Search NASA⌕ Search

SEARCH · Search NASA

Results for “electrode aging”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Interplay of Electrode Heterogeneity and Lithium Plating

Lateral microstructure heterogeneity in anodes is known to induce nonuniform current density, state of charge, and lithium plating. This means that such electrode heterogeneity can limit the fast charging of lithium-ion batteries. In this work, a combination of experiments and simulation is employed to understand the effect of mm scale lateral heterogeneity on cell aging. A previously developed model was extended to efficiently simulate SEI formation and Li plating for independent regions of an electrode. The model consists of three parallel regions each described under a P2D framework and with a distinct ionic resistance and possibly active material loading. The results suggest that during fast charge when the active material is uniformly distributed across the three regions, the region with the highest resistance reaches the end of life sooner than the other regions. There is also positive feedback from Li metal filling the pores near the separator interface that further accelerates lithium plating. Lastly, when there is a non-uniform active material distribution associated with the ionic resistance heterogeneity, tight competition between regions can occur, leading to less overall lithium plating and plating that is more uniform between regions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Interfacial thermal degradation in inverted organic solar cells

The efficiency of organic photovoltaic (OPV) solar cells is constantly improving; however, the lifetime of the devices still requires significant improvement if the potential of OPV is to be realised. In this study, several series of inverted OPV were fabricated and thermally aged in the dark in an inert atmosphere. It was demonstrated that all of the devices undergo short circuit current-driven degradation, which is assigned to morphology changes in the active layer. In addition, a previously unreported, open circuit voltage-driven degradation mechanism was observed that is highly material specific and interfacial in origin. This mechanism was specifically observed in devices containing MoO{sub 3} and silver as hole transporting layers and electrode materials, respectively. Devices with this combination were among the worst performing devices with respect to thermal ageing. The physical origins of this mechanism were explored by Rutherford backscattering spectrometry and atomic force microscopy and an increase in roughness with thermal ageing was observed that may be partially responsible for the ageing mechanism.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Relating neuromuscular control to functional anatomy of limb muscles in extant archosaurs

Abstract Electromyography (EMG) is used to understand muscle activity patterns in animals. Understanding how much variation exists in muscle activity patterns in homologous muscles across animal clades during similar behaviours is important for evaluating the evolution of muscle functions and neuromuscular control. We compared muscle activity across a range of archosaurian species and appendicular muscles, including how these EMG patterns varied across ontogeny and phylogeny, to reconstruct the evolutionary history of archosaurian muscle activation during locomotion. EMG electrodes were implanted into the muscles of turkeys, pheasants, quail, guineafowl, emus (three age classes), tinamous and juvenile Nile crocodiles across 13 different appendicular muscles. Subjects walked and ran at a range of speeds both overground and on treadmills during EMG recordings. Anatomically similar muscles such as the lateral gastrocnemius exhibited similar EMG patterns at similar relative speeds across all birds. In the crocodiles, the EMG signals closely matched previously published data for alligators. The timing of lateral gastrocnemius activation was relatively later within a stride cycle for crocodiles compared to birds. This difference may relate to the coordinated knee extension and ankle plantarflexion timing across the swing‐stance transition in Crocodylia, unlike in birds where there is knee flexion and ankle dorsiflexion across swing‐stance. No significant effects were found across the species for ontogeny, or between treadmill and overground locomotion. Our findings strengthen the inference that some muscle EMG patterns remained conservative throughout Archosauria: for example, digital flexors retained similar stance phase activity and M. pectoralis remained an ‘anti‐gravity’ muscle. However, some avian hindlimb muscles evolved divergent activations in tandem with functional changes such as bipedalism and more crouched postures, especially M. iliotrochantericus caudalis switching from swing to stance phase activity and M. iliofibularis adding a novel stance phase burst of activity.

