Search NASA⌕ Search

SEARCH · Search NASA

Results for “damage threshold”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Theory of suppressing avalanche process of carrier in short pulse laser irradiated dielectrics

A theory for controlling avalanche process of carrier during short pulse laser irradiation is proposed. We show that avalanche process of conduction band electrons (CBEs) is determined by the occupation number of phonons in dielectrics. The theory provides a way to suppress avalanche process and a direct judgment for the contribution of avalanche process and photon ionization process to the generation of CBEs. The obtained temperature dependent rate equation shows that the laser induced damage threshold of dielectrics, e.g., fused silica, increase nonlinearly with the decreases of temperature. Present theory predicts a new approach to improve the laser induced damage threshold of dielectrics.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Quantitative Evaluation of Nanosecond Pulsed Laser-Induced Photomodification of Plasmonic Gold Nanoparticles

The rapid growth of gold nanoparticle applications in laser therapeutics and diagnostics has brought about the need for establishing innovative standardized test methods for evaluation of safety and performance of these technologies and related medical products. Furthermore, given the incomplete and inconsistent data on nanoparticle photo-modification thresholds provided in the literature, further elucidation of processes that impact the safety and effectiveness of laser-nanoparticle combination products is warranted. Therefore, we present a proof-of-concept study on an analytical experimental test methodology including three approaches (transmission electron microscopy, dynamic light scattering, and spectrophotometry) for experimental evaluation of damage thresholds in nanosecond pulsed laser-irradiated gold nanospheres, and compared our results with a theoretical model and prior studies. This thorough evaluation of damage threshold was performed based on irradiation with a 532nm nanosecond-pulsed laser over a range of nanoparticle diameters from 20 to 100nm. Experimentally determined damage thresholds were compared to a theoretical heat transfer model of pulsed laser-irradiated nanoparticles and found to be in reasonably good agreement, although some significant discrepancies with prior experimental studies were found. This study and resultant dataset represent an important foundation for developing a standardized test methodology for determination of laser-induced nanoparticle damage thresholds.

59 BASIC BIOLOGICAL SCIENCES↗

Laser damage in silicon: Energy absorption, relaxation, and transport

Silicon irradiated with an ultrashort 800 nm-laser pulse is studied theoretically using a two temperature description that considers the transient free carrier density during and after irradiation. A Drude model is implemented to account for the highly transient optical parameters. We analyze the importance of considering these density-dependent parameters as well as the choice of the Drude collision frequency. In addition, degeneracy and transport effects are investigated. The importance of each of these processes for resulting calculated damage thresholds is studied. We report damage thresholds calculations that are in very good agreement with experimental results over a wide range of pulse durations.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Antireflection coating of diamond elements of power optics for CO{sub 2} lasers

A technology of deposition of a single-layer PbF{sub 2} coating, antireflecting for the CO{sub 2} laser radiation, on diamond substrates is developed. As substrates, use is made of plates of polycrystalline CVD diamond. The transmission coefficient of diamond plates with two-side coating attains 98.5 % – 99 %. The measured laser-induced damage threshold of such plates under normal environment conditions for the pulsed (τ ∼ 100 ns) and continuous-wave radiation of CO{sub 2} lasers amounts to 250 and 4 MW cm{sup –2}, respectively. These values are comparable with the thresholds of the diamond substrate damage. The increase in the damage threshold of the AR coating under continuous-wave irradiation to 5.5 MW cm{sup –2} is found in the case of preliminary multiple irradiation of samples by weaker laser pulses. This effect can be explained by the pollutant removal from the surface of the film without its damage (laser cleaning effect). The bibliography includes 28 references. (paper)

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

New acousto-ultrasonic techniques applied to aerospace materials

The use of an NdYAG pulsed laser for generating ultrasonic waves for NDE in resin matrix composites was investigated. A study was conducted of the use of the 1.064 micron wavelength NdYAG pulsed laser with the neat, unreinforced resin as well as graphite fiber/polymer composite specimens. In the case of the neat resins it was found that, at normal incidence, about 25 percent of the laser pulse energy was reflected at the incident surface. An attenuation coefficient for the polyimide resin, PMR-15 was determined to be approximately 5.8 np/cm. It was found in energy balance studies that graphite fiber/polymer specimens attenuate the laser beam more than do neat resins. The increase absorption is in the graphite fibers. The occurrence of laser induced surface damage was also studied. For the polymer neat resin, damage appears as pit formation over a small fraction of the pulse impact area and discoloration over a larger part of the area. A damage threshold was inferred from observed damage as a function of pulse energy. The 600 F cured PMR-15 and PMR-11 exhibit about the same amount of damage for a given laser pulse energy. The damage threshold is between 0.06 and 0.07 J/sq cm.

