Search NASA⌕ Search

SEARCH · Search NASA

Results for “dislocation loops”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

MAX Phases for the Nuclear Industry: Possibilities and Pitfalls

By now it is well-established that the layered, machinable, hexagonal carbides and nitrides, with the general formula, M{sub n+1}AX{sub n}, (MAX) where n = 1 to 3, M is an early transition metal, A is an A-group (mostly groups 13 and 14) element and X is either C and/or N - sometimes referred to as polycrystalline nanolaminates because every basal plane is a potential deformation or delamination plane - combine some of the best attributes of metals and ceramics. Like metals, they are electrically and thermally conductive, most readily machinable (manual hack saw will suffice) not susceptible to thermal shock, plastic at high temperatures, and exceptionally damage tolerant. Like ceramics, some of them are elastically quite rigid, lightweight, and maintain their strengths to high temperatures. The ternaries Ti{sub 3}SiC{sub 2} and Ti{sub 2}AlC are also creep, fatigue and oxidation resistant. The impetus for this work was our conjecture - proven herein - that the presence of the pure A-layers in the MAX phases would result in extraordinary damage tolerance to neutron. After irradiation to 0.14 dpa at 121 deg. C and 735 deg. C, black spots are observed in both ternaries. After irradiation to higher doses, at 735 deg. C, basal dislocation loops, with a Burgers vector of b = 1/2 [0001] are observed in TAC with loop diameters of the order of the order of 25 nm. In TAC larger dislocation loops (75±34 nm) are observed after 3.4 dpa at 735 deg. C, in addition to stacking faults. In sharp contrast to the MAX phases, the TiC impurity particles in the former, form extensive dislocation loops at all conditions. Voids are observed at grain boundaries and within stacking faults after 3.4 dpa irradiation, with extensive void formation in the TiC regions at 1085 deg. C. Most remarkably, defect free, denuded zones, of the order of 1 μm, were observed after irradiation to 3.4 dpa at 735 deg. C. Small grains, 3-5 μm in diameter were totally damage free after irradiation at 1085 deg. C to this dose. When these results are compared to those of TiC, there is little doubt that the A-layers in the MAX phases, provide enhanced neutron irradiation tolerance. Based on these, and other results that will be touched upon, it is reasonable to conclude that Ti{sub 3}SiC{sub 2} is quite a promising candidate for high (> 500 deg. C) temperature nuclear applications. At lower temperatures anisotropic swelling results in microcracking. (authors)

36 MATERIALS SCIENCE↗

TEM characterization of 14YWT and 12YWT ODS ferritic alloys neutron irradiated at 500C using in-situ helium injection

This report summaries TEM characterization of 14YWT and 12YWT, ODS ferritic alloys with 14 and 12 wt % of Cr respectively, to compare the effect of neutron irradiation with and without concurrent He injection using ISHI. The density and average size of <100>/{100} type dislocation loops are always larger than those of 1/2<111>/{111} type, but this difference is significantly affected by He implantation. The density of dislocation loops of both types ranges from ~1 to 4x1021 m-3 with average size ranging from 5~20 nm. 14YWT has lower density but larger size dislocation loops than 12YWT, while the line dislocation density of 14YWT is 3 times lower than that of 12YWT. Helium bubble densities of both 14YWT and 12YWT are 1.9x1023 m-3, the average He bubbles size of 14YWT and 12YWT are 1.4 and 1.2 nm, respectively. 14YWT exhibits α-α’ phase separation, Y-rich particles and uniformly distributed W. In addition to those features, 12YWT exhibits Y-Ti-O particles (not Y-O rich) and elongated Cr-rich phases.

36 MATERIALS SCIENCE↗

Improved irradiation resistance of accident-tolerant high-strength FeCrAl alloys with heterogeneous structures