Cuff, Andrew R.↗

Characterization of Sodium Ion Electrochemical Reaction with Tin Anodes: Experiment and Theory

Tin anodes show a rich structure and reaction chemistry which we have investigated in detail. Upon discharge five plateaus are observed corresponding to -Sn, an unidentified phase (Na/Sn = 0.6), an amorphous phase (Na/Sn = 1.2), a hexagonal R-3m Na5Sn2, and fully sodiated Na15Sn 4. With charging there are six plateaus, which are related to the formation of Na5Sn2 followed by the formation of amorphous phases and -Sn. Upon cycling the formation of metastable Na5Sn2 seems to be suppressed, leading to a single charge plateau at 0.2 V. Theoretical voltages calculated from existing crystal structures using DFT provide a good match with constant current measurements, however, the voltage is more negative compared to quasi-equilibrium measurements (GITT). Search for additional (meta)stable phases using cluster-expansion method predicts many phases lower in energy than the convex hull, including the R-3m Na5Sn2 phase characterized experimentally. The presence of multiple phases in varying lattices with very similar formation energy suggests why the reaction mechanism is non-reversible. Interpretation of M ssbauer spectroscopy data is not yet elucidated due to the very low recoil-free fraction of the materials. The electrode surface is terminated with a SEI layer rich in carbonates such as Na2CO3 and Na alkyl carbonates as evidenced by XPS. After a full charge at 2V, strong evidence for the formation of oxidized Sn4+ is obtained. Subjecting the electrode to a rest after a full charge at 2 V reveals that aging in the electrolyte reduces the oxidized Sn4+ into Sn2+ and Sn0, and concomitantly suppresses the electrolyte decomposition represented by an anomalous discharge plateau at 1.2 V. Thereby, the catalytic decomposition of the electrolyte during discharge is caused by nanosized Sn particles covered by oxidized Sn4+ and not by pure metallic Sn.

Na5Sn2 metastable phase (XRD)↗

Prelithiated SiO x /Graphite-NMC811 Cells: Capacity Loss, Impedance Rise and Hidden Degradation Pathways Revealed Using Three-Electrode Diagnostics

Electrodes containing SiO x /graphite (Gr) materials are attractive as anodes for high-energy lithium-ion batteries. However, their mechanical deformation, electrochemical response, and impedance evolution during long-term cycling are strongly coupled, complicating accurate diagnosis of performance fade mechanisms. In this work, the behavior of electrochemically prelithiated SiO x /Gr anodes paired with NMC811 cathodes is systematically investigated using techniques that include in-situ dilatometry, three-electrode electrochemistry, and multiscale post-cycling microscopy. The SiO x /Gr electrode exhibits a maximum expansion of 49% upon lithiation to 10 mV vs Li + /Li, with 84% of the expansion and 91% of the capacity being reversible. In full cells, relatively stable cycling with only 12% capacity fade over 500 cycles is observed. Three-electrode experiments reveal cell-level impedance growth, which is dominated by the NMC811 cathode: the SiO x /Gr anode exhibits minimal net impedance rise and an initial impedance decrease at low potentials. Despite this apparent electrochemical stability, cross-sectional SEM, PFIB tomography, and cryo-STEM reveal irreversible anode thickening caused by the accumulation of an inorganic-rich solid electrolyte interphase (SEI) permeating the anode bulk. Electrode potential-shift analysis further demonstrates that Li + ions released from lithium reservoirs in the prelithiated anode mask true lithium inventory loss during aging. These results demonstrate that low-expansion SiO x /Gr anodes can simultaneously exhibit favorable cycling and impedance metrics while undergoing substantial, hidden degradation, underscoring the importance of electrode-resolved diagnostics for evaluating prelithiated silicon-based anodes.

