Search NASA⌕ Search

SEARCH · Search NASA

Results for “WELDING, GAS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Welding shield for coupling heaters

Systems for coupling end portions of two elongated heater portions and methods of using such systems to treat a subsurface formation are described herein. A system may include a holding system configured to hold end portions of the two elongated heater portions so that the end portions are abutted together or located near each other; a shield for enclosing the end portions, and one or more inert gas inlets configured to provide at least one inert gas to flush the system with inert gas during welding of the end portions. The shield may be configured to inhibit oxidation during welding that joins the end portions together. The shield may include a hinged door that, when closed, is configured to at least partially isolate the interior of the shield from the atmosphere. The hinged door, when open, is configured to allow access to the interior of the shield.

Menotti, James Louis↗

A Comparative Study of Fracture Toughness at Cryogenic Temperature of Austenitic Stainless Steel Welds

The ITER magnet system is based on the “cable-in-conduit” conductor (CICC) concept, which consists of stainless steel jackets filled with superconducting strands. The jackets provide high strength, limited fatigue crack growth rate and fracture toughness properties to counteract the high stress imposed by, among others, electromagnetic loads at cryogenic temperature. Austenitic nitrogen-strengthened stainless steels have been chosen as base material for the jackets of the central solenoid and the toroidal field system, for which an extensive set of cryogenic mechanical property data are readily available. However, little is published for their welded joints, and their specific performance when considering different combinations of parent and filler metals. Moreover, the impact of post-weld heat treatments that are required for Nb{sub 3}Sn formation is not extensively treated. Welds are frequently responsible for cracks initiated and propagated by fatigue during service, causing structural failure. It becomes thus essential to select the most suitable combination of parent and filler material and to assess their performance in terms of strength and crack propagation at operation conditions. An extensive test campaign has been conducted at 7 K comparing tungsten inert gas (TIG) welds using two fillers adapted to cryogenic service, EN 1.4453 and JK2LB, applied to two different base metals, AISI 316L and 316LN. A large set of fracture toughness data are presented, and the detrimental effect on fracture toughness of post-weld heat treatments (unavoidable for some of the components) is demonstrated. In this study, austenitic stainless steel TIG welds with various filler metals have undergone a comprehensive fracture mechanics characterization at 7 K. These results are directly exploitable and contribute to the cryogenic fracture mechanics properties database of the ITER magnet system. Additionally, a correlation between the impact in fracture toughness and microstructure resulting from the above treatment is provided.

36 MATERIALS SCIENCE↗

Hydrogen-assisted fracture resistance of pipeline welds in gaseous hydrogen

Fracture resistance of pipeline welds from a range of strength grades and welding techniques was measured in air and 21 MPa hydrogen gas, including electric resistance weld of X52, friction stir weld of X100 and gas metal arc welds (GMAW) of X52, X65 and X100. Welds exhibited a decrease in fracture resistance in hydrogen compared to complementary tests in air. A general trend was observed that fracture resistance in 21 MPa hydrogen gas decreased with increasing yield strength. To accommodate material constraints, two different fracture coupon geometries were used in this study, which were shown to yield similar fracture resistance values in air and 21 MPa hydrogen gas; values using different coupons resulted in less than 15% difference. In addition, fracture coupons were removed from controlled locations in select welds to examine the potential influence of orientation and residual stress. The two orientations examined in the X100 GMAW exhibited negligible differences in fracture resistance in air and, similarly, negligible differences in hydrogen. Residual stress exhibited a modest influence on fracture resistance; however, a consistent trend was not observed between tests in air and hydrogen, suggesting further studies are necessary to better understand the influence of residual stress. A comparison of welds and base metals tested in hydrogen gas showed similar susceptibility to hydrogen-assisted fracture. The overall dominant factor in determining the susceptibility to fracture resistance in hydrogen is the yield strength.