In this work, post–neutron irradiation examination is performed on advanced accident-tolerant fuel (ATF) cladding iron-chromium-aluminum (FeCrAl) alloys with ~10–13at. % Cr, ~10–12 at. % Al, ~1 at. % Mo, and minor alloying elements including Y irradiated to a damage level of 7 displacements per atom (dpa) at irradiation temperatures of 267–282 °C. A compositional dependency of the Cr and Al content is observed on the ratio of sessile and glissile dislocation loops, where the density of a$\langle$100$\rangle$ type loops is somewhat higher than the a/2$\langle$111$\rangle$ type loops. The α' precipitate number density is inversely correlated to the starting Cr concentration of the alloys of interest. The irradiation to a higher dose of 7 dpa results in a higher density of dislocation loops and α' precipitates for the same alloys at a lower irradiation dose, such as 1.8 dpa. In this work, the effect of α' precipitates on the dislocation loop density is discussed, and the presence of α' appears to inhibit the nucleation of loops. Compared with first-generation FeCrAl alloys, these advanced alloys with heterogeneous structure exhibit a lower Cr concentration in α' precipitation at the same dose level; they act as weaker obstacles deviating from the primary hardening contribution from the mature α'. Hence, the overall irradiation-induced hardening decreases; our alloys show improved radiation resistance because of their stronger sink strengths. The results presented in this paper could provide insights for the design and optimization of ATF cladding materials for future fission and space applications.

36 MATERIALS SCIENCE↗

Effect of H and He Irradiation on Cavity Formation and Blistering in Ceramics

Single- or poly-crystalline specimens of SiC, Si{sub 3}N{sub 4}, MgO, Al{sub 2}O{sub 3} and MgAl{sub 2}O{sub 4} were implanted with 0.4-1 MeV H{sup +} or He{sup +} ion beams at room temperature and 650 C up to fluences of {approx}1 x 10{sup 22}/m{sup 2}. This produced peak implanted gas and displacement damage levels as high as {approx}50 at.% and 34 displacements per atom (dpa). The specimens were subsequently examined optically, and in cross-section using transmission electron microscopy. Subsurface blistering occurred for specimens irradiated to H or He fluences greater than about 3 x 10{sup 21}/m{sup 2} ({approx}15 at.% peak implanted gas concentration), and surface exfoliation occurred for fluences above {approx}1 x 10{sup 22}/m{sup 2} ({approx}40 at.% implanted gas). Both helium and hydrogen had comparable effectiveness for inducing blistering and exfoliation on an atomic basis. The threshold blistering and exfoliation fluences for both ions were weakly dependent on temperature between 25 and 650 C. Both H and He were found to be very effective in inducing matrix cavity formation, due to their low solubility in these ceramics. The implanted gas concentrations that resulted in visible cavity formation generally ranged from 1 to 5 at.%. Visible cavity formation was readily induced during room temperature irradiation despite the limited vacancy mobility in these ceramics at room temperature. Three general types of cavity morphologies were observed: isolated cavities, clusters of small cavities (typically associated with dislocation loops), and two-dimensional platelets. Cavity formation was observed to initiate at the periphery of dislocation loops in some cases. During elevated temperature irradiation, cavity formation was often observed to be preferentially associated with certain low-index habit planes, particularly if the habit plane was oriented nearly parallel to the irradiated surface: (0001) and {l_brace}1{bar 1}00{r_brace} for Al{sub 2}O{sub 3}, (0001) for a-SiC, {l_brace}001{r_brace} and {l_brace}110{r_brace} for MgO, and {l_brace}110{r_brace} and {l_brace}111{r_brace} for MgAl{sub 2}O{sub 4}. The bubble formation and blistering behavior of the ceramics was similar to that observed in other studies of metals irradiated at comparable homologous temperatures. Ionization-induced diffusion effects associated with dual-beam light ion irradiation appeared to exert only a weak effect on cavity and dislocation loop growth compared to the single ion irradiation conditions.

08 HYDROGEN↗

Dynamic observation of dual-beam irradiated Fe and Fe-10Cr alloys at 435 °C

The attractive mechanical properties and superior resistance to void-swelling make ferritic/martensitic alloys a promising structural material for advanced nuclear reactors. However, one anomaly that has intrigued researchers for more than 50 years is the proportion of two types of dislocation loops in Fe and Fe-Cr alloys with Burger vectors b=½<111> and b=<100>. Although the possible mechanisms responsible for the presence of <100> loops continue to be the subject of intense modeling studies, there remains incomplete experimental understanding of fundamental irradiation processes in Fe(Cr) alloys. Here, the dose dependence of the irradiation-induced microstructural evolution was examined from 0 to 20 displacement per atom (dpa) in high purity Fe and Fe-10Cr during simultaneous dual-beam (1 MeV Kr + 10 appm He/dpa) irradiation at 435 °C. We experimentally revealed that the mechanism for the formation of <100> loops may not follow the conventional simple dislocation reaction between two 1½<111> loops. Real-time dynamic formation and evolution of defects including black dot loops, loop coarsening, loop decoration, network dislocations, and cavities were demonstrated. Several results indicated that the addition of Cr and He could impede dislocation loop motion. The evolution of the defect size/density and relative fraction of ½<111> vs <100> loops were quantitatively summarized. With increasing dose, ½<111> loops became the dominant type of loop in both materials. Notably, <100> loops were predominantly observed near grain boundaries only for pure Fe, while arrays of nanoscale black dot defects composing the <100> loop strings were observed in plenty in Fe-10Cr.

