Protective coating system for a regeneratively cooled thrust chamber Final report, 30 Jun. 1967 - 31 Jan. 1969
Ceramic thermal protective coating system for regeneratively cooled hydrogen oxygen thrust chamber
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Ceramic thermal protective coating system for regeneratively cooled hydrogen oxygen thrust chamber
Development of protective coating system for regeneratively cooled thrust chambers
The cold plasma techniques for deposition of various types of protective coatings are reviewed. The main advantage of these techniques for deposition of ceramic films is the lower process temperature, which enables heat treating of the metal prior to deposition. In the field of surface hardening of steel, significant reduction of treatment time and energy consumption were obtained. A simple model for the plasma - surface reactions in a cold plasma system is presented, and the plasma deposition techniques are discussed in view of this model.
Protective aluminum coatings for chromium alloys
Microbend tester and heat-treating apparatus development for study of high temperature protective coatings for refractory metals
Iridium coatings for high temperature oxidation protection on tantalum, niobium, molybdenum, and tungsten
Apparatus, systems, and methods that provide coats on a glass optical fiber including of an inner layer and an outer layer. The method includes two steps. First, a conductive polymer coating is applied to the optical fiber as it is being produced. Second, a protective coating is applied to that conductive polymer coating. The conductive polymer coating is applied immediately after the fiber is drawn from preform to fiber.
Stable photoelectrochemical solar fuel production requires protective coatings to achieve effective charge separation, transport, and injection at the semiconductor–liquid interfaces, implying that the coating should energetically align its intermediate band (IB) with both the photoabsorber's band edge and co-catalyst's potentials. Yet approaches to adjust coating IB positions to accommodate various semiconductor light absorbers for constructing efficient and stable photoelectrodes have not been developed. In this report, three types of transition metal (M = Mn 2+ , Mn 3+ , and Cr 3+ ions) alloyed TiO2 coatings are discovered using atomic layer deposition (ALD). The IB energetics of these coatings are characterized by X-ray photoelectron spectroscopy and are found to be tunable inside the TiO 2 bandgap, through varying ALD growth conditions. By applying these coatings to n-type GaP and integrating with IrO x co-catalysts, the water-oxidation J–E performance is comparable to an uncoated corroding GaP photoanode. It reaches the bulk recombination limit of the GaP and achieves ≈28% absorbed photon to current efficiency under 475-nm light excitation (6.48 mW cm -2 ) and 100-h stable water oxidation. The outstanding performance and stability are attributed to the efficient charge separation and hole transport, as allowed by the energy alignment of the coating IB and the GaP valence band edge.
Atomic oxygen (AO) erodes most organic materials. and ultraviolet radiation embrittles polymers. A previous study indicated untreated polymers such as ultra-high molecular weight polyethylene (UHMWPE) are severely degraded when exposed to AO. This test series was performed to determine the effect of AO and UV on the mechanical integrity of tether materials that were treated with AO-protective coatings. Three coating systems were evaluated for their ability to protect the underlying material from AO erosion. The first coating system is the Photosil surface modification process which incorporates silicon-containing functional groups into the top micron of an organic material. The Photosil process has had favorable results with polyurethane- and epoxy-based thermal control coatings . The second coating system is metallization, in this case nickel. The third coating system is silsesquioxane. The Marshall Space Flight Center Atomic Oxygen Beam Facility (AOBF) was used to simulate low Earth orbit AO of 5 eV energy. In addition, some tether samples were exposed to ultraviolet radiation then evaluated for any changes in mechanical strength. Tether missions, such as a momentum-exchange/electrodynamic reboost (MXER) tether, may benefit from this research.
The paper describes a field-applicable technique for the repair of damage to SiC protective coatings on carbon/carbon composites, using commercial preceramic polymers, such as perhydropolysilazane developed by the Southwest Research Institute and several commercial polymers (NICALON, PS110, PS116, PS117, NCP-200, and PHPS were tested). After being applied on the damaged panel and oxidized at 1400 C, these polymers form either SiC or Si3N4 (or a mixture of both). It was found that impact damaged carbon/carbon specimens repaired with perhydropolysilazane exhibit substantial oxidation resistance. Many of the other tested preceramic polymer were found to be unsuitable for the purpose of repair due to either low ceramic yield, foaming, or intumescence.
Different polyaniline (PANI) based lightning strike protection (LSP) coating thicknesses were tested against simulated lightning strike tests to evaluate the threshold thickness of the coating. A series of lightning strike tests were performed on carbon/glass fiber reinforced polymer (CFRP/GFRP) composites subjected to simulated lightning currents ranging from 40 to 100 kA. Five LSP-coated specimens were considered herein: two CFRP and three GFRP composites. A minimum of ~ 345 μm thick PANI-based LSP coating on CFRP and GFRP composites under a 40 kA peak current retained 83 % and 100 % residual strength, respectively. Additionally, GFRP specimens tested against 60 and 100 kA peak currents exhibited 100 % residual strength. Finally, this study proposes that a PANI-based LSP coating is suitable for protecting GFRP composites, while the careful design is necessary for CFRP composites to avoid any catastrophic failure.
