At least 109 records · Page 6

In-line, High-Throughput Quality Monitoring for Fuel Cell and Electrolyzer Components Based on Transmission and Reflection Imaging

During the manufacturing of fuel cell and electrolyzer membranes and membrane electrode assemblies (MEAs), real-time, in-line, high-throughput optical-based quality monitoring methods are essential for detecting defects and monitoring thickness variations, thus improving the performance and increasing the durability of fuel cell and electrolyzer in the hydrogen industry. For the MEAs with very opaque coatings, optical transmission-based imaging has been developed and applied in the Roll-to-Roll system using a flashlight and a high-sensitivity CCD camera. We observed high signal-to-noise ratio images while the Roll-to-Roll system ran at 5 ft/min. The entire sample image could quickly be recovered from the discrete frames using customized Python codes for automatic frame cropping and stitching. We detected significant non-uniformities in our experimental MEAs specimen. For fuel cell and low-temperature electrolysis (LTE) transparent membranes, we used optical reflectance hyperspectral imaging with interference fringe-based thickness mapping. We set up a hyperspectral camera to measure various rolls of commercial membranes. The measurement results are analyzed to find the thickness distribution of each roll and to check for defects. Transmission and reflection imaging-based quality monitoring techniques demonstrated in this project can be widely used in the mass production environment to improve the production yield and performance of hydrogen devices.

DIRECT ENERGY CONVERSION,ENGINEERING↗

Blended conventional and high oxygen permeability ionomers as a fuel cell electrode binder

Ionomer strongly influences the performance of proton exchange membrane fuel cells (PEMFCs), affecting catalyst activity and reactant transport within the electrodes. While recent work on high oxygen permeability ionomers (HOPI) has demonstrated improved performance compared to conventional perfluorosulfonic acid (PFSA) ionomers such as Nafion™, there have also been reports of increased cracking in fabricated electrodes. We investigated the effects of blending HOPI with Nafion™ ionomer dispersions when fabricating cathode catalyst layers (CCLs). Small-angle x-ray scattering suggests that the ionomers mix well, and adsorption measurements indicate that HOPI adsorbs less strongly to the carbon-supported platinum (Pt) catalyst, and in blends, the Nafion™ ionomer exhibits a greater degree of adsorption. Imaging CCLs revealed a decrease in crack formation in blended samples as HOPI content decreased, with 14% HOPI having the lowest crack density. In a membrane electrode assembly (MEA) using a high surface area carbon support, the 14% HOPI blend exhibited similar performance to 100% HOPI. However, similar performance enhancements were not achieved with a medium surface area carbon support. These findings suggest a path for low-crack CCLs with enhanced oxygen transport, while highlighting a need for further investigation of ionomer blending towards efficient and durable PEMFCs.

25 ENERGY STORAGE↗

Identifying electrochemical processes by distribution of relaxation times in proton exchange membrane electrolyzers

Distribution of relaxation time (DRT) is used to interpret electrochemical impedance spectroscopy (EIS) for proton exchange membrane (PEM) water electrolyzers, with an attempt to separate overlapped relaxation processes in Nyquist plots. By varying operating conditions and catalyst loadings, four main relaxation peaks arising from EIS can be identified and successfully separated from low to high frequencies as (P1) mass transport, (P2) oxygen evolution reaction kinetics, (P3) reaction kinetics (with faster time constant than P2), and (P4) ionic transport. Here, the shape, height, and frequency of the DRT peaks change with different membrane electrode assembly (MEA) configurations. Electron microscopy reveals distinct features from the cross-sectioned MEAs which verify critical DRT results in that increasing the iridium (Ir)-anode loading from 0.2 mgIr/cm 2 to 1.5 mgIr/cm 2 reduces kinetic losses due to higher site-access; a thick and compacted anode, however, also triggers higher ohmic resistances from membrane/catalyst layer hydration and increases transport losses due to longer ionomer pathways. DRT provides higher resolution to EIS for deconvoluting processes with different relaxation times and the quantification of DRT peaks improves the accounting of total losses from each process.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Pt Nanoparticles on Atomic-Metal-Rich Carbon for Heavy-Duty Fuel Cell Catalysts: Durability Enhancement and Degradation Behavior in Membrane Electrode Assemblies

