Search NASA⌕ Search

SEARCH · Search NASA

Results for “interface stability”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Fundamental Understanding of “Fresh” Lithium Nucleation and Growth in Sulfide-Based Anode-Free Solid-State Batteries: Effects of Substrate, Current Density, and Li + Supply

Understanding the electrochemical extraction and deposition of lithium (Li) from cathode is crucial for advancing anode-free solid-state batteries (AFSSBs). Herein, cryo-transmission electron microscopy (cryo-TEM) and electrochemical studies are employed to investigate how current collector surface properties, current densities, and cathode loadings influence the morphology of fresh electrochemically deposited Li and the electrochemical performance in sulfide-based AFSSBs. Cryo-TEM reveals that Cu current collectors induce irregular, dendritic Li deposits due to their lithiophobic nature and reactivity with Li 5.4 PS 4.4 Cl 1.6 (LPSC), while Ni and Au facilitate more uniform, planar-like Li growth. The morphology of the deposited Li also depends on current density: higher rates produce smaller, porous particles versus larger, denser deposits at lower rates. Importantly, for the first time, we discovered that low cathode loadings lead to poor cycling stability due to insufficient Li + supply for complete anode coverage, contrary to conventional solid-state batteries with preloaded Li metal anodes. This finding establishes a design principle where adequate cathode Li + reservoirs are essential for anode interface stability in AFSSBs. Overall, this work elucidates the interplayed effect of current collectors, current densities, and cathode loadings on Li morphology and cycle stability, offering fundamental insights into cathode-derived Li behavior and practical guidelines for optimizing AFSSBs performance through nucleation control and interface engineering.

25 ENERGY STORAGE↗

Small Fatigue Crack Growth Mechanisms and Interfacial Stability in Cold-Spray 6061 Aluminum Alloys and Coatings

Cold-spray-processed aluminum alloys have static mechanical properties superior to those of aerospace cast alloys, and similar to those of their wrought counterparts, making them good candidates for structural applications. However, their broad and confident use relies upon systematic fatigue crack growth studies to investigate and demonstrate the materials' performance in critical high-integrity components. In this work, the fatigue crack growth behavior in early stages (small crack growth regime) was investigated for cold-spray processed 6061 aluminum alloys and coatings, at stress ratio R = 0.1, in room temperature laboratory air. The effects of the characteristic microstructure and initial flaw size on the fatigue crack growth response were systematically examined, and the crack growth mechanisms at the microstructural scale were established and compared to those of long cracks. The mechanical interfacial stability of coatings was examined in cold-spray 6061-rolled 6061-T6 couples. An original method of quantifying the deposition-substrate interfacial strength, and correlating it to the response under cyclic loading via crack-interface stability maps, was developed. The proposed methodology is based on combined scratch testing and fracture mechanics formulations, and failure at the coating-substrate interface can be predicted for any crack growth scenario under cyclic loading. The method can be broadly used for the design and optimization of cold-spray and other coatings, as well as in structural repair.

36 MATERIALS SCIENCE↗

Strain-induced phase and oxygen-vacancy stability in ionic interfaces from first-principles calculations

Understanding interfacial chemistry is becoming crucial in materials design for heterointerfaces. Using density functional theory, we elucidate the effect of strained interfaces on phase and oxygen-vacancy stability for CeO2 | ZrO2, ThO2 | ZrO2 and CeO2 | ThO2 interfaces. The calculations show that ZrO2 transforms from cubic fluorite to the orthorhombic columbite under tensile strain providing evidence of a previous experimental speculation of an unrecognized ZrO2 phase. We also show that oxygen vacancies could be preferably stabilized on either side of the interface by manipulating strain. We predict that they are stable in tensile-strain, and unstable in compressivestrained materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Temperature dependent interfacial microstructure in HIP-bonded Al6061/Zr joints