25 ENERGY STORAGE↗

Transparent and Conductive Inorganic/Polymer‐Composite Encapsulants for Long‐Term Perovskite Solar Cells Operation

An innovative inorganic/polymer-composite encapsulation scheme comprising a polymer-based transparent conductive composite (TCC) coupled with a transparent conductive oxide is introduced to extend the lifetime of moisture-sensitive devices such as perovskite solar cells (PSC). The TCC comprises conductive silver-coated polymethyl methacrylate (Ag-PMMA) microsphere fillers protruding from a transparent non-conductive polymer matrix. TCC samples (5% Ag-PMMA by area) demonstrate high optical transparencies (%T approx. 85% in the 370–1200 nm region), low out-of-plane electrical resistivities (R < 0.2 Ω cm 2 ), and equilibrium permeabilities of less than 1 g mm/m 2 /day, all of which are well-maintained after 1,000 hours of environmental exposure. In practice, the TCC is employed between two indium zinc oxide (IZO) thin films, with the in-plane conductivity of IZO and the out-of-plane conductivity of TCC working collectively to function as a single encapsulating electrode. This encapsulation scheme is exemplified by benchmarking performances of PSCs subjected to accelerated aging conditions of quasi-maximum power point tracking under light soaking in air at 50 °C, 40% R.H. to 60% R.H. Notable improvements in operational lifetimes are observed, with a champion encapsulated PSC maintaining over 90% of its initial efficiency of 21.65% for up to 1,430 hours, compare to less than 300 hours for an unencapsulated control.

14 SOLAR ENERGY↗

ZrO 2 atomic layer deposition into Sr 0.5 Sm 0.5 CoO 3-δ –Ce 0.9 Gd 0.1 O 2-δ solid oxide fuel cell cathodes: mechanisms of stability enhancement

The application of atomic layer deposition (ALD) on solid oxide fuel cell (SOFC) cathodes has previously yielded mixed results and has been seen to depend on the ALD species, catalyst chemistry, catalyst morphology, and the conditions for deposition. Illustrated here is the effect of an ALD zirconia coating within an SOFC oxygen electrode: Sr 0.5 Sm 0.5 CoO 3- δ infiltrated into Gd-doped ceria, Ce 0.9 Gd 0.1 O 2- δ , scaffolds (SSC–GDC). Island-like ALD-ZrO 2 coatings with approximately monolayer coverage initially yield a higher electrode polarization resistance, R P , but thereafter the coated electrodes show lower R P and slower degradation. For example, after~1000 hour accelerated ageing tests carried out at 750 °C, SSC–GDC coated with ~0.3 nm of ALD-ZrO 2 showed an R P increase of 18% compared to 30% for uncoated SSC–GDC. Strontium surface segregation was not found to be a significant degradation factor. At 750 °C, a reaction between the Zr-overlayer and the SSC was observed, producing SrZrO 3 , Co 3 O 4 , and SmCoO 3 . The low R P values achieved indicate that the reactant products were thin enough to be discontinuous and thus not hinder the oxygen surface exchange process, and yet they acted as a barrier to SSC particle coarsening.

25 ENERGY STORAGE↗

Quantifying the Impact of Charge Rate and Number of Cycles on Structural Degeneration of Li-Ion Battery Electrodes

A quantitative link between crack evolution in lithium-ion positive electrodes and the degrading performance on cells is not yet well established nor is any single technique capable of doing so widely available. Here, we demonstrate a widely accessible high-throughput approach to quantifying crack evolution within electrodes. The approach applies super-resolution scanning electron microscopy (SEM) imaging of cross-sectioned NMC532 electrodes, followed by segmentation and quantification of crack features. Crack properties such as crack intensity, crack width and length are quantified as a function of charge rate (1C, 6C, and 9C) and cycle number (25, 225, and 600 cycles). Hundreds of particles are characterized for statistical confidence in the quantitative crack measurements. The data on crack evolution is compared to electrochemical data from full cells and half cells with the NMC532 positive electrodes. We show that while crack evolution strongly correlates with capacity fade in the first 25 cycles, it does not correlate well for the following hundreds of cycles indicating that cracking may not be the dominant cause of capacity fade throughout the cycle-life of cells.