Proton exchange membrane fuel cells (PEMFCs) are a promising zero-emission power source for heavy-duty vehicles (HDVs). However, long-term durability of up to 25,000 h is challenging because current carbon support, catalyst, membrane, and ionomer developed for traditional light-duty vehicles cannot meet the stringent requirement. Therefore, understanding catalyst degradation mechanisms under the HDV condition is crucial for rationally designing highly active and durable platinum group metal (PGM) catalysts for high-performance membrane electrode assemblies (MEAs). Herein, we report a PGM catalyst consisting of platinum nanoparticles with a high content (40 wt %) on atomic-metal-site (e.g., MnN 4 )-rich carbon support. MEAs with the Pt (40 wt %)/Mn–N–C cathode catalyst achieved significantly enhanced performance and durability, generating 1.41 A cm –2 at 0.7 V under HDV conditions (0.25 mgPt cm –2 and 250 kPa abs pressure) and retaining 1.20 A cm –2 after an extended and accelerated stress test up to 150,000 voltage cycles. Electron microscopy studies indicate that most fine Pt nanoparticles are retained on or/and in the carbon support covered with the ionomer throughout the catalyst layer at the end of life. During the long-term stability test, the observed electrochemical active surface area reduction and performance loss primarily result from Pt depletion in the catalyst layer due to Pt dissolution and redeposition at the interface of the cathode and membrane. Importantly, the first-principle density functional theory calculations further reveal a support entrapment effect of the Mn–N–C, in which the MnN 4 site can specifically adsorb the Pt atom and further retard the Pt dissolution and migration, therefore enhancing long-term MEA durability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Elucidating the Role of Ionomer in the Performance of Platinum Group Metal-free Catalyst Layer via in situ Electrochemical Diagnostics

The ionomer content in platinum group metal (PGM)-free polymer electrolyte fuel cell (PEFC) cathode catalyst layer (CCL) plays an important role in the electrode gas transport properties, proton conductivity, and hence, membrane electrode assembly (MEA) performance. In this work, the ionomer content in the CCL is varied, influencing electrode microstructure by altering porosity, tortuosity, as well as ionomer distribution and coverage of the catalyst particles. A novel technique consisting of a H 2 pump, combined with a Pt black sensor layer, is used to measure the bulk mass transport resistance of a series of PGM-free CCL prepared with different ionomer contents. The values for bulk electrode mass transport resistance are contrasted with electrode proton transport resistance in the cathode catalyst layer, establishing a clearly defined trade-off between two key performance limiting phenomena and identifying a need for novel PGM-free electrode fabrication strategies.

25 ENERGY STORAGE↗

Unraveling the core of fuel cell performance: engineering the ionomer/catalyst interface

The biggest obstacle to the widespread implementation of polymer electrolyte membrane fuel cells (PEMFCs) is their cost, primarily due to the use of platinum catalysts. The high intrinsic catalyst activity exhibited on a rotating disk electrode (RDE) is rarely realized in a membrane electrode assembly (MEA), which is a long-standing challenge for PEMFCs and a cause of low catalyst utilization. To translate the high RDE performance of a catalyst into a MEA, the design of an ideal ionomer/catalyst interface is proposed: a thin, conformal ionomer film covers the maximum surface of a Pt nanoparticle and thus simultaneously maximizes catalyst utilization, (i.e., high mass activity and electrochemically active surface area) and O 2 diffusion rate (i.e., high current density performance) without compromising proton conduction. Building such an interface is a long-standing challenge due to the lack of interaction between the ionomer and catalyst particles, resulting in large ionomer agglomerates and inhomogeneous ionomer coverage over the catalyst nanoparticle, with consequent poor fuel cell performance. In this work, this ionomer/catalyst interface has been engineered, utilizing the electrostatic attraction between positively charged catalyst and negatively charged ionomer particles in a catalyst ink and preserved in a solid catalyst layer. As a result, this interface leads to previously unachieved proton exchange membrane fuel cell performance in terms of both catalyst utilization (75% vs. 45%) and peak/rated power density (i.e., 1.430/0.930 W cm -2 , H 2 /air, cathode Pt loading: 0.1 mgPt cm -2 ) for pure Pt catalysts, even better than those of Pt alloy catalysts. This work demonstrates the formation of an interface in the liquid phase (using ultra-small-angle X-ray scattering in combination with cryo-TEM, isothermal–titration–calorimetry) and the preservation of the interface in the solid catalyst layer (using TEM) and estimates the effective coverage and thickness of the ionomer film (using limiting current density, RDE and fuel cell performance).

