Search NASA⌕ Search

SEARCH · Search NASA

Results for “ZIRCONIUM OXIDES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Pyroprocessing of Oxidized Sodium-Bonded Fast Reactor Fuel -- an Experimental Study of Treatment Options for Degraded EBR-II Fuel

An experimental study was conducted to assess pyrochemical treatment options for degraded EBR-II fuel. As oxidized material, the degraded fuel would need to be converted back to metal to enable electrorefining within an existing electrometallurgical treatment process. A lithium-based electrolytic reduction process was studied to assess the efficacy of converting oxide materials to metal with a particular focus on the impact of zirconium oxide and sodium oxide on this process. Bench-scale electrolytic reduction experiments were performed in LiCl-Li2O at 650 °C with combinations of manganese oxide (used as a surrogate for uranium oxide), zirconium oxide, and sodium oxide. The experimental study illustrated how zirconium oxide and sodium oxide present different challenges to a lithium-based electrolytic reduction system for conversion of select metal oxides to metal.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Pyroprocessing of oxidized sodium-bonded fast reactor fuel - An experimental study of treatment options for degraded EBR-II fuel

An experimental study was conducted to assess pyrochemical treatment options for degraded EBR-II fuel. As oxidized material, the degraded fuel would need to be converted back to metal to enable electrorefining within an existing electro-metallurgical treatment process. A lithium-based electrolytic reduction process was studied to assess the efficacy of converting oxide materials to metal with a particular focus on the impact of zirconium oxide and sodium oxide on this process. Bench-scale electrolytic reduction experiments were performed in LiCl-Li{sub 2}O at 650 C. degrees with combinations of manganese oxide (used as a surrogate for uranium oxide), zirconium oxide, and sodium oxide. In the absence of zirconium or sodium oxide, the electrolytic reduction of MnO showed nearly complete conversion to metal. The electrolytic reduction of a blend of MnO-ZrO{sub 2} in LiCl - 1 wt% Li{sub 2}O showed substantial reduction of manganese, but only 8.5% of the zirconium was found in the metal phase. The electrolytic reduction of the same blend of MnO-ZrO{sub 2} in LiCl - 1 wt% Li{sub 2}O - 6.2 wt% Na{sub 2}O showed substantial reduction of manganese, but zirconium reduction was even less at 2.4%. This study concluded that ZrO{sub 2} cannot be substantially reduced to metal in an electrolytic reduction system with LiCl - 1 wt% Li{sub 2}O at 650 C. degrees due to the perceived preferential formation of lithium zirconate. This study also identified a possible interference that sodium oxide may have on the same system by introducing a parasitic and cyclic reaction of dissolved sodium metal between oxidation at the anode and reduction at the cathode. When applied to oxidized sodium-bonded EBR-II fuel (e.g., U-10Zr), the prescribed electrolytic reduction system would not be expected to substantially reduce zirconium oxide, and the accumulation of sodium in the electrolyte could interfere with the reduction of uranium oxide, or at least render it less efficient.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Rapid assessment of structural and compositional changes during early stages of zirconium alloy oxidation

A multimodal chemical imaging approach has been developed and applied to detail the dynamic, atomic-scale changes associated with oxidation of a zirconium alloy (Zircaloy-4). Scanning transmission electron microscopy, a gas-phase reactor chamber attached to an atom probe tomography instrument, and synchrotron-based X-ray absorption near-edge spectroscopy were employed to reveal morphology, composition, crystal, and electronic structure changes that occur during initial stages of oxidation at 300 °C. Oxidation was carried out in 10 mbar O 2 gas for short exposure times of 1 and 5 min. A multilayered oxide film with a cubic ZrO adjacent to the oxide/metal interface, a nanoscopic transition region with a graded composition of ZrO 2-x (where 0 < x < 1), and tetragonal ZrO 2 in the outermost oxide were formed. Partitioning of the major alloying element (tin) to the oxide/metal interface and heterogeneously within the oxide accompanied the development of the layered oxide. Our work provides a rapid, high-throughput approach for detailed characterisation of initial stages of zirconium alloy oxidation at an accelerated time scale, with implications for several other alloy systems.

