OECD MCCI Project: Category 4 Integral Test to Validate Severe Accident Codes and Core-Concrete Interaction Test Six (CCI-6) (Rev. 2, Final Report)
Ex-vessel debris coolability is an important light water reactor (LWR) technical challenge. For existing plants, resolution of this challenge will confirm the technical basis for severe accident management guidelines (SAMGs). For new reactors, understanding this challenge will help confirm the effectiveness of the design and implementation of new accident mitigation features and severe accident management design alternatives (SAMDAs). The first OECD-MCCI program conducted reactor material experiments focused on achieving the following technical objectives: i) provide confirmatory evidence and data for various cooling mechanisms through separate effect tests for severe accident model development, and ii) provide long-term 2-D coreconcrete interaction data for code assessment and improvement. In addition to the experimental work, an analysis task was defined to develop and validate coolability models to form the basis for extrapolating the experiment findings to plant conditions. In response to the PRG mandate, a summary test plan for this sixth Core-Concrete Interaction (CCI-6) experiment was prepared, reviewed by the PRG, and subsequently approved for test conduct. The experiment approach was to incorporate an array of water nozzles into the core-concrete interaction test apparatus. The test section was enlarged to incorporate a 70 cm x 70 cm basemat. The initial melt depth was increased to 28 cm, which corresponds to a thermite charge mass of 900 kg. The melt depth is noted to be slightly less than the 30 cm level requested by the PRG. The thermite charge was redesigned to include a reduced amount of concrete decomposition products (i.e., 6 wt %) relative to the previously performed CCI tests. The concrete sidewalls allow for 24 cm of lateral erosion, and the sidewall design was modified to include refractory MgO with a UO 2 pellet and U 3 O 8 powder liner to stop the ablation if the 24 cm ablation depth was reached. The basemat and sidewalls also included an array of 45 concrete nozzles that were arranged on a 14 cm lateral pitch and were located at a uniform depth of 27.5 cm below the initial concrete basemat surface elevation. The nozzles were originally sealed at the top, and were fed with water from a common water supply tank that provided a static water head of nominally 10 kPa measured at the upper surface of the nozzles. The planned operating sequence was to ignite the thermite and then provide 210 kW Direct Electrical Heating (DEH) to simulate decay heat. The concrete would then heat up and begin erosion. At this point, the cavity would be flooded from the top. If the melt did not cool, then the core-concrete interaction would continue until the 27.5 cm axial ablation depth was reached. At this point, the nozzles would open by erosion and thus initiate cooling by bottom water injection. The test would continue to operate until the melt was quenched, or the maximum axial ablation depth of 32.5 cm was reached. The experiment would then be terminated. The CCI-6 experiment was carried out on 18 March 2010. The balance of this report documents the facility, actual test operating procedure, and results from this experiment.