25 ENERGY STORAGE↗

Influence of Ink Formulation and Drying Conditions on Ionomer Distribution in High-Performance Roll-to-Roll-Coated Gas-Diffusion Electrodes

To enable mass production of fuel cell membrane electrode assemblies (MEAs) catalyst layers production will require continuous roll-to-roll (R2R) coating processes. Gas diffusion electrodes (GDEs) are advantageous for mass production because the catalyst layer can be directely coated on the microporous layer of the gas diffusion media without the need for a decal-transfer process. It is known that the water-to-alcohol ratio in the catalyst ink influences the interactions of the ionomer with the catalyst leading to different distributions of ionomer in spray-coated catalyst layers. It is also known that during drying of colloidal mixtures, like fuel cell inks, factors such as drying rate, particle size, and agglomeration influence how the materials distribute themselves throughout the thickness of the dired film. Thus far there have only been limited studies to understand how process conditions such as ink formulation and drying temperature influence the distribution of ionomer and catalyst coated using scalable methods. This understanding is especially important for GDEs since it is known that having a sufficient amount of ionomer at the catalyst layer-membrane interface is critical for high performance. In this study we have focused on determining how the ratio of water to 1-propanol in the catalyst ink ink and drying temperature influence the distribution of ionomer throughout the thickness of the catalyst layer. Using a combination of Kelvin probe and x-ray photoelectron spectroscopy we show that an ionomer-rich surface is promoted by a higher drying rate and a water-rich catalyst ink. In contrast, a 1-propanol catalyst ink leads to a lower concentration of ionomer on the top surface. Using x-ray computed tomography, we are able to characterize the ionomer distribution throughout the thickness of the layer. We find that, in addition to promoting an ionomer-rich top surface, water-rich inks lead to a more homogenous distribution of ionomer, whereas a 1-propanol-rich ink leads to a more irregular distribution. It is found that MEA performance is improved by selecting conditions and ink formulations that promote ionomer enrichment at the top surface to facilitate a good interface with the membrane. MEAs prepared with a 75 wt% water catalyst ink with a 0.9 I/C have equivalent performance to spray-coated GDEs. Critically, these R2R-coated GDEs do not need an additional ionomer overlayer like the spray-coated GDEs do, reducing the number of processing steps in a manufacturing setting. This work shows that with the appropriate selection of materials, ink formulation, and processing conditions gas-diffusion electrodes are a viable pathway for fuel cell manufacturing.

ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATION↗

Parasitic Effects in Impedance Spectrum of PEM Water Electrolysis Cells: Case Study of High-Frequency Inductive Effects

Electrochemical impedance spectroscopy (EIS) is a powerful tool to characterize and distinguish electrochemical, electrical, and diffusive processes in an electrolysis cell. The EIS response with small impedance (mΩ) depends on components and materials of the cell, but often also on the electrical setup, cables, and connectors, leading to incorrect conclusions about the performance of the electrolysis cells. These parasitic effects are assessed via a short-circuit measurement and confirmed to be external from the membrane electrode assembly (MEA). In the setup, the inductive characteristic is described by a modified inductive reactance and must be included in the equivalent circuit model (ECM) which is fitting the cell EIS spectra in operation (in situ). If points of the spectra showing inductive characteristic (below x-axis in Nyquist plot) are excluded from the ECM evaluation, an artificially increased ohmic resistance at high frequencies is obtained. In addition, considerations on other components of the ECM can be misleading and significantly incorrect. The only way to avoid that inductive behavior caused by the external setup is incorrectly assigned to the ECM describing properties of the MEA is to include the inductive effects in the ECM analysis of in situ EIS measurements.

