Long-term interactive corrosion between International Simple Glass and stainless steel

The interactive corrosion between stainless steel 316 (SS) and International Simple Glass (ISG) has been studied for 12 months. The samples were placed in intimate contact to create crevice corrosion conditions on SS in a 0.6 M NaCl solution with and without 142 ppm dissolved silica species enriched in 29 Si. Corrosion on SS was observed with large pits located close to the crevice mouth at the end of 1 year in 0.6 M NaCl solution. The SS corrosion was also associated with the dissolution of nearby glass in a highly localized manner. When the leaching solution was saturated with silica species, the corrosion rate of SS was suppressed. However, the presence of SS enhances ISG dissolution in both conditions. The implications of the observed phenomena on the long-term storage of nuclear waste are discussed.

36 MATERIALS SCIENCE↗

Influence of temperature and the role of chromium on the kinetics of sulfidation of 310 stainless steel

The sulfidation of 310 stainless steel was studied over the temperature range from 910 K to 1285 K. By adjusting the ratio of hydrogen sulfide, variations in sulfur potential were obtained. The effect of temperature on sulfidation was determined at three different sulfur potentials: 39/sqNm, 0.014/sqNm, and 0.00015/sqNm. All sulfide scales contained one or two surface layers in addition to a subscale. The second outer layer (OL-II), furthest from the alloy, contained primarily Fe-Ni-S. The first outer layer (OL-I), nearest the subscale, contained FE-Cr-S. The subscale consisted of sulfide inclusions in the metal matrix. At a given temperature and sulfur potential, the weight gain data obeyed the parabolic rate law after an initial transient period. The parabolic rate constants obtained at the sulfur potential of 39/sqNm did not show a break when the logarithm of the rate constant was plotted as a function of the inverse of absolute temperature. Sulfidation carried out at sulfur potentials below 0.02/sqNm, however, did show a break at 1145 K, which is termed as the transition temperature. This break was found to be associated with the changes which had occurred in the Fe:Cr ratio of OL-I. Below the transition temperature the activation energy was found to be approximately 125 kj/mole. Above the transition temperature the rate of sulfidation decreased with temperature but dependent on the Fe:Cr ratio in the iron-chromium-sulfide layers of the OL-I. A reaction mechanism consistent with the experimental results has been proposed.

Rao, D. B.↗

Durable nonslip stainless-steel drivebelts

Two toothed stainless-steel drive belt retains its strength and flexibility in extreme heat or cold, intense radiation, or under high loading. Belt does not stretch or slip and is particularly suited to machinery for which replacement is difficult or impossible.

Bahiman, H.↗

The effects of surface pretreatment and nitrogen tetroxide purification on the corrosion rate of Type 304L stainless steel

Corrosion rates of 304L stainless steel coupons in MON-1 oxidizer have been measured as a function of cleaning procedures employed, surface layer positions, propellant impurity levels, and short-term exposure durations (14 to 90 days). Of special interest was propellant contamination by buildup of soluble iron, which may cause flow decay. Surface treatments employed were combinations of cleaning, pickling, and passivation procedures. Propellants used were MIL-SPEC MON-1 and several types of purified NTO (i.e., low water, low chloride) which may, at a later time, be specified as spacecraft grade. Pretest coupon surface analysis by X-ray photoelectron spectroscopy (XPS-ESCA) has revealed important differences, for the different cleaning procedures, in the make-up of the surface layer, both in composition and state of chemical combination of the elements involved. Comparisons will be made of XPS/ESCA data, for different cleaning procedures, for specimens before and after propellant exposure.

Blue, G. D.↗

Defect Production and Microstructural Feature Impact for Radiation Damage in Additively Manufactured 316 Stainless Steel

This milestone presents multi-scale modeling research results for additively manufactured 316 stainless steel. A combination of phase field, cluster dynamics, molecular dynamics, and density functional theory with machine learning is used, allowing for predictions of radiation-driven microstructural evolution in additively manufactured 316 stainless steel over a range of temperatures, damage rates, neutron spectra, and microstructures, and supporting the development of combined ion and neutron irradiation for material qualification. Informed by ion irradiation and neutron irradiation results across the Advanced Materials and Manufacturing Technologies program, we investigate the unique aspects of radiation-driven microstructure evolution in additively manufactured 316 stainless steel. In particular, we focus on understanding the impact of carbon concentration (varying, for example, between the 316L and 316H standards) on void formation; radiation-induced segregation at dislocation cells and grain boundaries; and the evolution of dislocation loops and network dislocation populations. We find that the unique characteristics of the additively manufactured microstructures must be accounted for in understanding the evolution of dislocation populations under thermal and irradiation conditions, such as the variation in sink strengths arising due to the variation in dislocation density. We also find that the radiation-induced segregation of Cr and Ni to grain boundaries and cell walls differs due to the differences in their defect sink biases. We also find that increasing the Ni content can slow vacancy diffusion, which may provide a mechanism for the observed reduction in transient swelling rate for austenitic Fe-Cr-Ni alloys with increasing Ni content. In addition, ion irradiations have shown that increasing carbon content in 316 SS results in a larger population of smaller voids, suggesting reduced vacancy diffusion. Our results show that the carbon content of additively manufactured 316 SS has a significant impact on the migration rate of defect clusters. The presence of carbon atoms results in carbon-vacancy trapping, significantly reducing the diffusion rate of vacancies. Carbon atoms may also be trapped near the surface of a void, which may reduce void growth by trapping vacancies that diffuse toward the void.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Evolution of the role of molybdenum in duplex stainless steels during thermal aging: From enhancing spinodal decomposition to forming heterogeneous precipitates

