At least 109 records · Page 6

Role of cobalt in nickel base superalloys

The effect of cobalt or substituting for cobalt on the mechanical properties of nickel-based superalloys is discussed. Waspaloy, UDIMET 700, and NIMONIC 115, which are representative of Ni-Cr-Co-Al-Ti-Mo superalloys having different gamma prime contents which are strengthened by a heavily alloyed matrix, coherent gamma prime precipitates, and carbides at the grain boundaries. Microstructure and in situ and extracted phase STEM micro-analysis were used to evaluate the three alloys.

Jarrett, R.↗

Reduction of chromium in Ni-base superalloys through element substitution and rapid solidification processing

The reduction in the use of Cr in Ni base superalloys by the combined approaches of both elemental substitution and rapid solidification processing is studied. The elements Si, Zr, Y and Hf were chosen as potential partial substitutes for Cr in Waspaloy and IN 713LC sine their separate addition to other alloys has previously resulted in enhanced oxidation resistance. The roles of Cr and these replacement elements in determining the microstructure and properties are evaluated. The elements Si, Zr, and Y and Hf are used as partial replacements for Cr in the base superalloys and these resultant alloys are processed using rapid solidification techniques. The mechanical properties and oxidation resistance of the processed materials are evaluated. The microstructure is characterized using state of the art techniques (e.g. analytical transmission electron microscopy), and the mechanism by which these structures are produced is determined.

Fraser, H. D.↗

Effects of cobalt in nickel-base superalloys

A study has been carried out to assess the role of cobalt in Udimet 700, a representative nickel-base superalloy containing 17 percent or more cobalt. The study spans the spectrum of microstructural, microchemical, and mechanical behavior aspects which together form a basis for superalloy performance in jet engines. The results suggest that cobalt affects the solubility of elements in the gamma matrix, which leads to enhanced gamma-prime volume fraction and to the stabilization of MC-type carbides and sigma phase. However, these microstructural and microchemical changes are too slight to significantly affect the strength and ductile properties. Depending on the heat treatment, the creep and stress rupture resistance can be cobalt-sensitive. In the coarse-grained, fully solutioned and aged condition, all of the alloy's 17 percent Co can be replaced by nickel without decreasing the creep and stress rupture resistance. These findings are discussed with reference to existing theories and experimental data obtained by other workers.

Tien, J. K.↗

Replacing critical and strategic refractory metal elements in nickel-base superalloys

Because of the import status and essential nature of their use, cobalt, chromium, tantalum, and niobium were identified as strategic and critical in the aerospace industry. NASA's Conservation of Strategic Aerospace Materials (COSAM) program aims to reduce the need for strategic materials used in gas turbine engines. Technological thrusts in two major areas are under way to meet the primary objective of conserving the use of strategic materials in nickelbase superalloys. These thrusts consist of strategic element substitution and alternative material identification. The program emphasizes cooperative research teams involving NASA Lewis Research Center, universities, and industry. The adoption of refractory metals in nickel-base superalloys is summarized including their roles in mechanical strengthening and environmental resistance; current research activities under way in the COSAM Program are presented as well as research findings to date.

Stephens, J. R.↗

Effects of cobalt in nickel-base superalloys

The role of cobalt in a representative wrought nickel-base superalloy was determined. The results show cobalt affecting the solubility of elements in the gamma matrix, resulting in enhanced gamma' volume fraction, in the stabilization of MC-type carbides, and in the stabilization of sigma phase. In the particular alloy studied, these microstructural and microchemistry changes are insufficient in extent to impact on tensile strength, yield strength, and in the ductilities. Depending on the heat treatment, creep and stress rupture resistance can be cobalt sensitive. In the coarse grain, fully solutioned and aged condition, all of the alloy's 17% cobalt can be replaced by nickel without deleteriously affecting this resistance. In the fine grain, partially solutioned and aged condition, this resistance is deleteriously affected only when one-half or more of the initial cobalt content is removed. The structure and property results are discussed with respect to existing theories and with respect to other recent and earlier findings on the impact of cobalt, if any, on the performance of nickel-base superalloys.