30 DIRECT ENERGY CONVERSION↗

Porous transport electrodes for oxygen evolution reaction in proton exchange membrane water electrolysis -cells: Materials, designs, and diagnoses

H 2 production using proton exchange membrane (PEM) water electrolysis (PEMWE) cells has received considerable attention because of the high efficiencies of these cells and no harmful emissions from the related process. In PEMWE cells, porous transport electrodes (PTEs) composed of a catalyst layer (CL) comprising O 2 evolution reaction (OER) catalysts, porous transport layer (PTL), and PEM play key roles in the stack performance and lifetime. Herein, Ir-based and non-precious-metal OER catalysts that are highly active and stable at low pH values and high anodic potentials are reviewed to understand their OER mechanisms. Various strategies are proposed for engineering CLs and PTLs to improve the interfacial properties and mass transfers of reactants and products to and from the active sites. Additionally, diagnoses of PTEs is significantly crucial for interpreting electrochemical processes and addressing their current challenges. Therefore, half-cell analyses, including diffusion electrode (DE), floating electrode (FE), and modified rotating disk electrode (MRDE) techniques, are explored, and membrane electrode assembly (MEA)-based analyses, such as the polarization technique, electrochemical impedance spectroscopy, and magnetic field analysis, are established. In conclusion, this study aims to provide an overview of recent technologies used for the engineering and diagnostic tools of PEMWE cells and insights into the advanced components and systems to be developed in this field.

Diagnosis of PEMWE Cells↗

Constructing Highly Porous Low Iridium Anode Catalysts Via Dealloying for Proton Exchange Membrane Water Electrolyzers

Iridium (Ir) is the most active and durable anode catalyst for the oxygen evolution reaction (OER) for proton exchange membrane water electrolyzers (PEMWEs). However, their large-scale applications are hindered by high costs and scarcity of Ir. Lowering Ir loadings below 1.0 mgcm -2 causes significantly reduced PEMWE performance and durability. Therefore, developing efficient low Ir-based catalysts is critical to widely commercializing PEMWEs. Herein, an approach is presented for designing porous Ir metal aerogel (MA) catalysts via chemically dealloying IrCu alloys. In this study, the unique hierarchical pore structures and multiple channels of the Ir MA catalyst significantly increase electrochemical surface area (ECSA) and enhance OER activity compared to conventional Ir black catalysts, providing an effective solution to design low-Ir catalysts with improved Ir utilization and enhanced stability. An optimized membrane electrode assembly (MEA) with an Ir loading of 0.5 mg Ir cm -2 generated 2.0 A cm -2 at 1.79 V, higher than the Ir black at a loading of 2.0 mg Ir cm -2 (1.63 A cm -2 ). The low-Ir MEA demonstrated an acceptable decay rate of ≈40 µV h -1 during durability tests at 0.5 (>1200 h) and 2.0 A cm -2 (400 h), outperforming the commercial Ir-based MEA (175 µV h -1 at 2.0 mg Ir cm -2 ).

