Search NASA⌕ Search

SEARCH · Search NASA

Results for “Nickel-based superalloy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

103 records · Page 6

Accelerated Creep Testing of Inconel 718 Using the Stepped Isostress Method (SSM)

This paper demonstrates the stepped isostress method (SSM); an accelerated creep test (ACT) for the rapid assessment of metallic materials. The SSM test is based on the time-temperature-stress superposition principle (TTSSP) where temperature and/or stress are step increased to accelerate the time-to-rupture. The SSM test has proven successful for the ACT of polymers and polymeric composites but has yet to be proven for metallic materials. In this study, new test matrix design rules for the SSM of metals are established based on deformation mechanism, time-temperature transformation, and time-temperature precipitation maps. A test matrix of SSM and conventional creep tests (CCTs) are executed for alloy Inconel 718 at 750°C (1382°F) with stress levels ranging from 100 to 350 MPa. Validation CCT data is gathered from the Japan National Institute of Material Science (NIMS). Material constants for the Sine-hyperbolic (Sinh) constitutive model are calibrated using the SSM data and employed to predict the conventional creep response. Here, when blindly compared to the CCT data, the SSM calibrated Sinh model can accurately predict the conventional creep response across logarithmic decades and thus accelerate the capture of conventional creep data. Fractography indicates ductile fracture by transgranular microvoid coalescence (TMVC) with the same fracture mode observed in both SSM and CCT specimens. Creep cavitation is indicated by the population, smoothness, and size of microvoids.

36 MATERIALS SCIENCE↗

Innovative Method for Welding in Generation 3 CSP to Enable Reliable Manufacturing of Solar Receivers to withstand Daily Cycling at Temperatures Above 700°C (Final Technical Report)

Inconel® Alloy 740H® (alloy 740H) was the first age-hardenable nickel-based alloy approved by the ASME Boiler & Pressure Vessel Code for use in pressure-boundary applications. Over the past ~20 years the alloy has been optimized for weldability and high-temperature stability, approved for use in different applications. Development of a supply chain combined with the advantageous properties of the alloy (high-temperature creep strength, oxidation and corrosion resistance, etc.) have resulted in the alloy being applied to new high-temperature power cycle demonstration projects, and of particular interest are applications to concentrating solar power (CSP) to enable higher-efficiency Generation 3 CSP systems and the corresponding supercritical CO 2 (sCO 2 ) power cycle components (heat exchangers, piping, etc.). The high allowable stresses of alloy 740H also make it a desirable material for current Generation 2 CSP solar power receivers to improve cyclic capability and/or reduce receiver height. Recent experiences in demonstration projects utilizing alloy 740H identified cracking issues during welding and fabrication. In this project, a detailed study was done to confirm and clarify the Stress Relaxation Cracking (SRxC) mechanism, also known as stress relief cracking or strain-age cracking (SAC), during post-weld heat-treatment (PWHT). This involved detailed microscopy and advanced characterization to understand the root cause(s) of three failures obtained from industry. Based in-part on these findings, a targeted laboratory based SRxC test method was utilized to evaluate variables such as heat-to-heat variations, strain level, PWHT temperature, and starting material condition on three heats of alloy 740H. Industrial shop welding of cold-worked plates was also conducted. The research showed the following: SRxC was confirmed as the cracking mechanism for all field failures; Stress state (from residual stresses, constraint, deformation, and local stress concentrations) was playing a significant role in field failures and laboratory testing confirmed increasing susceptibility for all heats with increasing strain levels. High levels of microstructural strain were identified at crack initiation locations, in some cases leading to local recrystallization; Precipitate free zones (PFZs) at grain boundaries were found at relaxation cracks and crack initiation locations uniquely associated with SRxC in alloy 740H. Laboratory testing reproduced this microstructural feature which had only previously been reported in long-term creep testing of weldments. Advanced nano-scale characterization confirmed the presence of a moving boundary leading to coarsening of precipitates and PFZs where damage accumulated; The research suggested heat-to-heat variations due to local chemistry and processing may influence SRxC susceptibility, but more work is needed to fully clarify these effects. To disseminate the key learnings from this research to the scientific and engineering communities and alloy 740H end users, multiple technical publications and presentations were made, an industrial alloy 740H users meeting was held, and a new industry guideline specification document which can be directly implemented by end-users of alloy 740H was produced.