08 HYDROGEN↗

Stress and Diffusion in Stored Pu ZPPR Fuel from Alpha Generation

ZPPR (Zero Power Physics Reactor) is a research reactor that has been used to investigate breeder reactor fuel designs. The reactor has been dismantled but its fuel is still stored there. Of concern are its plutonium containing metal fuel elements which are enclosed in stainless steel cladding with gas space filled with helium–argon gas and welded air tight. The fuel elements which are 5.08 cm by 0.508 cm up to 20.32 cm long (2 in × 0.2 in × 8 in) were manufactured in 1968. A few of these fuel elements have failed releasing contamination raising concern about the general state of the large number of other fuel elements. Inspection of the large number of fuel elements could lead to contamination release so analytical studies have been conducted to estimate the probability of failed fuel elements. This paper investigates the possible fuel failures due to generation of helium in the metal fuel from the decay of Pu and its possible damage to the fuel cladding from metal fuel expansion or from diffusion of helium into the fuel gas space. This paper (1) calculates the initial gas loading in a fuel element and its internal free volume after it has been brought into the atmosphere at ZPPR, (2) shows that the amount of helium generated by decay of Pu over 46 years since manufacture is significantly greater than this initial loading, (3) determines the amount of fuel swelling if the helium stays fixed in the fuel plate and estimates the amount of helium which diffuses out of the fuel plate into the fuel plenum assuming the helium does not remain fixed in the fuel plate but can diffuse to the plenum and possibly through the cladding. Since the literature is not clear as to which possibility occurs, as with Schroedinger’s cat, both possibilities are analyzed. The paper concludes that (1) if the gas generated is fixed in the fuel, then the fuel swelling it can cause would not cause any fuel failure and (2) if the helium does diffuse out of the fuel (in accordance diffusivities estimated from the literature), then it is unlikely that fuel element bulging will occur.

99 GENERAL AND MISCELLANEOUS↗

A Technique for the Quantitative Characterization of Weld Microstructure and Application to Mo Welds

The choice of weld parameters determines the size, shape, and curvature of grains in the fusion zone (FZ) and heat-affected zone (HAZ) of welds while the mechanical properties of the welds are correlated to this microstructure. Here, a new technique to quantitatively evaluate these microstructural characteristics in both zones of welds has been applied to molybdenum gas tungsten arc welds fabricated using different weld parameters. Trends in microstructural characteristics in the FZ and HAZ were evaluated and correlated with changes to heat input, weld speed, and weld technique. The use of this approach showed that a 20 pct decrease in heat input caused a 20 pct decrease in the number of FZ grains with aspect ratios ≥ 4. The orientations of the FZ grain segments as a function of distance from the FZ centerline were significantly affected by the weld speed and its effect on weld pool shape. A 50 pct increase in weld speed caused a 20 pct decrease in grain segments orientated 60 to 90 deg from the normal to the direction of welding. This technique also captured differences in grain sizes and grain size anisotropy in the FZ between welds made with a constant current, pulsed current, and use of a 4-pole-magnetic oscillator.

36 MATERIALS SCIENCE↗

Characterization of different forms of Zr-2.5Nb samples before and after neutron irradiation

Deleterious effects of hydride precipitation on the mechanical properties of Zr-based alloy systems have been studied for many years. Most of these studies have been conducted at high-temperature irradiation conditions that are compatible with those in commercial reactor systems, such as light water and pressurized water reactors. Evaluations of hydride effects on the mechanical properties of welded Zr-2.5Nb are sparse among these reported studies. Research on the mechanical properties of Zr-based alloys neutron irradiated at low temperatures (<100 °C) is also very rare in the literature. Since some companies are interested in using Zr-based alloys as structural materials and in other parts such as pressure tubes in small reactor systems, low-temperature irradiation studies of these materials are important. The current work presents an evaluation of the tensile properties of Zr-2.5Nb welded using tungsten inert gas and electron beam welding as a function of hydrogen charging and neutron irradiation at low temperatures (60–100 °C).

