Search NASA⌕ Search

SEARCH · Search NASA

Results for “silicate glass”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Nondestructive monitoring damage in composites using scanning laser acoustic microscopy

Several Nicalon fiber reinforced LAS (lithium alumino-silicate) glass matrix composites were tested to study the relation between the residual strength and the different amounts of damage. The samples were fatigued by four-point cyclic loading at a 5 Hz rate at 500 C for a different number of cycles. 10 MHz scanning laser acoustic microscope (SLAM) images were taken to monitor damage on the samples. Our SLAM results indicate that there were defects already existing throughout the sample before fatigue, and the resultant damage pattern from fatigue could be related to the initial defect distribution in the sample. Finally, the fatigued samples were fractured and the residual strength data could not be explained by the cyclic fatigue alone. Rather, the damage patterns evident in the SLAM images were needed to explain the scatter in the data. The results show that SLAM is useful in nondestructively monitoring damage and estimating residual strength of fatigued ceramic composites.

Wey, A. C.↗

Second Annual Research Center for Optical Physics (RCOP) Forum

The Research Center for Optical Physics (RCOP) held its Second Annual Forum on September 23-24, 1994. The forum consisted of two days of technical sessions with invited talks, submitted talks, and a student poster session. Participants in the technical sessions included students and researchers from CCNY/CUNY, Fisk University, Georgia Institute of Technology, Hampton University, University of Maryland, the Univeristy of Michigan, NASA Langley Research Center, North Caroline A and T University, Steven's Institute of Technology, and NAWC-Warminster. Topics included chaotic lasers, pumped optical filters, nonlinear responses in polythiophene and thiophene based thin films, crystal growth and spectroscopy, laser-induced photochromic centers, raman scattering in phorphyrin, superradiance, doped fluoride crystals, luminescence of terbium in silicate glass, and radiative and nonradiative transitions in rare-earth ions.

Allario, Frank↗

Hot Hydrogen Exposure Degradation of the Strength of Mullite

This study deals with the corrosion of near stoichiometric mullite (3Al2O3-2SiO2) by pure dry hydrogen gas. Exposure of the mullite samples was at temperatures of 1050 and 1250 C for times up to 500 hours. Preferential attack of the alumino-silicate glass present in the grain boundaries of the mullite occurred after 125 hours at 1250 C. Hydrogen scrubbing of the SiO2 from the glassy grain boundaries and the mullite grains yielded a porous alumina-rich surface. The room temperature strength increased after short exposure times at 1250 C (up to 125 hours), then decreased by 53 percent after exposure for 500 hours. At 1050 C, all exposure times (25 to 500 hours) decreased the strength. After 500 hours in hydrogen at 1050 C, the room temperature strength of mullite decreased 22 percent. We also observed a rapid 25 percent strength loss after short exposure times at 1050 C. This is attributed to the calcium/hydrogen assisted crystallization of the glassy, grain-boundary phase.

Herbell, Thomas P.↗

Trace element and isotope studies in oxide/phosphate/silicate inclusions of iron meteorites

Under the above grant research was funded in the following areas: 1. Pallasites: Rare earth element measurements in phosphates to determine if all pallasites fit into only two trace element groups. This work has been completed. 2. HIAB irons: To complete work on the only known silicate inclusion in a IIIAB iron meteorite. This work has been completed. 3. IIIAB irons: To continue the search for Cr-53 excesses in IIIAB iron meteorite phosphates. A part of this work has been completed 4. IIIAB irons: To complete the identification of the phosphate minerals in IIIAB iron meteorites and try to determine the phase relations and chemical history of trace element distributions during the core formation process. Work on this has been largely completed and preliminary results have been reported. The final work is being assessed prior to preparation of a manuscript for publication. 5. IIE irons: To complete work on the unique silicate assemblage in the IIE iron meteorite. Work on this was completed and a paper published. 6. Ungrouped irons: A partially devitrified silicate glass inclusion has been found in the ungrouped iron meteorite. Preliminary work on this has been reported. All the work on this has been now completed and a manuscript has been prepared and submitted for publication.

