Search NASA⌕ Search

SEARCH · Search NASA

Results for “ZIRCONIUM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Zirconium Oxide Nanostructures Prepared by Anodic Oxidation

Zirconium oxide is an advanced ceramic material highly useful for structural and electrical applications because of its high strength, fracture toughness, chemical and thermal stability, and biocompatibility. If highly-ordered porous zirconium oxide membranes can be successfully formed, this will expand its real-world applications, such as further enhancing solid-oxide fuel cell technology. Recent studies have achieved various morphologies of porous zirconium oxide via anodization, but they have yet to create a porous layer where nanoholes are formed in a highly ordered array. In this study, electrochemical methods were used for zirconium oxide synthesis due to its advantages over other coating techniques, and because the thickness and morphology of the ceramic films can be easily tuned by the electrochemical parameters, such as electrolyte solutions and processing conditions, such as pH, voltage, and duration. The effects of additional steps such as pre-annealing and post-annealing were also examined. Results demonstrate the formation of anodic porous zirconium oxide with diverse morphologies, such as sponge-like layers, porous arrays with nanoholes ranging from 40 to 75 nm, and nanotube layers. X-ray powder diffraction analysis indicates a cubic crystallographic structure in the zirconium oxide. It was noted that increased voltage improved the ability of the membrane to stay adhered to the zirconium substrate, whereas lower voltages caused a propensity for the oxide film to flake off. Further studies are needed to define the parameters windows that create these morphologies and to investigate other important characteristics such as ionic conductivity.

30 DIRECT ENERGY CONVERSION↗

Alloying effect of niobium and tin on the zirconium alloy fuel cladding behavior at high temperature oxidation in steam - 2016-0072

As the materials for fuel claddings for water-cooled reactors, binary and multicomponent zirconium alloys zirconium-niobium (Zr-Nb) (E110, M5), zirconium-tin-iron (Zr-Sn-Fe) (Zircaloy-2,-4), and zirconium-niobium-tin-iron (Zr-Nb-Sn-Fe) (E635, ZIRLO{sup R} ) most commonly are used. Improvement extends, in particular, by varying their composition by niobium, tin, and iron. At the same time, importance is given to ensuring the safe operation of the fuel rods not only in normal conditions but also in emergency situations such as a loss of coolant accident. In this paper, we present the research results of studies of the influence of alloying elements niobium, tin, and iron on corrosion resistance and embrittlement at high-temperature steam oxidation of fuel claddings based on the alloy types Zr-xNb (x=1.0/2.5) and Zr-xNb-ySn-zFe (x=0.6/2.4; y=0.24/1.1; z=0.18/0.34) made by using zirconium sponge. We conducted high-temperature steam oxidation tests at temperatures of 1,000 deg. C, 1,100 deg. C, and 1,200 deg. C with continuous measurement of the weight gain during the experiment and subsequent cooling in steam with rate ∼ 20 deg. C/s. We conducted studies of kinetics of high-temperature oxidation in steam, structural-phase state changes, alloying elements distribution, absorbed hydrogen content, and residual ductility after rapid cooling of the oxidized specimens. We revealed the difference in the oxidation kinetics of the materials studied, which decreased as the oxidation temperature increased. Likewise, an increase of the tin content in the alloy influenced a specimen's breakaway oxidation intensification at 1,000 deg. C. This shows that the mechanical properties of fuel claddings oxidized under the same conditions depend on their alloying composition, and the hydrogen fraction is absorbed by the specimen and formed by the oxidation of ZrO{sub 2}, α-Zr(O), and ex-β layer structures, which in turn varies depending on the alloy composition. The increase of niobium, tin, and iron content in the zirconium alloy leads to a decrease in the residual ductility of fuel claddings after high-temperature steam oxidation. According to obtained results, among the materials studied, Zr-1.0Nb alloy is the most resistant to embrittlement during high-temperature steam oxidation at temperatures of 1,000-1,200 deg. C. (authors)