36 MATERIALS SCIENCE↗

Elucidating the impact of the ionomer equivalent weight on a platinum group metal-free PEMFC cathode via oxygen limiting current

Leveraging the interactions between ionomer and catalyst can increase the performance of proton exchange membrane fuel cells. The impacts of the equivalent weight (EW) of perfluorosulfonic acid–based ionomers on the platinum group metal-free electrode structure and fuel cell performance have not been fully explored. Four membrane electrode assemblies (MEAs) were prepared by using a commercial Fe–N–C catalyst, two perfluorosulfonic acid ionomers with different EWs, that is, Aquivion 720 (A720) and Nafion 1100 (N1100), and two ionomer-to-catalyst (I/C) ratios. The four MEAs were characterized to understand the impact of the ionomer EW and content on the capacitance, proton conductivity, and mass transport on the cathode. The mass transport resistance was measured for the first time using a new oxygen reduction reaction limiting current method enabling to couple the effects of oxygen diffusion with liquid water generation. Low EW ionomer combined with a moderate I/C results in improved performance due to its enhanced proton conductivity. However, when used at high I/C, it can cause severe water flooding at high current density due to the enhanced liquid water uptake, especially at high relative humidity, resulting in lower catalyst utilization and higher mass transport resistance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Final Technical Report for project entitled Highly Active, Durable, and Ultra-Low PGM NSTF Thin Film ORR Catalysts and Support

In this project, the objective was to develop new oxygen reduction reaction (ORR) electrocatalysts for proton exchange membrane fuel cells (PEMFCs) which could exceed all of the Department of Energy (DOE) 2020 targets listed in DE-FOA-0001224, Subtopic 1b, Table I. The expected outcome was development of one or more electrocatalysts which are substantially improved over the current state-of-the-art in terms of overall activity, durability, and cost, and are suitable for automotive traction and stationary fuel cell applications. This report summarizes this project’s progress towards meeting the stated objectives and includes a summary of key findings and conclusions. The development activities towards new highly active and durable thin film electrocatalysts has led to the discovery of several electrocatalysts which approached or exceeded several DOE 2020 targets for activity, durability, and performance in proton exchange membrane fuel cell (membrane electrode assemblies (MEAs). In this project, electrocatalyst development focused on systematic physical and electrochemical characterization of electrocatalyst activity, durability, and performance in MEAs as a function of electrocatalyst fabrication, compositional and structural variables. The project approach was to develop relationships between the catalyst functional responses (activity, durability and performance) with catalyst physical properties and catalyst fabrication methods. Additionally, the thin film catalysts were integrated onto the unique and durable 3M Nanostructured Thin Film (NSTF) support, consisting of arrays of self-assembled organic crystalline whiskers. The catalysts were evaluated against the project targets via extensive electrochemical characterization in MEA format at 3M, advanced structural and compositional microscopy at Oak Ridge National Laboratory (ORNL), and atomic structure analysis via XAFS at Argonne National Laboratory (ANL). The extensive electrochemical and physical characterization resulted in development of several trends which correlate the catalysts’ electrochemical properties to their physical properties, including composition, structure, and method of fabrication. The development was guided by density functional theory (DFT) modeling at Purdue University and kinetic Monte Carlo (kMC) modeling at Johns Hopkins University. The catalyst simulations provided key insights into the observed experimental activity and durability trends, and additionally were utilized to assess new electrocatalyst concepts prior to or coincident with physical catalyst development. This development has led to several electrocatalyst candidates with activity and durability which approach or exceed DOE targets. One class of catalysts, based on nm-scale thin layers of Pt on Ir, met or exceeded 6 of the 6 DOE targets the project addressed.

08 HYDROGEN↗

Recreating Fuel Cell Catalyst Degradation in Aqueous Environments for Identical-Location Scanning Transmission Electron Microscopy Studies