36 MATERIALS SCIENCE↗

Evolution of extended defects in UO 2 during high temperature annealing

The evolution of thermophysical characteristics of uranium oxide (UO 2 ) under irradiation is a critical aspect of nuclear fuel performance of light water reactors. This study examines the effect of high-temperature annealing at 1000 °C - 1600 °C on defect evolution in krypton irradiated UO 2 at room temperature. Transmission electron microscopy analysis reveals that the size of irradiation-induced bubbles and dislocation loops increases but their density decreases with annealing temperatures. Perfect dislocation loops with = <110> dominate, regardless of the annealing temperature. A rate theory model for extended defect evolution is applied to conclude that current understanding of dynamical loop and bubble evolution at high-temperature annealing is governed by defect coalescence.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Reversible Movement of Homogenously Nucleated Dislocations in a {beta}-Titanium Alloy

We demonstrate reversible movement of (1/2)[110](110) dislocation loops generated from nanodisturbances in a {beta}-titanium alloy. High resolution transmission electron microscope observations during an in situ tensile test found three reversible deformation mechanisms, nanodisturbances, dislocation loops and martensitic transformation, that are triggered in turn with increasing applied stress. All three mechanisms contribute to the nonlinear elasticity of the alloy. The experiments also revealed the evolution of the dislocation loops to disclination dipoles that cause severe local lattice rotations.

36 MATERIALS SCIENCE↗

Temperature and radiation effects on brittle versus ductile fracture behavior in miscible phase boundaries: insight from atomistic simulations

Temperature- and irradiation-assisted failure mechanisms in miscible phase boundaries are clarified via atomistic calculations. We first establish the temperature-dependent brittle-to-ductile transition in U–Zr miscible phase boundaries. Our results confirm that these boundaries are mostly brittle at low temperatures and ductile at elevated temperatures. We then investigate the changes induced by irradiation on the fracture mechanisms in such phase boundaries. The irradiation-induced defect accumulation follows a multi-stage process that starts with the accumulation of isolated small dislocation loops before transitioning to the saturation and growth of larger dislocation loops and end up with a reorganization into forest dislocations. The accumulation of loops is the primary feature to participate in the delineation between brittle and ductile interfacial fracture in irradiated phase boundaries. At low damage levels, radiation defect interactions with the crack tip are limited and U–Zr miscible boundaries fail through the emission of dislocations ahead of the crack tip followed by brittle cleavage in agreement with the classical Griffith’s criterion for crack stability. At higher damage levels, the failure mode transitions from brittle crack growth to ductile void growth. In this case, the microcrack tip is blunted by the high density of pre-existing, radiation-induced defects in the vicinity of the crack. This interaction leads to the development and growth of a cavity at the interface as opposed to interfacial cleavage.

36 MATERIALS SCIENCE↗

Theoretical Investigation of Microstructure Evolution and Deformation of Zirconium Under Cascade Damage Conditions

This work is based on our reaction-diffusion model of radiation growth of Zr-based materials proposed recently in "On the Origin of Radiation Growth of HCP Crystals". In "On the Origin of Radiation Growth of HCP Crystals", the equations for the strain rates in unloaded pure crystal under cascade damage conditions of, e.g., neutron or heavy-ion irradiation were derived as functions of dislocation densities, which include contributions from dislocation loops, and spatial distribution of their Burgers vectors. The model takes into account the intra-cascade clustering of self-interstitial atoms and their one-dimensional diffusion; explains the growth stages, including the break-away growth of pre-annealed samples; and accounts for some striking observations, such as of negative strain in prismatic direction, and co-existence of vacancy- and interstitial-type prismatic loops. In this report, the change of dislocation densities due to accumulation of sessile dislocation loops is taken into account explicitly to investigate the dose dependence of radiation growth. The dose dependence of climb rates of dislocations is calculated, which is important for the climb-induced glide model of radiation creep. The results of fitting the model to available experimental data and some numerical calculations of the strain behavior of Zr for different initial dislocation structures are presented and discussed. The computer code RIMD-ZR.V1 (Radiation Induced Microstructure and Deformation of Zr) developed is described and attached to this report.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