Pressing (HIP) at 450 °C and 560 °C under 103 MPa for 90 minutes to evaluate interfacial diffusion and microstructural evolution. Sound metallurgical bonding was achieved at both temperatures, with Zr serving as an effective diffusion barrier. Microstructural analysis revealed the the formation of a (Al,Si)3Zr intermetallic layer at the Al/Zr interface, whose thickness increased from ~100 nm at 450 °C to ~2100 nm at 560 °C, consistent with temperature-driven diffusion kinetics. The thin and continuous reaction layer observed at 450 °C indicates controlled interdiffusion and minimal reaction zone growth, favorable for maintaining interface stability and ductility. At 560 °C, enhanced atomic mobility led to pronounced intermetallic development, confirming diffusion-controlled growth behavior. These results provide valuable insights for optimizing Al/Zr interface design and diffusion barrier performance in advanced structural and energy systems.

Al/Zr interface↗

Inertial dynamics of an interface with interfacial mass flux: Stability and flow fields’ structure, inertial stabilization mechanism, degeneracy of Landau’s solution, effect of energy fluctuations, and chemistry-induced instabilities

This work focuses on the long-standing problem of inertial dynamics of an interface with interfacial mass flux and reports new mechanisms for the interface stabilization and destabilization. The interface is a phase boundary separating fluids of different densities and having interfacial mass flux. To analyze the interface dynamics from a far field, we develop and apply the general matrix method to rigorously solve the boundary value problem involving the governing equations in the fluid bulk and the boundary conditions at the interface and at the outside boundaries of the domain. We find the fundamental solutions for the linearized system of equations and analyze the interplay of interface stability with flow fields’ structure by directly linking rigorous mathematical attributes to physical observables. We find that the interface is stable when the dynamics conserves the fluxes of mass, momentum, and energy; the stabilization is due to an inertial mechanism causing small oscillations of the interface velocity. In the classic Landau’s dynamics, the postulate of perfect constancy of the interface velocity leads to the development of Landau–Darrieus instability. This destabilization is also linked to the imbalance of the perturbed energy at the interface. The classic Landau’s solution is found to have degeneracy; lifting of the degeneracy may lead to singularity and self-similar dynamics. Our results compare well with traditional theories of combustion and propose new experiments to study the dynamics of the interface and the flow fields in combustible systems. We further conduct reactive molecular dynamics simulations to elucidate the complexity of chemical processes, to study the destabilizing effect of energy fluctuations on the interface stability, and to illustrate the chemistry-induced instabilities. In summary, we identify the extreme sensitivity of the interface dynamics to the interfacial boundary conditions, including the formal properties of fundamental solutions and the qualitative and quantitative properties of the flow fields. This provides new opportunities for studies, diagnostics, and control of multiphase flows in a broad range of processes in nature and technology.

42 ENGINEERING↗

Ionic Conductive and Highly-Stable Interface for Alkali Metal Anodes

Alkali metals are regarded as the most promising candidates for advanced anode for the next-generation batteries due to their high specific capacity, low electrochemical potential, and lightweight. However, critical problems of the alkali metal anodes, especially dendrite formation and interface stabilization, remain challenging to overcome. The solid electrolyte interphase (SEI) is a key factor affecting Li and Na deposition behavior and electrochemical performances. Herein, a facile and universal approach is successfully developed to fabricate ionic conductive interfaces for Li and Na metal anodes by modified atomic layer deposition (ALD). In this process, the Li metal (or Na metal) plays the role of Li (or Na) source without any additional Li (or Na) precursor during ALD. Moreover, the key questions about the influence of ALD deposition temperature on the compositions and structure of the coatings are addressed. The optimized ionic conductive coatings have significantly improved the electrochemical performances. In addition, the electrochemical phase-field model is performed to prove that the ionic conductive coating is very effective in promoting uniform electrodeposition. Further, this approach is universal and can be potentially applied to other different metal anodes. At the same time, it can be extended to other types of coatings or other deposition techniques.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Long–Cycling Sulfide–Based All–Solid–State Batteries Enabled by Electrochemo–Mechanically Stable Electrodes

