Lubrication with sputtered MoS2 films
Friction experiments in ultrahigh vacuum to evaluate sputtered MoS2 film lubricants
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Friction experiments in ultrahigh vacuum to evaluate sputtered MoS2 film lubricants
Auger emission spectroscopy, low energy electron diffraction, sputtering studies, and adhesion and friction experiments on single crystals of Cu-Sn, Cu-Al, and Fe-Al alloys
Sputtered MoS2 films (2000-6500 A) were deposited on highly polished metal surfaces. These films have a low coefficient of friction (0.03-0.04) at speeds of 40-80 rpm and loads of 250-1000 grams. At loads of 250 grams the wear lives are over 0.5 million cycles, but at 1000 gram loads, it decreases to 38,000 cycles. Friction experiments and tensile tests have indicated that sputtered films have a strong adherence to metal surfaces. Electron transmission, diffraction and scanning electron microscopy show that these films have an extremely small particle size, less than 30 A in diameter, and are very dense and free from observable pinholes. The high kinetic energy of these sputtered species, the submicroscopic particle size and the sputter-etched substrate surface is responsible for strong adhesion and cohesion of the sputtered film.
Sputtered MoS2 films (2000-6500 A) were deposited on highly polished metal surfaces. These films have a low coefficient of friction (0.03-0.04) at speeds of 40-80 rpm and loads of 250-1000 grams. At loads of 250 grams, the wear lives are over 0.5 million cycles, but at 1000 gram loads, it decreases to 38,000 cycles. Friction experiments and tensile tests have indicated that sputtered films have a strong adherence to metal surfaces. Electron transmission, diffraction, and scanning electron microscopy show that these films have an extremely small particle size less than 30 A in diameter and are very dense and free from observable pinholes.
Sliding friction experiments were conducted with copper, nickel, iron, and cobalt sliding on themselves in air and argon. The resulting wear surfaces were examined with X-ray analysis to determine if surface texturing had occurred as a result of sliding. Results of the investigation indicate that, for the face-centered-cubic metals copper and nickel, a (111) texture develops with the (111) planes tilted 10 deg in the direction of sliding. The body-centered-cubic metal iron exhibited a (110) texture with the (100) direction oriented in the direction of sliding. It also exhibited a 10 deg tilt in the direction of sliding. The environment influenced the results in that the degree of texture observed in argon was less than that seen in air for iron. No texturing was observed for the close-packed-hexagonal metal cobalt. Recrystallization was observed with copper as a result of sliding.
The interaction of sulfur and oxygen with an iron surface was studied with Auger spectroscopy analysis both statically and during sliding-friction experiments in a vacuum environment. Oxygen, hydrogen sulfide, methyl mercaptan, and sulfur dioxide were adsorbed to an iron surface. Results indicate that sulfide films formed on clean iron surfaces are completely displaced by oxygen. Hydrocarbons containing sulfur, such as methyl mercaptan, adsorb dissociatively. Less sulfur is adsorbed during sliding with hydrogen sulfide and methyl mercaptan than in the absence of sliding. With both oxygen and sulfur dioxide, sliding did not affect the amount of material adsorbed to iron.
Friction experiments were conducted in air with polytetrafluoroethylene (PTFE) sliding on aluminum single crystals. Mechanical scoring of the crystals with (110) and (100) orientations was observed with a single pass of the PTFE slider. No scoring was observed on the (111). The degree of scoring of the crystals is related to the hardness, with the hardest surface (111) showing no damage and the softest surface (110) showing the most severe scoring. Scoring is caused by work-hardened pieces of aluminum which, as a consequence of the adhesion between PTFE and aluminum, were pulled out of the bulk and became embedded in the PTFE polymer.