Olsen, Edward J.↗

Coupling, Q-Factor, and Integration Aspects of Microsphere Applications

With suggested applications varying from microlaser and cavity QED through optical locking of diode lasers to modulators and sensors, high-Q silica microspheres with whispering-gallery (WG) modes so far remain the subject of tabletop feasibility demonstrations. Despite the uniquely high quality-factor and submillimeter dimensions suitable for tight packaging, this novel type of high-finesse cavity still has to be adapted to fiber- and integrated-optic hardware. In the visible and near infrared-band experiments (633-850nm) measuring the ringdown time tau of free oscillations, Q = (0.6 to 0.8 ) x 10(exp 10) has been obtained in silica spheres of diameter -800 microns (corresponding tau = 3 to 4 microseconds). It was proved that under normal laboratory conditions, quality-factor is subject to deterioration within several-minute scale down to (2 ... 3 ) x 10(exp 9). The responsible mechanism was identified as adsorption of a monolayer of atmospheric water, so that preservation of the ultimate Q requires manipulation in dry environment, or fast packaging into sealed devices. Larger Q can be expected closer to minimum of attenuation in fused silica alpha = 0.2 dB/km; Q greater than or equal to 1 x 10(exp 11) at lambda=1.55 microns, with corresponding energy storage time tau approx. 0.1ms. Experiments are currently underway to determine whether this high Q can be realized experimentally. The evident difficulty is that OH-related optical absorption has its peaks located near the reported minimum of attenuation in silica. We can also mention here that some of proposed fiber materials, yet not ready for fiber drawing, have been predicted to have smaller attenuation than fused silica and may be suitable for microsphere fabrication (sodium-magnesium silicate glass, alpha = 0.06dB/km). WG modes possess very small radiative loss (it does not prevent Q-10(exp 20) and more) and therefore are electromagnetically isolated and cannot be excited by free-space beams. If no modification (such as grating) is made on the sphere surface, the coupling has to he provided by an appropriate near-field device. A systematic theoretical approach has been recently developed to quantify the performance of near-field couplers for WG modes. Efficient coupling can be obtained upon fulfillment of two main conditions: (1) mode matching and (2) sufficient coupling strength to provide the buildup of a WG mode with a given intrinsic loss. In other words, the wave in the coupler has to be phase-matched and sufficiently overlapped with the WG mode to provide enough buildup in the cavity. If the coupling efficiency is characterized by the fractional depth K(sup 2) of the resonance dip in intensity transmittance observed upon varying the frequency of the exciting wave in the coupler.

Ilchenko, V. S.↗

Fe-57 Moessbauer Spectroscopy of Fulgurites: Implications for Chemical Reduction

The high temperature (superliquidus) processing of silicates often results in very reduced products, such as Si-bearing Fe metal in type-1 chondrules and in lunar regolith agglutinates. Previous work on fulgurites (the glassy products of the lightning strike fusion of sand, soil, or rock) found silicon metal and iron-silicon alloys inside the silicate glass. The mechanism for this extreme reduction is not yet understood. In this work, we begin a Fe-57 Moessbauer spectroscopy study as well as continuing a microprobe study of several fulgurites in order to better constrain the extent and process of Fe reduction.

Sheffer, A. A.↗

Vapor Deposition and Solar Wind Implantation on Lunar Soil-Grain Surfaces as Comparable Processes

Vapor deposited patinas (VDP) on lunar soil grains consist of a thin (less than 1 micron) layer of amorphous silicate (glass) embedded with nanoscale Fe(sup 0) globules as seen in many TEM images. VDPs are also present on larger space-weathered lunar rocks; these larger samples will not be discussed here although the process of vapor deposition is common to exposed grains of all sizes. Whether or not the majority of the Fe(sup 0) globules present in lunar soils reside in vapor deposited patina is a matter of some concern. Some Fe(sup 0) globules are clearly seen to reside within the glass of agglutinates and might represent remobilized Fe(sup 0) in agglutinitic melts. remobilized Fe(sup 0) in agglutinitic melts. We argue that because VDP coatings are present only on the surfaces of lunar soil grains, their distribution as a surface correlated component (SCC) of lunar soils should parallel those of Solar Wind Elements (SWE) implanted in the outermost rinds of lunar soil grains. SWE residing in the interior of soils grains make up the volume correlated component (VCC). Relative to Fe(sup 0) in VDP, the distribution of various SWE have been studied well. The reason is understandable because instrumentation for nanoscale imaging is not ubiquitous. In this study we use the distribution of SWE in lunar soils as a guide to understanding the fate of Fe(sup 0) in VDP.