Tien, J. K.↗

Understanding the roles of the strategic element cobalt in nickel base superalloys

Research progress in understanding the effects of cobalt and some possible substitute on microstructure, mechanical properties, and environmental resistance of turbine alloys is discussed. The United States imports over 90 percent of its cobalt, chromium, tantalum and columbium, all key elements in high temperature nickel base superalloys for aircraft gas turbine disks and airfoils. NASA, through joint government/industry/university teams, undertook a long range research program aimed at reducing or eliminating these strategic elements by examining their basic roles in superalloys and identifying viable substitutes.

Stephens, J. B.↗

Effects of processing and microstructure on the fatigue behaviour of the nickel-base superalloy Rene95

Forms of the nickel-base superalloy Rene95 produced by three processing methods were evaluated in tensile, low cycle fatigue and fatigue crack propagation tests at 540 and 650 C. Two powder-metallurgy (PM) forms, hot-isostatically-pressed and extruded-and-forged, and a conventionally cast-and-wrought form were all given the same heat treatment. The extruded-and-forged form showed superior fatigue life in low strain range tests though the two PM forms exhibited nearly identical mechanical behavior in all other respects. Further, this life difference could not be explained by significant differences in the types, sizes or shapes of the defects initiating failure. The cast-and-wrought Rene95, however, had lower strength, ductility and fatigue life, but higher fatigue crack propagation resistance because of a larger grain size. It did not exhibit the environmentally-assisted intergranular mode of propagation which occurs in PM Rene95 and other fine-grained superalloys at these test temperatures and frequencies.

Miner, R. V.↗

Orientation and temperature dependence of some mechanical properties of the single-crystal nickel-base superalloy Rene N4. 3: Tension-compression anisotropy

Single crystal superalloy specimens with various crystallographic directions along their axes were tested in compression at room temperature, 650, 760, 870, and 980 deg C. These results are compared with the tensile behavior studied previously. The alloy, Rene N4, was developed for gas turbine engine blades and has the nominal composition 3.7 Al, 4.2 Ti, 4 Ta, 0.5 Nb, 6 W, 1.5 Mo 9 Cr. 7.5 Co, balance Ni, in weight percent. Slip trace analysis showed that primary cube slip occurred even at room temperature for the 111 specimens. With increasing test temperature more orientations exhibited primary cube slip, until at 870 deg C only the 100 and 011 specimens exhibited normal octahedral slip. The yield strength for octahedral slip was numerically analysed using a model proposed by Lall, Chin, and Pope to explain deviations from Schmid's Law in the yielding behavior of a single phase Gamma prime alloy, Ni3(Al, Nb). The Schmid's Law deviations in Rene N4 were found to be largely due to a tension-compression anisotropy. A second effect, which increases trength for orientations away from 001, was found to be small in Rene N4. Analysis of recently published data on the single crystal superalloy PWA 1480 yielded the same result.

Miner, R. V.↗

Design overview of fiber-reinforced superalloy composites for the Space Shuttle main engine

This preliminary design study evaluated the potential of fiber-reinforced superalloys (FRS) for hot-section components of Space Shuttle Main Engine turbopumps. Emphasis was placed on uncooled turbine blades, with a more limited evaluation of FRS turbine stator vanes. The study included FRS properties evaluation, current structural design capability, and preliminary design and structural analysis. In addition, key technology needs were identified, and a plan was generated to develop operational hardware for advanced versions of the SSME. Based on projections of design properties for FRS composites comprising 50 volume percent of W-4Re-0.38Hf-0.02C wire filaments in a ductile superalloy matrix, it was concluded that FRS turbine blades offer the potential of significant improved operating life and higher temperature capability over the MAR-M-246(Hf) (DS) blades currently used in the SSME.