(S)TEM/EDS study of native precipitates and irradiation induced Nb-rich platelets in high-burnup M5®

We have investigated microstructure and microchemistry of precipitates and dislocation loops in high-burnup M5® using (scanning) transmission electron microscopy ((S)TEM) equipped with energy dispersive X-ray spectroscopy (EDS). Two (S)TEM lamellae were made by cryo-FIB from the same cladding sample. The Nb-rich native precipitates were found in the metal, in the suboxide and in the oxide. Upon diffraction analysis, most of the Nb-rich native precipitates in the metal matrix remain as β-Nb phase, while no β-Nb native precipitates were found in the oxide. Nearby the oxide and metal (O/M) interface, the native precipitates in the oxide were already oxidized into t-NbO2 phase. At further distance away from the O/M interface, the Nb-rich native precipitates were gradually oxidized and became amorphous. Besides the native precipitates, Nb-rich irradiation induced precipitates (IIPs) were found in the metal matrix. Using g = <0002> vector for imaging, the length of the IIPs was aligned with dislocation loops. However, no Nb segregation to the dislocation loops themselves was observed. For the first time, we report that IIPs indeed exist in the oxide but only within about 1.5 µm away from O/M interface. However, the oxidation state of the IIPs in the oxide is still unclear. The presence of both native precipitates and IIPs in the oxide may indicate the Nb concentration in the oxide solid solution remain low nearby the O/M interface, which may explain the reduced corrosion kinetics of in-pile M5®. On the other hand, no IIPs were observed in the oxide at further distance and this may indicate that they have eventually dissolved back into the oxide. A few mechanisms related to IIPs stability in the oxide are presented.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Response of 14YWT alloys under neutron irradiation: A complementary study on microstructure and mechanical properties

Nanostructured ferritic alloys (NFAs) having sub-micron grain size with a high density of nano-oxides (NOs) (size of ~2-3 nm) are one of the best candidates for structural components in Generation IV nuclear systems. In this study, 14YWT NFA cladding tubes were irradiated in BOR60 reactor up to 7 dpa at 360-370 °C. Detailed microstructural analysis has been conducted using bright field transmission electron microscopy, bright field scanning transmission electron microscopy, energy filtered transmission electron microscopy, energy dispersive X-ray spectroscopy, electron energy loss spectroscopy and transmission Kikuchi diffraction techniques. This revealed cavities, <100> and <111> type dislocation loops, and α' precipitates forming after irradiation with relationships between cavities and NOs, and α' precipitates and NOs. Cavities mostly form on the NOs; whereas, α' precipitates form between the NOs where the point defect concentration is high. Moreover, α' precipitates are distributed homogenously on and around the dislocation loops which is consistent with the observation that there is no Cr segregation on dislocation loops. Grain boundaries were found to be mostly depleted in Cr; however, the characteristics of each grain boundary determines the Cr behavior and the α' denuded zone around the grain boundaries. Mechanical properties of the irradiated tubes have been determined by using both low force and high force nanoindentation techniques, resulting in 1.03±0.33 GPa and 0.82±0.20 GPa hardening, respectively. Dispersed barrier hardening calculations and nanoindentation measurements are in good agreement. In this paper, 14YWT NFA has been systematically studied after neutron irradiation to better understand its superior performance: low α' concentration, low swelling and low radiation-induced hardening.

