An advanced arc track resistant airframe wire

Tensolite, a custom cable manufacturer specializing in high temperature materials as the dielectric medium, develops an advance arc track resistant airframe wire called Tufflite 2000. Tufflite 2000 has the following advantages over the other traditional wires: lighter weight and smaller in diameter; excellent wet and dry arc track resistance; superior dynamic cut-through performance even at elevated temperatures; flight proven performance on Boeing 737 and 757 airplanes; and true 260 C performance by utilizing Nickel plated copper conductors. This paper reports the different tests performed on Tufflite 2000: accelerated aging, arc resistance (wet and dry), dynamic cut through, humidity resistance, wire-to-wire abrasion, flammability, smoke, weight, notch sensitivity, flexibility, and markability. It particularly focuses on the BSI (British Standards Institute) dry arc resistance test and BSI wet arc tracking.

Beatty, J.↗

Magnetically Damped Furnace Bitter Magnet Coil 1

A magnet has been built by the National High Magnetic Field Laboratory for NASA on a cost reimbursement contract. The magnet is intended to demonstrate the technology and feasibility of building a magnet for space based crystal growth. A Bitter magnet (named after Francis Bitter, its inventor) was built consisting of four split coils electrically in series and hydraulically in parallel. The coils are housed in a steel vessel to reduce the fringe field and provide some on-axis field enhancement. The steel was nickel plated and Teflon coated to minimize interaction with the water cooling system. The magnet provides 0.14 T in a 184 mm bore with 3 kW of power.

Bird, M. D.↗

RF Bonding Investigation: The Effects of a Space Environment on Coatings

Coatings are commonly used in the aerospace industry for corrosion control of metals. The impedance of these coatings can reduce the effectiveness of EMI filters. This paper documents the effects of a space environment on a variety of coatings applied to electrical bonding surfaces. Nickel plating, anodizing, and chemical conversion coatings of alodine and iridite are investigated. The test fixture is designed to simulate a feed-through filter in a metal chassis. The filter insertion loss will be shown as a function of frequency and coating.

Krome, Mark E.↗

Constellation-X Cylinder Figuring and Polishing Studies

In support of Goddard's Constellation-X mandrel manufacturing effort a series of fabrication experiments are being performed to determine a best approach. Currently, polishing immediately after diamond turning, produces a RMS surface roughness of 0.31 nm, on a nickel plated aluminum mandrel. Studies currently under way will incorporate an abrasive figuring step followed by a polishing operation. The current diamond turning, figuring and polishing procedures will be described and the results presented.

Waluschka, Eugene↗

A Microfabricated Segmented-Involute-Foil Regenerator for Enhancing Reliability and Performance of Stirling Engines

An actual-size microfabricated regenerator comprised of a stack of 42 disks, 19 mm diameter and 0.25 mm thick, with layers of microscopic, segmented, involute-shaped flow channels was fabricated and tested. The geometry resembles layers of uniformly-spaced segmented-parallel-plates, except the plates are curved. Each disk was made from electro-plated nickel using the LiGA process. This regenerator had feature sizes close to those required for an actual Stirling engine but the overall regenerator dimensions were sized for the NASA/Sunpower oscillating-flow regenerator test rig. Testing in the oscillating-flow test rig showed the regenerator performed extremely well, significantly better than currently used random-fiber material, producing the highest figures of merit ever recorded for any regenerator tested in that rig over its approximately 20 years of use.

Ibrahim, Mounir↗

Assessment of MODIS Scan Mirror Reflectance Changes On-Orbit

Since launch, the NASA EOS Terra and Aqua MODIS have operated successfully for more than 8 and 6 years, respectively. MODIS collects data using a two-sided scan mirror over a large scan angular range. The scan mirror is made of a polished, nickel-plated beryllium base coated with high purity silver, which is then over-coated with the Denton proprietary silicon monoxide and silicon dioxide mixture. The scan mirror's reflectance was characterized pre-launch using its witness samples, and the response versus scan angle was measured at the sensor system level. In this study, we present an assessment of MODIS scan mirror on-orbit degradation by examining changes of spectral band response over each sensor's mission lifetime. Results show that the scan mirror's optical properties for both Terra and Aqua MODIS have experienced significant degradation since launch in the VIS spectral region, which is mirror side dependent as well as scan angle dependent. In general, the mirror degradation is more severe for Terra MODIS than Aqua MODIS, especially during recent years. For Terra MODIS, the degradation rate is noticeably different between the mirror sides. On the other hand, there has been little mirror side dependent difference for Aqua MODIS.