25 ENERGY STORAGE↗

Lithium-Ion Battery Life Model with Electrode Cracking and Early-Life Break-in Processes

This paper develops a physically justified reduced-order capacity fade model from accelerated calendar- and cycle-aging data for 32 lithium-ion (Li-ion) graphite/nickel-manganese-cobalt (NMC) cells. The large data set reveals temperature-, charge C-rate-, depth-of-discharge-, and state of charge (SOC)-dependent degradation patterns that would be unobserved in a smaller test matrix. Model structure is informed by incremental capacity analysis that shows loss of lithium inventory and cathode-material loss as the dominant capacity fade mechanisms. The model includes terms attributable to solid-electrolyte interface (SEI) growth, electrode cracking, cycling-driven acceleration of SEI growth, and "break-in" mechanisms that slightly decrease or increase available Li inventory early in life. The study explores what mathematical couplings of these mechanisms best describe calendar aging, cycle aging, and mixed calendar/cycle aging. Various approaches are discussed for extracting relevant stress factors from complex cycling profiles to predict lifetime during real-world battery loads using models trained on constant-current laboratory test results. The complexity of the present human-driven model identification process motivates future work in machine learning to more widely search and statistically discern the optimal model that correctly extrapolates capacity fade based on physical knowledge.

25 ENERGY STORAGE↗

Temporal change in the electromechanical properties of dielectric elastomer minimum energy structures

Dielectric elastomer minimum energy structures (DEMES) are soft electronic transducers and energy harvesters with potential for consumer goods. The temporal change in their electromechanical properties is of major importance for engineering tasks. Therefore, we study acrylic DEMES by impedance spectroscopy and by optical methods for a total time period of approx. 4.5 months. We apply either compliant electrodes from carbon black particles only or fluid electrodes from a mixture of carbon black particles and silicone oil. From the measurement data, the equivalent series capacitances and resistances as well as the bending angles of the transducers are obtained. We find that the equivalent series capacitances change in average between −12 %/1000 h and −4.0 %/1000 h, while the bending angles decrease linearly with slopes ranging from −15 %/1000 h to −7 %/1000 h. Transducers with high initial bending angles and electrodes from carbon black particles show the smallest changes of the electromechanical characteristics. The capacitances decrease faster for DEMES with fluid electrodes. Some DEMES of this type reveal huge and unpredictable fluctuations of the resistances over time due to the ageing of the contacts. Design guidelines for DEMES follow directly from the observed transient changes of their electromechanical performance.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Nafion Structural Phenomena at the Platinum and Carbon Interfaces

Neutron Reflectometry (NR) was used to examine the interactions of Polymer Electrolyte Fuel Cell (PEFC) materials that comprise the triple-phase interface. Smooth, idealized layers of Nafion on glassy carbon (GC) and Pt surfaces were used to experimentally model the PEFC electrode interfaces. Different multilayer structures of Nafion were found in contact with the Pt or GC surfaces. These structures showed separate hydrophobic and hydrophilic domains formed within the Nafion layer when equilibrated with saturated D2O vapor. A hydrophobic Nafion region was formed adjacent to a Pt film. However, when Nafion was in contact with a PtO surface, the Nafion at the Pt interface became hydrophilic. The adsorbed oxide layer caused a long-range restructuring of the perfluorosulfonic acid (PFSA) polymer chains that comprise Nafion . The thicknesses of the hydrophobic and hydrophilic domains changed to the same magnitude when the oxide layer was present compared to a thin hydrophobic domain in contact with Pt. A three-layer Nafion structure was formed when Nafion was in direct contact with GC. The findings in this research are direct experimental evidence that both the interfacial and long-range structural properties of Nafion are affected by the material with which it is in contact. Evidence of physical changes of aged Nafion films was obtained, and the results showed a permanent increase in the thickness of the Nafion film and a decrease in scattering length density (SLD), which are attributed to irreversible swelling of the Nafion film. The aging also resulted in a decrease in SLD of the GC substrate, which is likely due to either an increase in surface oxidation of the carbon or loss of carbon mass at the GC surface.