Anode significantly determines the energy density of all-solid-state Lithium batteries (ASLBs). Silicon (Si) and Lithium (Li) metal are two of the most attractive anodes because of their ultrahigh theoretical capacities. However, most investigations focus on Li metal; the great potential of Si is underrated. This study investigates Si anode's stability, processability, and cost in ASLBs and compares them with Li metal. Moreover, the single-crystal LiNi 0.8 Co 0.1 Mn 0.1 O 2 is stabilized with a lithium silicate (Li 2 SiO x ) through a scalable sol-gel method. ASLBs with a cell-level energy density of 285 Wh kg -1 are obtained through sandwiching Si anode, thin sulfide solid-state electrolyte membrane, and interface stabilized LiNi 0.8 Co 0.1 Mn 0.1 O 2 . The full cell delivered a high capacity of 145 mAh g -1 at C/3 and maintained stability for 1000 cycles. This work inspires commercializing the ASLBs on a large scale with exciting manufacturing lines for large-scale, safe, and economical energy storage.

25 ENERGY STORAGE↗

Accurately constituting robust interfaces for high-performance high-energy lithium metal batteries

High-energy lithium metal batteries (LMBs) have received ever-increasing interest. Among them, coupling lithium metal (Li) with nickel-rich material, LiNi x Mn y Co z O 2 (NMCs, x ≥ 0.6, x + y + z = 1), is promising because Li anodes enable an extremely high capacity (∼3860 mA h g −1 ) and the lowest redox potential (−3.04 V vs. standard hydrogen electrode), while NMCs can achieve a much higher capacity of ∼200 mA h g −1 and lower cost than those of LiCoO 2 . However, the resultant Li‖NMC cells have been hindered from commercialization due to a series of challenges related to the interface stability of both Li anodes and NMC cathodes. Specifically, Li anodes suffer from Li dendritic growth and the formation of solid electrolyte interphase (SEI), while NMC cathodes suffer from the formation of cathode electrolyte interphase (CEI) and other interface-related issues, including transition metal dissolution, oxygen release, cracking, and so on. To tackle these issues, recently, two sister techniques, atomic and molecular layer deposition (ALD and MLD), have emerged and exhibit tremendous capabilities to accurately constitute robust interfaces to achieve high-performance Li‖NMC LMBs. They can uniquely develop uniform and conformal films as surface coatings of LMBs in a precisely controllable mode at the atomic/molecular level, while proceeding with film deposition at low temperatures (e.g., ≤250 °C). In this Feature Article, we review the latest research progress in developing novel surface coatings via ALD and MLD for Li‖NMC LMBs and discuss outcomes for pursuing high performance.

25 ENERGY STORAGE↗

In Situ Monitoring the Nucleation and Growth of Nanoscale CaCO 3 at the Oil–Water Interface

Interfaces can actively control the nucleation kinetics, orientations, and polymorphs of calcium carbonate (CaCO 3 ). Prior studies have revealed that CaCO 3 formation can be affected by the interplay between chemical functional moieties on solid–liquid or air–liquid interfaces as well as CaCO 3 ’s precursors and facets. Yet little is known about the roles of a liquid–liquid interface, specifically an oil–liquid interface, in directing CaCO 3 mineralization which are common in natural and engineered systems. Here, in this study, by using in situ X-ray scattering techniques to locate a meniscus formed between water and a representative oil, isooctane, we successfully monitored CaCO 3 formation at the pliable isooctane–water interface and systematically investigated the pivotal roles of the interface in the formation of CaCO 3 (i.e., particle size, its spatial distribution with respect to the interface, and its mineral phase). Different from bulk solution, ∼5 nm CaCO 3 nanoparticles form at the isooctane–water interface. They stably exist for a long time (36 h), which can result from interface-stabilized dehydrated prenucleation clusters of CaCO 3 . There is a clear tendency for enhanced amounts and faster crystallization of CaCO 3 at locations closer to isooctane, which is attributed to a higher pH and an easier dehydration environment created by the interface and oil. Our study provides insights into CaCO 3 nucleation at an oil–water interface, which can deepen our understanding of pliable interfaces interacting with CaCO 3 and benefit mineral scaling control during energy-related subsurface operation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Functionalization of Cathode–Electrolyte Interface with Ionic Liquids for High-Performance Quasi-Solid-State Lithium–Sulfur Batteries: A Low-Sulfur Loading Study

