At least 109 records · Page 6

The role of peel stresses in cyclic debonding

When an adhesively bonded joint is undergoing cyclic loading, one of the possible damage modes that occurs is called cyclic debonding - progressive separation of the adherends by failure of the adhesive bond under cyclic loading. In most practical structures, both peel and shear stresses exist in the adhesive bonding during cyclic loading. The results of an experimental and analytical study to determine the role of peel stresses on cyclic debonding in a mixed mode specimen are presented. Experimentally, this was done by controlling the forces that create the peel stresses by applying a clamping force to oppose the peel stresses. Cracked lap shear joints were chosen for this study. A finite element analysis was developed to assess the effect of the clamping force on the strain energy release rates due to shear and peel stresses. The results imply that the peel stress is the principal stress causing cyclic debonding.

Everett, R. A., Jr.↗

Further developments in the design and analysis of adhesive-bonded structural joints

Previously developed computer programs for analyzing stepped-lap adhesive-bonded joints and doublers have been modified to permit the inclusion of variable adhesives as well as nonuniform adherends. The new version of the analysis program is described with reference to examples illustrating the effects of load redistribution around flaws and porosity. The loss of strength associated with pinched-off edges is illustrated, and the benefits of deliberately thickening the adhesive layer in the immediate vicinity of the ends of the overlap are demonstrated. The changes in shear load transfer due to softening of some of the adhesive by moisture absorption while the remainder either has never been soaked or has dried out locally are discussed.

Hart-Smith, L. J.↗

The application of surface analysis to polymer/metal adhesion

The use of scanning electron microscopy (SEM) and X-ray photoelectron spectroscopy (XPS) in the analysis of Ti 6-4 adherend surfaces is described. Differences in Ti 6-4 surface composition as determined by XPS after different chemical pretreatments are detailed. Analysis of fractured surfaces by SEM/XPS is used to establish the failure mode. The surface acidity of Ti 6-4 coupons can be established by reflectance visible spectroscopy using indicator dyes.

Wightman, J. P.↗

Strength and Mechanics of Bonded Scarf Joints for Repair of Composite Materials

Experimental and analytical investigations of scarf joints indicate that slight bluntness of adherend tips induces adhesive stress concentrations which significantly reduce joint strength, and the stress distribution through the adhesive thickness is non-uniform and has significant stress concentrations at the ends of the joint. The laminate stacking sequence can have important effects on the adhesive stress distribution. A significant improvement in joint strength is possible by increasing overlap at the expense of raising the repair slightly above the original surface. Although a surface grinder was used to make most experimental specimens, a hand held rotary bur can make a surprisingly good scarf. Scarf joints wit doublers on one side, such as might be used for repair, bend under tensile loads and may actually be weaker than joints without doublers.

Pipes, R. B.↗

Material characterization of structural adhesives in the lap shear mode

A general method for characterizing structual adhesives in the bonded lap shear mode is proposed. Two approaches in the form of semiempirical and theoretical approaches are used. The semiempirical approach includes Ludwik's and Zhurkov's equations to describe respectively, the failure stresses in the constant strain rate and constant stress loading modes with the inclusion of the temperature effects. The theoretical approach is used to describe adhesive shear stress-strain behavior with the use of viscoelastic or nonlinear elastic constitutive equations. Two different model adhesives are used in the single lap shear mode with titanium adherends. These adhesives (one of which was developed at NASA Langley Research Center) are currently considered by NASA for possible aerospace applications. Use of different model adhesives helps in assessment of the generality of the method.

Sancaktar, E.↗

Viscoelastic study of an adhesively bonded joint

The plane strain problem of two dissimilar orthotropic plates bonded with an isotropic, linearly viscoelastic adhesive is considered. Both the shear and the normal stresses in the adhesive are calculated for various geometries and loading conditions. Transverse shear deformations of the adherends are taken into account, and their effect on the solution is shown in the results. All three inplane strains of the adhesive are included. Attention is given to the effect of temperature, both in the adhesive joint problem and to the heat generation in a viscoelastic material under cyclic loading. This separate study is included because heat generation and or spatially varying temperature are at present too difficult to account for in the analytical solution of the bonded joint, but whose effect can not be ignored in design.

Joseph, P. F.↗

Fatigue behavior of adhesively bonded joints

The fatigue damage mechanism of composite to composite adhesively bonded joints was characterized. The mechanics of the possible modes of fatigue damage propagation in these joints when subjected to constant amplitude cyclic mechanical loading were investigated. The possible failure modes in composite bonded joints may be cyclic debonding (i.e., progressive separation of the adhesive), interlaminar damage (delamination), adherend fatigue or a combination of these. Two composite systems - graphite/epoxy adhesively bonded to graphite/epoxy and Kevlar 49/epoxy adhesively bonded to Kevlar 49/epoxy were investigated. Both composite systems consisted of quasi-isotropic lay-ups, i.e., 0 deg/-45 deg/+45 deg/90 degs. The two adhesives, employed in the study were (1) EC 3445 with cure temperature of 250 F for secondary bonding and (2) FM 300 with cure temperature of 350 F for co-cure bonding.