30 DIRECT ENERGY CONVERSION↗

Electrochemical Aging and Halogen Oxides Formation on Multiwalled Carbon Nanotubes and Fe 3 O 4 @g-C 3 N 4 Coated Conductive Membranes

Electrochemical membrane filtration is widely reported to enhance water contaminants' degradation or rejection via anodic oxidation or cathodic repulsion. Despite their advances, electrochemical membranes or electrocatalysts often suffer from corrosion or passivation, especially under strong electrode potentials or reactions. Moreover, the formation of toxic byproducts, such as chlorinated organic compounds and oxyhalides (e.g., ClO 4 - ) is another major concern. This study investigated the membrane aging processes of two types of conductive membranes, multiwalled carbon nanotubes (MWCNTs) and ferrite/graphitic carbon nitride hybrids (Fe 3 O 4 @g-C 3 N 4 ) coated on ceramic membranes. Under high current densities (~ 20 mA∙cm -2 ) with anodic potentials (~10 V), MWCNTs and Fe 3 O 4 @g-C 3 N 4 catalysts underwent evident oxidation as indicated by an increase of the intensity ratio of the Raman spectral bands (I D /I G ) and charge transfer resistance (R ct ) of two electrochemical membranes. Under variations of electrode potentials, chloride or bromide were shown to be oxidized to bromate (BrO 3 - ) and chlorate (ClO 3 - ) at levels of 1-10 mmol∙L -1 . The formation of BrO 3 - and ClO 3 - was dependent on the solution pH, current densities (1-20 mA∙cm -2 ), and initial concentrations of Br or Cl ions. Finally, to warrant a safe and rational design and operation of electrochemically reactive membrane processes, membrane aging and toxic byproduct's formation deserve careful characterization under relevant water filtration environments.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Impacts of Dissolved Ni 2+ on the Solid Electrolyte Interphase on a Graphite Anode

Transition metal (e.g. Ni) ions dissolved from layered-structured Ni-rich cathodes can migrate to the anode side and accelerate the failure of lithium-ion batteries. The investigations of the impact and distribution of Ni species on the solid electrolyte interphase (SEI) on the anode are crucial to understand the failure mechanism. Herein, we used time-of-flight secondary ion mass spectroscopy (TOF-SIMS) coupled with multivariate curve resolution (MCR) analysis to intuitively characterize the distribution of Ni species in the SEI. We find that the SEI on the graphite electrode using an EC-based electrolyte exhibits a multi-stratum structure. During accelerated aging of the LiNi 0.88 Co 0.08 Mn 0.04 O 2 /graphite full cell, the dissolution of Ni aggravates significantly upon cycling. A strong correlation between the dissolved-Ni and organic species in the SEI on graphite is illustrated. Here, the ion-exchange reaction between Ni 2+ and Li + ions in the SEI is demonstrated to be the main reason for the increase of SEI resistivity.

25 ENERGY STORAGE↗

Extended investigation of sol aging effect on TiO2 electron transporting layer and performances of perovskite solar cells

