Comparative Analysis of Reactivity of Al and Ga Doped Garnet Solid State Electrolyte at the Interface with Li Metal

Lithium garnet (Li 7 La 3 Zr 2 O 12 , LLZO) based solid electrolytes are leading candidate materials for all-solid-state batteries with lithium metal anodes because of their high ionic conductivity, high mechanical toughness, and superior electrochemical stability. While doping LLZO with Al and Ga increases its ionic conductivity by stabilizing the cubic phase, the impact of dopants on its (electro)chemical stability at the interfaces with Li metal is critical. Here, our study of differences between Al- and Ga-doped LLZO when interfaced with lithium metal using X-ray photoelectron spectroscopy and density functional theory shows a higher propensity of Ga to move across LLZO interface with Li metal and form Ga-Li alloy. Additionally, neutron diffraction reveals loss of cubic phase resulting from the loss of dopant that explains electrochemical behavior differences between Ga- and Al-doped LLZO. Overall, our study reveals the key role of dopant chemistry in enabling stable solid electrolyte materials for all-solid-state batteries.

Klenk, Matthew↗

Multimodal quantification of degradation pathways during extreme fast charging of lithium-ion batteries

Enabling fast charging of Li-ion batteries will be a key step towards realizing the technology's full potential in electric vehicles. Currently, fast charging is limited by a variety of processes that reduce cell capacity upon extended cycling. Using a multimodal approach combining incremental capacity analysis (dQ/dV), high energy X-ray diffraction (HEXRD), and mass spectrometry titration (MST), we identify specific degradation mechanisms—including Li plating, dead Li x C 6 formation, Li 2 C 2 formation, solid carbonate solid-electrolyte interphase (SEI) deposition, and loss of positive electrode active material (LAM PE )—that occur during extended fast charge cycling. We find that Li plating is the major source of capacity loss in cells cycled at 6C, while non-carbonate SEI species deposition on the graphite anode is the main source of capacity loss when cycled at 4C. We also study local degradative phenomena by examining specific ~1–5 cm 2 regions of the cells using HEXRD and MST. Here, we find that plated Li is often collocated with dead Li x C 6 , Li 2 C 2 , and solid carbonate SEI species, and these additional species cumulatively account for ~20% of the capacity lost during 6C cycling. Finally, in a cell with an anomalously high amount of LAM PE (quantified via dQ/dV), we find that regions of cathode degradation were accompanied by non-carbonate SEI products on the adjacent region of the anode. We postulate that this phenomenon arises due to crosstalk between the electrodes, wherein soluble electrolyte oxidation products formed at the delithiated cathode migrate to the graphite anode and are ultimately deposited on the graphite surface. This work demonstrates the utility of combining multiple characterization techniques to reveal a more holistic understanding of degradative phenomena that occur across multiple length scales during fast charge.

25 ENERGY STORAGE↗

Mixed Cationic and Anionic Redox in Ni and Co Free Chalcogen-Based Cathode Chemistry for Li-Ion Batteries

Mixed cationic and anionic redox cathode chemistry is emerging as conventional cationic-redox of transition metal based layered oxides are reaching their theoretical capacity limit. However, these anionic redox in transition metal oxide-based cathodes attained by taking excess lithium has resulted in stability issues due to weak metal - oxygen ligand covalency. Here, we present an alternative approach of improving metal - ligand covalency by introducing less electronegative chalcogen ligand (sulfur) in the cathode structural framework where the metal dband penetration into ligand p-band thereby utilizing reversible mixed anionic and cationic redox chemistry. Through this design strategy, we report possibility of developing a new family of layered cathode materials when partially filled d orbital redox couples like Fe 2+/3+ are introduced in the Li-ion conducting phase (Li 2 SnS 3 ). Further, the electron energy loss spectroscopy (EELS) and X-ray absorption near-edge structure (XANES) analysis are used to qualitatively identify the charge contributors at the metal and ligand sites during Li + extraction. The detailed high-resolution transmission electron microscopy (HR-TEM) and high annular dark field-scanning transmission electron microscopy (HAADF-STEM) investigation reveal the multi redox induced structural modifications and its surface amorphization with nanopore formation during cycling. Findings from this study will shed light on designing Ni and Co free chalcogen cathodes and various functional materials in the chalcogen based dual anionic and cationic redox cathode avenue.