Xiong, Xiaoxiong↗

Long-Term Effects of Soldering By-Products on Nickel-Coated Copper Wire

An analysis of thirty-year-old, down graded flight cables was conducted to determine the makeup of a green material on the surface of the shielded wire near soldered areas and to ascertain if the green material had corroded the nickel-coated copper wire. Two likely candidates were possible due to the handling and environments to which these cables were exposed. The flux used to solder the cables is known to contain abietic acid, a carboxylic acid found in many pine rosins used for the soldering process. The resulting material copper abietate is green in color and is formed during the application of heat during soldering operations. Copper (II) chloride, which is also green in color is known to contaminate flight parts and is corrosive. Data is presented that shows the material is copper abietate, not copper (II) chloride, and more importantly that the abietate does not aggressively attack nickel-plated copper wire.

Rolin, T. D.↗

An Experimental Investigation of Silicone-to-Metal Bond Strength in Composite Space Docking System Seals

The National Aeronautics and Space Administration (NASA) is currently developing a new universal docking mechanism for future space exploration missions called the Low Impact Docking System (LIDS). A candidate LIDS main interface seal design is a composite assembly of silicone elastomer seals vacuum molded into grooves in an electroless nickel plated aluminum retainer. The strength of the silicone-tometal bond is a critical consideration for the new system, especially due to the presence of small areas of disbond created during the molding process. In the work presented herein, seal-to-retainer bonds of subscale seal specimens with different sizes of intentional disbond were destructively tensile tested. Nominal specimens without intentional disbonds were also tested. Tension was applied either uniformly on the entire seal circumference or locally in one short circumferential length. Bond failure due to uniform tension produced a wide scatter of observable failure modes and measured load-displacement behaviors. Although the preferable failure mode for the seal-to-retainer bond is cohesive failure of the elastomer material, the dominant observed failure mode under the uniform loading condition was found to be the less desirable adhesive failure of the bond in question. The uniform tension case results did not show a correlation between disbond size and bond strength. Localized tension was found to produce failure either as immediate tearing of the elastomer material outside the bond region or as complete peel-out of the seal in one piece. The obtained results represent a valuable benchmark for comparison in the future between adhesion loads under various separation conditions and composite seal bond strength.

Gaier, James R.↗

Space Shuttle Columbia Aging Wiring Failure Analysis

A Space Shuttle Columbia main engine controller 14 AWG wire short circuited during the launch of STS-93. Post-flight examination divulged that the wire had electrically arced against the head of a nearby bolt. More extensive inspection revealed additional damage to the subject wire, and to other wires as well from the mid-body of Columbia. The shorted wire was to have been constructed from nickel-plated copper conductors surrounded by the polyimide insulation Kapton, top-coated with an aromatic polyimide resin. The wires were analyzed via scanning electron microscope (SEM), energy dispersive X-Ray spectroscopy (EDX), and electron spectroscopy for chemical analysis (ESCA); differential scanning calorimetry (DSC) and thermal gravimetric analysis (TGA) were performed on the polyimide. Exemplar testing under laboratory conditions was performed to replicate the mechanical damage characteristics evident on the failed wires. The exemplar testing included a step test, where, as the name implies, a person stepped on a simulated wire bundle that rested upon a bolt head. Likewise, a shear test that forced a bolt head and a torque tip against a wire was performed to attempt to damage the insulation and conductor. Additionally, a vibration test was performed to determine if a wire bundle would abrade when vibrated against the head of a bolt. Also, an abrasion test was undertaken to determine if the polyimide of the wire could be damaged by rubbing against convolex helical tubing. Finally, an impact test was performed to ascertain if the use of the tubing would protect the wire from the strike of a foreign object.