Thermal aging of ferrite in duplex stainless steels leads to a complex microstructural evolution that can give way to large deleterious changes in mechanical properties. The microstructural evolution mechanisms that happen concurrently are strongly linked to minor changes in composition. By characterizing duplex stainless steels with various compositions over a range of aging conditions, it was revealed that adding a modest amount of Mo to cast austenitic stainless steel (such as changing from grade CF3 to grade CF3M) not only increases the kinetics of spinodal decomposition and Ni-Si-Mn-rich G-phase precipitation, but it also forms a separate Mo-rich phase. At shorter equivalent aging times, Mo segregates from Fe and towards Cr accelerating spinodal decomposition. At longer aging times, Mo enriches in the Ni-Si-Mn clusters before phase separating into an adjoined Mo-rich cluster. We found that these phase changes and precipitation events result in a rather steep drop in fracture and impact toughness. These results will inform the design of similar alloys for use at high temperatures.

36 MATERIALS SCIENCE↗

Friction behavior of 304 stainless steel of varying hardness lubricated with benzene and some benzyl structures

The lubricating properties of some benzyl and benzene structures were determined by using 304 stainless steel surfaces strained to various hardness. Friction coefficients and wear track widths were measured with a Bowden-Leben type friction apparatus by using a pin-on-disk specimen configuration. Results obtained indicate that benzyl monosulfide, dibenzyl disulfide, and benzyl alcohol resulted in the lowest friction coefficients for 304 stainless steel, while benzyl ether provided the least surface protection and gave the highest friction. Strainhardening of the 304 stainless steel prior to sliding resulted in reduced friction in dry sliding. With benzyl monosulfide, dibenzyl disulfide, and benzyl alcohol changes in 304 stainless steel hardness had no effect upon friction behavior.

Buckley, D. H.↗

Forming Limits of Thin Ferritic Stainless Steel for Fuel Cell Application

To lower the cost of fuel cell bipolar plate (BPP), less expensive ferritic stainless steel (FSS) BPP substrate materials are investigated. A series of tensile tests and multistage microchannel-forming tests were conducted on 85-µm-thick ferritic stainless steel foils, 439L, 444, and Chromeshield® 22, to understand the effect of the forming temperatures, tooling geometry, and processes on their formability. Three microchannel-forming processes were conducted, which are 1-Hit (single-stage forming), 2-Hit (two-stage forming) with 50% preform, and 2-Hit with 80% preform. FLC o s at various microchannel-forming conditions were obtained to address the formability of the ferritic stainless steel foils under plane strain conditions. It has been found that the larger the microchannel radius, the better the formability, two-stage forming is superior to the single-stage process, and a larger draw percentage in preform (stage I) leads to a higher FLC o or better formability. It has also been found from tensile tests that the thermal effect (higher temperature) has a negative impact on the failure strains. A similar phenomenon was also observed through channel-forming tests conducted at room temperature, 100 °C, and 200 °C.

08 HYDROGEN↗

Microstructural development in DED stainless steels: applying welding models to elucidate the impact of processing and alloy composition

Austenitic stainless steel microstructures produced by directed energy deposition (DED)are analogous to those developed during welding, particularly high energy density welding. To better understand microstructural development during DED, theories of microstructural evolution,which have been established to contextualize weld microstructures, are applied in this study to microstructural development in DED austenitic stainless steels. Phenomenological welding models that describe the development of oxide inclusions, compositional microsegregation, ferrite,matrix austenite grains, and dislocation substructures are utilized to clarify microstructural evolution during deposition of austenitic stainless steels. Two different alloys, 304L and 316L, arecompared to demonstrate the broad applicability of this framework for understanding microstmctural development during the DED process. Despite differences in grain morphology and solidification mode for these two alloys (which can be attributed to compositional differences),similar tensile properties are achieved. It is the fine-scale compositional segregation and dislocation structures that ultimately determine the strength of these materials. The evolution of microsegregation and dislocation structures is shown to be dependent on the rapid solidification and thermomechanical history of the DED processing method and not the composition of the starting material.

