Weldability of high-toughness iron - 12 percent-nickel alloys with reactive metal additions of titanium, aluminum, or niobium

Three exceptionally high toughness Fe-12Ni alloys designed for cryogenic service were welded by using the gas tungsten arc welding process. Evaluation of their weldability included equivalent energy fracture toughness tests, transverse weld tensile tests at -196 and 25 C, and weld crack sensitivity tests. The Fe-12Ni-0.25Ti alloy proved extremely weldable for cryogenic applications, having weld and heat affected zone properties comparable to those of the wrought base alloy. The Fe-12Ni-0.5Al alloy had good weld properties only after the weld joint was heat treated. The Fe-12Ni-0.25Nb alloy was not considered weldable for cryogenic use because of its poor weld joint properties at -196 C and its susceptibility to hot cracking.

Delvetian, J. H.↗

Welding of Crack Sensitive Aluminum Alloys for Liquid Rocket Propulsion Applications

In this welding test campaign, electron beam welding (EBW) and manual gas tungsten arc welding (GTAW) processes were utilized to join an additively manufactured aluminum alloy nozzle to a wrought aluminum flange. Both aluminum alloys were 6061, which in their conventional form are susceptible to solidification cracking issues. The AM nozzle utilized a novel high-performance modified version of 6061 which exhibits crack resistant properties during the AM process and during welding. When manually conducting GTAWs a filler wire with the same modified version of 6061 was utilized to weld different combinations of 6061 coupons (either modified or unmodified). Due to the grain refinement technology in the modified 6061, either as filler material or base material, there was complete elimination of weld solidification cracking. During EBW development a combination of wrought 6061 with a modified and additively manufactured 6061 was investigated. The EBWs developed exhibited no crack like defects. Each weld development program utilized non-destructive evaluation, metallography, and mechanical testing to determine the final weld acceptance. Mechanical testing involved hardness evaluation and tension testing on welded coupons. Both welding techniques were successfully developed and exhibited adequate properties for the final test articles and met all requirements of the development campaign. These welds were ultimately developed to be utilized on a set of all-aluminum liquid rocket nozzles to demonstrate additively manufactured aluminum alloys for propulsion applications. These aluminum nozzles were tested at NASA Marshall Space Flight Center’s hot fire test facility and subsequently underwent a test campaign involving a variety of chamber pressures and liquid propellant combinations. Following the hot fire test campaign each weldment was investigated for post operation performance and any defects that may have evolved during testing.

Welding↗

Weld procedure produces quality welds for thick sections of Hastelloy-X

Welding program produces premium quality, multipass welds in heavy tube sections of Hastelloy-X. It develops semiautomatic tungsten/inert gas procedures, weld wire procurement specifications material weld properties, welder-operator training, and nondestructive testing inspection techniques and procedures.

Flens, F. J.↗

Copper Gas Diffusers For Purging Line-Focus Laser Welds

Modified flow diffusers built for inert-gas purging of welds made with 5-kW CO(2) lasers operating with line-focus optics in conduction mode instead of with point-focus optics in customary keyhole mode. Diffusers made of copper components brazed together, robust enough to withstand strong reflections of line-focused laser energy.

Fonteyne, Steve L.↗

Ceramic backup ring prevents undesirable weld-metal buildup

Removable ceramic backup material butted against weld zone back prevents weld metal buildup at that site. Method is successful with manual tungsten-inert gas /TIG/ welding of 316 corrosion resistant steel /CRES/ pieces with 0.76 cm throat diameter and 1.57 cm pipe internal diameter.

Leonard, G. E.↗

Welding investigation of a wrought FeMnAl steel for armor application

A new wrought FeMnAl steel contains high Mn content and high Al content. This steel has high strength. When it is compared to conventional steels with the similar strength, its density is lower. FeMnAl steels can be used in armor vehicle manufacturing, in which welding is a common practice to join the steel plates together. The welding of FeMnAl steels has not been sufficiently studied before. Here, this work studied the weldability and weld microstructure of an FeMnAl steel and provided useful data for the welding practice of FeMnAl steels. The influences of weld filler metals and shielding gases were studied, using single-pass bead-on-plate gas metal arc welding (GMAW) and gas tungsten arc welding (GTAW) two processes. The optimal filler metals and shielding gases have been determined to achieve the better weldability. Autogenous GTAW and electron beam welding were also conducted. Cracks were found in the HAZ in the GMAW welds and electron beam welds. Fewer or no cracks were found in the HAZ of GTAW welds. SEM, SEM/EDX, TEM, TEM/EDX, and EBSD were used to analyze the grain boundaries in the HAZ and the cracks. The grain boundaries of FeMnAl base metal are mostly high angle grain boundaries (HAGBs), which attract impurity and solute atoms and cause intergranular cracking. The proposed cracking mechanisms are liquation cracking and ductility-dip cracking. It was found that GTAW provides much better weldability for the FeMnAl steel than GMAW and EBW.