Mall, S.↗

A fracture mechanics approach for designing adhesively bonded joints

An analytical and experimental investigation was undertaken to determine if the adhesive debond initiation stress could be predicted for arbitrary joint geometries. The analysis was based upon a threshold total strain-energy-release rate (Gth) concept. Two bonded systems were tested: T300/5208 graphite/epoxy adherends bonded with either EC-3445 or FM-300 adhesive. The Gth for each adhesive was determined from cracked-lap-shear (CLS) specimens by initiation tests. Finite-element analyses of various tapered CLS specimen geometries predicted the specimen stress at which the total strain-energy-release rate (GT) equaled Gth at the joint tip. Experiments verified the predictions. The approach described herein predicts the maximum stress at which an adhesive joint can be cycled yet not debond. Furthermore, total strain-energy-release rate appeared to be the driving parameter for cyclic debonding and debond initiation in structural adhesives. In addition, debond initiation and growth were found to occur with virtually no peel stress present.

Johnson, W. S.↗

Surface characterization and failure analysis of thermally aged, polyimide bonded titanium

This study of high temperature stable adhesive systems using 6Al-4V titanium adherends found that certain adhesive/adherends exhibit a change from cohesive to adhesive failure mode during long term 450 F thermal aging. Lap-shear specimens which exhibited adhesive failures were subjected to failure analysis using scanning transmission electron microscopy (STEM) and surface analysis techniques. Data is presented which supports the conclusion of interfacial failures for these samples.

Peters, P. D.↗

A critical study of the role of the surface oxide layer in titanium bonding

Scanning electron microscope/X-ray photoelectron spectroscopy (SEM/XPS) analysis of fractured adhesively bonded Ti 6-4 samples is discussed. The text adhesives incuded NR 056X polyimide, polypheylquinoxaline (PPQ), and LARC-13 polyimide. Differentiation between cohesive and interfacial failure was based on the absence of presence of a Ti 2p XPS photopeak. In addition, the surface oxide layer on Ti-(6A1-4V) adherends is characterized and bond strength and durability are addressed. Bond durability in various environmental conditions is discussed.

Dias, S.↗

Material characterization of structural adhesives in the lap shear mode

A general method for characterizing structural adhesives in the bonded lap shear mode is proposed. Two approaches in the form of semi-empirical and theoretical approaches are used. The semi-empirical approach includes Ludwik's and Zhurkov's equations to describe respectively, the failure stresses in the constant strain rate and constant stress loading modes with the inclusion of the temperature effects. The theoretical approach is used to describe adhesive shear stress-strain behavior with the use of viscoelastic or nonlinear elastic constitutive equations. Three different model adhesives are used in the simple lap shear mode with titanium adherends. These adhesives (one of which was developed at NASA Langley Research Center) are currently considered by NASA for possible aerospace applications. Use of different model adhesives helps in assessment of the generality of the method.

Schenck, S. C.↗

Processing study of a polyimidesulfone adhesive

An adhesive bonding process cycle study was performed for a polyimidesulfone (PISO2) recently developed as a promising structural adhesive. The high molecular weight, linear aromatic system possesses properties which make it attractive as a processable, low-cost material for elevated temperature applications. The results of a study to better understand the parameters that affect the adhesive properties of the polymer for titanium alloy adherends are detailed. These include the tape preparation, the use of a primer, and press and simulated autoclave processing conditions. The polymer was characterized using Fourier Transform Infrared Spectroscopy, glass transition temperature determination, flow measurements, and weight loss measurements. The adhesive's strength determined by lap shear strength tests was used to evaluate the effects of the bonding process variations. Higher lap shear strengths were obtained at room temperature when a primer (PISO2) was used; however, the results were the same at 232 C (450 F) with or without a primer. The use of a vacuum (simulated autoclave cycle) during titanium bonding produced similar lap shear strengths to those specimens bonded without a vacuum.