An iron surface was exposed to the extreme-pressure type lubricant benzyl chloride, dichlorophenyl phosphine, dichlorophenyl phosphine sulfide, ophenyl phosphine oxide. Iron, in the sputter-cleaned state, was exposed to these materials statically and during dynamic friction experiments. With benzyl chloride only chlorine adsorbed to the surface, and with dichlorophenyl phosphine no adsorption occurred, while the addition of sulfur to that same molecular structure resulted in the promotion of carbon and chlorine adsorption. substitution of oxygen for sulfur in the dichlorobenzyl phosphine molecule resulted in carbon, chlorine, and oxygen adsorption. With none of the phosphorus containing molecules was phosphorus detected on the surface. Sliding in an atmosphere of benzyl chloride promoted adsorption of chlorine to the iron surface. Increases in load resulted in a decrease in the surface concentration of iron chloride.
An investigation was conducted to determine the nature of the chemical interactions of oxygen and sulfur with iron when surfaces are stationary and also during sliding in a vacuum environment. Various gases that contained sulfur, oxygen, or both were adsorbed to iron at 23 C. The gases included oxygen, hydrogen sulfide, methyl mercaptan, and sulfur dioxide. Friction experiments were conducted with a hemispherical rider sliding on a rotating disk. An Auger cylindrical mirror analyzer was used to monitor the iron surface chemistry. The results of this study indicate that oxygen will completely displace sulfide films from iron surfaces. Organic thiols containing sulfur, such as methyl mercaptan, adsorb to an iron surface dissociatively. Only sulfur is detected on the iron surface. Sliding inhibits the formation of sulfide films on iron with the adsorption of hydrogen sulfide and methyl mercaptan. With oxygen and sulfur dioxide, the sliding process does not affect adsorption behavior.
Sliding friction experiments were conducted with copper, nickel, iron and cobalt sliding on themselves in air and argon. The resulting wear surfaces were examined by X-ray analysis to determine if surface texturing had occurred as a result of sliding. Results of the investigation indicate that, for the face-centered-cubic metals copper and nickel, a (111) texture develops with the (111) planes tilted 10 deg in the direction of sliding. The body-centered-cubic metal iron exhibited a (110) texture with the (111) direction oriented in the direction of sliding. It also exhibited a 10 deg tilt in the direction of sliding. The environment influenced the results in that the degree of texture observed in argon was less than that seen in air for iron. No texturing was observed for the close-packed-hexagonal metal cobalt. Recrystallization was observed with copper as a result of sliding.
Sliding friction experiments were conducted with molybdenum disulfide single crystals in contact with sputter cleaned surfaces of copper, nickel, gold, and 304 stainless steel. Transfer of the molybdenum disulfide to the metals was monitored with Auger electron spectroscopy. Results of the investigation indicate molybdenum disulfide transfers to all clean metal surfaces after a single pass over the metal surface with film thickness observed to increase with repeated passes over the same surfaces. Large particle transfer occurs when the orientation of the crystallites is other than basal. This is frequently accompanied by abrasion of the metal. Adhesion of molybdenum disulfide films occurred readily to copper and nickel, less readily to 304 stainless steel, and even less effectively to the gold, which indicates a chemical effect.
Sliding friction experiments were conducted in vacuum with single crystal silicon carbide (0001) surface in contact with transition metals (tungsten, iron, rhodium, nickel, titanium, and cobalt), copper, and aluminum. The hexagon shaped cracking and fracturing of silicon carbide that occurred is believed to be due to cleavages of both the prismatic and basal planes. The silicon carbide wear debris, which was produced by brittle fracture, slides or rolls on both the metal and silicon carbide and produces grooves and indentations on these surfaces. The wear scars of aluminum and titanium, which have much stronger chemical affinity for silicon and carbon, are generally rougher than those of the other metals. Fracturing and cracking along the grain boundary of rhodium and tungsten were observed. These may be primarily due to the greater shear moduli of the metals.