Basu, A.↗

Diffusion Bonding of Silicon Carbide for a Micro-Electro-Mechanical Systems Lean Direct Injector

Robust approaches for joining silicon carbide (SiC) to silicon carbide sub-elements have been developed for a micro-electro-mechanical systems lean direct injector (MEMS LDI) application. The objective is to join SiC sub-elements to form a leak-free injector that has complex internal passages for the flow and mixing of fuel and air. Previous bonding technology relied upon silicate glass interlayers that were not uniform or leak free. In a newly developed joining approach, titanium foils and physically vapor deposited titanium coatings were used to form diffusion bonds between SiC materials during hot pressing. Microscopy results show the formation of well adhered diffusion bonds. Initial tests show that the bond strength is much higher than required for the component system. Benefits of the joining technology are fabrication of leak free joints with high temperature and mechanical capability.

Halbig, Michael C.↗

Metallic Concepts for Repair of Reinforced Carbon-Carbon Space Shuttle Leading Edges

The Columbia accident has focused attention on the critical need for on-orbit repair concepts for wing leading edges in the event that potentially catastrophic damage is incurred during Space Shuttle Orbiter flight. The leading edge of the space shuttle wings consists of a series of eleven panels on each side of the orbiter. These panels are fabricated from reinforced carbon-carbon (RCC) which is a light weight composite with attractive strength at very high temperatures. The damage that was responsible for the loss of the Colombia space shuttle was deemed due to formation of a large hole in one these RCC leading edge panels produced by the impact of a large piece of foam. However, even small cracks in the RCC are considered as potentially catastrophic because of the high temperature re-entry environment. After the Columbia accident, NASA has explored various means to perform on-orbit repairs in the event that damage is sustained in future shuttle flights. Although large areas of damage, such as that which doomed Columbia, are not anticipated to re-occur due to various improvements to the shuttle, especially the foam attachment, NASA has also explored various options for both small and large area repair. This paper reports one large area repair concept referred to as the "metallic over-wrap." Environmental conditions during re-entry of the orbiter impose extreme requirements on the RCC leading edges as well as on any repair concepts. These requirements include temperatures up to 3000 F (1650 C) for up to 15 minutes in the presence of an extremely oxidizing plasma environment. Figure 1 shows the temperature profile across one panel (#9) which is subject to the highest temperatures during re-entry. Although the RCC possesses adequate mechanical strength at these temperatures, it lacks oxidation resistance. Oxidation protection is afforded by converting the outer layers of the RCC to SiC by chemical vapor deposition (CVD). At high temperatures in an oxidizing environment, the SiC layer forms a protective SiO2 scale. However, CVD processing to form the SiC layer can result in the formation of small cracks in the outer surface. Hence, as a final fabrication step, a sodium silicate glass, known as "Type A," is applied as a sealant to fill any surface porosity and/or cracks in the coating and the outer portions of the RCC[1]. At relatively low temperatures, the Type A glass melts and flows into the cracks providing oxidation protection at the higher temperatures. In addition, the Type A coating, provides a "dark" coating with a high emissivity. This high emissivity allows the RCC to transfer heat by radiating outward to space as well as dispersing heat within the leading edge cavity. Lastly, the Type A possesses low catalycity which reduces surface temperatures by limiting oxygen recombination on the surface during re-entry.

Ritzert, Frank↗

Coated silicon comprising material for protection against environmental corrosion

In accordance with an embodiment of the invention, an article is disclosed. The article comprises a gas turbine engine component substrate comprising a silicon material; and an environmental barrier coating overlying the substrate, wherein the environmental barrier coating comprises cerium oxide, and the cerium oxide reduces formation of silicate glass on the substrate upon exposure to corrodant sulfates.