14 SOLAR ENERGY↗

Development of a high-temperature Inconel 625 heat exchanger by model design and binder jetting additive manufacturing

A nickel-based Inconel 625 superalloy heat exchanger for high-temperature applications was developed via binder jetting additive manufacturing. The material properties were characterized first on printed and sintered parts. Two sintering temperatures were used to investigate the effects of the temperature on densification and microstructure. For channel geometry design, the heat transfer capabilities of the heat exchanger were optimized for the cross-section geometry of fluid flow channels in a counterflow configuration, and a stress analysis was conducted to investigate the effects of channel geometry. After headers were incorporated into the heat exchanger as a one-piece component, a prototype was printed. A complete depowdering was achieved via compressed air blowing, and sintering was performed with the developed profile. Ultimately, a one-piece heat exchanger with a nearly full density was obtained. Heat transfer tests were performed on this unit, and the results were compared with those from the simulations. In this study, systematic processes were developed for an additively manufactured Inconel-based heat exchanger for high-pressure, high-temperature heat transfer applications.

36 MATERIALS SCIENCE↗

Deformation of binary and boron-doped Ni 3 Al alloys at high pressures studied with synchrotron x-ray diffraction

In situ x-ray synchrotron diffraction experiments were carried out on nickel-based high-strength superalloys under pressure to understand their deformation mechanism using a diamond anvil cell (DAC). Radial x-ray diffraction determines the room-temperature equations of state and yield strengths of binary Ni 3 Al alloy and 500 ppm boron-doped Ni 3 Al to pressures of 20 and 46 GPa, respectively. Crystallographic preferred orientations observed in these superalloys due to anisotropic stress field in DAC indicate the onset of plastic deformation. Inverse pole figure analysis reveals that the underlying deformation mechanisms change from an octahedral slip to a simultaneous activation of octahedral and cube slips upon doping with boron. The yield-strength values were found to increase with pressure and are comparable to those determined from axial diffraction experiments. The results indicate that the yield strength of Ni 3 Al:B is about 0.5 GPa higher (at pressures below 20 GPa) due to grain boundary strengthening by boron. It is shown that due to high elastic anisotropy of Ni 3 Al alloy, the yield-strength estimations from diffraction experiments strongly depend on the micromechanical model used to convert the measured elastic strains into stresses.

42 ENGINEERING↗

Design of Novel Hot Gas Path Component for Gas Turbine Engines Enabled by Materials and Additive Manufacturing Process Development

This report covers the activities associated with the development and evaluation of two high-γ’ superalloys that were designed by external partners on this project, namely Carpenter Technologies Corporation and the University of California-Santa Barbra. One alloy was GammaPrint-700, a cobalt-base superalloy, and the other a nickel-base (Ni-base) superalloy GammaPrint-1100. Both were found to be printable through laser powder bed fusion (LPBF) additive manufacturing, with optimal process parameter sets being identified for each alloy. Further, high temperature mechanical testing was conducted on each alloy that showed both materials performed better than the comparative baseline (LPBF Hastelloy X), with the Ni-base superalloy being down-selected for scaling and printing of the tip shoe components.

36 MATERIALS SCIENCE↗

Design of Novel Hot Gas Component for Gas Turbine Engines Enabled by Materials and Additive Manufacturing Process Development

This CRADA project was the result of a project award under FOA-DOE-0001980. The overarching FOA project team consisted of researchers from Carpenter Technology Corporation (CTC), Solar Turbines Incorporated (Solar), Pennsylvania State University (PSU), University of California-Santa Barbara (UCSB), and Oak Ridge National Laboratory (ORNL). Evaluations were conducted on two high-γ’ superalloys that were designed by CTC and the UCSB. One alloy named GammaPrint-700 (GP-700) is a cobalt-base superalloy. The other alloy named GammaPrint-1100 (GP-1100) is a nickel-base (Ni-base) superalloy. PSU provided expertise and experimental testing of the thermal performance of AM micro-cooling architectures. ORNL provided expertise with the AM superalloy materials characterization and AM processing science. Solar provided turbine component design expertise. The focus of this CRADA report is to document the efforts between ORNL and CTC towards the development of superalloys designed for AM. The project goal was to use an AM processable high-temperature superalloy and design for Additive Manufacturing (DfAM) techniques to design an efficient turbine component (i.e. a turbine tip shoe) with enhanced cooling features that can only be fabricated through additive manufacturing (AM). The efficiencies of existing combined heat and power (CHP) engines are capped by both component design and materials limitations. However, AM of a tip shoe component from a γ’strengthened superalloy offers the design flexibility to increase the efficiency and power of an industrial gas turbine. This project brought about advancements in the DfAM tip shoe design space and in the area of high temperature superalloys processable through laser powder bed fusion (LPBF) AM. State of art computation design tools were utilized to optimize unique cooling features into a tip shoe component design. A two-prong materials development approach was taken to support development of the AM tip shoe geometry. The first approach centered on investigating the processability and the appropriate process science for the industry standard high-γ’ nickel-base (Ni-base) superalloy Mar-M247. This superalloy is typically cast and considered non-weldable by traditional welding standards. In the course of this work, the alloy was not deemed feasible for process scale-up due to significant cracking issues during printing. The second approach focused on the development and evaluation of a novel cobalt-base superalloy, GammaPrint™-700 (GP-700 and a Ni-base superalloy, GammaPrint™-1100 (GP-1100) designed to mitigate the significant AM processing issues with Mar-M247. The processability of these two alloys were investigated through electron beam melting (EBM) binder-jet AM (BJAM), and LPBF as a risk mitigation for manufacturability. To be considered a candidate material for down-selection to proceed to full-scale AM tip shoe engine testing trials, the high temperature creep rupture strength was required to achieve at a minimum, a Larsen Miller Parameter (LMP) increase of 10.9% over the baseline material LPBF AM Hastelloy X.