Sliding friction experiments were conducted in a vacuum with binary-copper alloy riders sliding against a conventional bearing-steel surface with normal residual oxides present. The binary alloys contained 1 atomic percent of various alloying elements. Auger spectroscopy analysis was used to monitor the adhesive transfer of the copper alloys to the bearing-steel surface. A relation was found to exist between adhesive transfer and the reaction potential and free energy of formation of the alloying element in the copper. The more chemically active the element and the more stable its oxide, the greater was the adhesive transfer and wear of the copper alloy. Transfer occurred in all the alloys except copper-gold after relatively few (25) passes across the steel surface.
Sliding friction experiments were conducted with aluminum and other riders rubbing on disks of various elemental metals in the presence of a thin film of zinc dialkyldithiophosphate (ZDP). Auger emission spectroscopy was used to in situ monitor the changes in surface chemistry with rubbing under various loads. The metal disks examined included iron, titanium, rhodium, tungsten, molybdenum, and copper. For equivalent films of ZDP the film is a more effective lubricant for some metals than it is for others. The important active element in the compound varies with the metal lubricated and is a function of metal chemistry. The zinc in the ZDP is susceptible to electron beam induced desorption.
Sliding friction experiments, conducted in vacuum with silicon carbide /000/ surface in contact with iron based binary alloys are described. Multiangular and spherical wear particles of silicon carbide are observed as a result of multipass sliding. The multiangular particles are produced by primary and secondary cracking of cleavage planes /000/, /10(-1)0/, and /11(-2)0/ under the Hertzian stress field or local inelastic deformation zone. The spherical particles may be produced by two mechanisms: (1) a penny shaped fracture along the circular stress trajectories under the local inelastic deformation zone, and (2) attrition of wear particles.
Sliding friction experiments were performed in vacuum at room temperature on a plane-type SiC surface in contact with iron-based binary alloys. Multiangular and spherical wear particles were found to form as a result of multipass sliding. The multiangular particles were produced by primary and secondary cracking of the 0001, 10(-)10, and 11(-)20 plane-type cleavage planes under the Hertzian stress field or local inelastic deformation zone. When alloy surfaces are in contact with silicon carbide under a load of 0.2 N, the alloy around the contact area is subjected to stresses that are close to the elastic limit in the elastic deformation region and/or exceed it. It was also found that spherical wear particles may be produced by two mechanisms: a penny-shaped fracture along the circular stress trajectories under the local inelastic deformation zone, and the attrition and fatigue of wear particles.
A model of crustal deformation during the interseismic phase is developed and applied (using the improved Bayesian inversion algorithm described by Jackson and Matsu'ura, 1985) to trilateration data for the USGS Hollister (CA) network. In the model, rigid blocks in motion relative to each other experience friction only in a brittle upper zone, while their ductile lower zones slide freely; the Hollister model comprises five blocks and nine rectangular fault patches. The data and results are presented in tables, graphs, and maps and characterized in detail. The model predicts steady block motion on time scales between 10 yr and 1 Myr, with net motion across the San Andreas/Calaveras fault system 38 + or - 3 mm/yr and brittle/ductile transition depths ranging from 0.4 to 11 km. Two San Andreas segments with higher probabilities of moderate-to-large earthquakes are identified.
This work presents the results of the X-Ray Photoelectron Spectroscopy (XPS) analysis of AISI 440C ball surfaces lubricated with perfluoropolyether (PFPE) oils after friction experiments under sliding conditions at high load in air and vacuum environments. The PFPE lubricants tested were Demnum S100, Fomblin Z-25, and Krytox 143AB. It was found that all the PFPE lubricants were degraded by sliding contact causing the formation of inorganic fluorides on the metallic surfaces and a layer of organic decomposition products. KRYTOX 143AB was the least reactive of the three lubricants tested. It was also found that metal fluoride formed at off-scar areas. This suggests the formation of reactive species, such as COF2 or R(sub f)COF, during sliding experiments, which can diffuse through the lubricant film and react with the metallic surfaces away from the contact region. Comparison of reference specimens before sliding with those that had undergone the sliding tests showed that the amount of non-degraded PFPE remaining on the surface of the balls after the sliding experiments was greater than that of the balls without sliding.