36 MATERIALS SCIENCE↗

Strategic Buffer Layer Development for YBCO Coated Conductors

We have developed a simplified buffer layer architecture for the rolling-assisted biaxially textured substrates (RABiTS) template approach. The overall purpose of this research is to enable potentially a low-cost, high throughput and high yield manufacturing processes for buffer fabrication and to gain fundamental understanding of the growth of buffer layers for RABiTS templates. This understanding is critical to the development of a reliable, robust, and long-length manufacturing process for second generation wires. In this study, efforts are being made to either reduce the number of vacuum deposited layers or to replace one or more of these vacuum deposited layers with a solution based layer. We have chosen Gd{sub 2}O{sub 3} - ZrO{sub 2} system as a potential barrier layer for this study. We have deposited epitaxial Gadolinia Stabilized Zirconia (GSZ) (Zr{sub 1-x}Gd{sub x}O{sub y}; x = 0-1) films on 30-nm thick e-beam evaporated Y{sub 2}O{sub 3} seeded Ni-W (3 at. %) (Ni-3W) substrates using a metal-organic decomposition (MOD) process. Detailed X-ray studies indicated that all of the MOD-GSZ layers were cube textured and both in-plane and out-of-plane lattice parameters increases linearly with increasing the Gd content. We have also developed process conditions for reactively sputter deposited epitaxial Gd{sub 2}Zr{sub 2}O{sub 7} (Gadolinium Zirconium Oxide (GZO); Zr{sub 1-x}Gd{sub x}O{sub y} (x = 0.5)) films on the e-beam evaporated Y{sub 2}O{sub 3}/Ni - 3W substrates. YBCO films with a critical current density J{sub c} of 2.14 times 10{sup 6} A/cm{sup 2} and 1.4 times 10{sup 6} A/cm{sup 2} at 77 K and self-field were grown on the newly developed architectures of Gd{sub 2}Zr{sub 2}O{sub 7}/Y{sub 2}O{sub 3}/Ni - 3W and Zr{sub 1-x}Gd{sub x}O{sub y} (x = 0.2)/Y{sub 2}O{sub 3}/Ni - 3W substrates, respectively using a pulsed laser deposition (PLD) process. This work promises a route for producing cost-effective simplified buffer architectures for the RABiTS-based YBCO coated conductors.

36 MATERIALS SCIENCE↗

Oven rack having integral lubricious, dry porcelain surface

A lubricious glass-coated metal cooking article capable of withstanding repeated heating and cooling between room temperature and at least 500.degree. F. without chipping or cracking the glass coating, wherein the glass coating includes about 0.1 to about 20% by weight of a homogeneously distributed dry refractory lubricant material having a particle size less than about 200 .mu.m. The lubricant material is selected from the group consisting of carbon; graphite; boron nitride; cubic boron nitride; molybdenum (FV) sulfide; molybdenum sulfide; molybdenum (IV) selenide; molybdenum selenide, tungsten (IV) sulfide; tungsten disulfide; tungsten sulfide; silicon nitride (Si.sub.3N.sub.4); TiN; TiC; TiCN; TiO.sub.2; TiAlN; CrN; SiC; diamond-like carbon; tungsten carbide (WC); zirconium oxide (ZrO.sub.2); zirconium oxide and 0.1 to 40 weight % aluminum oxide; alumina-zirconia; antimony; antimony oxide; antimony trioxide; and mixtures thereof.