Kautz, Harold E.↗

Glancing-angle-deposited magnesium oxide films for high-fluence applications

Here, Birefringent magnesium oxide thin films are formed by glancing angle deposition to perform as quarter-wave plates at a wavelength of 351 nm. These films are being developed to fabricate a large aperture distributed-polarization rotator for use in vacuum, with an ultimate laser-damage–threshold goal of up to 12 J/cm 2 for a 5-ns flat-in-time pulse. The laser-damage threshold, ease of deposition, and optical film properties are evaluated. While the measured large-area laser-damage threshold is limited to ~4 J/cm 2 in vacuum, initial results based on small-spot testing in air (>20 J/cm 2 ) suggest MgO may be suitable with further process development.

36 MATERIALS SCIENCE↗

Foam-based optical absorber for high-power laser radiometry

We report damage threshold measurements of novel absorbers comprised of either liquid-cooled silicon carbide or vitreous carbon foams. The measurements demonstrate damage thresholds up to 1.6x104 W/cm2 at an incident circular spot size of 2 mm with an absorbance of 96% at 1.064 {mu}m. We present a summary of the damage threshold as a function of the water flow velocity and the absorbance measurements. We also present a qualitative description of a damage mechanism based on a two-phase heat transfer between the foam and the flowing water.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Large aperture and durable glass-engraved optical metasurfaces using nanoparticle etching masks: prospects and future directions

Abstract Metasurfaces (MSs), or surfaces consisting of engineered spatially oriented sub-wavelength elements—also known as meta-atoms—are quickly becoming a burgeoning field of interest due to their seemingly unparalleled control over the propagation of light. This article will discuss the emergence of a MS technology that is based on dewetting thin metal films to form dry etching masks for MS fabrication. The novelty this process presents is the ability to spatially vary mask features—which translates into spatially varying index of the finished surface—in a way that, rather than writing subwavelength elements one-by-one, writes entire areas at once to provide a route to easily scale the process up to meter-sized optics. Glass-engraved MSs have shown to be laser damage resistant, with damage thresholds close to the parent substrate damage thresholds. Furthermore, these surfaces have proven to be mechanically durable and capable of handling normal loads two orders of magnitude higher than that of an average fingerprint pressure. This indicates that accidental handling contact is not detrimental to the MS optical performance. Also discussed are the foreseeable technological challenges, potential solutions for those obstacles, and some currently unexplored directions for future efforts.

47 OTHER INSTRUMENTATION↗

Minimizing Contamination to Mulitlayer Dielectric Diffraction Gratings Within a Large Vacuum System

The University of Rochester's Laboratory for Laser Energetics (LLE) has recently completed the construction of the OMEGA EP short-pulse, petawatt laser system. A major structure for OMEGA EP is the grating compressor chamber (GCC). This large (15,750-ft^3) vacuum chamber contains numerous optics used in laser-pulse compression of two 40-cm-sq-aperture, IR (1054-nm) laser beams. Critical to this compression, within the GCC, are eight sets (four per beamline) of tiled (e.g., three optical elements precisely held side by side to act as one element) multilayer-dielectric (MLD)-diffraction-grating assemblies (three gratings per assembly) that provide the capability for producing 2.6-kJ output IR energy per beam at 10 ps. The primary requirements for each of the 24 lareg-aperture (43-cm x 47-cm) gratings are a high diffraction efficiency greater than 95%, a peak-to-valley wavefront quality of less than lamba/4 waves at 1054 nm, and a laser-induced-damage threshold greater than 2.7 J/cm^2 at 10-ps pulse width (measured at normal beam incidence). Degradation of grating laser-damage thresholds due to adsorption of contaminants must be prevented to maintain system performance. The presence of extrinsic contaminants (either particulate or molecular) in the vacuum system puts the MLD gratings at risk with respect to lowered damage threshold. A number of protocols have been developed and implemented at LLE to minimize MLD grating contamination and to characterize the performance of the GCC. In this paper, we describe component-cleaning procedures; the qualification, testing methods, and studies undertaken for materials intended for use within the chamber; as well as the necessary cleaning procedures to integrate and operate the MLD grating assemblies.

laser-pulse compression, vacuum chamber, cleaning,↗

Pulse-length dependence of the laser-induced damage behavior of a fused-silica antireflective metasurface