99 GENERAL AND MISCELLANEOUS↗

Design of Novel Hot Gas Component for Gas Turbine Engines Enabled by Materials and Additive Manufacturing Process Development

This CRADA project was the result of a project award under FOA-DOE-0001980. The overarching FOA project team consisted of researchers from Carpenter Technology Corporation (CTC), Solar Turbines Incorporated (Solar), Pennsylvania State University (PSU), University of California-Santa Barbara (UCSB), and Oak Ridge National Laboratory (ORNL). Evaluations were conducted on two high-γ’ superalloys that were designed by CTC and the UCSB. One alloy named GammaPrint-700 (GP-700) is a cobalt-base superalloy. The other alloy named GammaPrint-1100 (GP-1100) is a nickel-base (Ni-base) superalloy. PSU provided expertise and experimental testing of the thermal performance of AM micro-cooling architectures. ORNL provided expertise with the AM superalloy materials characterization and AM processing science. Solar provided turbine component design expertise. The focus of this CRADA report is to document the efforts between ORNL and CTC towards the development of superalloys designed for AM. The project goal was to use an AM processable high-temperature superalloy and design for Additive Manufacturing (DfAM) techniques to design an efficient turbine component (i.e. a turbine tip shoe) with enhanced cooling features that can only be fabricated through additive manufacturing (AM). The efficiencies of existing combined heat and power (CHP) engines are capped by both component design and materials limitations. However, AM of a tip shoe component from a γ’strengthened superalloy offers the design flexibility to increase the efficiency and power of an industrial gas turbine. This project brought about advancements in the DfAM tip shoe design space and in the area of high temperature superalloys processable through laser powder bed fusion (LPBF) AM. State of art computation design tools were utilized to optimize unique cooling features into a tip shoe component design. A two-prong materials development approach was taken to support development of the AM tip shoe geometry. The first approach centered on investigating the processability and the appropriate process science for the industry standard high-γ’ nickel-base (Ni-base) superalloy Mar-M247. This superalloy is typically cast and considered non-weldable by traditional welding standards. In the course of this work, the alloy was not deemed feasible for process scale-up due to significant cracking issues during printing. The second approach focused on the development and evaluation of a novel cobalt-base superalloy, GammaPrint™-700 (GP-700 and a Ni-base superalloy, GammaPrint™-1100 (GP-1100) designed to mitigate the significant AM processing issues with Mar-M247. The processability of these two alloys were investigated through electron beam melting (EBM) binder-jet AM (BJAM), and LPBF as a risk mitigation for manufacturability. To be considered a candidate material for down-selection to proceed to fullscale AM tip shoe engine testing trials, the high temperature creep rupture strength was required to achieve at a minimum, a Larsen Miller Parameter (LMP) increase of 10.9% over the baseline material LPBF AM Hastelloy X.

36 MATERIALS SCIENCE↗

Improving Economics of Generation 3 CSP System Components Through Fabrication and Application of High Temperature Nickel-Based Alloys

To improve the efficiency and lower the cost of Concentrating Solar Power (CSP) plants, new Generation 3 ‘Gen 3’ CSP concepts using novel salts, solids, or gas heattransfer media envisaged to integrated with a supercritical CO 2 (sCO 2 ) power block at temperatures >715ºC are being investigated. Regardless of the specific pathway, critical components including receivers, piping, and heat-exchangers (HXs) will require the use of heat-resistant nickel-based alloys. Furthermore, the use of age-hardenable alloys, such as INCONEL® alloy 740H® (alloy 740H) may be needed to reduce capital cost. The unique challenges presented by CSP plants to material manufacture, such as small diameter thin-walled tubing in receivers, large diameter thin wall piping, and thin sheet and tubes for HXs can add to the cost to produce such alloys when compared to traditional wrought and cast processing. The goal of this project was to facilitate a reduction of plant cost by developing alternate manufacturing routes and quantifying the performance and economic benefits for alloy 740H in comparison to other candidate nickel-based alloys through fabrication trials, high-temperature mechanical property studies, and interactions with technology developers and codes and standards.