Highlights: • Conditions of deposition of compact sol-gel TiO{sub 2} significantly influence the parameters of perovskite cells. • Sol aging originally considered as beneficial was proved to be adverse due to no repeatability, defects and residual water. • Free from such disadvantages TiO{sub 2} made from fresh sol can support as good cell parameters. • Roughness of transparent conductive oxide influences the optimal thickness of electron transporting layer. - Abstract: Organic−inorganic hybrid perovskites have created significant opportunities for low-cost and high-performance solar cells. The electron transporting layer (ETL) is one of the main components of the solar cell, which selectively transports electrons and at the same time acts as a barrier for holes. This paper focuses on the ETL composed of titanium dioxide deposited by sol-gel method. In particular, perovskite solar cells with ETL from aged titanium sol revealed significant differences of short circuit current which is 8% higher than their counterpart with ETL from fresh sol. Analysis of ETL morphology by atomic force microscopy combined with electrochemical impedance spectroscopy and optical properties measurements enabled to determine the source of this diversity. Additionally, the role of roughness of transparent electrode was indicated. The in-depth material analysis revealed some disadvantages of the ETL material, originally considered as supporting higher photovoltaic performance. The results indicated several problems associated with hardly controlled aging conditions, defects and presence of residual water, strongly advocate for TiO{sub 2} ETL form the fresh sol, which after optimization can guarantee the same good solar cell performance.

14 SOLAR ENERGY↗

A new model for estimating total body water from bioelectrical resistance

Estimation of total body water (T) from bioelectrical resistance (R) is commonly done by stepwise regression models with height squared over R, H(exp 2)/R, age, sex, and weight (W). Polynomials of H(exp 2)/R have not been included in these models. We examined the validity of a model with third order polynomials and W. Methods: T was measured with oxygen-18 labled water in 27 subjects. R at 50 kHz was obtained from electrodes placed on the hand and foot while subjects were in the supine position. A stepwise regression equation was developed with 13 subjects (age 31.5 plus or minus 6.2 years, T 38.2 plus or minus 6.6 L, W 65.2 plus or minus 12.0 kg). Correlations, standard error of estimates and mean differences were computed between T and estimated T's from the new (N) model and other models. Evaluations were completed with the remaining 14 subjects (age 32.4 plus or minus 6.3 years, T 40.3 plus or minus 8 L, W 70.2 plus or minus 12.3 kg) and two of its subgroups (high and low) Results: A regression equation was developed from the model. The only significant mean difference was between T and one of the earlier models. Conclusion: Third order polynomials in regression models may increase the accuracy of estimating total body water. Evaluating the model with a larger population is needed.

Siconolfi, S. F.↗

Polymer electrolyte fuel cell with vertical aligned carbon nanotubes as electrode catalyst support.

We successfully prepared membrane electrode assemblies (MEAs) for polymer electrolyte fuel cells using aligned carbon nanotubes (ACNTs) as the cathode catalyst support and evaluated their performances in single-cell tests. The ACNT-based MEAs demonstrated improved performance over a commercial carbon-black-based reference MEA in voltage-current polarization studies, particularly in the high current, mass-transport-limited region. The ACNT-MEAs also showed a significantly higher stability in conductivity and corrosion resistance than that of the reference during an accelerated aging test through potential cycling, which can be attributed to the vertical alignment and high graphiticity of the carbon nanotubes.

30 DIRECT ENERGY CONVERSION↗

Investigating the effects of proton exchange membrane fuel cell conditions on carbon supported platinum electrocatalyst composition and performance

Changes that carbon-supported platinum electrocatalysts undergo in a proton exchange membrane fuel cell environment were simulated by ex situ heat treatment of catalyst powder samples at 150 C and 100% relative humidity. In order to study modifications that are introduced to chemistry, morphology, and performance of electrocatalysts, XPS, HREELS and three-electrode rotating disk electrode experiments were performed. Before heat treatment, graphitic content varied by 20% among samples with different types of carbon supports, with distinct differences between bulk and surface compositions within each sample. Following the aging protocol, the bulk and surface chemistry of the samples were similar, with graphite content increasing or remaining constant and Pt-carbide decreasing for all samples. From the correlation of changes in chemical composition and losses in performance of the electrocatalysts, we conclude that relative distribution of Pt particles on graphitic and amorphous carbon is as important for electrocatalytic activity as the absolute amount of graphitic carbon present

08 HYDROGEN↗