36 MATERIALS SCIENCE↗

Diffusion bonding of tungsten-vanadium-zirconium using vacuum hot pressing for the development of a low decay heat cladding solution for tungsten spallation targets

Tantalum has been used as cladding material for water-cooled solid tungsten targets at many leading spallation neutron production facilities thanks to its high neutron yield, manageable radiation damage behavior, and excellent corrosion/erosion resistance in radiation environments. However, from a safety hazard perspective, thermal neutron capture of tantalum in spallation environments causes a high specific decay heat in the target volume, which often becomes a limiting factor in increasing the beam power on the target. In this paper, we studied vacuum hot pressing (VHP) parameters to diffusion bond zirconium to tungsten to explore the feasibility of using zirconium alloys as an alternative cladding material to tantalum. Zirconium alloys have long been used as cladding material for early generation solid spallation targets, and nuclear fuel rods. In spallation environments zirconium has significantly lower decay heat with shorter decay time compared to tantalum. The hot isostatic pressing (HIP) of zirconium and tungsten is known to produce limited bonding quality due to the formation of the brittle ZrW2 intermetallic layer. To overcome this problem, placing a vanadium interlayer between tungsten and zirconium has been proposed by exploring parameter space in binary alloy phase diagrams. Under the VHP conditions, 860 ◦C at 70 MPa for 4 hours, Zr-V and V-W showed good diffusion bonding, which demonstrates the feasibility of a single step HIP process to make the zirconium alloy clad tungsten spallation volumes.

Lee, Yong Joong↗

Capture of Tritium Released from Cladding in the Zirconium Recycle Process

Zirconium may be recovered from the Zircaloy® cladding of used nuclear fuel (UNF) for recycle or to reduce the quantities of high-level waste destined for a geologic repository. Recovery of zirconium using a chlorination process is currently under development at the Oak Ridge National Laboratory. The approach is to treat the cladding with chlorine gas to convert the zirconium in the alloy (~98 wt % of the alloy mass) to zirconium tetrachloride. A significant fraction of the tritium (0–96%) produced in nuclear fuel during irradiation may be found in zirconium-based cladding and could be released from the cladding when the solid matrix is destroyed by the chlorination reaction. To prevent uncontrolled release of radioactive tritium to other parts of the plant or to the environment, a method to recover the tritium may be required. The focus of this effort was to (1) identify potential methods for the recovery of tritium from the off-gas of the zirconium recycle process, (2) perform scoping tests on selected recovery methods using nonradioactive gas simulants, and (3) select a process design appropriate for testing on radioactive gas streams generated by the engineering-scale zirconium recycle demonstrations on radioactive used cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Capture of Tritium Released from Cladding in the Zirconium Recycle Process

This report is issued as the first revision to FCRD-MRWFD-2016-000297. Zirconium may be recovered from the Zircaloy® cladding of used nuclear fuel (UNF) for recycle or to reduce the quantities of high-level waste destined for a geologic repository. Recovery of zirconium using a chlorination process is currently under development at the Oak Ridge National Laboratory. The approach is to treat the cladding with chlorine gas to convert the zirconium in the alloy (~98 wt % of the alloy mass) to zirconium tetrachloride. A significant fraction of the tritium (0–96%) produced in nuclear fuel during irradiation may be found in zirconium-based cladding and could be released from the cladding when the solid matrix is destroyed by the chlorination reaction. To prevent uncontrolled release of radioactive tritium to other parts of the plant or to the environment, a method to recover the tritium may be required. The focus of this effort was to (1) identify potential methods for the recovery of tritium from the off-gas of the zirconium recycle process, (2) perform scoping tests on selected recovery methods using non-radioactive gas simulants, and (3) select a process design appropriate for testing on radioactive gas streams generated by the engineering-scale zirconium recycle demonstrations on radioactive used cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

