Search NASA⌕ Search

SEARCH · Search NASA

Results for “STRESS INTENSITY FACTORS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Stress Intensity of Delamination in a Sintered-Silver Interconnection: Preprint

In automotive power electronics packages, conventional thermal interface materials such as greases, gels, and phase-change materials pose bottlenecks to heat removal and are also associated with reliability concerns. The industry trend is toward high thermal performance bonded interfaces for large-area attachments. However, because of coefficient of thermal expansion mismatches between materials/layers and resultant thermomechanical stresses, adhesive and cohesive fractures could occur, posing a reliability problem. These defects manifest themselves in increased thermal resistance. This research aims to investigate and improve the thermal performance and reliability of sintered-silver for power electronics packaging applications. This has been experimentally accomplished by the synthesis of large-area bonded interfaces between metalized substrates and copper base plates that have subsequently been subjected to thermal cycles. A finite element model of crack initiation and propagation in these bonded interfaces will allow for the interpretation of degradation rates by a crack-velocity (V)-stress intensity factor (K) analysis. A description of the experiment and the modeling approach are discussed.

30 DIRECT ENERGY CONVERSION↗

Large Plate Experiment of Chloride-induced Stress Corrosion Cracking in Spent Nuclear Fuel Storage Canisters

This report provides a description of the testing (in progress at the Savannah River National Laboratory) to evaluate the corrosion behavior of a large section of welded plate material harvested from the Sandia National Laboratories’ full-size mockup of a spent nuclear fuel (SNF) dry storage canister. The details of the establishment of this plate test, the interim corrosion results (from visual examination), and the general plan for examination of the plate in CY21 to evaluate crack growth behavior (if any) are provided. This work is intended to inform aging management programs for SNF canisters under conditions of extended dry storage. A “large plate” (approximately 51 x 46 cm with thickness 16 mm and weight about 30 kg) and containing a circumferential weldment from the mockup is the test specimen. The knowledge of the salt, temperature, humidity conditions for chloride-induced stress corrosion cracking (CISCC) including the threshold stress intensity factor, K iscc , were used to setup the large plate test in which a set of part-through-wall and through-wall electrical discharge machined (EDM) defects were positioned in the weld residual stress field of the welded plate material from the mockup canister. A marine salt solution was applied to this plate specimen with an air-brush spray, then dried, and then exposed to a sustained 71-73% RH condition at an ambient room temperature of 22 °C. The salt loading and environmental condition is expected to be aggressive to cause CISCC

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

3D J-Integral Capability in Grizzly

This report summarizes work done to develop a capability to evaluate fracture contour J-Integrals in 3D in the Grizzly code. In the current fiscal year, a previously-developed 2D implementation of a J-Integral evaluation capability has been extended to work in 3D, and to include terms due both to mechanically-induced strains and due to gradients in thermal strains. This capability has been verified against a benchmark solution on a model of a curved crack front in 3D. The thermal term in this integral has been verified against a benchmark problem with a thermal gradient. These developments are part of a larger effort to develop Grizzly as a tool that can be used to predict the evolution of aging processes in nuclear power plant systems, structures, and components, and assess their capacity after being subjected to those aging processes. The capabilities described here have been developed to enable evaluations of Mode- stress intensity factors on axis-aligned flaws in reactor pressure vessels. These can be compared with the fracture toughness of the material to determine whether a pre-existing flaw would begin to propagate during a pos- tulated pressurized thermal shock accident. This report includes a demonstration calculation to show how Grizzly is used to perform a deterministic assessment of such a flaw propagation in a degraded reactor pressure vessel under pressurized thermal shock conditions. The stress intensity is calculated from J, and the toughness is computed using the fracture master curve and the degraded ductile to brittle transition temperature.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Efficient co-solution of time step size and independent state in simulations of fluid-driven fracture propagation with embedded meshes

Here we present an efficient time-continuation scheme for fluid-driven fracture propagation problems in the extended finite element method framework. The approach applies a monolithic solution strategy to a fully coupled and implicit approximation of hydro-mechanical systems in conjunction with simultaneous linear elastic propagation of multiple fractures. At the end of each time step, the process ensures that the weakest fracture tip is in an equilibrium propagation regime. Furthermore, the solution process provides an initialization procedure for the newly created fracture spaces and an a priori estimate of the stress intensity factor growth rate, improving simulation robustness, and efficiency. The solution process is validated using the Kristianovich-Geertsma-de Klerk analytical solution under the toughness- and viscosity-dominated regimes. It is also extended to and demonstrated on problems with multiple fractures undergoing simultaneous propagation with stress shadow interactions. Numerical examples demonstrate that the solution process can reduce the required computational cost by one order of magnitude compared to other existing methods.