36 MATERIALS SCIENCE↗

3D numerical investigation of a free-burning argon arc with metal electrodes using a novel sheath coupling procedure

In this study, a novel coupling procedure describing the complicated plasma-electrode interaction process has been developed and applied into the 3D finite volume simulation of a direct current tungsten inert gas (TIG) welding system. This is achieved by making the space charge layer (sheath) incorporated into the computation domain and interact with both bulk plasma and cathode through the effective electrical conductivity. Both chemical and thermal nonequilibrium phenomena as well as the self-induced magnetic fields have been taken into consideration by the model to ensure a realistic numerical description of a non-thermal arc. The applicability of this coupling procedure is further improved by calculating the real electric potential, which is capable of accounting for the effects of the complicated drift and diffusion processes. Numerical results of both 100 and 200A discharge currents are presented, field reversal is obtained at near-anode regions in both cases, which is followed by the negative anode sheath potential drop. The region of the strongest electron overpopulation appears at the intersection of plasma fringes and electrode surface. Finally, numerical results of plasma temperature and voltage show good agreement with experimental measurements.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Challenges in Making Metal Large-scale Complex Parts for Additive Manufacturing: A Case Study Based on the Additive Manufacturing Excavator (AME)

The Additive Manufacturing Excavator (AME) contained several key components that were 3D printed at The Manufacturing Demonstration Facility (MDF) of Oak Ridge National Laboratory (ORNL); it was presented at and performed a live demonstration for the CONEXPO 2017 exhibition in Las Vegas, Nevada in March of 2017. This paper presents challenges in building functional, large-scale metal parts based on a case study of the excavator. The excavator’s metal arm was 3D printed using a modified Wolf Robotics automated metal inert gas (MIG) welding cell. Tasks included designing a new type of slicer for the metal additive manufacturing (AM) process, integrating the slicing software with the Wolf Robotics system, developing the deposition process, characterizing geometric features and material properties, managing heat, designing mechanical components for metal AM, and developing a machining approach to achieve the final part. Two fully functional excavator arms were printed and machined. Integrated hydraulics passageways that also served as structural stiffeners were included in the build for demonstration purposes. As a direct result of this project, Wolf Robotics is now working towards a commercially available large-scale metal AM system.

Nycz, Andrzej↗

Feasibility Analysis of Utilizing Maraging Steel in a Wire Arc Additive Process for High-Strength Tooling Applications

Traditional tool and die development require skilled labor, long lead time, and is highly expensive to produce. Metal Big Area Additive Manufacturing (mBAAM) is a wire-arc additive process that utilizes a metal inert gas (MIG) welding robot to print large-scale parts layer-by-layer. By using mBAAM, tooling can be manufactured rapidly with low costs. For cold work tooling applications, a high hardness level is desired to increase the life-time of the tool. A promising material that can achieve this is maraging steel. Maraging steel is known to have good weldability; however, further testing must be conducted to ensure it is feasible for printing using mBAAM. In this paper, initial process parameters were obtained by printing single bead welds. Multi-bead walls were then printed with some refinement of process parameters to construct homogenous outer features of the walls. Lastly, the walls were heat-treated, and hardness data was gathered through Rockwell Hardness tests.

Masuo, Chris↗

The Effect of Reduced Pressure on Laser Keyhole Weld Porosity and Weld Geometry in Commercially Pure Titanium and Nickel

Here, the beneficial effect of reduced pressure laser welding in vacuum at 10 -1 mBar was investigated in commercially pure titanium and nickel and compared to atmospheric pressure welding in Ar shielding gas. Partial penetration keyhole welds were made in these materials using a continuous wave disk laser operating at 2-4 kW and travel speeds of 12 and 17 mm/s, where moderate to severe porosity is observed under normal atmospheric pressure welding conditions. Additional welds were made in nickel using an electron beam welding process and the same parameters for comparison. Optical metallography, x-ray radiography, and computed x-ray tomography (CT) were used to characterize the porosity levels in the welds. Quantitative CT results show a monotonically decreasing pore size distribution for all of the welds, and the distributions can be fit with a 2-parameter Wiebull relationship with a beta shape factor that varied between 0.37 and 0.61 depending on the welding conditions. Other results show that laser vacuum essentially eliminates porosity in titanium, and significantly reduces porosity in nickel, but does not completely eliminate porosity in nickel. Laser vacuum welds have increased keyhole penetration and reduced weld widths compared to their atmospheric pressure counterparts, with similar beneficial geometric weld shapes as electron beam welds that are also made in vacuum. Finally, laser vacuum welds showed approximately one-half the volumetric porosity in nickel than electron beam welds, with less porosity at the weld root.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Incoloy 925 Welds in the As-Welded and Direct Aged Conditions