ZIRCONIUM OXIDE NANOSTRUCTURES PREPARED BY ANODIC OXIDATION

Zirconium oxide is an advanced ceramic material highly useful for structural and electrical applications because of its high strength, fracture toughness, chemical and thermal stability, and biocompatibility. If highly-ordered porous zirconium oxide membranes can be successfully formed, this will expand its real-world applications, such as further enhancing solid-oxide fuel cell technology. Recent studies have achieved various morphologies of porous zirconium oxide via anodization, but they have yet to create a porous layer where nanoholes are formed in a highly ordered array. In this study, electrochemical methods were used for zirconium oxide synthesis due to its advantages over other coating techniques, and because the thickness and morphology of the ceramic fi lms can be easily tuned by the electrochemical parameters, such as electrolyte solutions and processing conditions, such as pH, voltage, and duration. The effects of additional steps such as pre-annealing and post-annealing were also examined. Results demonstrate the formation of anodic porous zirconium oxide with diverse morphologies, such as sponge-like layers, porous arrays with nanoholes ranging from 40 to 75 nm, and nanotube layers. X-ray powder diffraction analysis indicates a cubic crystallographic structure in the zirconium oxide. It was noted that increased voltage improved the ability of the membrane to stay adhered to the zirconium substrate, whereas lower voltages caused a propensity for the oxide fi lm to fl ake off. Further studies are needed to defi ne the parameters windows that create these morphologies and to investigate other important characteristics such as ionic conductivity.

Dang, Y Y↗

The Effect of Boron and Zirconium on the Structure and Tensile Properties of the Cast Nickel-Based Superalloy ATI 718Plus

The effects of boron and zirconium on cast structure, hardness, and tensile properties of the nickel-based superalloy 718Plus were investigated. For this purpose, five alloys with different contents of boron and zirconium were cast via vacuum induction melting and then purified via vacuum arc remelting. Microstructural analysis by light-optical microscope and scanning electron microscope equipped with energy-dispersive x-ray spectroscopy and phase studies by x-ray diffraction analysis were performed. The results showed that boron and zirconium tend to significantly reduce dendritic arm spacing and increase the amount of Laves, Laves/gamma eutectic, and carbide phases. It was also found that boron led to the formation of B{sub 4}C and (Cr, Fe, Mo, Ni, Ti){sub 3}B{sub 2} phases and zirconium led to the formation of intermetallic phases and ZrC carbide. In the presence of boron and zirconium, the hardness and its difference between dendritic branches and inter-dendritic spaces increased by concentrating such phases as Laves in the inter-dendritic spaces. These elements had a negative effect on tensile properties of the alloy, including ductility and strength, mainly because of the increase in the Laves phase. It should be noted that the largest degradation of the tensile properties occurred in the alloys containing the maximum amount of zirconium.

36 MATERIALS SCIENCE↗

Ion flux characteristics and efficiency of the deposition processes in high power impulse magnetron sputtering of zirconium

High power impulse magnetron sputtering of zirconium was investigated at the average target power density of up to 2.22 kW cm{sup -2} in a pulse. The depositions were performed using a strongly unbalanced magnetron with a planar zirconium target of 100 mm diameter at the argon pressure of 1 Pa. The repetition frequency was 500 Hz at duty cycles ranging from 4% to 10%. Time-averaged mass spectroscopy was carried out at the substrate positions of 100 and 200 mm from the target. The increase in the average target power density from 0.97 kW cm{sup -2} to 2.22 kW cm{sup -2} in shortened voltage pulses (from 200 to 80 {mu}s) at an average target power density of 100 W cm{sup -2} in a period led to high fractions (21%-32%) of doubly charged zirconium ions in total ion fluxes onto the substrate located 100 mm from the target. However, the respective fractions of singly charged zirconium ions decreased from 23% to 3%. It was observed that ion energy distributions were extended to high energies (up to 100 eV relative to the ground potential) under these conditions. The increased target power densities during the shortened voltage pulses resulted in a reduced deposition rate of films from 590 to 440 nm/min and in a weakly decreasing ionized fraction (from 55% to 49%) of the sputtered zirconium atoms in the flux onto the substrate. The doubly charged zirconium ions became strongly predominant (up to 63%) in the total ion flux onto the substrate at the distance of 200 mm from the target. Model calculations were carried out to explain the complicated deposition processes.