Lewis, J. R.↗

On the fatigue crack propagation behavior of superalloys at intermediate temperatures

Two superalloys used in gas-turbine disks, Rene 95 and IN-100 were tested in several forms at 0.33 Hz in air, and the results were compared with earlier data on Astroloy to gain a better understanding of the effects of grain size, strength, and alloy composition on the fatigue crack propagation behavior. In addition, selected forms of Rene 95 were tested at 0.33 Hz in vacuum and in air using a cycle with a 120-sec tensile dwell to evaluate the effects of environment and creep. Results of the study emphasize the beneficial effect of large grain size on the fatigue and crep-fatigue crack growth resistance of the superalloys in the temperature range corresponding to the operating temperatures of aircraft gas-turbine engine disk rims.

Gayda, J.↗

Diffusion welding of MA 6000 and a conventional nickel-base superalloy

A feasibility study of diffusion welding the oxide dispersion strengthened (ODS) alloy MA 6000 to itself and to conventional Ni-base superalloy Udimet 700 was conducted. Butt joints between MA 6000 pieces and lap joints between Udimet 700 and the ODS alloy were produced by hot pressing for 1.25 hr at temperatures ranging from 1000 to 1200 C (1832-2192 F) in vacuum. Following pressing, all weldments were heat treated and machined into mechanical property test specimens. While three different combinations of recrystallized and unrecrystallized MA 6000 butt joints were produced, the unrecrystallized to unrecrystallized joint was most successful as determined by mechanical properties and microstructural examination. Failure to weld the recrystallized material probably related to a lack of adequate deformation at the weld interface. While recrystallized MA 6000 could be diffusion welded to Udimet 700 in places, complete welding over the entire lap joint was not achieved, again due to the lack of sufficient deformation at the faying surfaces. Several methods are proposed to promote the intimate contact necessary for diffusion welding MA 6000 to itself and to superalloys.

Moore, T. J.↗

Forging Oxide-Dispersion-Strengthened Superalloys

Cladding of mild steel prevents surface cracking when alloy contacts die. Continual need for improvements in properties of alloys capable of withstanding elevated temperatures. Accomplished by using oxide-dispersion-strengthed superalloys such as Inconel Alloy MA 6000. Elevated tensile properties of forged alloy equal those of hot-rolled MA 6000 bar. Stress-rupture properties somewhat lower than those of bar stock but, at 1,100 degrees C, exceed those of strongest commercial single crystal, directionally solidified and conventionally cast superalloys.

Harf, F. H.↗

Microstructure-property relationships in directionally solidified single crystal nickel-base superalloys

Some of the microstructural features which influence the creep properties of directionally solidified and single crystal nickel-base superalloys are discussed. Gamma precipitate size and morphology, gamma-gamma lattice mismatch, phase instability, alloy composition, and processing variations are among the factors considered. Recent experimental results are reviewed and related to the operative deformation mechanisms and to the corresponding mechanical properties. Special emphasis is placed on the creep behavior of single crystal superalloys at high temperatures, where directional gamma coarsening is prominent, and at lower temperatures, where gamma coarsening rates are significantly reduced. It can be seen that very subtle changes in microstructural features can have profound effects on the subsequent properties of these materials.

Mackay, R. A.↗

Impact wear of iron rich superalloys

The impact-sliding wear resistance of chill cast and aligned eutectic Fe-base superalloys against M42 and 17-4 PH steel counterface materials is examined. The aligned material tests were run with carbide fibers perpendicular to the counterface contact surface and the characterization focused on fracture processes as observed in the subsurface microstructure of the worn materials. Metallographic analyses were performed on specimens exposed to various numbers of repetitive impact load cycles, and for comparison, two other aligned composites were tested with the same fiber orientation under identical test conditions against hardened M42 tool steel. A strong improvement was found in wear resistance of an aligned eutectic structure as compared to the corresponding randomized chill cast structure. Experiments with the softer 17-4 counterface were characterized by transfer onto the Fe-base superalloy, and the cracks formed were oriented transverse to the relative sliding direction and occurred in a periodic fashion. Observations in subsurface regions of the worn materials indicated crack intergranularity with an occasional transgranular fracture of the M7C3 carbide phase.