36 MATERIALS SCIENCE↗

Effects of neutron irradiation and post-irradiation annealing on the microstructure of HT-UPS stainless steel

Microstructural changes resulted from neutron irradiation and post-irradiation annealing in a high-temperature ultra-fine precipitate strengthened (HT-UPS) stainless steel were characterized using transmission electron microscopy (TEM) and atom probe tomography (APT). Three HT-UPS samples were neutron-irradiated to 3 dpa at 500 °C, and after irradiation, two of them were annealed for 1 h at 600 °C and 700 °C, respectively. Frank dislocation loops were the dominant defect structure in both the as-irradiated and 600 °C post-irradiation-annealed (PIAed) samples, and the loop sizes and densities were similar in these two samples. Unfaulted dislocation loops were observed in the 700 °C PIAed sample, and the loop density was greatly reduced in comparison with that in the as-irradiated sample. Nano-sized MX precipitates were observed under TEM in the 700 °C PIAed sample, but not in the 600 °C PIAed or the as-irradiated samples. The titanium-rich clusters were identified in all three samples using APT. The post-irradiation annealing (PIA) caused the growth of the Ti-rich clusters with a stronger effect at 700 °C than at 600 °C. The irradiation caused elemental segregations at the grain boundary and the grain interior, and the grain boundary segregation behavior is consistent with observations in other irradiated austenitic steels. Here, APT results showed that PIA reduced the magnitude of irradiation induced segregations.

36 MATERIALS SCIENCE↗

Microstructural evolution in nickel alloy C-276 after Ar-ion irradiation at elevated temperature

In present work, the irradiation damage in nickel-base alloy C-276 irradiated with Ar-ions was studied. Specimens of C-276 alloy were subjected to an irradiation of Ar-ions (with 120 keV) to dose levels of 6 and 10 dpa at 300 and 550 Degree-Sign C, respectively. The size distributions and densities of dislocation loops caused by irradiation were investigated with transmission electron microscopy. Irradiation hardening due to the formation of the loops was calculated using the dispersed barrier-hardening model, showing that irradiation hardening was greatest at 300 Degree-Sign C/6 dpa. The microstructure evolution induced by Ar-ion irradiation (0-10 dpa) in nickel-base alloy C-276 has been studied using a multi-scale modeling code Radieff constructed based on rate theory, and the size of dislocation loops simulated by Radieff was in good agreement with the experiment. - Highlights: Black-Right-Pointing-Pointer High density of dislocation loops appeared after Ar ions irradiation. Black-Right-Pointing-Pointer Irradiation hardening due to the formation of loops was calculated by the DBH model. Black-Right-Pointing-Pointer Size of loops simulated by Radieff was in good agreement with the experiment.

36 MATERIALS SCIENCE↗

Aging and Embrittlement of High Fluence Stainless Steels

Irradiation of austenitic stainless steels results in the formation of dislocation loops, stacking fault tetrahedral, Ni-Si clusters and radiation-induced segregation (RIS). Of these features, it is the formation of precipitates which is most likely to impact the mechanical integrity at high dose. Unlike dislocation loops and RIS, precipitates exhibit an incubation period that can extend from 10 to 46 dpa, above which the cluster composition changes and a separate phase, (G-phase) forms. Both neutron and heavy ion irradiation showed that these clusters develop slowly and continue to evolve beyond 100 dpa. Overall, this work shows that the irradiated microstructure features produced by heavy ion irradiation are remarkably comparable in nature to those produced by neutron irradiation at much lower dose rates. The use of a temperature shift to account for the higher damage rate in heavy ion irradiation results in a fairly good match in the dislocation loop microstructure and the precipitate microstructure in austenitic stainless steels. Both irradiations also show segregation of the same elements and in the same directions, but to achieve comparable magnitudes, heavy ion irradiation must be conducted at a much higher temperature than that which produces a match with loops and precipitates. First-principles modeling has confirmed that the formation of Ni-Si precipitates under irradiation is likely caused by supersaturation of solute to defect sinks caused by highly correlated diffusion of Ni and Si. Thus, the formation and evolution of Ni-Si precipitates at high dose in austenitic stainless steels containing Si is inevitable.