McDaniels, Steven J.↗

Lunar Glovebox Balance with Wireless Technology

The most important equipment required for processing lunar samples is a high-quality mass balance for maintaining accurate weight inventory, security, and scientific study. After careful review, a Curation Office memo by Michael Duke in 1978 chose the Mettler PL200 to be used for sample weight measurements inside the gloveboxes (Fig. 3). These commercial off-the-shelf (COTS) balances did not meet the strict accepted material requirements in the Lunar lab. As a result, each balance housing, weighing pan, and wiring was custom retrofitted to meet Lunar Operating Procedure (LOP) 54 requirements [for material construction restrictions]. The original design drawings for the custom housings, readout support stands, and wiring were done by the JSC engineering directorate. The 1977- 1978 schematics, drawings, and files are now housed in the curation Data Center. Per the design specifications, the housing was fabricated from aluminum grade 6061 T6, seamless welds, and anodized per MIL-A-8625 type I, class I. The balance feet were TFE Teflon and any required joints were sealed with Viton A gaskets. The readout display and support stands outside the glovebox were fabricated from 300 series stainless steel with #4 finish and mounted to the glovebox with welded bolts. Wire harnesses that linked the balance with the outside display and power were encapsulated with TFE Teflon and transported through custom Deutsch wire bulk head pass-through systems from inside to outside the glovebox. These Deutsch connectors were custom fabricated with 316L stainless steel bodies, Viton A O-rings, aluminum 6061 with electroless nickel plating, Teflon (replacing the silicone), and gold crimp connectors (no soldering). Many of the Deutsch connectors may have been used in the Apollo program high vacuum complex in building 37 and date to about 1968 to 1970.

Zeigler, Ryan A.↗

The Realuminizing of the 7-Meter Diameter Solar Simulator Collimating Mirror

This paper describes the modification of a three-electron-beam (EB) gun system for vacuum depositing a highly reflective aluminum coating on a 7.01-m (23-ft) -diam nickel-plated aluminum collimating mirror. The mirror is part of the JPL 7.62-m space simulator that was recently modernized with a new high vacuum pumping system, solar lamp power supplies, solar optic lens system, and refurbished collimating mirror. The mirror is the primary reflector for the solar simulation system and the aluminized reflective surface is its most critical performance element. The uniformity of thickness and high reflectivity of the coating is visible and near-ultraviolet (UV) light governs the accuracy of the beam for solar testing. The uniformity of the thin-film thickness also controls the durability of the mirror over time.

solar↗

Ground-Based Cryogenic Leak Test of Fittings for Cryogenic Fluid Management

Mechanically connected fluid joints are virtually unavoidable in complex cryogenic system designs. In the case of spacecraft, the performance of these joints is critical to mission success. This is especially true for long-duration space missions where even very low leak rates can eventually lead to significant propellant losses or failure of vital cryogenic cooling systems. NASA has recently undertaken an effort to quantify the leak rate of Vacuum Coupling Radiation (VCR) fittings over the temperature range from ambient to 20 K, both before and after exposure to a launch vibration profile. A test apparatus employing a cryocooler and a calibrated helium mass spectrometer was developed, validated, and used to obtain quantifiable leak rates at a fitting test pressure of 31 bar (450 psig). Three different fitting sizes were tested, 25.4 mm (¼ inch), 12.7 mm (½ inch), and 6.35 mm (1 inch) and two gasket materials, stainless steel, and silver-plated nickel. Each fitting configuration (size/seal material) was subjected to two consecutive cryogenic thermal cycles/measurement tests, followed by a launch vibration test profile at ambient temperature, and then two additional cryogenic thermal cycles/measurement tests. The design and development of the test apparatus, and test data are presented and discussed in detail.

G J Tamasy↗

ENVIRONMENTAL DEGRADATION OF HARD AND SOFT MAGNETIC MATERIALS IN GASEOUS AND SUPERCRITICAL CO2 ENVIRONMENTS

It may be beneficial to use hermetic designs for supercritical CO2 (sCO2) cycles machinery as they would eliminate CO2 leakage through shaft end seals. This would reduce CO2 emissions and operating costs for makeup of lost process fluid. Those designs may replace traditional oil-lubricated bearings with actively controlled magnetic bearings operating at high temperatures in the process fluid environment (to reduce the need for active cooling). This paper investigates the material degradation of various types of magnets in CO2. Included are several permanent and soft magnetic materials (Alnico 9C, Alnico 5-7C, and 18-T550 grade SmCo, and Hiperco 50) with or without coatings (nickel plating or C5 coating). The materials were exposed to: (1) flowing gaseous CO2 at 1,022 °F (550 °C) and atmospheric pressure in a furnace and (2) sCO2 at 842 °F (450 °C) and 1,500 psi (103 bar) in an autoclave. The preliminary mass change measured after total exposures of 1,000 hours and 2,000 hours are included.

supercritical CO2, magnetic material↗

Improved black nickel coatings for flat plate solar collectors

A new black nickel formula was developed which had a solar absorptance of 0.92 and an infrared emittance (at 100 C) of less than 0.10 after 14 days at 38 C and 95 percent relative humidity. The electroplating bath and conditions were changed to obtain the more stable coating configuration. The effect of bath composition, temperature, pH, and plating current density and time on the coating composition, optical properties and durability were investigated.

Lin, J. H.↗