The recent surge in interest of proton exchange membrane fuel cells (PEMFCs) for heavy-duty vehicles increases the demand on the durability of oxygen reduction reaction electrocatalysts used in the fuel cell cathode. This prioritizes efforts aimed at understanding and subsequently controlling catalyst degradation. Identical-location scanning transmission electron microscopy (IL-STEM) is a powerful method that enables precise characterization of degradation processes in individual catalyst nanoparticles across various stages of cycling. Recreating the degradation processes that occur in PEMFC membrane electrode assemblies (MEAs) within the aqueous cell used for IL-STEM experiments is vital for generating an accurate understanding of these processes. In this work, we investigate the type and degree of catalyst degradation achieved by cycling in an aqueous cell compared to a PEMFC MEA. While significant degradation is observed in IL-STEM experiments performed on a traditional Pt catalyst using the standard accelerated stress test potential window (0.6-0.95 VRHE), degradation of a PtCo catalyst designed for heavy-duty vehicle use is very limited compared to that observed in MEAs. We therefore explore various experimental parameters such as temperature, acid type, acid concentration, ionomer content, and potential window to identify conditions that reproduce the degradation observed in MEAs. We find that by extending the cycling potential window to 0.4-1.0 V RHE in an electrolyte containing Pt ions, the degraded particle size distribution and alloy composition better match that observed in MEAs. In particular, these conditions increase the relative contribution of Ostwald ripening, which appears to play a more significant role in the degradation of larger alloy particles supported on high-surface-area carbons than coalescence. Results from this work highlight the potential for discrepancies between ex situ aqueous experiments and MEA tests. While different catalysts may require a unique modification to the AST protocol, strategies provided in this work enable future in situ and identical-location experiments that will play an important role in the development of robust catalysts for heavy-duty vehicle applications.

30 DIRECT ENERGY CONVERSION↗

Evaluating the Effects of Anode Porous Transport Layer on the Performance and Durability of Anion Exchange Membrane Electrolyzers

As anion exchange membrane systems have emerged as a competitive low temperature electrolysis technology, research has expanded to other components and device integration. In this study, nickel (Ni) and stainless steel (SS)-based porous transport layers (PTLs) are investigated in membrane electrode assemblies (MEAs). Compared to MEAs using Ni, the SS PTL shows higher performance due to less kinetics and residual loss and possibly due to a combination of iron mobility improving oxygen evolution reactivity and electron conduction pathways, as well as higher porosity increasing site access. Voltage decay rates of approximately 144 and 115 μV/h, respectively, for the Ni and SS PTLs are found, although the long-term durability and lifetime implications are convoluted. Voltage breakdown analysis confirms that both PTLs saw significant increases in residual loss possibly due to catalyst/PTL property changes that affected electronic, ionic, and mass transport pathways. For the Ni PTL, a higher proportion of the losses were due to cell kinetics; comparatively, more of the SS PTL losses were due to increases in the high frequency resistance. The experimental findings presented here provide insights on the impact of the PTL materials and their properties.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Low‐PGM and PGM‐Free Catalysts for Proton Exchange Membrane Fuel Cells: Stability Challenges and Material Solutions

Abstract Fuel cells as an attractive clean energy technology have recently regained popularity in academia, government, and industry. In a mainstream proton exchange membrane (PEM) fuel cell, platinum‐group‐metal (PGM)‐based catalysts account for ≈50% of the projected total cost for large‐scale production. To lower the cost, two materials‐based strategies have been pursued: 1) to decrease PGM catalyst usage (so‐called low‐PGM catalysts), and 2) to develop alternative PGM‐free catalysts. Grand stability challenges exist when PGM catalyst loading is decreased in a membrane electrode assembly (MEA)—the power generation unit of a PEM fuel cell—or when PGM‐free catalysts are integrated into an MEA. More importantly, there is a significant knowledge gap between materials innovation and device integration. For example, high‐performance electrocatalysts usually demonstrate undesired quick degradation in MEAs. This issue significantly limits the development of PEM fuel cells. Herein, recent progress in understanding the degradation of low‐PGM and PGM‐free catalysts in fuel cell MEAs and materials‐based solutions to address these issues are reviewed. The key factors that degrade the MEA performance are highlighted. Innovative, emerging material concepts and development of low‐PGM and PGM‐free catalysts are discussed.