We introduce a quasi-solid-state electrolyte lithium-sulfur (Li–S) battery (QSSEB) based on a novel Li-argyrodite solid-state electrolyte (SSE), Super P–Sulfur cathode, and Li-anode. The cathode was prepared using a water-based carboxymethyl cellulose (CMC) solution and styrene butadiene rubber (SBR) as the binder while Li6PS5F0.5Cl0.5 SSE was synthesized using a solvent-based process, via the introduction of LiF into the argyrodite crystal structure, which enhances both the ionic conductivity and interface-stabilizing properties of the SSE. Ionic liquids (IL) were prepared using lithium bis(trifluoromethyl sulfonyl)imide (LiTFSI) as the salt, with pre-mixed pyrrolidinium bis(trifluoromethyl sulfonyl)imide (PYR) as solvent and 1,3-dioxolane (DOL) as diluent, and they were used to wet the SSE–electrode interfaces. The effect of IL dilution, the co-solvent amount, the LiTFSI concentration, the C rate at which the batteries are tested and the effect of the introduction of SSE in the cathode, were systematically studied and optimized to develop a QSSEB with higher capacity retention and cyclability. Interfacial reactions occurring at the cathode–SSE interface during cycling were also investigated using electrochemical impedance spectroscopy, cyclic voltammetry, and X-ray photoelectron spectroscopy supported by ab initio molecular dynamics simulations. This work offers a new insight into the intimate interfacial contacts between the SSE and carbon–sulfur cathodes, which are critical for improving the electrochemical performance of quasi-solid-state lithium–sulfur batteries.

25 ENERGY STORAGE↗

Structural Basis for Autoregulation of the Zinc Transporter YiiP

Zinc transporters have crucial roles in cellular zinc homeostatic control. The 2.9-A resolution structure of the zinc transporter YiiP from Escherichia coli reveals a richly charged dimer interface stabilized by zinc binding. Site-directed fluorescence resonance energy transfer (FRET) measurements and mutation-activity analysis suggest that zinc binding triggers hinge movements of two electrically repulsive cytoplasmic domains pivoting around four salt bridges situated at the juncture of the cytoplasmic and transmembrane domains. These highly conserved salt bridges interlock transmembrane helices at the dimer interface, where they are well positioned to transmit zinc-induced interdomain movements to reorient transmembrane helices, thereby modulating coordination geometry of the active site for zinc transport. The cytoplasmic domain of YiiP is a structural mimic of metal-trafficking proteins and the metal-binding domains of metal-transporting P-type ATPases. The use of this common structural module to regulate metal coordination chemistry may enable a tunable transport activity in response to cytoplasmic metal fluctuations.

59 BASIC BIOLOGICAL SCIENCES↗

Optimizing $\mathrm{ACRT}$ to reduce inclusion formation during the $\mathrm{VGF}$ growth of cadmium zinc telluride: I. Computational approach

Theoretical computations reveal insight into parameters that govern the accelerated crucible rotation technique (ACRT) applied to the gradient freeze (VGF) growth of cadmium zinc telluride (CZT). A metric based on the classic Mullins and Sekerka instability criterion is put forth that provides a quantitative means of assessing the impact of different ACRT rotation schedules on morphological stability and inclusion formation during CZT growth. Here this metric is employed in a 2-k factorial design of experiments that identifies the maximum rotation rate as the most important ACRT parameter, followed by the acceleration period and the rest period. Subsequent optimization of rotation schedule is performed for a specific VGF growth system, and mechanistic explanations are provided for the preferred ACRT schedule, which improves interface stability via slower rotation rates and longer acceleration periods than would be applied using classical ACRT schedules.