Hazel, Brian Thomas↗

The Strata-l Experiment on Microgravity Regolith Segregation

The Strata-1 experiment studies the segregation of small-body regolith through long-duration exposure of simulant materials to the microgravity environment on the International Space Station (ISS). Many asteroids feature low bulk densities, which implies high values of porosity and a mechanical structure composed of loosely bound particles, (i.e. the "rubble pile" model), a prime example of a granular medium. Even the higher-density, mechanically coherent asteroids feature a significant surface layer of loose regolith. These bodies will evolve in response to very small perturbations such as micrometeoroid impacts, planetary flybys, and the YORP effect. A detailed understanding of asteroid mechanical evolution is needed in order to predict the surface characteristics of as-of-yet unvisited bodies, to understand the larger context of samples from sample return missions, and to mitigate risks for both manned and unmanned missions to asteroidal bodies. Due to observation of rocky regions on asteorids such as Eros and Itokawa, it has been hypothesized that grain size distribution with depth on an asteroid may be inhomogeneous: specifically, that large boulders have been mobilized to the surface. In terrestrial environments, this size-dependent sorting to the surface of the sample is called the Brazil Nut Effect. The microgravity and acceleration environment on the ISS is similar that of a small asteroid. Thus, Strata-1 investigates size segregation of regolith in an environment analogous to that of small bodies. Strata-1 consists of four regolith simulants in evacuated tubes, as shown in Figure 1 (Top and Middle). The simulants are (1) a crushed and sieved ordinary chondrite meteorite to simulate an asteroidal surface, (2) a carbonaceous chondrite simulant with a mixture of fine and course particles, and two simplified silicate glass simulants; (3) one with angular and (4) another with spherical particles. These materials were chosen to span a range of granular complexity. The materials were sorted into three size species pre-launch, and maintained during launch and return by a device called the Entrapulator. The hypothesis under test is that the particles that constitute a granular medium in a micro-gravity environment, subjected to a known vibration environemnt, will segregate in accordance to modeled predictions. Strata-1 is currently operating on ISS, with cameras capturing images of simulant motion throughout the one year mission. Vibration data is recorded and downlinked, and the simulants will be analyzed after return to Earth.

Fries, M.↗

A Fiber-Coupled Erbium-Doped Microsphere Laser

We report a demonstration of an erbium-doped silicate glass microsphere laser with both pumping (at~980nm) and the pickup of laser output (~1550nm) provided by novel angle-polished singel-mode fiber coupler.

microsphere↗

C-O-H ratios of silicate melt inclusions in basalts from the Galapagos Spreading Center near 95 degrees W: a laser decrepitation mass spectrometry study

Volatile ratios (primarily of H2O and CO2) in individual silicate melt (glass) inclusions in minerals have been analyzed using laser volatilization and mass spectrometry. A Nd-glass laser was used to produce 50-micrometer diameter pits in silicate melt inclusions. Released volatiles were analyzed directly with a computer-controlled quadrupole mass spectrometer. The detection limits for CO2 and H2O were on the order of 3 x 10(-14) and 3 x 10(-13) moles, respectively. The reproducibility for CO2/H2O was better than +/- 9%. The total range of volatile ratios from vitreous silicate glass inclusions contained in a suite of Galapagos lavas were: 0.018 to 1.193 for CO2/H2O; 0.002 to 0.758 for CO/H2O; 0 to 0.454 for CH4/H2O; and 0 to 0.432 for Ar/H2O. The mean CO2/H2O from the propagating rift (0.245 +/- 0.068) silicate glass inclusions is significantly lower than that of the actively failing rift (0.641 +/- 0.241); this difference probably reflects different degrees of degassing during magmatic histories for the two regions. Relatively undifferentiated failing rift magmas must have relatively short crustal residence times prior to eruption and, therefore, have not undergone significant degassing of CO2, as would appear to be the case for the more highly fractionated propagating rift magmas. The laser-mass spectrometric system described herein has the ability to act as a point-source probing device that can differentiate between the various volatile sites in minerals and rocks (as well as synthetic materials) on a micrometer scale.

NASA Discipline Exobiology↗

Absorption and fluorescence of alexandrite and of titanium in sapphire and glass

The fluorescence and absorption data for titanium in crystalline sapphire and titanium doped into two silicate and one phosphate glass structures are analyzed. It is observed that the Ti-doped silicate glass sample exhibits no absorption related to the Ti(III) ion, the Ti-doped phosphate glass is deep blue, the absorption line width of the glass samples are a factor of two larger than that of sapphire, and the absorption peak for the Ti in the glass shifted about 100 nm to the red from the Ti:sapphire absorption peak. This shift reveals that the Ti(III) ion is sensitive to the crystalline environment and not to the glass environment. The photoluminescence spectra for Ti-doped sapphire and alexandrite are compared. It is detected that the Ti:sapphire exhibits a broader spectrum than that for alexandrite with a peak at 750 nm. The three zero phonon transitions of Ti:Al2O3 at liquid nitrogen temperatures are studied.

