Optical transparency of LiF (100) shock compressed to ∼360 GPa

High-purity [100] lithium fluoride (LiF) is the most widely used optical window in dynamic compression experiments due to its wide bandgap and well-characterized mechanical response. Recent plate-impact experiments established the [100] LiF Hugoniot to ∼230 GPa and demonstrated shock-induced melting onset at 182 GPa with complete melting by 195 GPa; theoretical models predict LiF optical transparency to nearly 900 GPa. To experimentally examine the optical transparency of [100] LiF at higher pressures and in the liquid state, laser-driven shock experiments were performed at peak stresses ranging from 223 to 363 GPa. Optical response was examined by measuring the particle velocity histories at the Kapton/LiF interface using laser interferometry at 532 and 1550 nm wavelengths; in-material particle velocities were obtained using established refractive-index corrections. Continuous photonic Doppler velocimetry fringes were observed across the entire stress range, demonstrating that LiF remains transparent to 1550 nm light throughout the multi-megabar regime investigated. At 532 nm, fringe visibility depended on the reflector coating: aluminum mirrors provided signals to ∼235 GPa, while gold mirrors extended this limit to 270.5 GPa, indicating that the shorter-wavelength response is likely sensitive to experimental configuration rather than to the loss of LiF transparency. Continued optical transparency to at least 360 GPa indicates that shock-melted LiF does not display bandgap closure over the stress range explored. Furthermore, these results provide direct experimental constraints on the high-pressure optical response and establish LiF (100) as a robust optical window material for laser-driven dynamic compression experiments approaching 400 GPa.

Renganathan, P. [Argonne National Laboratory (ANL)

Hydrogen Production and Li-Ion Battery Performance with MoS2-SiNWs-SWNTs@ZnONPs Nanocomposites

This study explores the hydrogen generation potential via water-splitting reactions under UV-vis radiation by using a synergistic assembly of ZnO nanoparticles integrated with MoS2, single-walled carbon nanotubes (SWNTs), and crystalline silicon nanowires (SiNWs) to create the MoS2-SiNWs-SWNTs@ZnONPs nanocomposites. A comparative analysis of MoS2 synthesized through chemical and physical exfoliation methods revealed that the chemically exfoliated MoS2 exhibited superior performance, thereby being selected for all subsequent measurements. The nanostructured materials demonstrated exceptional surface characteristics, with specific surface areas exceeding 300 m2 g−1. Notably, the hydrogen production rate achieved by a composite comprising 5% MoS2, 1.7% SiNWs, and 13.3% SWNTs at an 80% ZnONPs base was approximately 3909 µmol h−1g−1 under 500 nm wavelength radiation, marking a significant improvement of over 40-fold relative to pristine ZnONPs. This enhancement underscores the remarkable photocatalytic efficiency of the composites, maintaining high hydrogen production rates above 1500 µmol h−1g−1 even under radiation wavelengths exceeding 600 nm. Furthermore, the potential of these composites for energy storage and conversion applications, specifically within rechargeable lithium-ion batteries, was investigated. Composites, similar to those utilized for hydrogen production but excluding ZnONPs to address its limited theoretical capacity and electrical conductivity, were developed. The focus was on utilizing MoS2, SiNWs, and SWNTs as anode materials for Li-ion batteries. This strategic combination significantly improved the electronic conductivity and mechanical stability of the composite. Specifically, the composite with 56% MoS2, 24% SiNWs, and 20% SWNTs offered remarkable cyclic performance with high specific capacity values, achieving a complete stability of 1000 mA h g−1 after 100 cycles at 1 A g−1. These results illuminate the dual utility of the composites, not only as innovative catalysts for hydrogen production but also as advanced materials for energy storage technologies, showcasing their potential in contributing to sustainable energy solutions.

Chemistry

Universal Relationship between Limiting Current and Electrochemical Transport Properties in Malonate-Based Polymer Electrolytes

There is considerable interest in developing high-performance electrolytes for rechargeable lithium batteries. For practical applications, the electrolyte must support large dc currents. However, the parameters most often reported in the literature, conductivity, κ, and current fraction, ρ + , reflect ion transport in the limit of infinitesimal currents. In this limit, the efficacy of an electrolyte is given by the product κρ + . The limiting current density, i lim , is the maximum current density that can be applied across an electrolyte; the cell voltage diverges if the applied current density exceeds ilim. This parameter reflects ion transport in the limit of large dc currents and is therefore of practical interest. It would therefore be convenient if i lim could be predicted from measurements of κρ + . In order to explore this possibility, we studied six malonate-based polymers and PEO at a fixed salt concentration (r = 0.08) and temperature (90°C) using symmetric cells with planar electrodes. Unfortunately, there is no correlation between ilim and κρ + . When the applied current density, i, is less than ilim, the cell voltage approaches a stable plateau, ϕ plateau . Here, we found a linear dependence between i and thickness-normalized plateau potential, ϕ plateau L –1 , irrespective of the magnitude of the applied current. In all seven polymer electrolytes, we found a linear correlation between ilim and the slopes of these lines, σ. In other words, measurements of σ can be used to predict the limiting current.

Jana, Rounak [Lawrence Berkeley National Laborator

Understanding Discharge‐Driven Growth of Cathode Impedance in Ni‐Rich NMC Cathodes

Degradation of LiNi x Mn y Co 1-x-y O 2 (NMC)-based lithium-ion batteries depends strongly on cut-off voltage ranges. In addition to the high upper cut-off voltage, a high depth of discharge (i.e., lower cut-off voltage) significantly worsens cathode impedance growth and capacity fade during long-term cycling. However, there is currently no consensus on the mechanism behind the negative role of a deep discharge. Here, this phenomenon was investigated in graphite||NMC cells with single-crystal cathodes (LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC622) or LiNi 0.76 Co 0.14 Mn 0.10 O 2 (NMC76)) using targeted aging protocols (constant high-voltage holds vs. charge–discharge cycling), while monitoring transition-metal (TM) dissolution, cathode-electrolyte interface (CEI) impedance, and NMC surface composition. We demonstrate a correlation between discharge-driven CEI impedance growth and increased TM dissolution. Furthermore, this degradation pathway is more pronounced in lower-Ni NMC622 than in higher-Ni (NMC76) under comparable delithiation states at charge, with both compositions undergoing the H2→H3 phase transition. X-ray photoelectron spectroscopy (XPS) reveals NMC composition-dependent evolution of surface lattice oxygen and restructured surface layer composition between charged and discharged states. These findings add mechanistic depth to the role of discharge as an active driver of interfacial degradation and provide new insights into its composition dependence.

25 ENERGY STORAGE