Comprehensive study of the conditions for obtaining hydrogenated amorphous erbium- and oxygen-doped silicon suboxide films, a-SiO{sub x}:H Left-Pointing-Angle-Bracket Er,O Right-Pointing-Angle-Bracket , by dc-magnetron deposition
The results of a comprehensive study of the conditions for growing a-SiO{sub x}:H Left-Pointing-Angle-Bracket Er,O Right-Pointing-Angle-Bracket films are presented. The effect of the composition of various erbium-containing targets (a-SiO{sub x}:H , ErO{sub x}, Er{sub 2}SiO{sub 5}, Er{sub 2}O{sub 3}, and Er), substrate temperature, and annealing temperatures in argon, air, and under conditions of SiH{sub 4} + Ar + O{sub 2} plasma glow is studied. In order to obtain a-SiO{sub x}:H Left-Pointing-Angle-Bracket Er,O Right-Pointing-Angle-Bracket films with the highest photoluminescence intensity of erbium ions, it is recommended for the following technological conditions to be used: the substrate holder should be insulated from dc-magnetron electrodes and the working gas mixture should include silane, argon, and oxygen. Single-crystal silicon and metal erbium should be used as targets. The erbium target should be placed only in the Si-target erosion zone.