A broadband, antireflective metasurface optic on a silica substrate is subjected to laser-induced damage-threshold measurements to quantify its performance under exposure to high-intensity/fluence laser pulses in the near-infrared at four pulse durations, ranging from 20 fs to 1.4 ns. The performance of the metasurface is benchmarked against that obtained from an equivalent bare fused-silica substrate that did not receive reactive-ion-etching metasurface treatment. Results showed that the damage threshold of the antireflective metasurface was always lower than the input-surface damage threshold of the untreated substrate. The damage initiations with nanosecond and picosecond pulses resulted in localized modification and removal of the nanostructures, whereas the onset of laser-induced modification with 20-fs pulses in a vacuum environment manifested as changes in the optical and electronic properties without significant material removal. The broader goal of this work is to develop a preliminary understanding of the laser-induced failure mechanisms of silica-based metasurface optics.

antireflection↗

Soft x-ray free-electron laser induced damage to inorganic scintillators

An irreversible response of inorganic scintillators to intense soft x-ray laser radiation was investigated at the FLASH (Free-electron LASer in Hamburg) facility. Three ionic crystals, namely, Ce:YAG (cerium-doped yttrium aluminum garnet), PbWO4 (lead tungstate), and ZnO (zinc oxide), were exposed to single 4.6 nm ultra-short laser pulses of variable pulse energy (up to 12 μJ) under normal incidence conditions with tight focus. Damaged areas produced with various levels of pulse fluences, were analyzed on the surface of irradiated samples using differential interference contrast (DIC) and atomic force microscopy (AFM). The effective beam area of 22.2 ± 2.2 μm2 was determined by means of the ablation imprints method with the use of poly(methyl methacrylate) - PMMA. Applied to the three inorganic materials, this procedure gave almost the same values of an effective area. The single-shot damage threshold fluence was determined for each of these inorganic materials. The Ce:YAG sample seems to be the most radiation resistant under the given irradiation conditions, its damage threshold was determined to be as high as 660.8 ± 71.2 mJ/cm2. Contrary to that, the PbWO4 sample exhibited the lowest radiation resistance with a threshold fluence of 62.6 ± 11.9 mJ/cm2. The threshold for ZnO was found to be 167.8 ± 30.8 mJ/cm2. Both interaction and material characteristics responsible for the damage threshold difference are discussed in the article.

36 MATERIALS SCIENCE↗

Studies on the growth and physical properties of nonlinear optical crystal: 2-Amino-5-nitropyridinium-toluenesulfonate

Graphical abstract: 2-Amino-5-nitropyridinium-toluenesulfonate is identified as potential candidate for efficient frequency conversion. Research highlights: {yields} Single crystals of 2A5NPT have been grown from saturated solution. {yields} Powder test with Nd:YAG laser radiation shows a high second harmonic generation. {yields} Single shot and multiple shot surface laser damage thresholds are determined. {yields} The thermal parameters of 2A5NPT were measured by an improved photopyroelectric technique. {yields} The high value of damage threshold is related to the specific heat of the crystal which is reasonably high. -- Abstract: Single crystals of 2-amino-5-nitropyridinium-toluenesulfonate (2A5NPT) were grown by the slow cooling method. The unit cell dimensions were determined from single crystal X-ray diffraction studies. The thermal parameters - thermal diffusivity ({alpha}), thermal effusivity (e), thermal conductivity (K) and heat capacity (C{sub p}) of 2A5NPT were measured by an improved photopyroelectric technique at room temperature. Single and multiple shot experiments performed on the grown crystals for the second harmonic of pulsed Nd:YAG laser (532 nm) show that it exhibits a high laser damage threshold which is a favorable property for nonlinear optical applications. Dielectric constant and dielectric loss of the grown crystal were evaluated for the frequency range 1 kHz-1 MHz in the temperature region 40-130 {sup o}C. Hardness values were measured using Vickers hardness measurement.

36 MATERIALS SCIENCE↗

Methods for improving the damage performance of fused silica polished by magnetorheological finishing

The laser-induced damage threshold of fused-silica samples processed via magnetorheological finishing is investigated for polishing compounds depending on the type of abrasive material and the post-polishing surface roughness. The effectiveness of laser conditioning is examined using a ramped pre-exposure with the same 351-nm, 3-ns Gaussian pulses. Lastly, we examine chemical etching of the surface and correlate the resulting damage threshold to the etching protocol. A combination of etching and laser conditioning is found to improve the damage threshold by a factor of ~3, while maintaining <1-nm surface roughness.