36 MATERIALS SCIENCE↗

Temperature-dependent mechanism on hardening mitigation in thermomechanically processed 800H alloys under neutron irradiation

Irradiation induced hardening is commonly observed in structural materials, and is often associated with the degraded ductility. This study explores the role of thermomechanical processing (TMP) in mitigating irradiation-induced hardening in Incoloy 800H. The radiation response of solution-annealed and TMP-treated samples was systematically investigated to elucidate the underlying mechanisms of hardening reduction. Neutron irradiation was performed on solution-annealed and TMP-treated samples at 359, 431, and 580 °C, revealing consistently lower hardening in TMP samples. Microstructural characterization compared dislocation loops, cavities, clusters, and precipitates to assess their contributions to hardening. The strengthening contributions from individual microstructural features were estimated, and the microstructure-derived yield strength is consistent with the hardness-converted yield strength. The microstructure–properties correlation revealed the temperature-dependent primary hardening mechanism: dislocation loops dominated at lower temperature, whereas Ni3(Al,Ti) γ′ precipitates were predominant at higher temperature. TMP reduced radiation-induced hardening through two mechanisms: (1) increased sink strength from dislocations and Ti(C,N) precipitates limited dislocation loop formation at lower temperatures, and (2) reduced Ti solute within the matrix in TMP samples suppressed γ′ precipitate formation at higher temperatures. These findings identify the mechanisms governing radiation-induced hardening across different temperatures, which lays the foundation for TMP optimization for the development of advanced radiation-tolerant materials.

Zhong, Weicheng [ORNL] (ORCID:0000000231589271)↗

Second Annual Progress Report on Correlation Between Microstructure and Mechanical Properties of Neutron-Irradiated Ferritic-Martensitic and Austenitic Steels

Ferritic-martensitic steels G92-2b (an optimized Grade 92 heat), NF616 and T91, and austenitic stainless steel 800H and its Grain Boundary Engineering (GBE)-treated version 800H-TMP (ThermoMechanical Processing) were irradiated in the High Flux Isotope Reactor (HFIR) of Oak Ridge National Laboratory (ORNL) and the Advanced Test Reactor (ATR) of Idaho National Laboratory (INL). Selected G92-2b samples were irradiated up to 14.66 dpa in the HFIR at two temperature ranges: 400–496.7°C and 683.3– 720°C. NF616 and T91 were irradiated in the ATR up to 8.16 dpa with the irradiation temperatures ranged from 241°C to 447.5°C. Alloy 800H and 800H-TMP samples were irradiated in both the HFIR and the ATR. Selected 800H and 800H-TMP samples had HFIR irradiation to 1.28 dpa at 580°C and ATR irradiation up to 9.12 dpa at 359°C to 431°C. Vickers hardness measurements, fractography, and microstructural characterization were performed on the selected samples in the Low Activation Materials Design and Analysis (LAMDA) laboratory. Radiation-hardening of G92-2b was observed at the lower doses and lower irradiation temperatures (400- 496.7°C), with GB03 (0.52 dpa at 400°C) and GB04 (7.44 dpa at ~490°C) showing ~12% and ~8% hardening, respectively. Softening by ~14% was observed for GB05 (14.66 dpa at 496.7°C). Radiationsoftening of G92-2b was more prevalent at the higher irradiation temperatures (683.3-~720°C), with GB10 (0.46 dpa at 683.3°C), GB11 (7.44 dpa at ~720°C), and GB12 (14.63 dpa at ~720°C) showing ~8%, ~8%, and ~40% softening, respectively. Radiation-hardening of NF616 and T91 was observed with the hardness increased by ~37% to ~65% depending on the irradiation doses and irradiation temperatures. Within the studied irradiation conditions of NF616 and T91, samples with a higher dose had a larger hardness after irradiation. All the tested alloy 800H and 800H-TMP samples in this work showed radiation-hardening by ~96±7% to ~152±10%. Alloy 800H-TMP tended to have slightly smaller radiation-hardening than alloy 800H. The fractography results of G92-2b sample GB03, GB10, and GB11, together with the previously characterized fractography of GB04, GB05, and GB12, indicated that the ductility of G92-2b was maintained up to 14.66 dpa at the lower irradiation temperatures of 400-496.7°C, while some loss of ductility (less necking) was observed for higher doses at the higher irradiation temperatures of 683.3-720°C. This agrees with the previously reported tensile test results of G92-2b, where the elongation of G92-2b was reduced at higher doses at the higher irradiation temperatures. Dimple sizes increased at higher doses, which are more evident at the higher irradiation temperatures of 683.3-~720°C. The fractography of NF616 sample D2 (2.96 dpa at 291.5°C), D4 (5.91 dpa at 359°C), and D6 (8.16 dpa at 431°C) indicated loss of ductility with negligible necking for sample D2, while ductile failure for samples D4 and D6. Fractography of alloy 800H and 800H-TMP samples in various irradiation conditions showed ductile failure with obvious necking. Dimples were observed, with some of them containing large Ti-rich particles, in all the 800H/800H-TMP samples. Electron backscatter diffraction characterization of GB12 indicated the recovery of the lath structure, which was generally replaced by an equiaxed grain structure. Transmission electron microscopy (TEM) characterization showed the presence of frequent M 23 C 6 (M = primarily Cr), MX (M = primarily V), spherical Nb(C,N) precipitates, and occasional Laves phase precipitates in the G92-2b samples. MX precipitates with sizes of 20-30 nm were observed at boundaries of smaller grains, indicating the pinning effect of the V-rich precipitates. The lath structure recovery was more evident at the higher irradiation temperatures (683.3-~720°C), with decreased densities of line dislocations and M23C6 precipitates. The irradiated T91 (TA04) showed the growth of M23C6 precipitates to 101 ± 40 nm from the initial 68 ± 22 nm in the unirradiated condition. Dislocation loops of both {100} and {111} types were present in TA04. TEM characterization was also performed on the irradiated 800H (N4, N5, N6, and AR2) and 800H-TMP (P4, P5, P6, and HG1). Accumulation of M 23 C 6 precipitates at grain boundaries was observed in all the xii 800H/800H-TMP samples, and the presence of Ti(C,N) precipitates at grain boundaries and in the matrix was observed in the irradiated 800H-TMP. Some Ti(C,N) precipitates are embedded in the M 23 C 6 precipitates, maintaining specific orientation relationships between the precipitates and between the precipitate and matrix. In addition, nanoscale Si-rich clusters were observed in the matrix of all the 800H/800H-TMP samples, with EDS Si maps tending to have a lower contrast in 800H-TMP samples. Atom probe tomography was conducted on the same samples, supported by a Rapid Turnaround Examination project under Nuclear Science User Facilities. The results are being analyzed to be integrated with the TEM results for a confident description of the γ’ precipitates. Dislocation loops also formed in all the 800H/800H-TMP samples. The density and the average size of dislocation loops were quantified to be in the order of 10 22 – 10 23 m -3 and 11.7 – 15.9 nm, respectively, in the ATR-irradiated 800H/800H-TMP samples. The loop densities in irradiated 800H were higher than that in irradiated 800H-TMP under the same irradiation conditions. Further systematic data analyses, together with some complementary experiments, will be pursued for these samples to foster peer-reviewed journal article publications.