01 COAL, LIGNITE, AND PEAT↗

Mesoporous Zirconium Titanium Oxides. Part 2: Synthesis, Porosity, and Adsorption Properties of Beads

Mesoporous zirconium titanium mixed-oxide beads having disordered wormhole textures and mole fractions of Zr (x) ranging from x = 0.25 to 0.67 have been prepared. The bead preparation method combined the forced hydrolysis of mixtures of zirconium-titanium alkoxides in the presence of long-chain carboxylates with external gelation. Uniformly sized beads could be produced in the size range 0.5--1.1 mm by varying the droplet size and viscosity of the mixed-oxide sol, thus making them suitable for large-scale column chromatographic applications. The beads exhibited narrow pore size distributions with similar mean pore diameters of around 3.7 nm. The specific surface areas of the beads were linked to the Zr mole fraction in the precursor solution and were generally greater than 350 m{sup 2}/g for x = 0.5. A combination of scanning transmission electron microscopy and X-ray absorption fine structure analysis indicated that the pore walls of the beads were composed of atomically dispersed Zr and Ti to form a continuous network of Zr-O-Ti bonds. Mass transport in the beads was evaluated by monitoring the kinetics of vanadate and vanadyl adsorption at pH 10.5 and 0.87, respectively.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

TEM Study of Zircaloy 2 with FeCrAl Layer under Simulated BWR Environment

Zircaloy 2 is widely used as nuclear fuel cladding in light-water nuclear reactors, which is resistive to corrosion, creep, and swelling. Due to water chemical reactivity and high-temperature steam exposure, oxidation in zirconium cladding is possible during transients. To mitigate the zirconium oxidation and the hydrogen generation at elevated temperature, we have coated Zircaloy 2 with oxide resistant FeCrAl thin film layers using magnetron sputtering. Transmission electron microscopy (TEM), scanning transmission electron microscopy (STEM), and electron energy-dispersive X-ray spectroscopy (EDX) are used to understand the behavior of the protective FeCrAl layer under typical BWR operation conditions. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Composite wall concept for high temperature turbine shrouds: Survey of low modulus strain isolator materials

Plasma sprayed yttria stabilized zirconium oxide turbine seal specimens, incorporating various low modulus porous metal strain isolator pads between the zirconium oxide and a dense metal substrate, were subjected to cyclic thermal shock testing. Specimens that had a low modulus pad composed of sintered FeNiCrAlY fibermetal survived 1000 thermal shock cycles without spalling of the ceramic. A figure of merit for the low modulus pad materials taking into consideration the elastic modulus, thermal conductivity, strength, and oxidation resistance of the pad was proposed, and showed reasonable agreement with the thermal shock results. A potential surface distress problem on the zirconium oxide, associated with nonuniform temperature distribution and rapid stress relaxation was identified. One approach to solving the surface distress problem through application of laser surface fusion of the zirconium oxide layer showed some promise, but improvements in the laser surface fusion process are necessary to prevent process associated damage to the ceramic.

Bill, R. C.↗

Grain size dependence of thermally induced oxidation in zirconium carbide

Here complementary analytical approaches were employed to probe the effect of grain size on thermally induced oxidation of zirconium carbide (ZrC) utilizing thermogravimetric analysis, differential scanning calorimetry, and Raman spectroscopy, as well as synchrotron-based and laboratory-based X-ray diffraction (XRD) experiments. The oxidation mechanism and phase behavior of nanocrystalline ZrC (grain size ~ 20 nm) were compared with that of the more documented microcrystalline ZrC (grain size ~ 1 µm). Synchrotron XRD at the Advanced Photon Source with a hydrothermal diamond anvil cell (HDAC) used as a sample chamber revealed that the onset of oxidation is at ~ 380 °C for microcrystalline ZrC which is in agreement with previous work. In contrast, the critical oxidation temperature was ~ 330 °C for nanocrystalline ZrC. Additional high-temperature synchrotron XRD experiments at the National Synchrotron Light Source II using a lamp furnace in combination with Raman analysis showed that tetragonal ZrO 2 forms as an initial oxidation product and transforms at higher temperatures to the monoclinic phase. Thermogravimetric analysis (TGA) coupled with differential scanning calorimetry (DSC) confirmed the X-ray results of a lower critical oxidation temperature for the nanocrystalline sample. The phase transformations in the oxide phase with associated critical temperatures were also evident in the thermodynamic data as exothermic heat events.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Grain boundary zirconia-modified garnet solid-state electrolyte