42 ENGINEERING↗

Residually Stressed Bimaterial Beam Specimen for Measuring Environmentally Assisted Crack Growth

Background: Subcritical crack growth can occur in a brittle material when the stress intensity factor is smaller than the fracture toughness if an oxidizing agent (such as water) is present at the crack tip. Objective: Here we present a novel bi-material beam specimen which can measure environmentally assisted crack growth rates. The specimen is “self-loaded” by residual stress and requires no external loading. Methods: Two materials with different coefficient of thermal expansion are diffusion bonded at high temperature. After cooling to room temperature a subcritical crack is driven by thermal residual stresses. A finite element model is used to design the specimen geometry in terms of material properties in order to achieve the desired crack tip driving force. Results: The specimen is designed so that the crack driving force decreases as the crack extends, thus enabling the measurement of the crack velocity versus driving force relationship with a single test. The method is demonstrated by measuring slow crack growth data in soda lime silicate glass and validated by comparison to previously published data. Conclusions: The self-loaded nature of the specimen makes it ideal for measuring the very low crack velocities needed to predict brittle failure at long lifetimes.

36 MATERIALS SCIENCE↗

Evaluation of a self-equilibrium cutting strategy for the contour method of residual stress measurement

An assessment of cutting-induced plasticity (CIP) is performed, by finite element (FE) prediction of the plastic strain accumulation along the cut tip when the EDM wire sections the NeT TG4 weld benchmark specimen along two cutting directions. The first direction corresponds to a conventional (C) cutting strategy, whereby the EDM wire cuts through the thickness of the weld specimen and travels in a direction transverse to the weld. The second direction corresponds to a self-equilibrating cutting (SE) strategy, whereby the EDM wire cuts across the transverse direction of the weld specimens and travels through the thickness of the plate. The cutting thus progresses simultaneously through the compression-tension-compression regions of present weld residual stress (WRS) field. This type of cutting strategy is believed to minimize the CIP by minimising residual stress redistribution during cutting, due to stress equilibration across the sectioned material. The simulated cutting procedures are conducted under a range of clamping conditions to assess whether mechanical restraint has a primary or secondary influence on CIP accumulation. Both predictions of CIP and the resultant back-calculated WRS demonstrate that (i) mechanical restraint is the primary variable influencing CIP development, and (ii) under no circumstance does a self-equilibrating cutting strategy perform significantly better than a conventional cutting approach. Furthermore, the reason that self-equilibrating cuts are not effective is illustrated by calculating the Mode I (K I ) stress intensity factor (SIF) along the cut tip, and correlating trends in K I to CIP development.

36 MATERIALS SCIENCE↗

Effect of Specimen Thickness on Fracture Toughness and Plane Stress to Plane Strain Transition in Medium-Density Polyethylene

This study investigates the effect of specimen thickness on fracture toughness and the transition from plane stress to plane strain conditions in Medium-Density Polyethylene (MDPE) using Single Edge Notched Bend (SENB) specimens. Three thickness groups (7.5 mm, 9.0 mm, and 12.1 mm) were tested following ASTM D5045 protocol. Conditional stress intensity factors (KQ) increased from 2.2 MPavm to 2.8 MPavm with increasing thickness, demonstrating significant size dependency. Confocal microscopy revealed a 34% reduction in maximum crack tip opening displacement (CTOD) from 0.478 mm to 0.314 mm as thickness increased, with plastic zone lateral extent decreasing by 32%. This quantitative evidence validates Irwin's theoretical prediction of plastic zone size transition from plane stress r_y˜ (1/2p) (K_I/s_y )^2 to plane strain conditions r_y˜ (1/6p) (K_I/s_y )^2.Scanning electron microscopy confirmed progressive suppression of shear lips and evolution from ductile tearing with extensive polymer chain drawing in thin specimens to localized crazing in thick specimens. Despite all specimens satisfying the ASTM D5045 criterion (B = 2.5(KQ/s_y )^2 ) ,residual shear lips persisted even in the thickest specimens, demonstrating that nominal size requirements alone are insufficient for achieving complete plane strain conditions in highly ductile polymers. The findings emphasize the necessity of integrated analytical and morphological assessment for valid fracture toughness characterization, with critical implications for life assessment and integrity prediction in thick-section polymer components such as natural gas distribution pipelines.