25 ENERGY STORAGE↗

Stabilizing Anionic Redox Chemistry in a Mn-Based Layered Oxide Cathode Constructed by Li-Deficient Pristine State

Li-rich cathode materials are of significant interest for coupling anionic redox with cationic redox chemistry to achieve high-energy-density batteries. However, lattice oxygen loss and derived structure distortion would induce serious capacity loss and voltage decay, further hindering its practical application. Herein, a novel Li-rich cathode material, O3-type Li 0.6 [Li 0.2 Mn 0.8 ]O 2 , is developed with the pristine state displaying both a Li excess in the transition metal layer and a deficiency in the alkali metal layer. Benefiting from stable structure evolution and Li migration processes, not only can high reversible capacity (≈329 mAh g -1 ) be harvested but also irreversible/reversible anionic/cationic redox reactions are comprehensively assigned via the combination of in/ex situ spectroscopies. Furthermore, irreversible lattice oxygen loss and structure distortion are effectively restrained, resulting in long-term cycle stability (capacity drop of 0.045% per cycle, 500 cycles). Altogether, tuning the Li state in the alkali metal layer presents a promising way for modification of high-capacity Li-rich cathode candidates.

anionic redox reactions↗

Li-ion and Na-ion intercalation in layered MnO 2 cathodes enabled by using bismuth as a cation pillar

Low-cost batteries based on Earth-abundant materials are needed for large-scale electrical storage for the grid. Cathodes based almost entirely on Mn oxides would reduce overall battery cost but cycling of Mn oxides is often not stable. In Li-ion cells, most polymorphs of MnO 2 undergo irreversible transformation to spinel LiMn 2 O 4 during cycling, causing capacity loss. Doping MnO 2 with Bi is known to stabilize the structure, but previous reports have relied on low-crystallinity material making it impossible to pinpoint the Bi location in the structure or its mechanism. In this work, we report a series of hydrated Bi-doped layered MnO 2 compounds and characterize their structures as a function of Bi amount. Bi is shown to reside in the material interlayer, provoking higher long-range structural order even at a low doping level of 1.3%. Doped material improves the specific capacity and stability of cycling in both Li-ion and Na-ion cells. A high level of Bi doping, 4.3%, causes loss of the interlayer crystal water in non-aqueous electrolyte, and this reduces the interlayer distance. Crystal water is shown to be beneficial in a Na-ion system, while its loss improves Li-ion cycling. This provides fundamental insight into how pillaring by a heavy, multivalent cation stabilizes layered oxides.

25 ENERGY STORAGE↗

Quantifying lithium loss in amorphous silicon thin-film anodes via titration-gas chromatography

Silicon with a high theoretical capacity (3,579 mAh/g) is a promising anode candidate for lithium-ion batteries. However, commercialization is still impeded by low Coulombic efficiency, caused by solid electrolyte interphase (SEI) formation and trapped lithium (Li)-silicon (Si) alloy during repeated volume change. Quantifying capacity losses from each factor is crucial to formulate rational design strategies for further improvement. In this work, titration-gas chromatography and cryogenic transmission electron microscopy are applied to characterize the evolution of trapped Li-Si alloy and SEI growth in a silicon thin-film anode. It is found that continuous growth of the SEI is the dominant factor for lithium inventory loss during cycling, with only a marginal increase in trapped Li-Si alloy. This study offers a quantitative approach to differentiate Li in the SEI from trapped Li in Li-Si alloy through a silicon thin-film anode, providing unique insights into identifying critical bottlenecks for developing Si anodes.

25 ENERGY STORAGE↗

Electroanalytical Measurement of Interphase Formation at a Li Metal–Solid Electrolyte Interface

The interphase between Li metal and solid electrolytes dictates performance in Li metal batteries. For the solid electrolyte Lipon, in this study we electroanalytically measure a capacity loss of 1.03 ± 0.16 μAh/cm 2 when Lipon first contacts Li metal. Assuming this capacity is all lost to interphase formation, this corresponds to a maximum Li consumption of 5.0 ± 0.8 nm to form an interphase ~4.7 nm thick. From dynamic electrochemical impedance spectroscopy (dEIS) during Li plating, we determine that nonlinear chaotic spectra demark this interphase formation and that this occurs immediately upon initiation of Li plating. dEIS also reveals interfacial resistance during both plating and stripping that decreases as the amount of plated Li increases.