36 MATERIALS SCIENCE↗

Synthesis of zirconium tungstate-zirconia core-shell composite particles

Highlights: {yields} ZrW{sub 2}O{sub 8}-ZrO{sub 2} core-shell particles to offer solutions for sintering problems. {yields} Core synthesis by a precursor based on tungstic acid and zirconium acetate. {yields} Shell phase by urea hydrolysis in the presence of zirconium ions. {yields} [Urea]/[ZrOCl{sub 2}] ratio controls the rate of shell precursor precipitation. -- Abstract: In this work, ZrW{sub 2}O{sub 8}-ZrO{sub 2} core-shell composite particles were synthesized. ZrW{sub 2}O{sub 8} that was used in the core is a material with negative coefficient of thermal expansion, and it was synthesized from a high-pH precursor based on use of tungstic acid and zirconium acetate. Shell layer was composed of ZrO{sub 2} nanocrystallites and precipitated from an aqueous solution by urea hydrolysis. While volume of the shell was effectively controlled by the initial zirconium ion concentration in the solutions, the rate of precipitation was a function of the ratio of initial concentrations of urea to zirconium ions. It is hypothesized that isolation of the ZrW{sub 2}O{sub 8} within a layer of ZrO{sub 2}, will be a key element in solving problems associated with reactivity of ZrW{sub 2}O{sub 8} towards other components in sintering of ceramic-ceramic composites with tuned or zero thermal expansion coefficient.

36 MATERIALS SCIENCE↗

Anticorrosive Behavior and Porosity of Tricationic Phosphate and Zirconium Conversion Coating on Galvanized Steel

This work evaluates the corrosion resistance of galvanized steel treated with tricationic phosphate and zirconium conversion coating after painting, by using electrochemical techniques, accelerated and field corrosion tests. A non-uniform and heterogeneous distribution of zirconium on the steel surface was observed due to preferential nucleation of the zirconium on the aluminum-rich sites on the surface of galvanized steel. The long-term anti-corrosion performance in a saline solution was better for the phosphate coating up to 120 days. The coating capacitance registered a higher increase for the zirconium coatings than the phosphate coatings up to 120 days of immersion. This result agrees with the higher porosity of zirconium coating in relation to the phosphate coating. After 3840 h of accelerated corrosion test, and after 1 year of accelerated field test, zirconium-treated samples showed an average scribe delamination length higher than the phosphate-treated samples.

36 MATERIALS SCIENCE↗

Nanoindentation study of bulk zirconium hydrides at elevated temperatures

Here, the mechanical properties of zirconium hydrides was studied using nano-indentation technique at a temperature range of 25 – 400 °C. Temperature dependency of reduced elastic modulus and hardness of δ- and ε-zirconium hydrides were obtained by conducting nanoindentation experiments on the bulk hydride samples with independently heating capability of indenter and heating stage. The reduced elastic modulus of δ-zirconium hydride (H/Zr ratio =1.61) decreased from ~113 GPa to ~109 GPa while temperature increased from room temperature to 400°C. For ε-zirconium hydrides (H/Zr ratio=1.79), the reduced elastic modulus decreased from 61 GPa to 54 GPa as temperature increased from room temperature to 300 °C. Whereas, hardness of δ-zirconium hydride significantly decreased from 4.1 GPa to 2.41 GPa when temperature increased from room temperature to 400 °C. Similarly, hardness of ε-zirconium hydride decreased from 3.06 GPa to 2.19 GPa with temperature increase from room temperature to 300°C.