Du, Lei↗

Constructing Highly Durable Fuel Cell Catalysts Through Integrating Graphitic Shell‐Protected Composite Carbon Support with Gaseous Co Deposition‐Driven PtCo Intermetallics

Metal dissolution, nanoparticle agglomeration, and carbon support corrosion cause significant performance degradation of current PtCo catalysts under acidic and oxidative oxygen reduction reaction. Here, in this study, an integrated strategy is presented to design high-performance Pt 3 Co intermetallic catalysts by regulating gaseous Co deposition-driven diffusion into Pt nanoparticles supported on a composite carbon. The composite carbon is derived from ZIF-8/polyaniline, consisting of a high-surface-area (HSC) core and a protective graphitic shell (GS), which is employed to design 40 wt.% Pt/HSC@GS catalyst. The corresponding membrane electrode assemblies (MEAs) can maintain 1.09 A cm −2 at 0.7 V (20. 7% loss) after 10 000 cycles (1.0–1.5 V for carbon stability) and 1.15 A cm −2 (16.1% loss) after 150 000 cycles (0.60–0.95 V for catalyst stability). A ordered Pt 3 Co intermetallic is synthesized via a gaseous Co-deposition process, which yields a homogeneous Co-rich layer onto the Pt nanoparticles on the composite support, thereby facilitating Co diffusion into Pt crystal during subsequent ordering annealing to form the ordered intermetallic structure. This gaseous deposition leads to a thin carbon layer on PtCo nanoparticles, inhibiting particle growth during the annealing and mitigating Co dissolution under dynamic electrochemical conditions. The PtCo catalyst achieves impressive MEA performance and long-term durability (1.45 A cm −2 at 0.7 V after 120 000 cycles) under heavy-duty conditions.

30 DIRECT ENERGY CONVERSION↗

Probing Heterogeneous Degradation of Catalyst in PEM Fuel Cells under Realistic Automotive Conditions with Multi-Modal Techniques

The heterogeneity of polymer electrolyte fuel cell catalyst degradation is studied under varied relative humidity and types of feed gas. Accelerated stress tests (ASTs) are performed on four membrane electrode assemblies (MEAs) under wet and dry conditions in an air or nitrogen environment for 30 000 square voltage cycles. The largest electrochemically active area loss is observed for MEA under wet conditions in a nitrogen gas environment AST due to constant upper potential limit of 0.95 V and significant water content. The mean Pt particle size is larger for the ASTs under wet conditions compared to dry conditions, and the Pt particle size under land is generally larger than under the channel. Observations from ASTs in both conditions and gas environments indicate that water content promotes Pt particle size growth. ASTs under wet conditions and an air environment show the largest difference in Pt particle size growth for inlet versus outlet and channel versus land, which can be attributed to larger water content at outlet and under land compared to inlet and under channel. From X-ray fluorescence experiments Pt particle size increase is a local phenomenon as Pt loading remains relatively uniform across the MEA.

25 ENERGY STORAGE↗

Probing Electrode Transformation under Dynamic Operation for Alkaline Water Electrolysis

Alkaline water electrolyzers (AWEs) play a pivotal role in the realm of large-scale hydrogen production. However, AWEs face significant challenges in electrode degradation particularly under dynamic operating conditions, induced by reverse current phenomenon during frequent startup/shutdown. Herein, this study aims to rationalize the degradation mechanisms of AWEs under these conditions. A three-electrode membrane electrode assembly (MEA) setup is first utilized to decouple polarization behaviors of anode and cathode in AWEs. Following a proposed accelerated stress testing protocol, the setup allows for tracking individual electrode performance transformations during frequent reverse current operation. Integrating operando cell studies with in situ and post-mortem characterizations, it is showed that continuous formation of highly active species, nickel (oxy)hydroxides, improves the anode performance for oxygen evolution reaction. On the contrary, irreversible oxidation of nickel to β-nickel hydroxide results in a severe degradation of cathode, leading to material dissolution, poor electrical conductivity and loss of catalytic activity for hydrogen evolution reaction. These results provide insights in nickel-based electrode transformation mechanisms for alkaline water electrolysis and indicate that cathode with higher redox reversibility can potentially improve durability of AWEs under dynamic conditions.

08 HYDROGEN↗