25 ENERGY STORAGE↗

Sequential Recovery of Critical Metals from Leached Liquor of Processed Spent Lithium-Ion Batteries

The processing and extraction of critical metals from black mass is important to battery recycling. Separation and recovery of critical metals (Co, Ni, Li, and Mn) from other metal impurities must yield purified metal salts, while avoiding substantial losses of critical metals. Solvent extraction in batch experiments were conducted using mixed metal sulphates obtained from the leach liquor obtained from spent and shredded lithium-ion batteries. Selective extraction of Mn 2+ , Fe 3+ , Al 3+ and Cu 2+ from simulated and real leached mixed metals solution was carried out using di-2-ethylhexylphophoric acid (D2EPHA) and Cyanex-272 at varying pH. Further experiments with the preferred extractant (D2EPHA) were performed under different conditions: changing the concentration of extractant, organic to aqueous ratio, and varying the diluents. At optimum conditions (40% v/v D2EPHA in kerosene, pH 2.5, O:A = 1:1, 25 °C, and 20 min), 85% Mn 2+ , 98% Al 3+ , 100% Fe 3+ , and 43% Cu 2+ were extracted with losses of only trace amounts (<5.0%) of Co 2+ , Ni 2+ , and Li + . The order of extraction efficiency for the diluents was found to be kerosene > Exxal-10 >>> dichloromethane (CH 2 Cl 2 ) > toluene. Four stages of stripping of metals loaded on D2EPHA were performed as co-extracted metal impurities were selectively stripped, and a purified MnSO 4 solution was produced. Spent extractant was regenerated after Fe 3+ and Al 3+ were completely stripped using 1.0 M oxalic acid (C 2 H 2 O 4 ).

25 ENERGY STORAGE↗

Impact of electrode porosity architecture on electrochemical performances of 1 mm-thick LiFePO4 binder-free Li-ion electrodes fabricated by Spark Plasma Sintering

Thick electrodes with high active material loadings have been intensively studied over the last couple of decades in pursuit of achieving high energy density systems. To optimize and enhance the electrochemical performance of such electrodes, one has to control the pore morphology by, for example, varying the pore size and shape, and the level of porosity. In the present work, the fabrication of thick binder-free LiFePO4 (LFP) electrodes with two different pore sizes (12 and 20 mu m) and porosities (21 vol% and 44 vol%) using Spark Plasma Sintering (SPS) and templating approach is reported. The well-controlled porous architecture inside the thick electrodes is realized by fine-tuning experimental parameters. The impact of porosity architecture on electrochemical performance is quantified and correlated with the 3D tortuosity values determined from both micro-computed tomography and electrochemical impedance-based experimental methods. Based on the micro-computed tomography data analysis, estimated tortuosity values along X, Y, and Z axes reveal an anisotropic effect perpendicularly to the SPS compression axis (Z-direction). This is particularly profoundly observed in the samples with larger pores (20 mu m). The correlation between morphological properties and the rate capability performance is established indicating that the capacity loss happens mainly due to the Li-ion diffusion limitations.

Cathode material↗

Probing the In Situ Pseudocapacitive Charge Storage in Ti 3 C 2 MXene Thin Films with X-ray Reflectivity

MXenes are a large family of two-dimensional materials that are attractive for energy storage due to their high-rate charging capabilities as well as for electrochemical actuators, water purification, and many other technologies. Ion intercalation during electrochemically driven charge and discharge processes is the fundamental process associated with MXene functionality, which we have characterized here using in situ and operando X-ray reflectivity (XRR). Experiments performed at the Advanced Photon Source at Argonne National Laboratory monitored the changes in the structure of a Ti 3 C 2 MXene film on a platinum current collector as a function of static applied potential between 0.3 and –0.7 V vs Ag/AgCl in an aqueous 0.1 M Li 2 SO 4 electrolyte. Negative potential sweeps lead to a contraction of 1.2 Å in the interlayer spacing and a loss of electron density between the layers, likely due to Li + ion insertion and water removal. The change in lattice spacing includes a continuous variation vs potential as well as an additional discrete contraction that occurs near –0.35 V that has the characteristics of a first-order transition. The continuous change in the MXene interlayer spacing is associated with the capacitive charge, while the discrete change in structure correlated to the weak feature in the cyclic voltammogram at –0.35 V can be interpreted as either a pseudocapacitive charging process or a potential-dependent change in capacity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding What Limits the Voltage of Polycrystalline CdSeTe Solar Cells