The joints of Incoloy 925 obtained from gas tungsten arc welding (GTAW) with pulsating current utilizing ERNiCrMo-3 and ERNiCrMo-10 were investigated under as-welded and direct aged conditions. The microstructure showed the microsegregation of Nb-Mo-, Ti-rich phases in the weld zone of ERNiCrMo-3 in the as-welded condition. Post-weld heat treatment (PWHT) involving direct aging was carried out on the weldments at 732 °C for 4 h followed by air cooling. On direct aging, the tensile strength of the base metal increases by 40% when compared to the as-received ones. The failures were experienced in the parent metal of Incoloy 925 upon tension testing in as-welded conditions. Although the tensile strength was improved considerably, the failures occurred at the fusion zones, for both the fillers in the direct aged conditions. The joint efficiencies of Incoloy 925 welds employing ERNiCrMo-3 and ERNiCrMo-10 were reported as 95 and 86%, respectively. The impact toughness of the weldments in both the as-welded and PWHT conditions was considerably greater compared to that of the candidate metal.

36 MATERIALS SCIENCE↗

Microstructural Investigation of VPPA–GMAW Welded 7A52 Aluminum Alloys

In this study, the microstructural features of 7A52 heat-treatable aluminum alloys welded by variable polarity plasma arc (VPPA) combined with gas metal arc welding (GMAW) (VPPA–GMAW) were investigated and compared with those of 7A52 aluminum alloys welded by GMAW. The grain structures and modification of the precipitates were analyzed by optical microscopy and transmission electron microscopy. Complementary to modification of the precipitates, the precipitation evolution in the heat-affected zone and magnesium loss in the fusion zone were measured by differential scanning calorimetry and inductively coupled plasma spectroscopy. In VPPA–GMAW, the weld only needs one pass by depositing on one side of the 10-mm-thick aluminum alloy plates because of the large penetration capability of VPPA and good fluidity of the molten metal in the weld pool. Accordingly, the effect of excessive heat input on the microstructure can be minimized. The results show that the grain growth is not obvious and the magnesium loss is small in the fusion zone of VPPA–GMAW compared with that of GMAW under the condition of equal heat input to the workpiece. Small precipitates inside the grains remain homogeneously distributed, and a large volume fraction of the η′ phase exists. The VPPA–GMAW weld exhibits less tendency to soften; thus, VPPA–GMAW is appropriate for welding thick-plate aluminum alloys with a high production rate.

36 MATERIALS SCIENCE↗

Effect of Shielding Gas on the Properties of AW 5083 Aluminum Alloy Laser Weld Joints

The paper deals with the evaluation of the shielding gas influence on the properties of AW 5083 aluminum alloy weld joints produced with disk laser. Butt weld joints were produced under different shielding gas types, namely Ar, He, Ar + 5 vol.% He, Ar + 30 vol.% He and without shielding weld pool. Light and electron microscopy, computed tomography, microhardness measurements and tensile testing were used for evaluation of weld joint properties. He-shielded weld joints were the narrowest ones. On the other hand, Ar-shielded weld joints exhibited largest weld width. The choice of shielding gas had significant influence on the porosity level of welds. The lowest porosity was observed in weld joint produced in Ar with the addition of 5 vol.% He shielding atmosphere (only 0.03%), while the highest level of porosity was detected in weld joint produced in pure He (0.24%). Except unshielded aluminum alloy weld joint, the lowest tensile strength was recorded in He-shielded weld joints. On the contrary, the highest average microhardness was measured in He-shielded weld joints.