FeMnAl steel↗

Effects of high frequency current in welding aluminum alloy 6061

Uncontrolled high frequency current causes cracking in the heat-affected zone of aluminum alloy 6061 weldments during tungsten inert gas ac welding. Cracking developed when an improperly adjusted superimposed high frequency current was agitating the semimolten metal in the areas of grain boundary.

Fish, R. E.↗

Weld bead reinforcement removal: A method of improving the strength and ductility of peaked welds in 2219-T87 aluminum alloy plate

The results of a study to determine the degree to which the ductility and tensile properties of peaked welds could be enhanced by removing the reinforcing bead and fairing the weld nugget into the adjacent parent metal are presented. The study employed 2219-T87 aluminum alloy plate, tungsten inert gas (TIG) welding, and 2319 filler wire. The study concluded that significant improvements in peak weld, ultimate strength, and ductility can be obtained through removal and fairing of the weld reinforcing bead. The specimens so treated and tested in this program exhibited ultimate strength improvements of 2 to 3 percent for peak angles of 5.8 to 10 degrees and 10 to 22 percent for welds with peak angles of 11.7 to 16.9 degrees. It was also determined that removal of the weld bead enhanced the ability of peaked welds to straighten when exposed to cyclic loading at stress levels above the yield strength.

Lovoy, C. V.↗

Sensor Control of Robot Arc Welding

The potential for using computer vision as sensory feedback for robot gas-tungsten arc welding is investigated. The basic parameters that must be controlled while directing the movement of an arc welding torch are defined. The actions of a human welder are examined to aid in determining the sensory information that would permit a robot to make reproducible high strength welds. Special constraints imposed by both robot hardware and software are considered. Several sensory modalities that would potentially improve weld quality are examined. Special emphasis is directed to the use of computer vision for controlling gas-tungsten arc welding. Vendors of available automated seam tracking arc welding systems and of computer vision systems are surveyed. An assessment is made of the state of the art and the problems that must be solved in order to apply computer vision to robot controlled arc welding on the Space Shuttle Main Engine.

Sias, F. R., Jr.↗

Internal Wire Guide For Gas/Tungsten-Arc Welding

Wire kept in shielding gas, preventing oxidation. Guide inside gas cup of gas/tungsten-arc welding torch feeds filler wire to weld pool along line parallel to axis of torch. Eliminates problem of how to place and orient torch to provide clearance for external wire guide.

Morgan, Gene E.↗

Trailer shield assembly for a welding torch

This invention relates generally to trailer shields for gas shielded arc welding torches, and more particularly to a trailer shield assembly provided with a shield gas manifold for providing an even dispersion of shield gas to the interior of the shield assembly, which generally encloses a joint being welded and a welding trailing portion of hot welded metal. The novelty of the invention lies in providing trailer shield with a manifold tube having a plurality of openings from which shield gas is distributed. A gas manifold region ahead of the torch is also provided with shield gas from a tube to protect metal preheated by the torch. Further novelty lies in constructing portions of sides and housing and portions of side walls of the guide of stainless steel screen having a tight mesh.

Dyer, Gerald E.↗

Trailing Shield For Welding On Pipes

Trailing shield ensures layer of inert gas covers hot, newly formed bead between two tubes or pipes joined by plasma arc welding. Inert gas protects weld bead from oxidation by air until cooler and less vulnerable to oxidation. Intended for use on nickel-base alloy pipes, on which weld beads remain hot enough to oxidize after primary inert-gas purge from welding-torch cup has passed.

Coby, John B., Jr.↗

A study of gas flow pattern, undercutting and torch modification in variable polarity plasma arc welding

A study on the plasma and shield gas flow patterns in variable polarity plasma arc (VPPA) welding was undertaken by shadowgraph techniques. Visualization of gas flow under different welding conditions was obtained. Undercutting is often present with aluminum welds. The effects of torch alignment, shield gas flow rate and gas contamination on undercutting were investigated and suggestions made to minimize the defect. A modified shield cup for the welding torch was fabricated which consumes much less shield gas while maintaining the weld quality. The current torch was modified with a trailer flow for Al-Li welding, in which hot cracking is a critical problem. The modification shows improved weldablility on these alloys.

Mcclure, John C.↗

Materials and processes for space shuttle's engines

It is pointed out that over 50 different alloys are used in construction of the space shuttle main engines (SSME). Primary construction of the SSME is by welding or brazing of wrought and cast components. Welding processes involve both gas tungsten-arc welds and electron-beam welds. Electroforming has been developed as a process to fabricate and bond structural members for the SSME. Important aspects in the selection of materials and processes are related to weight saving considerations and the high-pressure hydrogen environment. Special problems and their solution in the case of various engine components are discussed, giving attention to the oxidizer preburner, the high pressure oxidizer turbopump, and the heat exchanger.

J. R. Lewis↗