The origin of voltage deficits in polycrystalline cadmium selenide telluride (CdSeTe) solar cells is unclear. Here, we present a comprehensive voltage loss analysis performed on state-of-the-art CdSeTe devices - fabricated at Colorado State University and First Solar - using photoluminescence techniques, including external radiative efficiency (ERE) measurements. More specifically, we report the thermodynamic voltage limit Voc,ideal, internal voltage iVoc and external voltage Voc of partially and fully finished cells fabricated with different dopant species, dopant concentrations and back contacts. Arsenic-doped aluminium-oxide-passivated cells made at Colorado State University present remarkably high ERE (>1%) - translating into iVoc above 970 mV - but suffer from poor back-contact selectivity. On the other hand, arsenic-doped devices from First Solar present almost perfect carrier selectivity (Voc=iVoc), leading to Voc above 840 mV, and are limited by recombination in various parts of the device. Thus, development of contact structures that are both passivating and selective in combination with highly luminescent absorbers is key to reducing voltage losses.

CdSeTe devices↗

Inhomogeneous distribution of lithium and electrolyte in aged Li-ion cylindrical cells

Carbonate-based electrolytes in Li-ion batteries exhibit long range order in a frozen state, which enables their non-destructive analysis by diffraction methods. In the current study the spatial distribution of lithium and electrolyte inside the graphite anode was determined in cycled Li-ion cells using monochromatic spatially-resolved neutron diffraction measurements at 150 K. The results indicate a loss of lithium and electrolyte and their non-uniform distribution in the graphite anode in aged Li-ion cells. The observed lithium and electrolyte losses are directly correlated with two electrochemical performance degradation mechanisms, which are responsible for the cell capacity fade.

18650-type↗

Mode connectivity in the loss landscape of parameterized quantum circuits

Variational training of parameterized quantum circuits (PQCs) underpins many workflows employed on near-term noisy intermediate scale quantum (NISQ) devices. It is a hybrid quantum-classical approach that minimizes an associated cost function in order to train a parameterized ansatz. In this work we adapt the qualitative loss landscape characterization for neural networks introduced in Goodfellow et al. (2014); Li et al. (2017) and tests for connectivity used in Draxler et al. (2018) to study the loss landscape features in PQC training. We present results for PQCs trained on a simple regression task, using the bilayer circuit ansatz, which consists of alternating layers of parameterized rotation gates and entangling gates. Multiple circuits are trained with 3 different batch gradient optimizers: stochastic gradient descent, the quantum natural gradient, and Adam. We identify large features in the landscape that can lead to faster convergence in training workflows.

97 MATHEMATICS AND COMPUTING↗

Porosity Development at Li-Rich Layered Cathodes in All-Solid-State Battery during In Situ Delithiation

Structural evolutions are crucial for determining the performance of high-voltage lithium, manganese-rich layered cathodes. Moreover, interface between electrode and electrolyte plays a critical role in governing ionic transfer in all-solid-state batteries. In this work, we unveil two different types of porous structure in Li 1.2 Ni 0.2 Mn 0.6 O 2 cathode with LiPON solid-state electrolyte. Na-nopores are found near the cathode/electrolyte interface at pristine state, where cation mixing, phase transformation, oxygen loss and Mn reduction are also found. In situ Li + extraction induces the evolution of nanovoids, initially formed near the inter-face then propagated into the bulk. Despite the development of nanovoids, layered structure is conserved, suggesting the nature of nanopores and nanovoids are different and their impact would be divergent. This work demonstrates the intrinsic interfacial layer, as well as the dynamic scenario of nanovoid formation inside high-capacity layered cathode, which help understanding the performance fading in cathodes and offer insights into the all-solid-state battery design.