36 MATERIALS SCIENCE↗

Modification in band gap of zirconium complexes

The optical properties of zirconium complexes with amino acid based Schiff bases are reported here. The zirconium complexes show interesting stereo chemical features, which are applicable in organometallic and organic synthesis as well as in catalysis. The band gaps of both Schiff bases and zirconium complexes were obtained by UV-Visible spectroscopy. It was found that the band gap of zirconium complexes has been modified after adding zirconium compound to the Schiff bases.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Methods to Capture the Tritium Released by Recovery/Recycle of Zirconium from Used Fuel Cladding: A Review

After uranium, the second largest mass contained in most used nuclear fuel (UNF) is the zirconium-based Zircaloy{sup R} cladding in the fuel cladding which accounts for about 25% of the mass. In current practice, the cladding requires disposal in a geologic repository. Zirconium may be recovered from the Zircaloy cladding of UNF for recycle. Alternatively, it may be decontaminated to recategorize it as low-level waste. Either approach reduces the quantities of high-level waste destined for a geologic repository, thereby reducing the overall cost of recycling UNF. Process development studies are under way in the United States and Republic of Korea based on dry chlorination using a mixture of chlorine (Cl{sub 2}) and an inert carrier such as argon (Ar) to convert the zirconium in the alloy, which is greater than 98 wt% of the alloy mass, to zirconium tetrachloride (ZrCl{sub 4}). The ZrCl{sub 4} is volatile and is easily separated from the non-volatile components. The residues include non-volatile chlorides such as CrCl{sub 3}, oxychlorides and oxides. The product ZrCl{sub 4} is recovered as a solid salt by condensation when cooled to less than about 300 deg. C. Feasibility tests with actual UNF cladding have demonstrated that the recovered zirconium chloride salt is sufficiently separated from fuel and fission product radionuclides that it emanates no significant dose and can be handled without shielding. Several methods for capturing tritium released from cladding during the chlorination process have been identified. A detailed description of the methodologies, advantages, drawbacks, and conceptual flowsheets will be presented. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Investigations into the Gas Phase Reactions of Zirconium Tetrachloride (ZrCl) from UNF Cladding

Zirconium-based cladding materials that surround used nuclear fuel (UNF) rods represent a significant fraction of the total amount of high level waste that must be disposed of in long term geological repositories. The decontamination, recovery and reuse of these materials would significantly reduce the high level waste associated with light water reactors and could provide a new source of hafnium free zirconium for the fabrication of new nuclear components. A step in a strategy to recycle zirconium from used cladding materials is the high yield chlorination of Zircaloys to produce zirconium tetrachloride (ZrCl{sub 4}). The ZrCl, is contaminated with other metal chloride species that originate from the alloying metals as well as contaminants from oxide layers on the cladding, trace fission products, fuel residues, activation byproducts, and tritium. The properties of these complex mixtures must be better understood before purification protocols can be developed that will allow zirconium chloride to be recycled further. First order thermodynamic modeling of high temperature mixtures of ZrCl, and other metal chlorides in the gas phase may not accurately predict their properties. Computational modeling studies indicate that mixed metal adducts may form under the conditions of sublimation-based purification protocols. In light of these predictions, alternate strategies may also be needed to obtain pure ZrCl, from such mixtures. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Overcoming the crystallization and designability issues in the ultrastable zirconium phosphonate framework system

Metal-organic frameworks (MOFs) based on zirconium phosphonates exhibit superior chemical stability suitable for applications under harsh conditions. These compounds mostly exist as poorly crystallized precipitates, and precise structural information has therefore remained elusive. Furthermore, a zero-dimensional zirconium phosphonate cluster acting as secondary building unit has been lacking, leading to poor designability in this system. We overcome these challenges and obtain single crystals of three zirconium phosphonates that are suitable for structural analysis. Furthermore, these compounds are built by previously unknown isolated zirconium phosphonate clusters and exhibit combined high porosity and ultrastability even in fuming acids. SZ-2 possesses the largest void volume recorded in zirconium phosphonates and SZ-3 represents the most porous crystalline zirconium phosphonate and the only porous MOF material reported to survive in aqua regia. SZ-2 and SZ-3 can effectively remove uranyl ions from aqueous solutions over a wide pH range, and we have elucidated the removal mechanism.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Design of Laboratory System to Recover Tritium from Zirconium Recycle and Plan to Test System

