Welding of high chromium steels

A brief description is given of different groups of high chromium steels (rustless iron and stainless steels) according to their composition and more generally accepted names. The welding procedure for a given group will be much the same regardless of the slight variations in chemical composition which may exist within a certain group. Information is given for the tensile properties (yield point and ultimate strength) of metal sheets and welds before and after annealing on coupons one and one-half inches wide. Since welds in rustless iron containing 16 to 18 percent chromium and 7 to 12 percent nickel show the best combination of strength and ductility in the 'as welded' or annealed condition, it is considered the best alloy to use for welded construction.

IRON - STAINLESS↗

Methods for the Identification of Aircraft Tubing of Plain Carbon Steel and Chromium-Molybdenum Steel

The survey of the possibilities for distinguishing between plain carbon and chromium-molybdenum steel tubing included the Herbert pendulum hardness, magnetic, sparks, and chemical tests. The Herbert pendulum test has the disadvantages of all hardness tests in being limited to factory use and being applicable only to scale-free, normalized material. The small difference in the range of hardness values between plain carbon and chromium-molybdenum steels is likewise a disadvantage. The Rockwell hardness test, at present used in the industry for this purpose, is much more reliable. It may be concluded on the basis of the experiments performed that of all methods surveyed, spark testing appears to be, at present, the most suitable for factory use from the standpoint of speed, accuracy, nondestructiveness and reliability. It is also applicable for field use.

Mutchler, W H↗

Femtosecond pulses generated from a synchronously pumped chromium-doped forsterite laser

Kerr lens mode-locking (KLM) has become a standard method to produce femtosecond pulses from tunable solid state lasers. High power inside the laser resonator propagating through the laser-medium with nonlinear index of refraction, coupled with the stability conditions of the laser modes in the resonator, result in a passive amplitude modulation which explains the mechanism for pulse shortening. Recently, chromium doped forsterite was shown to exhibit similar pulse behavior. A successful attempt to generate femtosecond pulses from a synchronously pumped chromium-doped forsterite laser with intracavity dispersion compensation is reported. Stable, transform limited pulses with duration of 105 fs were routinely generated, tunable between 1240 to 1270 nm.

Seas, A.↗

The Preparation Conditions of Chromium Doped ZnSe and Their Effect on The Infrared Luminescence Properties

We report the investigation by photoluminescence lifetime measurements of the near-IR emissions from a series of chromium-doped ZnSe samples, correlated to their preparation conditions. The samples were polycrystalline or single crystals prepared by post growth diffusion doping or single crystals doped during growth by the Physical Vapor Transport method. Room temperature lifetime values between 6 and 8 microseconds were measured for samples with Cr (2+) concentrations from low 10 (exp 17) to high 10 (exp 18) per cubic centimeter range. Lifetime data taken down to 78 K was found to be rather temperature independent, reconfirming previous reports indicating a quantum yield of the corresponding emission of close to 100% at room temperature. A strong decrease in the room temperature lifetime was found for chromium concentrations higher than 10 (exp 19) per cubic centimeter.

Burger, A.↗

The Preparation Conditions of Chromium Doped ZnSe and Their Effect on the Infrared Luminescence Properties

We report the investigation by photoluminescence lifetime measurements of the near-IR emissions from a series of chromium-doped ZnSe samples, correlated to their preparation conditions. The samples were polycrystalline or single crystals prepared by post growth diffusion doping or single crystals doped during growth by the physical vapor transport method. Room temperature lifetime values between 6 and 8 micro seconds were measured for samples with Cr2+ from low 10(exp 17) to high 10(exp 18) / cubic cm range. Lifetime data taken down to 78 K was found to be rather temperature independent, reconfirming previous reports indicating a quantum yield of the corresponding emission of close to 100% at room temperature. A strong decrease in the room temperature lifetime was found for chromium concentrations higher than 10(exp 19) / cubic CM.

Burger, A.↗

Chromium boron surfaced nickel-iron base alloys

Chromium boron diffusion coatings on nickel iron alloys uniquely provide them with improvement in high cycle fatigue strength (up to 30%) and erosion resistance (up to 15 times), compared to uncoated alloy. The diffused chromium layer extends in two essential concentration zones to a total depth of about 40.times.10.sup.-6 m, while the succeeding boron layer is limited to 50-90% of the depth of the richest Cr layer nearest the surface. Both coatings are applied using conventional pack diffusion processes.

Rashid, James M.↗

INVESTIGATION OF MECHANICAL PROPERTIES OF CHROMIUM, CHROMIUMRHENIUM, AND DERIVED ALLOYS

Tensile tests of iodide chromium have been carried out over the range 0 C to 400 C. The peaks which have been detected in the variation of yield stress with temperature are quite small and difficult to locate exactly. However, by dint of performing many tests at close temperature intervals, the peaks have been located as well as seems possible at this time. During this series of tests, it was found, contrary to previous experience, that recrystallized material which had been prestrained about 8 per cent and then recrystallized again was more ductile than recrystallized material which had not had such a treatment. The slow tensile transition temperature was depressed below room temperature, but was above 0 C.

PURIFICATION↗