25 ENERGY STORAGE↗

Substantial oxygen loss and chemical expansion in lithium-rich layered oxides at moderate delithiation

Delithiation of layered oxide electrodes triggers irreversible oxygen loss, one of the primary degradation modes in lithium-ion batteries. However, the delithiation-dependent mechanisms of oxygen loss remain poorly understood. Here we investigate the oxygen non-stoichiometry in Li 1.18–x Ni 0.21 Mn 0.53 Co 0.08 O 2–δ electrodes as a function of Li content by using cycling protocols with long open-circuit voltage steps at varying states of charge. Surprisingly, we observe substantial oxygen loss even at moderate delithiation, corresponding to 2.5, 4.0 and 7.6 ml O 2 per gram of Li 1.18–x Ni 0.21 Mn 0.53 Co 0.08 O 2–δ after resting at upper capacity cut-offs of 135, 200 and 265 mAh g −1 for 100 h. Our observations suggest an intrinsic oxygen instability consistent with predictions of high oxygen activity at intermediate potentials versus Li/Li + . In addition, we observe a large chemical expansion coefficient with respect to oxygen non-stoichiometry, which is about three times greater than those of classical oxygen-deficient materials such as fluorite and perovskite oxides. Furthermore, our work challenges the conventional wisdom that deep delithiation is a necessary condition for oxygen loss in layered oxide electrodes and highlights the importance of calendar ageing for investigating oxygen stability.

Atomistic models↗

Building interface bonding and shield for stable Li-rich Mn-based oxide cathode

Implementation of Li-rich Mn-based oxide cathode with high-energy-density has been restrained by capacity/voltage degradation that results from irreversible lattice oxygen loss and structure rearrangements. To resolve these challenges, in this work, Li 1.2 Mn 0.54 Ni 0.13 Co 0.13 O 2 encapsulated by amorphous Co x B (CB-LRM) is rationally designed via autocatalytic plating for highly reversible cationic/anionic hybrid cathode material. Band coherency is ingeniously evoked by interface-reconstruction between bulk structure and amorphous coating layer, which lower the energy of O $2p$ states. Furthermore, this is associated with strengthened orbital hybridization of O $2p$-Mn $3d$ and increased formation energy of oxygen vacancy, which mitigates the lattice oxygen loss considerably. Additionally, interface shielding effects that protect electrode against electrolyte corrosion and the reduction of surface oxygen are also present with fully coverage of amorphous Co x B coating layer. As a result, the as-designed CBLRM cathode exhibits excellent cycle stability after 100 loops with only 0.154% per cycle capacity fade and improved voltage degradation. Given this, this work provides a potential avenue for rational design of lattice oxygen-based electrode materials with high-energy-density.

25 ENERGY STORAGE↗

Magnetopause Reconnection and Indents Induced by Foreshock Turbulence

Abstract Based on global hybrid simulation results, we predict that foreshock turbulence can reach the magnetopause and lead to reconnection as well as Earth‐sized indents. Both the interplanetary magnetic field (IMF) and solar wind are constant in our simulation, and hence, all dynamics are generated by foreshock instabilities. The IMF in the simulation is mostly Sun‐Earth aligned with a weak northward and zero dawn‐dusk component, such that subsolar magnetopause reconnection is not expected without foreshock turbulence modifying the magnetosheath fields. We show a reconnection example to illustrate that the turbulence can create large magnetic shear angles across the magnetopause to induce local bursty reconnection. Magnetopause reconnection and indents developed from the impact of foreshock turbulence can potentially contribute to dayside loss of planetary plasmas.

58 GEOSCIENCES↗

Comparison of Real-Time Pressure Rail Selection Algorithms for the Hybrid Hydraulic Electric Architecture: Case Study on a Track Loader

Abstract The hybrid hydraulic electric architecture (HHEA) seeks to combine the high power/torque/force density of hydraulics with the efficiency of electric machines. A set of common pressure rails is used to provide a majority of the power and this power is modulated by small electric machines to provide precise control for the operator. The HHEA has been studied in previous work using off-line dynamic programming optimization to determine energy efficient pressure rail selections, but this approach requires drive cycle information apriori. A Lagrange multiplier method has also been investigated where a set of gains (Lagrange multipliers) are optimized off-line with the idea the these gains, once determined, could be used for real-time operation. In this work, three new real-time pressure rail selection algorithms that do not require future drive cycle information are investigated; greedy, torque minimizing, and thresholding. The greedy control is found to only use 1% more energy than the globally optimal dynamic programming solution; but a model of energy loss is required.

24 POWER TRANSMISSION AND DISTRIBUTION↗