Here, we report a method for promoting electrochemical stability in garnet Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 solid-state electrolyte based on a composite two-phase oxide–oxide microstructure. Grain boundary precipitation of the controlled distribution of amorphous zirconium oxide microparticles is achieved through the addition of reactive tantalum carbide. During ambient-atmosphere sintering, the carbide decomposes through an in situ reaction, the ‘extra’ Ta substituting for Zr within the Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 lattice. Density functional theory (DFT) calculations identify a thermodynamically favourable reaction path and show how substituting Ta 5+ at Zr 4+ sites affects the crystal structure as well as bulk ionic and electronic conductivities. Quantitative stereology highlights that zirconia also acts as a sintering aid, reducing compact porosity. Cryogenic focused-ion-beam scanning electron microscopy and fractography analysis of cycled solid-state electrolytes illustrates that near-universally observed intergranular Li-metal dendrite propagation is suppressed by the two-phase microstructure, favouring transgranular dendrites instead. Importantly, DFT demonstrates that compared with the Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 surface, the zirconium oxide surface per se is less electronically conductive and does not trap excess electrons to reduce Li ions. This is a key reason for the substantial improvement in the electrochemical properties over the single-phase baseline.

36 MATERIALS SCIENCE↗

Crystallization, densification and dielectric properties of CaO–MgO–Al{sub 2}O{sub 3}–SiO{sub 2} glass with ZrO{sub 2} as nucleating agent

SEM micrographs for the pure CaO–MgO–Al{sub 2}O{sub 3}–SiO{sub 2} glass sintered at 850–1000 °C (a) 850 °C, (b) 900 °C, (c) 950 °C, (d) 1000 °C. - Highlights: • ZrO{sub 2} effects on the crystallization of LTCC glass system were investigated. • ZrO{sub 2} effects on the dielectric properties of LTCC glass system were investigated. • LTCC with a dielectric constant of 6.65 and a low dielectric loss can be obtained. - Abstract: The zirconium oxide effects on the crystallization and dielectric properties of CaO–MgO–Al{sub 2}O{sub 3}–SiO{sub 2} (CMAS) glass were investigated. The results showed that phyllosiloxide and anorthite crystallites were observed in sequence during sintering. For glass added with 8 wt% ZrO{sub 2}, homogeneously dispersed tetragonal ZrO{sub 2} crystallites were observed at 850 °C. The as-prepared CMAS glass–ceramics exhibited a dielectric constant of about 6–7 and a dielectric loss below 0.005 at 100 MHz. The dielectric properties of CMAS glass with 8 wt% ZrO{sub 2} sintered at 850 °C show a low dielectric constant of 6.65 and a dielectric loss tangent of about 2.5 × 10{sup −3}, which provides a promising candidate for LTCC applications.