36 MATERIALS SCIENCE↗

Stabilizing Cathode–Electrolyte Interphase of Nickel-Rich Single-Crystal Cathodes for Lithium-Ion Batteries

Nickel-rich single-crystal (SC) layered oxides are promising cathode candidates for next-generation lithium-ion batteries (LIBs) owing to their high energy density and structural robustness against intergranular cracking. However, their intrinsic surface reactivity with liquid electrolytes accelerates parasitic reactions at the cathode–electrolyte interphase (CEI), leading to transition-metal dissolution, gas generation, and impedance buildup. In this work, we synthesized SC-Li x Ni 0.9 Mn 0.05 Co 0.05 O 2 (NMC9055, 1 ≤ x ≤ 1.2) using a eutectic-assisted method and investigated interface stabilization strategies. A nickel-deficient Li x Ni 0.6 Mn 0.2 Co 0.2 O 2 (NMC622, 1 ≤ x ≤ 1.2) coating was applied via evaporation-based deposition to suppress CEI degradation pathways. Structural and compositional analyses confirmed uniform shell formation and preserved particle integrity. Half-cell electrochemical testing against lithium metal revealed ∼10% higher capacity retention and improved reversibility compared with pristine SC NMC9055, particularly under high-voltage operation. In conclusion, these results highlight the critical role of controlled surface chemistry in mitigating CEI instability in nickel-rich SC cathodes, offering a pathway toward enabling durable high-energy LIBs.

Coating processes↗

Thermal stability of 3D interface Cu/Nb nanolaminates

Nanocrystalline alloys are promising structural materials yet lack thermal stability in many cases. Recent work shows that interface structure has an outsize effect on the thermal behavior of nanostructured alloys. Here, this work focuses on the role of controlled heterophase interface structure in the thermal evolution of model Cu/Nb nanolaminates. We introduce 3D interfaces containing nanoscale heterogeneities in all spatial dimensions between Cu and Nb, forming 3D Cu/Nb. TEM, nanoindentation, and DSC are used in tandem to establish thermal stability and to identify shifts in microstructure as a function of static annealing temperature. 3D interfaces are shown to survive annealing to 300 °C for 1 hr., while 3D Cu/Nb microstructure evolves to form low-density and voided regions correlating to the onset of layer pinch-off between 500 and 600 °C annealing temperatures. A diffusivity- and vacancy energetics-based mechanism is developed to explain void formation driven by 3D interface degradation at elevated temperature.

3D interfaces↗

An electrochemically stable homogeneous glassy electrolyte formed at room temperature for all-solid-state sodium batteries

All-solid-state sodium batteries (ASSSBs) are promising candidates for grid-scale energy storage. However, there are no commercialized ASSSBs yet, in part due to the lack of a low-cost, simple-to-fabricate solid electrolyte (SE) with electrochemical stability towards Na metal. In this work, we report a family of oxysulfide glass SEs (Na 3 PS 4-x O x , where 0 < x ≤ 60) that not only exhibit the highest critical current density among all Na-ion conducting sulfide-based SEs, but also enable high-performance ambient-temperature sodium-sulfur batteries. By forming bridging oxygen units, the Na 3 PS 4-x Ox SEs undergo pressure-induced sintering at room temperature, resulting in a fully homogeneous glass structure with robust mechanical properties. Furthermore, the self-passivating solid electrolyte interphase at the Na|SE interface is critical for interface stabilization and reversible Na plating and stripping. The new structural and compositional design strategies presented here provide a new paradigm in the development of safe, low-cost, energy-dense, and long-lifetime ASSSBs.

25 ENERGY STORAGE↗

A Cross‐Linked Flexible Metaferroelectrolyte Regulated by 2D/2D Perovskite Heterostructures for High‐Performance Compact Solid‐State Sodium Batteries