Wayne, S. F.↗

The cyclic stress-strain behavior of a nickel-base superalloy at 650 C

It is pointed out that examinations of the monotonic tensile and fatigue behaviors of single crystal nickel-base superalloys have disclosed orientation-dependent tension-compression anisotropies and significant differences in the mechanical response of octahedral and cube slip at intermediate temperatures. An examination is conducted of the cyclic hardening response of the single crystal superalloy PWA 1480 at 650 C. In the considered case, tension-compression anisotropy is present, taking into account primarily conditions under which a single slip system is operative. Aspects of a deformation by single slip are considered along with cyclic hardening anisotropy in tension and compression. It is found that specimens deforming by octahedral slip on a single slip system have similar hardening responses in tensile and low cycle fatigue loading. Cyclic strain hardening is very low for specimens displaying single slip.

Gabb, T. P.↗

Orientation and temperature dependence of some mechanical properties of the single-crystal nickel-base superalloy Rene N4. I - Tensile behavior

Single crystal specimens of a nickel-base superalloy with axes near 001, 011, and -112 were tested in tension at room temperature, 760, and 980 C. The alloy Rene N-4, was developed for gas turbine engine blades and has the nominal composition 3.7 Al, 4.2 Ti, 4 Ta, 0.5 Nb, 6 W, 1.5 Mo, 9 Cr, 7.5 Co, balance Ni, (all in weight percent). Analysis of slip band traces, specimen axis rotation, and dislocation Burgers vectors showed that at 760 and 980 C primary cube slip supplanted normal octahedral slip for the -112 line-oriented specimens. The other two orientations, which have lower resolved shear stresses on the cube system, exhibited octahedral slip at all three temperatures. The critical resolved shear stress is considerably greater on the cube system than on the octahedral system at room temperature. However, at 760 and 980 C the critical resolved shear stresses on the two systems are about the same. While the room temperature and 980 C yield strengths for the two orientations exhibiting octahedral slip could be rationalized on the basis of resolved shear stress, those at 760 C could not. Such violations of Schmid's law have previously been observed in other superalloys and single phase gamma-prime.

Miner, R. V.↗

Bithermal Low-Cycle Fatigue Behavior of a NiCoCrAlY-Coated Single Crystal Superalloy

Specimens of a single crystal superalloy, PWA 1480, both bare and coated with a NiCoCrAlY alloy, PWA 276, were tested in low-cycle fatigue at 650 and 1050 C, and in bithermal thermomechanical fatigue tests. In the two bithermal test types, tensile strain was imposed at one of the two temperatures and reversed in compression at the other. In the high-strain regime, lives for both bithermal test types approached that for the 650 C isothermal test on an inelastic strain basis, all being controlled by the low ductility of the superalloy at 650 C. In the low-strain regime, coating cracking reduced life in the 650 C isothermal test. The bithermal test imposing tension at 650 C, termed out-of-phase, also produced rapid surface cracking, but in both coated and bare specimens. Increased crack growth rates also occurred for the out-of-phase test. Increased lives in vacuum suggested that there is a large environmental contribution to damage in the out-of-phase test due to the 1050 C exposure followed by tensile straining at the low temperature.

Gayda, J.↗

A study of microstructural characteristics of Ni-based superalloys at high temperatures

The microstructure of the Ni-based superalloy MAR-M246 (Hf) which is used in manufacturing the components of the Space Shuttle Main Engine was investigated. In the first year, the superalloy will be studied using optical photomicrographs and the differential thermal analysis. During this period, the existing experimental equipment like cutting, grinding/polishing machines, metallurgical microscope will be used to but/polish and take the photomicrographs. At present, only a 35 mm camera attachment with the olympus inverted metallurgical microscope is being used. Due to this, there was considerable delay in processing photographs. A Perkin-Elmer Differential Thermal Analyzer (DTA-1700) was ordered and finally installed on April 28, 1987. Preliminary test runs were made on silver as well as MAR-M246 (Hf).

Lal, R. B.↗