36 MATERIALS SCIENCE↗

Cryogenic Brush Seal Test Results

Brush seals are compliant, contact seals that have long-life, low-leakage characteristics desirable for use in rocket engine turbopumps. 50.8-mm (2.0 inch) diameter brush seals with a nominal initial radial interference of 0.127-mm (0.005 inch) were tested in liquid nitrogen at shaft speeds up to 35,000 rpm and differential pressure loads up to 1.21 MPa (175 psi) per brush. The measured leakage rate of a single brush was 2-3 times less than that measured for a 12-tooth, 0.127-mm (0.005 inch) radial clearance labyrinth seal used as a baseline. Stage effects were studied and it was found that two brush seals with a large separation distance leaked less than two brushes tightly packed together. The maximum measured groove depth on the Inconel 718 rotor was 25.4 (mu)m (0.001 inch) after 4.31 hours of shaft rotation. The Haynes-25 bristles wore approximately 25.4-76.2 (mu)m (0.001-0.003 inch) under the same conditions. Three seal runner coatings, chromium carbide, Teflon impregnated chromium, and zirconium oxide, were tested in liquid hydrogen at 35,000 and 65,000 rpm with separate 50.8 mm diameter brush seals made of Haynes-25 bristles and having a nominal initial radial interference of 129 rpm. Two bare Inconel-718 rotors were also tested as a baseline. The test results revealed significant differences between the wear characteristics of the uncoated and coated seal runners. At both speeds the brush seal with the bare Inconel-718 seal runner exhibited significant bristle wear with excessive material transferring to the runner surface. In contrast, the coated seal runners inhibited the transfer and deposit of bristle material. The chromium carbide coating showed only small quantities of bristle material transferring to its surface. The Teflon impregnated chromium coating also inhibited material transfer and provided some lubrication. This coating, however, is self-sacrificing. The Teflon remained present on the low speed runner, but it was completely removed from the high speed brush seal, which was tested considerably longer. The tests of the Teflon coating revealed the importance of using a lubricating and low friction coating for brush seals to reduce bristle and seal runner wear. The zirconium oxide coating exhibited the greatest amount of coating wear, while the brushes incurred only slight wear. Further testing of ceramics is recommended before making a final judgement on the viability of ceramic coatings for brush seals because of the contrast between the results reported by Carlile and the results presented herein. Strictly based on the results presented hereinabove, the chromium carbide and Teflon impregnated chromium coatings were considered preferable to the uncoated Inconel-718 and zirconium oxide coatings because of their good wear resistance and characteristics to inhibit bristle material wear and transfer to the seal runner.

Proctor, Margaret P.↗

Oxygen partial pressure influenced structural and optical properties of DC magnetron sputtered ZrO{sub 2} films

Thin films of zirconium oxide (ZrO{sub 2}) were deposited on (100) p-silicon and quartz substrates by sputtering of metallic zirconium target under different oxygen partial pressures in the range 8 Multiplication-Sign 10{sup -3}-6 Multiplication-Sign 10{sup -2}Pa. The effect of oxygen partial pressure on the structural and optical properties of the deposited films was systematically investigated. The deposition rate of the films decreased from 3.3 to 1.83 nm/min with the increase of oxygen partial pressure from 8 Multiplication-Sign 10{sup -3}-6 Multiplication-Sign 10{sup -2}Pa respectively. The X-ray diffraction profiles revealed that the films exhibit (111) refection of zirconium oxide in monoclinic phase. The optical band gap of the films increased from 5.62 to 5.80 eV and refractive index increased from 2.01 to 2.08 with the increase of oxygen partial pressure from 8 Multiplication-Sign 10{sup -3}-6 Multiplication-Sign 10{sup -2}Pa respectively.

36 MATERIALS SCIENCE↗

Determination of the mechanical properties of blisters by nanoindentation

In light-water reactors, a zirconium oxide layer will be formed at the outer surface of the fuel cladding as a consequence of the chemical reaction which takes place between zirconium and the cooling water. This zirconium oxide layer is a good thermal insulator, but at some point, it may spall-out. As a consequence, a cold spot will be formed at the outer surface of the cladding. In this situation, the hydrogen will quickly migrate to this spot to form a highly-enriched hydride zone, known as blister. In this work, an experimental procedure has been devised to produce blisters with a similar shape to the ones reported in the literature for irradiated cladding with severe hydriding. Nano-indentation tests were performed on blisters prepared in laboratory. A numerical simulation by the finite element method was developed to fit the load versus penetration depth data from the aforementioned nano-indentation tests. By means of an inverse process which combines experimental data and numerical simulations, the constitutive equation of the blister was determined. The process has been used to calculate the plastic stress-strain curve of the blister under study at room temperature. The results show an almost perfect numerical fitting of the experimental data.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