Progar, D. J.↗

Repeatability of mixed-mode adhesive debonding

The repeatability of debond growth rates in adhesively bonded subjected to constant-amplitude cyclic loading was studied. Debond growth rates were compared from two sets of cracked-lap-shear specimens that were fabricated by two different manufacturers and tested in different laboratories. The fabrication method and testing procedures were identical for both sets of specimens. The specimens consisted of aluminum adherends bonded with FM-73 adhesive. Critical values of strain-energy-release rate were also determined from specimens that were monotonically loaded to failure. The test results showed that the debond growth rates for the two sets of specimens were within a scatter band which is similar to that observed in fatigue crack growth in metals. Cyclic debonding occurred at strain-energy-release rates that were more than an order of magnitude less than the critical strain-energy-release rate in static tests.

Everett, R. A., Jr.↗

Processing study of a high temperature adhesive

An adhesive-bonding process cycle study was performed for a polyimidesulphone. The high molecular weight, linear aromatic system possesses properties which make it attractive as a processable, low-cost material for elevated temperature applications. The results of a study to better understand the parameters that affect the adhesive properties of the polymer for titanium alloy adherends are presented. These include the tape preparation, the use of a primer and press and simulated autoclave processing conditions. The polymer was characterized using Fourier transform infrared spectroscopy, glass transition temperature determination, flow measurements, and weight loss measurements. The lap shear strength of the adhesive was used to evaluate the effects of the bonding process variations.

Progar, D. J.↗

Strain measurement within a single-lap joint using embedded strain gages

An experimental method used to measure the in-plane normal-axial strains produced within a single-lap joint is described in which a resistance-foil strain gage is embedded within the joint prior to curing of the adhesive. Nominal dimensions of the titanium Ti-6-4 adherends were 0.13 x 2.5 x 12.7 cm and an overlap of 2.5 cm was used. The joint was bonded with FM-300 structural adhesive. The average ultimate shear strength of the gaged specimens and control specimens was 16.1 MPa and 14.1 MPa. A significant advantage of the proposed method is that strains internal to the joint are measured, rather than strains at an external edge. The presence of the gage was found to be not detrimental to bond performance.

Tuttle, M. E.↗

Deformations and strains in adhesive joints by moire interferometry

Displacement fields in a thick adherend lap joint and a cracked lap shear specimen were measured by high sensitivity moire interferometry. Contour maps of in-plane U and V displacements were obtained across adhesive and adherent surfaces. Loading sequences ranged from modest loads to near-failure loads. Quantitative results are given for displacements and certain strains in the adhesive and along the adhesive/adherend boundary lines. The results show nonlinear displacements and strains as a function of loads or stresses and they show viscoelastic or time-dependent response. Moire interferometry is an excellent method for experimental studies of adhesive joint performance. Subwavelength displacement resolution of a few micro-inches, and spatial resolution corresponding to 1600 fringes/inch (64 fringes/mm), were obtained in these studies. The whole-field contour maps offer insights not available from local measurements made by high sensitivity gages.

Post, D.↗

Adhesive evaluation of LARC-TPI and a water-soluble version of LARC-TPI

The results of a study to evaluate two Langley Research Center thermoplastic polimide (TPI) materials, identified as TPI/MTC for the material from Mitsui Toatsu Chemicals Inc. and TPI/H2O for the material from United Technologies Research Center, as high temperature thermoplastic adhesives and primers for bonding titanium (6AL-4V) adherends are discussed. A limited characterization of the materials was performed using a Diffuse Reflectance-Fourier Transform Infrared Spectroscopy (DR-FTIR) technique. Thermomechanical Analysis (TMA) and torsional braid techniques were used to determine glass transition temperature. The adhesive's strength, as determined by simple lap shear tests, as used to evaluate the effects of long term thermal exposure (up to 1000 hrs) at 204 deg C and a 72-hour water-boil.

Progar, D. J.↗

A cracked orthotropic sheet stiffened by a semi-infinite orthotropic sheet

The stress intensity factor is determined for a cracked orthotropic sheet adhesively bonded to an orthotropic stringer. Since the stringer is modeled as a semiinfinite sheet, the solution is most appropriate for a crack tip located near a stringer edge. Both adherends are treated as homogeneous, orthotropic media. It is assumed they are in plane stress and the adhesive is in pure shear. From Green's functions and the complex variable theory of orthotropic elasticity developed by Lekhnitskiy, a set of integral equations is obtained. The integral equations are replaced by an equivalent set of algebraic equations which is solved to obtain the shear stress distribution in the adhesive layer. With these stresses, equations for the stress intensity factors at both crack tips are found. A parametric study is conducted to determine the sensitivity of the system to material properties and specimen configuration. Unless the crack tip is very close to or under the stringer the stress intensity factor is approximately that of an unstiffened sheet. However, as the crack propagates beneath the stringer, the stress intensity factor decreases significantly. Increasing the stiffness of the stringer or the adhesive also results in a decrease in the stress intensity factor.

Bigelow, C. A.↗