, microstructure and defect evolution in the oxidized SiC layer of surrogate TRISO fuel particles under 1.2 MeV krypton ion irradiation was observed by in-situ transmission electron microscopy. The SiC layers oxidized in water vapor at 1200 °C were irradiated azt room temperature and 800 °C and at damage levels of 0.28–11.2 dpa, respectively. SiC and SiO 2 were found to still be in their crystal structures at the damage level of 11.2 dpa at 800 °C, while SiC was observed to have been amorphized at only 0.56 dpa irradiation at room temperature. The defect number density at 800 °C was an order of magnitude lower than that in the sample irradiated at room temperature. Also, crystalline SiO 2 had higher radiation resistance compared to SiC. A defect reaction rate theory was utilized to understand the fundamental defect evolution process and irradiation resistance difference.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of boundary precipitation in a heavy ion irradiated tungsten heavy alloy under the simulated fusion environment

In the concerted effort to identify materials capable of surviving the adverse environment of a fusion reactor interior, tungsten heavy alloys have been put forth as leading candidates. Experimental trials and behavioral studies have yielded positive results for their adoption by taking advantage of the alloy’s unique balance of inherently high fracture toughness and low sputter yields; yet due to their relative novelty in the fusion community, there remains a lack of understanding on the response of these materials to the extended high temperature irradiation environment of the reactor interior. Further, to alleviate this issue and provide the necessary data on the behavior of tungsten heavy alloys to the simulated fusion environment, a 90W-7Ni-3Fe alloy has been subjected to elevated temperature sequential Ni + and He + ion irradiations to mimic the expected displacement damage and gas production expected after five years of service as a plasma facing material component. Atomic-scale structural analyses and nanoscale chemical mapping have identified the formation of two distinct precipitation structures, a surface localized η-carbide and an a-W 2 C type tungsten carbide, both of which appear to originate at the bi-phase interface between W and the ductile phase. This irradiation assisted and induced precipitate formation respectively is anticipated to adversely affect these materials by selective embrittlement at bi-phase interfaces leading to a reduction in the material’s overall fracture toughness during prolonged high temperature irradiation. It is asserted that any potential exposure to C during fusion reactor operational service should be minimized as to prevent the formation of these phases.

36 MATERIALS SCIENCE↗