This research addresses cost savings to achieve the SETO target of $15/kWh th for thermal energy storage and 6¢/kWh for levelized cost of energy. Next-generation solar power conversion systems require high-temperature, advanced fluids in the range of 600° to 900°C. The three major advanced fluid groups—supercritical CO 2 , liquid metal alloys, and molten salts—are very corrosive to common alloys used in vessels, heat exchangers, and piping at these temperatures. Understanding degradation mechanisms is essential for making recommendations on proper working conditions and suitable cost-effective coating materials for CSP applications at high temperatures. The implementation of the findings from this research will significantly reduce investment risk by increasing the lifetime of the CSP plant components. In the past, the majority of the hot corrosion evaluations have been performed for waste incinerators, gas turbine engines, and electric power generation (steam-generating equipment) applications for different materials, molten-salt systems, and coatings. Containment materials and resistant coatings for supercritical CO 2 , molten salts and liquid metal alloys have not being evaluated for CSP applications. We plan to understand the underlying degradation mechanisms to select protective approaches such as anodic passivation, cathodic protection, and coating designs.The novelty of the proposed research is the development of protective coatings and working conditions for materials in contact with high temperature TES and HTF. Current state-of-the-art materials and protection methods are non-existent. Novel approaches are: the use of graphite nanomaterials to enhance the non-wettability of the aggressive fluids with the coating; self-healing behavior of Si-coatings in liquid Al-Si alloys; anodic passivation in molten salts to protect metallic substrates and the modeling prediction of attack in liquid metal alloys.
Materials capable of withstanding the harsh lunar environment are critically needed to support long duration, sustainable missions on the Moon’s surface. Lunar dust significantly threatens the durability and reusability of components and vehicles due to possessing a fine, jagged morphology and highly abrasive nature. These characteristics result in the particles eroding, adhering and/or embedding onto component surfaces and into device confined geometries (e.g., gear housing, interlocking systems, etc.) potentially leading to premature failure. The aim of this study is to identify and characterize wear-resistant commercial-off-the-shelf (COTS) materials, including advanced ceramics, for use as protective coatings to minimize abrasion and adhesion caused by lunar dust. Preliminary testing that mimics various aspects of lunar dust degradation, such as abrasive wear and adhesion, suggests that COTS ceramic coatings can improve lunar dust tolerance and protect underlying metallic substrates.
Superior oxidation protection for nickel-base alloys at temperatures up to 1367 K was obtained with cobalt-base alloy coating. Coating had 25 Cr, 14 Al, and 0.5 Y weight percent composition. Coating was applied by electron beam vapor deposition to thickness of 76 to 127 microns.
Aluminized corner-cube polymethylmethacrylate retroreflectors were coated with 92% SiO(x) - 8% fluoropolymer (by volume) and flown on the EURECA spacecraft. The fluoropolymer-filled SiO(x) protective coating was found to be durable to atomic oxygen when exposed in a ground-based plasma asher to an anticipated mission fluence of 2x10(exp 20) atoms/cm(exp 2). Unprotected retroreflector surfaces were found to develop highly diffuse reflectance characteristics, thus inhibiting their use for laser retroreflector purposes. A noncontacting retroreflector optical characterization system was constructed and used to measure the optical retroreflection characteristics of the following retroreflector materials: uncoated unexposed, coated unexposed, both uncoated and coated ground laboratory atomic oxygen exposed, and coated exposed to space atomic oxygen on the EURECA spacecraft. A comparison of the optical characterizations is presented.
The compounds such as Yb14MnSb11 are relatively new p-type thermoelectric materials, respectively. NASA's interest in these material are to replace the state-of-the-art Si-Ge legs of the current radioisotope thermoelectric generators (RTGs). Ideally, the hot end of this leg would operate at 1000 degrees C in the vacuum of space. These materials, however, suffer from a high sublimation rate at elevated temperatures and would require a coating in order to survive the required RTG lifetime of 14 years. The purpose of present work is to develop sublimation protection coatings for Yb14MnSb11 at temperatures up to 1000 degrees C. Coatings for Yb14MnSb11 present many challenges. The coating must not significantly react or interdiffuse with the substrate thereby degrading the substrate or consuming the coating, must remain intact and not crack or spall during thermal cycling prior to launch, and must be a good insulator both electrically and thermally so as not to provide a short circuit for either electron flow or heat through the coating rather than through the leg. Based on these requirements, several oxides have been selected as possible coating candidates. This paper discusses the development of slurry processes to deposit these oxides coatings on thermoelectric materials.
Modified surfaces on metal anodes for batteries can help resist formation of malfunction-inducing surface defects. The modification can include application of a protective nanocomposite coating that can inhibit formation of surface defects. such as dendrites, on the anode during charge/discharge cycles. For example, for anodes having a metal (M'), the protective coating can be characterized by products of chemical or electrochemical dissociation of a nanocomposite containing a polymer and an exfoliated compound (M.sub.a'M.sub.b''X.sub.c). The metal, M', comprises Li, Na, or Zn. The exfoliated compound comprises M' among lamella of M.sub.b''X.sub.c, wherein M'' is Fe, Mo, Ta, W, or V, and X is S, O, or Se.
Composite films consisting of diamond crystallites and hard amorphous films such as diamond-like carbon, titanium nitride, and titanium oxide are provided as protective coatings for metal substrates against extremely harsh environments. A composite layer having diamond crystallites and a hard amorphous film is affixed to a metal substrate via an interlayer including a bottom metal silicide film and a top silicon carbide film. The interlayer is formed either by depositing metal silicide and silicon carbide directly onto the metal substrate, or by first depositing an amorphous silicon film, then allowing top and bottom portions of the amorphous silicon to react during deposition of the diamond crystallites, to yield the desired interlayer structure.