Graphene Oxide Reduces the Hydrolytic Degradation in Polyamide-11

Graphene oxide (GO) was incorporated into polyamide-11 (PA11) via in-situ polymerization. The GO-PA11 nano-composite had elevated resistance to hydrolytic degradation. At a loading of 1 mg/g, GO to PA11, the accelerated aging equilibrium molecular weight of GO-PA11 was higher (33 and 34 kg/mol at 100 and 120 °C, respectively) compared to neat PA11 (23 and 24 kg/mol at 100 and 120 °C, respectively). Neat PA11 had hydrolysis rate constants (kH) of 2.8 and 12 ( × 10(exp -2) day(exp -1)) when aged at 100 and 120 °C, respectively, and re-polymerization rate constants (kP) of 5.0 and 23 ( × 10(exp -5) day(exp -1)), respectively. The higher equilibrium molecular weight for GO-PA11 loaded at 1 mg/g was the result of a decreased kH, 1.8 and 4.5 ( × 10(exp -2) day(exp -1)), and an increased kP, 10 and 17 ( × 10(exp -5) day(exp -1)) compared with neat PA11 at 100 and 120 °C, respectively. The decreased rate of degradation and resulting 40% increased equilibrium molecular weight of GO-PA11 was attributed to the highly asymmetric planar GO nano-sheets that inhibited the molecular mobility of water and the polymer chain. The crystallinity of the polymer matrix was similarly affected by a reduction in chain mobility during annealing due to the GO nanoparticles' chemistry and highly asymmetric nano-planar sheet structure.

Samuel J A Hocker↗

Polyamides based on the renewable monomer, 1,13-tridecane diamine II: Synthesis and characterization of nylon 13,6

The nylon 13,6 was successfully synthesized and its chemical composition, thermal properties, crystal structure, and moisture absorption characterized. Melting temperature and glass transition temperature were determined to be 206 °C and 60 °C, respectively, while the equilibrium melting temperature was determined to be 248 °C. Characterization of the crystallization kinetics showed that nylon 13,6 exhibits very fast crystallization compared to the industrially important nylons, nylon 6 and nylon 6,6. Additionally, the moisture absorption of nylon 13,6 was dramatically lower than nylon 6 and nylon 6,6 which is consistent with the much lower amide content of nylon 13,6. The crystal structure was determined to be different from the expected γ-form, which possess a pseudohexagonal unit cell. Instead, the x-ray scattering pattern was more similar to the α-form. Furthermore, a similar result has been obtained for other odd–even nylons including nylon 5,6, nylon 5,10, nylon 9,2, nylon 11,10, and nylon 11,12.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Tailoring compatibilization potential of maleic anhydride–grafted polypropylene by sequential rheochemical processing of polypropylene and polyamide 66 blends

Reactive compatibilization of immiscible polymer blends using a preferred compatibilizer leaves the following question: How much loading of a compatibilizer is good enough and what maximum properties can be achieved? A good understanding of the process can help solve the reutilization of mixed waste plastics. Here, the reactive compatibilization of polypropylene-graft-maleic anhydride (PP-g-MAH) on polypropylene/polyamide 66 (PP/PA66) blends is quantitatively assessed using thermorheological, microoptical, spectroscopic, and x-ray scattering-based characterization tools. The overall compositions of all PP(60%)/PA66(30%)/PP-g-MAH(10%) blends are kept constant while systematically controlling the degree of the chemical reaction by varying the sequential addition of PP-g-MAH to the melt mixture. The first feeding of PP-g-MAH (x%, 0 ≤ x ≤ 10) is conducted at 280°C and the second feeding of (10–x)% is at 200°C. During the first step, a larger amount of chemical activity is observed up to 4%–6% addition of PP-g-MAH. Furthermore, the constant chemical composition allows a systematic comparison of the compatibilizer-dependent thermal, rheological, morphological, and mechanical properties. With an increased degree of interfacial reaction, the size of dispersed PA66 domains decreases to register improved interfacial adhesion with the PP matrix, yielding enhanced Young's modulus and absolute failure strength of the isotropic matrix.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Substitution of virgin carbon fiber with low-cost recycled fiber in automotive grade injection molding polyamide 66 for equivalent composite mechanical performance with improved sustainability

Recycled carbon fiber has historically proven challenging to integrate into composite manufacturing due in no small part to the low-density, randomly oriented, discontinuous fiber format that results from typical recycling. Discontinuous fiber requires the use of alternative technologies than those traditionally applied to continuous fiber (e.g., hand lay-up, winding). Extrusion compounding is one such applicable technology, but material transfer into the system requires alternative feeding equipment or the use of an altered procedure as trialed in this research. In this study, an injection molding compound for automotive applications was prepared with recycled carbon fiber and compared against an existing commercial compound. Input fibers and molded compound were evaluated for mechanical performance, while relevant variables such as compounded fiber alignment and aspect ratio were compared to the existing baseline material to confirm a like-for-like composite material structure. Overall, analysis indicates that recycled fiber performs similarly to virgin fiber reinforcement, demonstrating that recycled fiber may be a viable drop-in replacement for short-fiber discontinuous applications.