36 MATERIALS SCIENCE↗

Dual wavelength laser damage testing for high energy lasers.

As high energy laser systems evolve towards higher energies, fundamental material properties such as the laser-induced damage threshold (LIDT) of the optics limit the overall system performance. The Z-Backlighter Laser Facility at Sandia National Laboratories uses a pair of such kiljoule-class Nd:Phosphate Glass lasers for x-ray radiography of high energy density physics events on the Z-Accelerator. These two systems, the Z-Beamlet system operating at 527nm/ 1ns and the Z-Petawatt system operating at 1054nm/ 0.5ps, can be combined for some experimental applications. In these scenarios, dichroic beam combining optics and subsequent dual wavelength high reflectors will see a high fluence from combined simultaneous laser exposure and may even see lingering effects when used for pump-probe configurations. Only recently have researchers begun to explore such concerns, looking at individual and simultaneous exposures of optics to 1064 and third harmonic 355nm light from Nd:YAG [1]. However, to our knowledge, measurements of simultaneous and delayed dual wavelength damage thresholds on such optics have not been performed for exposure to 1054nm and its second harmonic light, especially when the pulses are of disparate pulse duration. The Z-Backlighter Facility has an instrumented damage tester setup to examine the issues of laser-induced damage thresholds in a variety of such situations [2] . Using this damage tester, we have measured the LIDT of dual wavelength high reflectors at 1054nm/0.5ps and 532nm/7ns, separately and spatially combined, both co-temporal and delayed, with single and multiple exposures. We found that the LIDT of the sample at 1054nm/0.5ps can be significantly lowered, from 1.32J/cm{sup 2} damage fluence with 1054/0.5ps only to 1.05 J/cm{sup 2} with the simultaneous presence of 532nm/7ns laser light at a fluence of 8.1 J/cm{sup 2}. This reduction of LIDT of the sample at 1054nm/0.5ps continues as the fluence of 532nm/7ns laser light simultaneously present increases. The reduction of LIDT does not occur when the 2 pulses are temporally separated. This paper will also present dual wavelength LIDT results of commercial dichroic beam-combining optics simultaneously exposed with laser light at 1054nm/2.5ns and 532nm/7ns.

43 PARTICLE ACCELERATORS↗

Fluence thresholds for grazing incidence hard x-ray mirrors

X-ray Free Electron Lasers (XFELs) have the potential to contribute to many fields of science and to enable many new avenues of research, in large part due to their orders of magnitude higher peak brilliance than existing and future synchrotrons. To best exploit this peak brilliance, these XFEL beams need to be focused to appropriate spot sizes. However, the survivability of X-ray optical components in these intense, femtosecond radiation conditions is not guaranteed. As mirror optics are routinely used at XFEL facilities, a physical understanding of the interaction between intense X-ray pulses and grazing incidence X-ray optics is desirable. We conducted single shot damage threshold fluence measurements on grazing incidence X-ray optics, with coatings of ruthenium and boron carbide, at the SPring-8 Angstrom compact free electron laser facility using 7 and 12 keV photon energies. The damage threshold dose limits were found to be orders of magnitude higher than would naively be expected. The incorporation of energy transport and dissipation via keV level energetic photoelectrons accounts for the observed damage threshold.

43 PARTICLE ACCELERATORS↗

The growth of benzophenone crystals by Sankaranarayanan-Ramasamy (SR) method and slow evaporation solution technique (SEST): A comparative investigation

Highlights: Black-Right-Pointing-Pointer Benzophenone single crystal was grown by Sankaranarayanan-Ramasamy method which has the sizes of 1060 mm length and 55 mm diameter for the first time. Black-Right-Pointing-Pointer The conventional and SR-grown benzophenone crystals were characterized and compared using HRXRD, etching, laser damage threshold, microhardness, UV-transmittance, birefringence and dielectric analysis. Black-Right-Pointing-Pointer The SR-grown benzophenone crystal has higher LDT, microhardness, transparency, dielectric permittivity, birefringence and lower FWHM, EPD, dielectric loss than the crystal grown by conventional method. Black-Right-Pointing-Pointer The probable reason for higher crystalline perfection in SR-grown crystal was discussed. -- Abstract: Longest unidirectional Left-Pointing-Angle-Bracket 1 0 0 Right-Pointing-Angle-Bracket benzophenone (BP) crystal having dimension of 1060 mm length and 55 mm diameter was grown by Sankaranarayanan-Ramasamy method. The growth rate was measured by monitoring the elevation of the crystal-solution interface at different temperatures. The high resolution X-ray diffraction and etching measurements indicate that the unidirectional grown benzophenone crystal has good crystalline perfection and less density of defects. The optical damage threshold of SEST and SR grown BP crystals has been investigated and found that the SR grown benzophenone crystal has higher laser damage threshold value than the conventional method grown crystal. Microhardness measurement shows that crystals grown by SR method have a higher mechanical stability than the crystals grown by SEST method. Dielectric permittivity and birefringence are high in SR grown crystal compared to SEST grown BP crystal. The UV-vis-NIR results show that SR method grown crystal exhibits 7% higher transmittance as against crystals grown by conventional method.