Byvik, C. E.↗

Internal strain analysis of ceramics using scanning laser acoustic microscopy

Quantitative studies of material behavior characteristics are essential for predicting the functionality of a material under its operating conditions. A nonintrusive methodology for measuring the in situ strain of small dimeter (to 11 microns) ceramic fibers under uniaxial tensile loading and the local internal strains of ceramics and ceramic composites under flexural loading is introduced. The strain measurements and experimentally observed mechanical behavior are analyzed in terms of the microstructural development and fracture behavior of each test specimen evaluated. Measurement and analysis of Nicalon silicon carbide (SiC) fiber (15 microns diameter) indicate that the mean elastic modulus of the individual fiber is 185.3 GPa. Deviations observed in the experimentally determined elastic modulus values between specimens were attributed to microstructural variations which occur during processing. Corresponding variations in the fracture surface morphology were also observed. The observed local mechanical behavior of a lithium alumino-silicate (LAS) glass ceramic, a LAS/SiC monofilament composite, and a calcium alumino-silicate (CAS)/SiC fully reinforced composite exhibits nonlinearities and apparent hysteresis due to the subcritical mechanical loading. Local hysteresis in the LAS matrices coincided with the occurrence of multiple fracture initiation sites, localized microcracking, and secondary cracking. The observed microcracking phenomenon was attributed to stress relaxation of residual stresses developed during processing, and local interaction of the crack front with the microstructure. The relaxation strain and stress predicted on apparent mechanical hysteresis effects were defined and correlated with the magnitude of the measured fracture stress for each specimen studied. This quantitative correlation indicated a repeatable measure of the stress at which matrix microcracking occurred for stress relief of each material system. Stress relaxation occurred prior to the onset of steady state cracking conditions. The relaxation stress occurred at 18.5 percent of the fracture stress in LAS and 11.0 percent of the yield stress in CAS/SiC. The relaxation stress ratio was dependent upon the dominant fracture mode of the LAS/SiC specimens. Relaxation stress ratios greater than 0.30 were observed for specimens which fractured due to shear at the fiber matrix interface; specimens which fracture due to tensile cracking had relaxation stress ratios less than 0.30. The stress relaxation ratio appeared to be a specific characteristic of the glass ceramic material. The measured stress relaxation for LAS indicated a measure of the inherent residual stresses in the material due to processing and suggested localized toughening mechanisms for brittle material structures.

Kent, Renee M.↗

Ceramic fiber-reinforced monoclinic celsian phase glass-ceramic matrix composite material

A hyridopolysilazane-derived ceramic fiber reinforced monoclinic celsian phase barium aluminum silicate glass-ceramic matrix composite material is prepared by ball-milling an aqueous slurry of BAS glass powder and fine monoclinic celsian seeds. The fibers improve the mechanical strength and fracture toughness and with the matrix provide superior dielectric properties.

Bansal, Narottam P.↗

An electromotive force series in a borosilicate glass-forming melt

An electromotive force series for redox couples was defined as a function of oxygen fugacity in a borosilicate melt at 1150 C. The resulting order of relative reduction potentials can be used to estimate the amounts of redox species in glass during processing. The electromotive force series in this melt is comparable to those in other silicate glass-forming melts and in aqueous systems but differs in detail because of interaction of the solvents with individual redox couples.

Schreiber, H. D.↗

Shock induced reaction in Chicxulub target materials (CaSO4 and SiO2) and their relation to extinctions

The global platinum element rich layer, the presence of shocked quartz grains (in some cases with stishovite), and the observation of a tektite-rich layer, precisely at the K-T boundary, are the three major arguments for the extinction bolide impact hypothesis of Alvarez et al. Tektites (spherules) from Beloc in Haiti and Mimbral in Mexico received particular interest because of their geological proximity to the Chicxulub impact structure, which is a leading candidate for at least one of the K-T impact craters. Although in most localities the original glass has weathered to clay minerals, some shock-induced glass is found in outcrops and drill cores which is used for Ar-38/Ar-39 dating. The glassy tektites were found to be chemically similar and coeval at 65.0 Ma with Chicxulub melt rock. Two kinds of K-T spherules were discovered: (1) a silic black glass; and (2) a yellow glass, enriched in Ca, Mg, and S. The high sulfur content of the glass and the abundance of anhydrite (CaSO4) in the carbonate-evaporite sequence observed in Drill Holes Y-1 and Y-2 at Chicxulub prompted studies of calcium sulfate devolatization. Further discussion of our experiments is presented.

Chen, Guangqing↗