36 MATERIALS SCIENCE↗

Characterization of microstructure and texture across dissimilar super duplex/austenitic stainless steel weldment joint by super duplex filler metal

In the present paper, microstructural changes across an as-welded dissimilar austenitic/duplex stainless steel couple welded by a super duplex stainless steel filler metal using gas tungsten arc welding process is characterized with optical microscopy and electron back-scattered diffraction techniques. Accordingly, variations of microstructure, texture, and grain boundary character distribution of base metals, heat affected zones, and weld metal were investigated. The results showed that the weld metal, which was composed of Widmanstätten austenite side-plates and allotriomorphic grain boundary austenite morphologies, had the weakest texture and was dominated by low angle boundaries. The welding process increased the ferrite content but decreased the texture intensity at the heat affected zone of the super duplex stainless steel base metal. In addition, through partial ferritization, it changed the morphology of elongated grains of the rolled microstructure to twinned partially transformed austenite plateaus scattered between ferrite textured colonies. However, the texture of the austenitic stainless steel heat affected zone was strengthened via encouraging recrystallization and formation of annealing twins. At both interfaces, an increase in the special character coincident site lattice boundaries of the primary phase as well as a strong texture with <100> orientation, mainly of Goss component, was observed. - Graphical abstract: Display Omitted - Highlights: • Weld metal showed local orientation at microscale but random texture at macroscale. • Intensification of <100> orientated grains was observed adjacent to the fusion lines. • The austenite texture was weaker than that of the ferrite in all duplex regions. • Welding caused twinned partially transformed austenites to form at SDSS HAZ. • At both interfaces, the ratio of special CSL boundaries of the primary phase increased.

36 MATERIALS SCIENCE↗

CHARACTERIZATION OF DEFECTS IN ALLOY 152, 52 AND 52M WELDS

Defect distributions have been documented by optical metallography, scanning electron microscopy and electron backscatter diffraction in alloy 152 and 52 mockups welds, alloy 52 and 52M overlay mockups and an alloy 52M inlay. Primary defects were small cracks at grain boundaries except for more extensive cracking in the dilution zone of an alloy 52 overlay on 304SS. Detailed characterizations of the dilution zone cracks were performed by analytical transmission electron microscopy identifying grain boundary titanium-nitride precipitation associated with the intergranular separations. I. INTRODUCTION Weldments continue to be a primary location of stress-corrosion cracking (SCC) in light-water reactor systems. While problems related to heat-affected-zone (HAZ) sensitization and intergranular (IG) SCC of austenitic stainless alloys in boiling-water reactors (BWRs) have been significantly reduced, SCC has now been observed in HAZs of non-sensitized materials and in dissimilar metal welds where Ni-base alloy weld metals are used. IGSCC in weld metals has been observed in both BWRs and pressurized water reactors (PWRs) with recent examples for PWR pressure vessel penetrations producing the most concern. This has led to the replacement of alloy 600/182/82 welds with higher Cr, more corrosion-resistant replacement materials (alloy 690/152/52/52M). Complicating this issue has been a known susceptibility to cracking during welding [1-7] of these weld metals. There is a critical need for an improved understanding of the weld metal metallurgy and defect formation in Ni-base alloy welds to effectively assess long-term performance. A series of macroscopic to microscopic examinations were performed on available mockup welds made with alloy 52 or alloy 152 plus selected overlay and inlay mockups. The intent was to expand our understanding of weld metal structures in simulated LWR service components with a focus on as-welded defects. Microstructural features, defect distributions, defect characteristics and weld residual strains were examined by optical metallography, scanning electron microscopy, electron backscatter diffraction and transmission electron microscopy. Industry-supplied mock-up welds were characterized including alloy 52 and 152 weldments, alloy 52M overlay and inlay welds, and an alloy 52 overlay. II. WELDMENTS II.A. Alloy 52 and 152 Weld Mockups The alloy 52 and 152 weld mockups were fabricated by MHI for the Kewaunee reactor and were obtained from the EPRI NDE Center. The mockups were U-groove welds joining two plates of 304SS as shown in Figure 1. Alloy 152 butter (heat 307380) was placed on the U-groove surface for both mockups by shielded metal arc welding (SMAW). For the alloy 152 weld mockup, the alloy 152 fill (heat 307380) was also applied using SMAW while for the alloy 52 weld mockup, the alloy 52 fill (heat NX2686JK) was applied using gas tungsten arc welding (GTAW). Welding parameters for the fill materials were substantially different with the alloy 152 SMAW having a deposition speed of 4-25 cm/min with a current of 95-145 A and the alloy 52 GTAW having a deposition speed of 4-10 cm/min with a current of 150-300 A. One prominent feature in these mockup welds is the presence of a crack starting at the 304SS butt joint at the bottom of the U-groove and extending up into the weld. It appears that the 304SS plate on either side of the butt joint acted as an anchor for the weld resulting in a stress rise across the slit that drove crack formation and extension up into the fill weld. As will be shown in the next section, the extent of the cracking around this stress riser was much greater in the MHI 52 weld mockup.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

