Bismuth borate zinc glass braze for bonding sapphire in air
Highlights: • Sapphire was brazed with a novel 50Bi{sub 2}O{sub 3}–40B{sub 2}O{sub 3}–10ZnO (mol.%) glass at temperatures of 600–700 °C for 20 min in air. • Bi{sub 4}B{sub 2}O{sub 9} and Bi{sub 24}B{sub 2}O{sub 39} were formed in the joints brazed at 600 and 625 °C, respectively. • ZnAl{sub 2}O{sub 4} particles were formed in the joints when the brazing temperature was 635 °C. • The maximum shear strength of 85 MPa was obtained for the joints brazed at 650 °C for 20 min. - Abstract: Reliable brazing of sapphire was successfully achieved by using a novel 50Bi{sub 2}O{sub 3}–40B{sub 2}O{sub 3}–10ZnO (mol%) glass braze and joining cycles that peak at temperatures of 600 − 700 °C for 20 min in air. The effect of the brazing temperature on microstructure evolution as well as mechanical properties of the sapphire/sapphire joints was investigated. The results showed that Bi{sub 4}B{sub 2}O{sub 9} and Bi{sub 24}B{sub 2}O{sub 39} were formed in the joints brazed at 600 and 625 °C, respectively. ZnAl{sub 2}O{sub 4} particles were formed in the joints when the brazing temperature was 635 °C due to a reaction between the glass and the sapphire substrate. With the brazing temperature increasing, ZnAl{sub 2}O{sub 4} particles exhibited steady growth, from ~ 160 nm at 635 °C to ~ 455 nm at 700 °C. Besides, ZnAl{sub 2}O{sub 4} particles began to aggregate when the temperature was 675 °C. The strength increased sharply when the brazing temperature increased to 635 °C, which was mainly attributed to the formation of ZnAl{sub 2}O{sub 4} particles in the joint domain. The maximum shear strength of 85 MPa was obtained for the joints brazed at 650 °C for 20 min. The joint shear strength decreased due to the aggregation of ZnAl{sub 2}O{sub 4} particles in the joint.