14 SOLAR ENERGY↗

AMMT 2025 Milestone

Idaho National Laboratory initiated the examination of nickel-based alloys manufactured laser powder directed energy deposition additive manufacturing for potential applications in nuclear, high temperature structural components. With the rapid push towards additive manufacturing, codes do not exist that definitively define what is or is not tolerable for each process and application, such as with conventional, wrought products. This report contains the initial work to understand possible manufacturing methods for high temperature alloys, and specifically, void formation, microstructure evolution, and mechanical properties. To generate mechanical test data, specimens were tested irrespective of voids and microstructures were analyzed to better understand how to negate/improve these issues. The preliminary results showed major decreases in mechanical performance for material tested. Test specimens will continue to be produced to further improve additive manufacturing processes, quantify void acceptance, and better understand the most suitable high temperature alloys receptive to additive manufacturing and high temperature nuclear applications.

36 - MATERIALS SCIENCE↗

A macro-micro approach for identifying crystal plasticity parameters for necking and failure in nickel-based alloy haynes 282

Here, this work develops a two-scales macro-micro approach to address the challenge in calibrating crystal plasticity microstructural models when samples undergo necking prior to fracture. The crystal plasticity models are crucial for predicting the materials’ plastic deformation and failure at the microstructure level, identifying the materials’ intrinsic properties as well as investigating the microstructure-properties relationships. However, after necking occurs, the experimentally measured stress-strain curves fail to reflect the materials ‘true’ stress-strain behavior and cannot be directly fitted into crystal plasticity models. The proposed macro-micro approach employs a top-down strategy to address this challenge, which has been studied with experimental tests on precipitation-strengthened Ni-based superalloy Haynes® 282®. In this approach, a macro rate-dependent anisotropic plasticity model with Voce-type hardening and Rice-Tracey damage law is first utilized to model the deformation and failure of the tensile bar, and calibrated by matching the stress-strain curves, necking strain, and reduction of area. Especially, to match the testing results under different applied strain rates, the rate-sensitivity parameter m and saturation stress in the elasticity model are modified to incorporate dependence on the local strain rate. Then, the ‘true’ stress-strain behaviors are extracted from the necking zone of the macro-model, which are used to calibrate a micro-model with explicit microstructures and governed by an extended crystal plasticity law. The consistency between the micro-model and macro-model are enforced during calibration. The calibration outcomes from the crystal plasticity model elucidate the materials intrinsic properties for slip, hardening, and failure, which is vital for further investigations into the microstructure-properties relationship and for accurate prediction of the material behavior under various test and service conditions.

36 MATERIALS SCIENCE↗

Crystal plasticity modeling and analysis for the transition from intergranular to transgranular failure in nickel-based alloy Inconel 740H at elevated temperature

The precipitation-strengthened Nickel alloy Inconel® 740H® (IN740H) exhibits increased ductility at higher applied strain rates during quasi-static tensile tests at an elevated temperature of 760°C. The examination of fracture surfaces in this context reveals a noteworthy transition of underlying fracture mechanisms from transgranular to intergranular fracture as the applied strain rate decreases from 1×10 -3 / s to 0.83×10 -4 / s . To thoroughly understand the mechanical response of IN740H under these conditions, this study develops a crystal plasticity finite element (CPFE) model. Further, this model incorporates various deformation mechanisms including dislocation slips, climb, and grain boundary sliding, which are relevant to the test conditions. The model is calibrated using data from both tensile tests at different strain rates and creep tests across a broad stress range at 760°C, enabling the accurate determination of model parameters for each mechanism. Simulation results well captured the experimental observations of different failure modes. At higher strain rates, the model shows a dominance of dislocation slip leading to heterogeneous plastic deformation and formation of transgranular shear bands causing the failure, while at lower strain rates, an increased activity of grain boundary sliding causes grain boundaries crack leading to intergranular failure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Impacts of Superalloys on the Surface Quality of Additively Manufactured Channels