The Effect of Weld Metal Composition on Microstructural and Mechanical Properties of Dissimilar Welds Between Monel 400 and Inconel 600

The current work was carried out to characterize welding of Inconel 600 superalloy and Monel 400. In the present study, gas tungsten arc welding (GTAW) with four types of filler metals (ENiCu, ENiCu-7, ENiCr-3 and ENiCrFe-3) was utilized. The filler metals were categorized into two groups based on the presence of Cr and Nb in their chemical composition. This paper describes the selection and application of welding consumables in manufacturing dissimilar metal combinations. It was found that (Nb/Cr) ratio and Fe content can affect on the size and amount of carbides. During solidification of ENiCr-3 and ENiCrFe-3 filler metals, Nb leaves dendritic cores and is rejected to inter-dendritic regions because of its high tendency for segregation. However, No brittle Laves phase was detected in the welds. The interface between weld metal and base metal and gradual changes in alloying elements were also investigated by scanning electron microscopy. EDX analysis was also applied for different samples. Microhardness measurements and tensile test were performed on the joints. The average hardness value in the weld metal obtained from ENiCrFe-3 is higher than the other welds. ENiCu-7 weld exhibited the highest tensile strength of 540 MPa and percent elongation of 53% in contrast to ENiCrFe-3 weld with the lowest tensile strength (518 MPa) and percent elongation (39%).

36 MATERIALS SCIENCE↗

Characterization of as-welded microstructure of heat-affected zone in modified 9Cr–1Mo–V–Nb steel weldment

Non-equilibrium microstructure of the heat-affected zone (HAZ) in the as-welded modified 9Cr–1Mo–V–Nb pipe steel (P91) weldment deposited by gas tungsten arc welding (GTAW) and flux core arc welding (FCAW) has been characterized by field-emission scanning electron microscope (FESEM) and electron backscatter diffraction (EBSD). The heterogeneous structures in the sub-layers of the as-welded HAZ are attributable to phase transformations caused by the welding thermal cycles and the local structure variations in the as-received base metal. Coarse-grained heat-affected zone (CGHAZ) has a prior austenite grain (PAG) size of 20 μm. Fine uniformly-distributed precipitates and a higher fraction of MX carbonitrides are observed in the CGHAZ. Fine-grained heat-affected zone (FGHAZ) consists of the finest grains (1.22 μm measured by EBSD, 5 μm PAG size), coarse undissolved M{sub 23}C{sub 6} carbides within the PAG boundaries and fine nucleated M{sub 23}C{sub 6} particles within the martensite laths. Inter-critical heat-affected zone (ICHAZ) consists of partially austenitized grains and over-tempered martensite laths. EBSD kernel average misorientation (KAM) map in the FGHAZ close to the ICHAZ illustrates the greatest local strain variations with a moderate normalized KAM value of 0.92°. The majority (88.1%) of the matrix grains in the CGHAZ are classified as deformed grains by EBSD grain average misorientation (GAM) evaluation. The FGHAZ close to the ICHAZ has the most recrystallized grains with an area fraction of 14.4%. The highest density variation of precipitates within grains in the FGHAZ originates from the inhomogeneous chemistry in the base metal. - Highlights: •A comprehensive characterization of the as-welded HAZ of P91 weldment is conducted. •Structural features in the each layer of the HAZ are quantified by EBSD. •Structural heterogenities in HAZ are due to welding cycle and base metal structure. •FGHAZ contains the finest grain structure and largest precipitate density variation.

36 MATERIALS SCIENCE↗