Medium-Density Polyethylene↗

The stress corrosion cracking behavior of alloys 690 and 152 WELD in a PWR environment.

Alloys 690 and 152 are the replacement materials of choice for Alloys 600 and 182, respectively. The latter two alloys are used as structural materials in pressurized water reactors (PWRs) and have been found to undergo stress corrosion cracking (SCC). The objective of this work is to determine the crack growth rates (CGRs) in a simulated PWR water environment for the replacement alloys. The study involved Alloy 690 cold-rolled by 26% and a laboratory-prepared Alloy 152 double-J weld in the as-welded condition. The experimental approach involved pre-cracking in a primary water environment and monitoring the cyclic CGRs to determine the optimum conditions for transitioning from the fatigue transgranular to intergranular SCC fracture mode. The cyclic CGRs of cold-rolled Alloy 690 showed significant environmental enhancement, while those for Alloy 152 were minimal. Both materials exhibited SCC of 10{sup -11} m/s under constant loading at moderate stress intensity factors. The paper also presents tensile property data for Alloy 690TT and Alloy 152 weld in the temperature range 25--870 C.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

An arc-length method for controlled cohesive crack propagation using high-order XFEM and Irwin’s crack closure integral

Numerical modeling of cohesive crack growth in quasi-brittle materials is challenging, primarily due to the combination of (i) nonlinearity associated with the fracture process zone (FPZ), (ii) arbitrary directions to which a crack may propagate, and (iii) snap-back or snap-through instabilities encountered in the response of the structure. To address these challenges, here we propose a novel arc-length method that can follow the equilibrium path of cohesive crack propagation. The proposed approach is based on the extended finite element method (XFEM) with scalar high-order enrichment functions and Irwin’s crack closure integral, which allows for direct control of the applied loads necessary to propagate cohesive cracks. This is achieved by augmenting a constraint equation written in terms of stress intensity factors (SIFs), and expressed explicitly in terms of the enriched degrees of freedom, which is an attractive feature achieved with Irwin’s integral, since SIFs can be written in closed-form. Note that singular enrichments are active in an unstable crack propagation state and automatically vanish in stable crack configurations. Furthermore, to propagate cracks in arbitrary directions, we employ a maximum circumferential stress criterion implemented by (i) direct usage of the SIFs, and by (ii) a new stress-based nonlocal implementation of this principle. Various benchmark problems including pure mode I and mixed-mode fracture are solved to demonstrate the predictive capability of the present framework for cohesive crack modeling.

42 ENGINEERING↗

The shear fracture toughness, K IIc , of graphite

In this study, the critical shear stress intensity factor, K IIc , here-in referred to as the shear fracture toughness, K IIc (MPa m), of two grades of graphite are reported. The range of specimen volumes was selected to elucidate any specimen size effect, but smaller volume specimen tests were largely unsuccessful, shear failure did not occur between the notches as expected. This was probably due to the specimen geometry causing the shear fracture stress to exceed the compressive failure stress. In subsequent testing the specimen geometry was altered to reduce the compressive footprint and the notches (slits) made deeper to reduce the specimen's ligament length. Additionally, we added the collection of Acoustic Emission (AE) during testing to assist with the identification of the shear fracture load. The means of K IIc from large specimens for PCEA and NBG-18 are 2.26 MPa m with an SD of 0.37 MPa m and 2.20 MPa m with an SD of 0.53 MPa m, respectively. The value of K IIc for both graphite grades was similar, although the scatter was large. In this work we found the ratio of K IIc / K Ic ≈ 1.6. .