36 MATERIALS SCIENCE↗

Synthesis, crystal growth and characterization of nonlinear optical organic crystal: p-Toluidinium p-toluenesulphonate

Graphical abstract: p-Toluidinium p-toluenesulphonate (p-TTS) an organic nonlinear optical crystal has been grown from the aqueous solution by slow evaporation solution growth technique. Single crystal X-ray diffraction analysis reveals that p-TTS crystallizes in monoclinic crystal system. p-TTS single crystal belongs to negative birefringence crystal. Second harmonic conversion efficiency of p-TTS has been found to be 1.3 times higher than that of KDP. Multiple shot surface laser damage threshold is determined to be 0.30 GW/cm{sup 2} at 1064 nm laser radiation. Highlights: Black-Right-Pointing-Pointer It deals with the synthesis, growth and characterization of p-TTS an organic NLO crystal. Black-Right-Pointing-Pointer Wide optical transparency window between 280 nm and 1100 nm. Black-Right-Pointing-Pointer Negative birefringence crystal and dispersion of birefringence is negligibly small. Black-Right-Pointing-Pointer Thermal study reveals that the grown crystal is stable up to 210 Degree-Sign C. Black-Right-Pointing-Pointer Multiple shot surface laser damage threshold is 0.30 GW/cm{sup 2} at 1064 nm laser radiation. -- Abstract: p-Toluidinium p-toluenesulphonate (p-TTS) an organic nonlinear optical crystal has been grown from the aqueous solution by slow evaporation solution growth technique. Single crystal X-ray diffraction analysis reveals that p-TTS crystallizes in monoclinic crystal system. The structural perfection of the grown p-TTS single crystal has been analyzed by high-resolution X-ray diffraction rocking curve measurements. Fourier transform infrared spectral studies have been performed to identify the functional groups. The optical transmittance window and the lower cutoff wavelength of the grown crystals have been identified by UV-vis-IR studies. Birefringence of p-TTS crystal has been studied using channel spectrum measurement. The laser damage threshold value was measured using Nd:YAG laser. The second harmonic conversion efficiency of p-TTS has been determined using Kurtz powder technique. Thermo gravimetric and differential thermal analyses were used to study its thermal properties. Dielectric constant, dielectric loss and AC conductivity of the grown p-TTS single crystal has been studied.

36 MATERIALS SCIENCE↗

Optimizing a cleaning process for multilayer-dielectric- (MLD) diffraction gratings

An essential component for the OMEGA EP short-pulse petawatt laser system is the grating compressor chamber (GCC). This large (12,375 ft 3 ) vacuum chamber contains critical optics where laser-pulse compression is performed at the output of the system on two 40-cm-sq-aperture, IR (1054-nm) laser beams. Critical to this compression, within the GCC, are four sets of tiled multilayer-dielectric- (MLD) diffraction gratings that provide the capability for producing 2.6-kJ output IR energy per beam at 10 ps. The primary requirements for these large-aperture (43-cm × 47-cm) gratings are diffraction efficiencies greater than 95%, peak-to-valley wavefront quality of less than λ/10 waves, and laser-induced-damage thresholds greater than 2.7 J/cm 2 at 10-ps measured beam normal. Degradation of the grating laser-damage threshold due to adsorption of contaminants from the manufacturing process must be prevented to maintain system performance. In this paper we discuss an optimized cleaning process to achieve the OMEGA EP requirements. The fabrication of MLD gratings involves processes that utilize a wide variety of both organic materials (photoresist processes) and inorganic materials (metals and metal oxides) that can affect the final cleaning process. Finally, a number of these materials have significant optical absorbance; therefore, incomplete cleaning of these residues may result in the MLD gratings experiencing laser damage.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