The objective of the tritium separations task is to develop a viable process to separate tritium from the zirconium recycle off-gas stream. In support of this long-term objective, the goal of the present work is to design a test system and prepare a test plan for an alternate tritium capture method suitable for, and compatible with, recycle of the reactive gas (i.e., chlorine) in the zirconium recycle process. The zirconium recycle process is under development to recover zirconium from the Zircaloy® cladding component of used nuclear fuel. Small quantities of all isotopes of hydrogen (all H) are trapped in the Zircaloy as zirconium hydride. Processing releases and converts this hydrogen to hydrogen chloride, including tritium-substitu ted hydrogen chloride, 3 HCl (a.k.a., TCl). This compound of tritium must be removed from the zirconium recycle process off-gas and sequestered to satisfy regulations governing emissions of tritium.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Thermomechanical Processing of Uranium Alloys with 10 and 50 Weight Percent Zirconium

This work focuses on casting and thermomechanical processing for moderate sized (500-1000g) 10% by weight and 50% by weight uranium-zirconium alloys. Three castings of uranium – 10wt% zirconium and a fourth casting of uranium – 50wt% zirconium were completed using different castings processes. The first casting process relied on only induction mixing within the VIM system thereby eliminating the need for an arc-melting feedstock preparation step. The second casting process used the arc-melting process prior for feedstock to the same VIM system. In this study, the induction mixing process alone with a graphite crucible appears insufficient for the fabrication of UZr alloys. Graphite is suitable with the use of master alloy UZr feedstock produced by arc-melting. There was a moderate increase of approximately 100 ppm of carbon within the U10Zr alloys. However, there was a near 1000 ppm increase of carbon in the U50Zr alloy. This carbon content is considered too high for forming processes, and therefore, warrants the use of a ceramic crucible for UZr castings near 50wt% zirconium. Zirconia does not appear suitable for UZr castings near 50wt% zirconium. The use of Beryllia or Thoria may be a more suitable option. However, due to the significantly lower liquidus and lower zirconium content, Zirconia crucibles do appear viable for carbon reduction in the U10Zr system. Two thermomechanical processes are also studied in this work - hot extrusion of the U50Zr system and heat treatment in an argon atmosphere. This work demonstrated that extrusion of the U50Zr alloy near 680°C is a viable choice even with +1000 ppm carbon. Extrusion of the U50Zr system near 630°C was unsuccessful and does not appear viable unless significant force and tooling strength is available. There appears to be a moderate increase in extrudate hardness when compared to as-cast. Heat-treatment reduced the hardness of as-cast alloys in the U10Zr castings as well as resolve some variance in the microstructures. However, for the U50Zr billet that did not successfully extrude at 630°C, heat treatment at 900°C for 96 hours did not have a significant impact on hardness or microstructure.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Technology Enabling Zero-EPZ Micro Modular Reactors: Fabrication of Zirconium Hydride with Controlled Hydrogen Loading

This report completes Milestone M2.2.2 - ZrH pellet fabricated with controlled hydride loading: ZrH1.5±0.1 single phase pellets fabricated with controlled and thermally stable hydride loading. Hydrogen content to be quantified and single-phase confirmed by X-ray diffraction. In this milestone, we report the successful fabrication of delta-phase zirconium hydride pellets using the ORNL bulk metal hydriding system. The successful deployment of zirconium hydride moderator in advanced reactors requires development of a consistent and affordable production pathway along with implementation of a hydrogen retention solution throughout the reactor life. Fabrication of delta-phase zirconium hydride is challenging since the absorption of a large amount of hydrogen into alpha-zirconium induces significant volume expansion and the present hydrogen concentration gradient results in cracking. A fully programmable hydriding system with continuous hydrogen partial pressure and flow control to facilitate processing of massive metal hydride has been developed at ORNL. In this report, the working principle of the hydriding system will be introduced. Characterization of the produced zirconium hydride includes X-ray powder diffraction to identify the present phases and X-ray Computed Tomography to visualize the internal microstructure (including cracks). The results indicate that single delta-phase zirconium hydride pellets with various sizes have been successfully produced.

36 MATERIALS SCIENCE↗