Abstract To address the issues of limited ionic conductivity and poor interface stability at room and low temperatures in solid‐state electrolytes, a robust intrinsic ferroelectrolyte or nanoferroelectrolyte strategy for engineering solid‐state flexible ferroelectric composite electrolytes utilizing strongly coupled intrinsic ion conducting 2D/2D sodium‐rich anti‐perovskite (NaRAP)/ferroelectric perovskite heterostructures is introduced. Herein, highly scalable PVDF‐based metaferroelectrolytes with Na 2.99 Ba 0.005 OCl/Ca 2 Na 2 Nb 5 O 16 − (CNNO − ) nanosheets into a ferroelectric poly(vinylidene fluoride‐co‐hexafluoropropylene) (PVDF‐HFP) matrix, through an in situ cross‐linking and spontaneous bridging method, for compact solid‐state sodium batteries (SSBs), are reported. Benefiting from unique well‐dispersed 3D ferroelectric coupled network and the Na 2.99 Ba 0.005 OCl/CNNO − ‐induced PVDF‐HFP ferroelectric β phase, the Na + flux is regulated, thereby inhibiting Na dendrite growth at the interface. Notably, the optimized PH‐5% NC metaferroelectrolyte exhibits rapid ion transport (1.11 × 10 −4 S cm −1 at 25 °C), a wide electrochemical window (> 4.8V), superior conformal mechanical compatibility, improved flexibility, good elasticity and flame retardancy. The solid‐state Na 3 V 2 (PO 4 ) 3 /PH‐5% NC/Na batteries present a stable cycling performance (remaining 56.4 mAh g −1 after 500 cycles at 1 C) even at 0 °C, potential for cost‐effective, safe, stable and compact SSB energy storage over 600 Wh L −1 , vastly surpassing 365 Wh L −1 of the current commercial sodium‐ion liquid‐electrolyte batteries.

Chemistry↗

In-situ TEM observation of hcp-Ti to fcc-Ti phase transformation in Nb-Ti-Si based alloys

Highlights: • Hcp-Ti to fcc-Ti phase transformation has been investigated by direct TEM observation. • Two periodic structures nucleate and act as modulated structures during the hcp-Ti to fcc-Ti phase transformation. • The transformation proceeds through formation of growth ledges at interfaces. • Stability of Ti might be decreased in the following order: hcp, periodic structures, fcc. - Abstract: Phase transformation process of interfacial Ti precipitates in Nb-Ti-Si based alloys is systematically investigated by in-situ transmission electron microscopy (TEM) observation. The Ti precipitates exhibit an uncommon face-centered cubic (fcc) structure, which can be identified by analyzing its chemical composition and phase transformation characteristics. Fcc-Ti precipitates precipitate from Nbss and partially transform into hexagonal close-packed Ti (hcp-Ti) lamellae during heat-treatment, which will reversely transform into fcc-Ti lamellae during heating in TEM. Two periodic structures nucleate and act as modulated structures in the process of hcp-Ti to fcc-Ti reverse phase transformation. The transformation proceeds through formation of growth ledges at interfaces. Origins of the two periodic structures and ledge model for the phase transformation have been discussed.

36 MATERIALS SCIENCE↗

Radiation Stability of Mixed Tin-Lead Halide Perovskites: Implications for Space Applications

Mixed organic-inorganic halide perovskite solar cells (PSCs) have received considerable attention in recent years for their impressive solar to electrical power efficiency gains and potentially lower material and processing costs for optoelectronic applications. In addition to terrestrial applications, PSCs are of interest to the space power markets for their low cost, low weight, adaptability to flexible architectures, and tolerance to high energy particle irradiation (mainly protons and electrons). Here we investigate the properties of mixed formamidinium-methylammonium tin-lead iodide (FASn)0.6(MAPb)0.4I3 perovskites which lower the lead content as well as the bandgap, making them attractive for the low bandgap absorber material in tandem PSCs. Through current density-voltage (JV) characterization at lower temperatures, majority carrier transport is hindered and a barrier to photogenerated carrier extraction is evident. This is attributed to the thermally induced change of the bandgap of the absorber layer relative to the energy selective contacts in the device. We find that although the architecture used here hinders the performance at temperatures below 225 K, the tolerance to high energy (3.7 MeV) protons is impressive, considerably out-performing commercially available thin-film CIGS. These results suggest further improvements to structural and interface stability as well as lightweight encapsulation could lead to all perovskite flexible tandem arrays deployed for power generation on missions to low Earth orbit, the moon, Mars, and beyond.

perovskite solar cells↗