36 MATERIALS SCIENCE↗

Corrosion Performance of Stainless Steels in a Simulated Launch Environment

At the Kennedy Space Center, NASA relies on stainless steel (SS) tubing to supply the gases and fluids required to launch the Space Shuttle. 300 series SS tubing has been used for decades but the highly corrosive environment at the launch pad has proven to be detrimental to these alloys. An upgrade with higher alloy content materials has become necessary in order to provide a safer and long lasting launch facility. In the effort to find the most suitable material to replace the existing AISI 304L SS ([iNS S30403) and AISI 316L SS (UNS S31603) shuttle tubing, a study involving atmospheric exposure at the corrosion test site near the launch pads and electrochemical measurements is being conducted. This paper presents the results of an investigation in which stainless steels of the 300 series, 304L, 316L, and AISI 317L SS (UNS S31703) as well as highly alloyed stainless steels 254-SMO (UNS S32154), AL-6XN (N08367) and AL29-4C ([iNS S44735) were evaluated using direct current (DC) electrochemical techniques under conditions designed to simulate those found at the Space Shuttle Launch pad. The electrochemical results were compared to the atmospheric exposure data and evaluated for their ability to predict the long-term corrosion performance of the alloys.

Calle, Luz Marina↗

Effects of Surface Treatments on the Outgassing of 3D-Printed 316L Stainless Steel.

Fermi National Accelerator Laboratory (Fermilab) is a world leader in designing and operating particle accelerators for nuclear and particle physics research. These accelerators rely on electric fields to propel particle beams, which are then directed and focused using magnetic fields. To ensure these beams travel without interference, they must move through an ultra-high vacuum environment, typically around 10⁻⁹ torr. Maintaining such a vacuum requires materials with exceptionally low outgassing rates. 316L stainless steel is a common material choice for vacuum systems due to its low outgassing rates, excellent corrosion resistance, non-magnetic properties, and high mechanical strength. When manufactured using traditional methods like machining, extrusion, and casting, the vacuum properties of 316L stainless steel are well understood. However, the behavior of 316L stainless steel produced through additive manufacturing, such as Direct Metal Laser Sintering (DMLS), is not as well documented. This study aims to determine the outgassing rate of 316L stainless steel fabricated using DMLS. The investigation focuses on measuring the outgassing rates of 1.5 2 vacuum reducers and evaluating the effects of surface preparation techniques, such as mechanical polishing and electropolishing, on the outgassing performance. Understanding the outgassing performance of 3D-printed 316L stainless steel could enable Fermilab engineers to adopt this fabrication method for producing complex parts designed for ultra-high vacuum environments. These advancements have the potential to benefit projects, such as the Long-Baseline Neutrino Facility (LBNF) and the Proton Improvement Plan-II (PIP-II), by improving design flexibility and fostering innovation in accelerator development.

Cloud, Jaiden [Central State University]↗

Tribocorrosion of stainless steel sliding against graphite in FLiNaK molten salt

The molten salt reactor (MSR) concept recently gained renewed interest in developing Generation IV nuclear reactors. One MSR design uses fluoride molten salts to cool tri-structural isotropic particle fuel encapsulated by a carbon matrix into spherical pebbles, which would inevitably contact the reactor's stainless steel container wall during salt circulation. Characterizing this interaction is crucial for reactor safety. Here, in this work, we report the tribocorrosion behavior of graphite sliding against Type 316H stainless steel lubricated by a FLiNaK (LiF:NaF:KF; 46.5:11.5:42 mol %) molten salt in an argon environment. Accelerated wear loss was observed at a higher temperature because of a lower molten salt viscosity and a higher corrosion rate. The graphite had a more rapid material loss at a higher sliding speed than stainless steel because of its higher vulnerability to vibration-induced microfracture. The salt-starved condition caused more material loss than either the no-salt or the salt-flooded condition because neither a graphite transfer film nor stable boundary lubrication could be established at salt starvation. An interesting dual-layer surface film was discovered on the stainless steel worn surface: a chromium-rich top film and a nickel-accumulated but chromium-depleted interlayer. The film composition and structure provide fundamental insights to the mechanochemical interactions between stainless steel and graphite in a molten salt environment.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

New Method For Joining Stainless Steel to Titanium

In new process, edge of stainless-steel sheet is perforated, and joined to titanium by resistance seam welding. Titanium flows into perforations, forming a strong interlocking joint. Process creates a quasi-metallurgical bond between the thin sheets of stainless steel and titanium.