36 MATERIALS SCIENCE↗

Deformation mechanisms of nanotwinned Al

The objective of this project is to investigate the role of different types of layer interfaces on the formation of high density stacking fault (SF) in Al in Al/fcc multilayers, and understand the corresponding deformation mechanisms of the films. Stacking faults or twins can be intentionally introduced (via growth) into certain fcc metals with low stacking fault energy (such as Cu, Ag and 330 stainless steels) to achieve high strength, high ductility, superior thermal stability and good electrical conductivity. However it is still a major challenge to synthesize these types of defects into metals with high stacking fault energy, such as Al. Although deformation twins have been observed in some nanocrystalline Al powders by low temperature, high strain rate cryomilling or in Al at the edge of crack tip or indentation (with the assistance of high stress intensity factor), these deformation techniques typically introduce twins sporadically and the control of deformation twin density in Al is still not feasible. This project is designed to test the following hypotheses: (1) Certain type of layer interfaces may assist the formation of SF in Al, (2) Al with high density SF may have deformation mechanisms drastically different from those of coarse-grained Al and nanotwinned Cu. To test these hypotheses, we have performed the following tasks: (i) Investigate the influence of layer interfaces, stresses and deposition parameters on the formation and density of SF in Al. (ii) Understand the role of SF on the deformation behavior of Al. In situ nanoindentation experiments will be performed to probe deformation mechanisms in Al. The major findings related to the formation mechanism of twins and mechanical behavior of nanotwinned metals include the followings: 1) Our studies show that nanotwins can be introduced into metals with high stacking fault energy, in drastic contrast to the general anticipation. 2) We show two strategies that can effectively introduce growth twins in high-stacking-energy metals: use Ag as a template to introduce high density growth twins in epitaxial Al; and the film thickness is important in determination of volume fraction of growth twins. 3) We prove that high density twin boundaries can lead to significant work hardening capability in nanotwinned Al. We have published 13 articles, including Nature Communications, Nano Letters, and two review articles, one in Annual Review of Materials Research; and one in MRS Bulletin. Two postdocs and three graduate students have worked on the project. Two of them have become postdoc at Sandia National Laboratory and Los Alamos National Laboratory. One of the postdoc has become a faculty at a University. One patent has been filed.

36 MATERIALS SCIENCE↗

The compelling case for indentation as a functional exploratory and characterization tool

The utility of indentation testing for characterizing a wide range of mechanical properties of brittle materials is highlighted in light of recent articles questioning its validity, specifically in relation to the measurement of toughness. Contrary to assertion by some critics, indentation fracture theory is fundamentally founded in Griffith–Irwin fracture mechanics, based on model crack systems evolving within inhomogeneous but well-documented elastic and elastic–plastic contact stress fields. Notwithstanding some numerical uncertainty in associated stress intensity factor relations, the technique remains an unrivalled quick, convenient and economical means for comparative, site-specific toughness evaluation. Most importantly, indentation patterns are unique fingerprints of mechanical behavior and thereby afford a powerful functional tool for exploring the richness of material diversity. At the same time, it is cautioned that unconditional usage without due attention to the conformation of the indentation patterns can lead to overstated toughness values. Limitations of an alternative, more engineering approach to fracture evaluation, that of propagating a precrack through a “standard” machined specimen, are also outlined. Thus misconceptions in the critical literature concerning the fundamental nature of crack equilibrium and stability within contact and other inhomogeneous stress fields are discussed.

36 MATERIALS SCIENCE↗

Measurement of Fatigue Crack Growth Relationships in Hydrogen Gas for Pressure Swing Adsorber Vessel Steels

We measured the hydrogen-assisted fatigue crack growth rates (da/dN) for SA516 Grade 70 steel as a function of stress-intensity factor range (ΔK) and load-cycle frequency to provide life-prediction data relevant to pressure swing adsorber (PSA) vessels. For ΔK values up to 18.5 MPa m 1/2 , the baseline da/dN versus ΔK relationship measured at 1Hz in 2.8 MPa hydrogen gas represents an upper bound with respect to crack growth rates measured at lower frequency. However, at higher ΔK values, we found that the baseline da/dN data had to be corrected to account for modestly higher crack growth rates at the lower frequencies relevant to PSA vessel operation.