Abstract Gas turbines feature many components that require superalloys capable of handling extreme thermal environments. Increasing the selection of materials available for these components is important to their use in these extremely high-temperature environments. This study investigated two recently developed materials intended to be used for additive manufacturing (AM), with one superalloy based on cobalt and the other on nickel. Sets of four test coupons were built using the materials, in addition to the commonly used Inconel-718, on multiple laser powder bed fusion machines. Several build conditions were varied between coupon sets, including coupon orientation, contour settings, and upskin and downskin treatment. Each set of test coupons featured four unique cooling designs to explore how different cooling technologies would be impacted by the variations in build conditions. After being built, coupons were computed tomography (CT) scanned to determine accuracy to design intent and quantify the surface roughness. The CT scans indicated that horizontally built test coupons had a significantly higher deviation from design intent and higher surface roughness than those built vertically. Results also indicated that the cobalt-based alloy consistently had a smoother surface quality with lower surface roughness compared to the nickel-based alloy. After geometric characterization, the cooling performance of the test coupons was measured experimentally. Pressure losses were found to correlate with increases in surface roughness; however, in some cases, the convective heat transfer did not increase proportionally to the pressure loss as a result of surface features significantly blocking the flow without proportionally increasing convective heat transfer.

Engineering↗

Final report on assessment of molten salt corrosion testing of unirradiated and ion irradiated advanced manufactured high entropy alloys

Generation IV reactors and future fusion reactor designs have led to more demanding materials performance requirements due to their increased operating temperatures, corrosive coolants, and increased radiation doses compared to the current light-water reactor fleet. Among the innovative nuclear technologies under development, molten salt reactors stand out for their potential to offer superior fuel utilization, intrinsic safety characteristics, and economic viability. Of the proposed Generation IV designs, the gas fast reactor operates at 450 to 850°C and the molten salt reactor operates at 565 to 850°C, with the molten salt reactor design needing molten salt corrosion resistant materials [1, 2]. These increased temperatures and more extreme corrosion environments necessitate higher material performance, such as creep strength, radiation-tolerant microstructures, corrosion resistance, and high-temperature tensile properties. Hastelloy-N, a nickel-based alloy with additions of molybdenum and chromium, has been successfully employed to contain molten fluoride salt at temperatures up to 705°C. However, Hastelloy-N becomes embrittled upon neutron irradiation, primarily due to the accumulation of helium produced by (n,a) transmutation reactions. Furthermore, the corrosive nature of molten fluoride and chloride salts presents a formidable challenge, as these salts can react with and dissolve alloying elements such as Cr, Mo, and Fe, leading to selective leaching, loss of protective oxide layers, and accelerated degradation. High entropy alloys (HEAs) and refractory high entropy alloys (RHEAs) have emerged as a prominent area of interest, due to their ability to achieve tailored chemical compositions for specific applications. Unlike conventional alloys, HEAs are characterized by having multiple principal elements in equimolar or near equimolar ratios, leading to an unconventional alloying strategy [3]. This alloying strategy is believed to promote unique properties, such as single-phase stabilization of chemically compatible elements, lattice distortion effects due to atomic radius differences, and proposed sluggish diffusion effects. For extreme-environment applications, RHEAs have garnered much research interest because of the possibility of creating relatively ductile materials that can operate in extremely high-temperature environments, beyond the operating temperatures where other Ni-based superalloys begin to lose strength [4-6]. Idaho National Laboratory (INL) initiated a joint international effort with the Czech Republic to explore the feasibility of manufacturing HEAs for high-temperature nuclear applications using advanced manufacturing. This effort was funded at INL by the United States Department of Energy's Office of Nuclear Energy under the Advanced Reactor Technologies and Advanced Materials and Manufacturing Technologies (AMMT) Program. The HEAs were specifically designed for the corrosive and irradiation environments experienced in gas-cooled fast reactors, molten salt reactors, and fusion power. These alloys have been manufactured by multiple processes to determine the impact of manufacturing processes on the performance of the alloys in corrosive and irradiation environments. Preliminary molten salt corrosion testing showed that equimolar MoNbTiV and MoNbTi alloys exhibit exceptional performance, with arc-melted variants demonstrating only minimal degradation after 1000 hours of exposure to molten chloride salt at 700°C. Conversely, Nb2TiVZr2 showed significant molten salt corrosion susceptibility and microstructural instability during high-temperature molten salt exposures, and was, therefore deemed unfit for molten salt reactor applications. The MoNbTiV, MoNbTi, and Nb2TiVZr2 alloys were further evaluated through ion irradiation experiments conducted at the Michigan Ion Beam Laboratory at the University of Michigan. The microstructural stability and the evolution of irradiation-induced defects were characterized to assess the irradiation resistance of each of these alloys.

36 - MATERIALS SCIENCE↗