36 MATERIALS SCIENCE↗

Multi-axial and multi-energy channeling study of disorder evolution in ion-irradiated nickel

In this study, to better understand defect structure and the evolution of irradiation-induced damage in single crystal Ni, in situ Rutherford backscattering spectroscopy in channeling geometry (RBS/C) is performed along the <100>, <110>, and <211> axes with different probing beam energies. The RBS/C data reveal that damage evolution occurs in three steps. The first step at low doses (up to 0.2 dpa), characterized by a linear increase with dose, is related to the formation of point defects and small clusters. The second step in the intermediate dose range (0.2–1.0 dpa) shows a sublinear increase in disorder to saturation. This sublinear increase is due to the growth of defect clusters resulting from the interaction of irradiation-induced defects with already existing damage from previous ion impacts. The third step at high doses (1.0–32.4 dpa) exhibits a surprising decrease in the disorder level, which may be attributed to defect evolution from black spot defects to large dislocation loops that leads to strain relaxation. In addition, the damage extends much deeper than the predicted depths and is attributed to long-range defect migration effects confirmed by transmission electron microscopy (TEM) observations. Although similar damage evolution trends have been observed along all channeling directions, the disorder accumulation is largest along the <100> and <211> axes than observed along <110> axis. This “preferential” disordering process along <100> and <211> suggests that more defects are shielded by the <110> atomic rows than the two other axes. Finally, the co-existence of both uncorrelated displaced lattice atoms and dislocation loops in Ni irradiated at 1 ion/nm 2 is revealed by the energy-dependent RBS/C studies along all three axes. In contrast, dislocation loops and stacking fault tetrahedral are simultaneously present in the crystal structure of Ni irradiated at 100 ions/nm 2 that is consistent with previous molecular dynamics simulations and TEM observations.

36 MATERIALS SCIENCE↗