36 MATERIALS SCIENCE↗

Grizzly: A Multi-scale and Multi-Physics Tool to Model Aging of Nuclear Power Plant Components

Grizzly is a multi-scale multi-physics tool being developed at Idaho National Laboratory (INL) as part of the US Department of Energy's Light Water Reactor Sustainability program to provide improved safety assessments of systems, components, and structures in nuclear power plants subjected to age-related degradation. Its goal is to provide an improved scientific basis for decisions surrounding license renewal, which would permit operation of commercial nuclear power plants beyond 60 years. Grizzly is based on INL's MOOSE framework, which enables multi-physics simulations in a massively parallel computing environment. The reactor pressure vessel (RPV) has been chosen as the initial application for Grizzly. The primary concern for the RPV is that it becomes increasingly susceptible to fracture initiation at the sites of pre-existing flaws over time. This is because exposure to irradiation and high temperatures embrittles the steel. Assessing the safety of an RPV under transient conditions involves simulations at multiple scales. At the engineering scale, strongly coupled equations of heat conduction and solid mechanics are solved to simulate the global response of the RPV to accident conditions. Sub-models are used to represent regions with pre-existing flaws and the stress intensity factors are evaluated from the domain integrals. Crack propagation is then determined using a model that provides the temperature and neutron fluence dependent fracture toughness of the RPV steel. The ability of Grizzly to provide accurate engineering scale estimates of RPV safety beyond 60 years of operation strongly relies on the predictability of the embrittlement model. Multiple models for embrittlement have been proposed, and the physically based empirical model is implemented in Grizzly. However, the formation of late blooming phases greatly reduces the confidence on the extrapolated values obtained from embrittlement model, which is further exacerbated by the absence of real field data for validation. Experimentally validated lower length scale models can significantly improve the predictability of the embrittlement model beyond the calibrated range and the development of such models is another ongoing effort in Grizzly. The modeling activity in Grizzly spans across different length scales, and can be divided into: (i) Irradiation induced microstructure evolution at the atomistic and single crystal length scale using molecular dynamics, atomistic kinetic Monte-Carlo, phase-field and rate theory; (ii) Effect of the irradiation induced defects on the flow stress and fracture processes at the polycrystalline scale using crystal plasticity. Subsequently, the prediction from these models can be used to obtain irradiation induced ductile-to-brittle transition temperature (DBTT) shifts from specimen-scale simulations; (iii) Global thermo-mechanical response of the RPV under normal and accident scenarios, and probabilistic risk analyses at the engineering scale using the DBTT shifts obtained from the lower length scale models. The item (i) has been discussed in a previous report. In this extended abstract an overview of items (ii) and (iii) is provided. The extended abstract summarizes the current status of the modeling effort under Grizzly. At the engineering scale, reduced order model development is underway using the statistical tool RAVEN. This will allow probabilistic analysis considering a wide range of flaw topologies in a computationally efficient manner. Coupling the irradiation induced defect growth predictions to crystal plasticity is also in progress. (authors)

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Evaluating methods to reduce duration of near-threshold fatigue crack growth rate measurements for low-alloy steels in hydrogen gas

Measurement of the near-threshold fatigue crack growth rate (da/dN) vs. stress-intensity factor range (∆K) relationship in hydrogen gas is essential for maximizing the calculated design fatigue life of high-pressure hydrogen storage vessels. However, such measurements are rarely performed, since the low cyclic loading frequencies applied in standard practice lead to prohibitively protracted test durations. The objective of this study was to demonstrate two means for reducing test durations when measuring near-threshold da/dN vs. ΔK relationships under decreasing ΔK for low-alloy pressure vessel steels in hydrogen gas: 1) imposing steeper K-gradients relative to the recommended limits in standards such as ASTM E647, and 2) increasing cyclic loading frequency relative to typical values applied during fatigue crack growth testing of low-alloy steels in hydrogen gas. Recognizing that steeper K-gradients could amplify loading-history effects, test methods employing this approach were designed to mitigate such effects by either maintaining constant K max or gradually increasing the K-gradient as the threshold was approached. Although the varying K-gradient method was vulnerable to loading-history effects in the form of plasticity-induced crack closure, particularly at lower stress ratio (R) and higher starting K max values, these effects could be compensated by applying the adjusted compliance ratio (ACR) method. Here, it was demonstrated that steeper K-gradients in concert with increased cyclic loading frequency reduced the duration of near-threshold fatigue crack growth tests in hydrogen gas by more than 99% relative to standard practices.

Fatigue threshold↗

An Improved Fracture Mechanics-Informed Multiscale Thermomechanical Damage Model for Ceramic Matrix Composites

This paper extends recent work done by the authors in modeling length scale-dependent damage behavior of ceramic matrix composites (CMCs) to include effects of local anisotropy introduced by matrix cracking. This model captures scale-dependent damage initiation and propagation behavior of the brittle matrix by employing internal state variable (ISV) theory within a multiscale modeling framework to obtain damaged matrix stress/strain constitutive relationships at each length scale. The damage ISV captures the effects of matrix cracking and growth by using fracture mechanics and the self-consistent scheme to determine the reduced stiffness of the cracked matrix. Matrix cracks, which activate when stress intensity factors near manufacturing induced cavities exceed the fracture toughness of the material, are assumed to be transversely isotropic in the plane of the crack, and matrix anisotropy occurs when the damaged stiffness tensor is rotated from the crack plane to the global axes. The crack progression and temporal evolution of the damage ISV are governed by fracture mechanics and crack growth kinetics. The model effectively captures first matrix cracking, which is the first significant deviation from linear elasticity. The nonlinear predictive capabilities of the material model are demonstrated for monolithic silicon carbide (SiC) and a 2D woven five-harness satin (5HS) carbon fiber SiC matrix (C/SiC) CMC.

Skinner, Travis↗

Modeling Three-Dimensional Fluid-Driven Propagation of Multiple Fractures using TOUGH-FEMM

Here, a novel numerical simulation tool named TOUGH-FEMM is presented and applied to model three-dimensional (3D) hydraulic fracturing in porous rock. The fluid flow in both fractures and porous rock is modeled using TOUGH2, which is a well-established code for analysis of multiphase and multi-component fluid flow. Rock deformations associated with fracture propagation are modeled using finite element-meshfree method (FEMM). FEMM is an approach to simulate fracture propagation without remeshing, in which the fracture path does not need to be predetermined. Fracture mechanics with mixed-mode stress intensity factors are employed to detect fracture instability and determine the direction of fracture propagation. TOUGH-FEMM is confirmed for modeling fluid-driven fracture propagation in 3D through a number of simulation examples, including modeling of hydraulic fracturing laboratory experiments and by comparison to independent numerical simulation results for multiple interacting hydraulic fractures at ten to hundred meter scale.

58 GEOSCIENCES↗

Quantitative In Situ Studies of Dynamic Fracture in Brittle Solids Using Dynamic X-ray Phase Contrast Imaging

Here, we demonstrate the use of X-ray phase contrast imaging with sub-microsecond temporal resolution to obtain quantitative visualization of dynamic fracture processes in brittle solids. We examine an amorphous solid (fused silica), a ceramic single crystal (single-crystal quartz), and a polycrystalline ceramic (boron carbide), in the form of single-edge notched specimens loaded using a three-point apparatus at nominal strain rates up to ~800 s -1 . We observe that the crack tip speed for boron carbide is relatively independent of mode I stress intensity factor rate ($\dot{K}$ I ) for these rates of loading, while that of fused silica and single-crystal quartz increases with $\dot{K}$ I . Further, for the amorphous and single crystal cases, we observe the development of a crack tip instability in the form of crack branching as the crack tip speed approaches 45% of the Rayleigh wave speed. This suggests that strain-rate-dependent mechanisms contribute to crack branching. Such mechanisms may, in turn, affect the macroscopic fracture properties of these materials.

36 MATERIALS SCIENCE↗