Search NASA⌕ Search

SEARCH · Search NASA

Results for “SINTERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,081 records · Page 60

Characterization of Al–Al{sub 4}C{sub 3} nanocomposites produced by mechanical milling

In this work, a mixture of Al–C–Al{sub 4}C{sub 3} nanopowder previously synthesized by mechanical milling and subsequent thermal treatment was used to reinforce the Al matrix. The nanocomposites were fabricated via high-energy ball milling and subsequent sintering process for different periods of time at 550 °C. Hardness and compression tests were performed to evaluate the mechanical properties of the nanocomposites in the as-milled and sintered conditions. According to the results the reinforcement located in the grain boundaries is responsible for the brittle behavior observed in the nanocomposites during the compression test. The combined effect of sintering and precipitation mechanisms produced an evident increase of the strength of the Al matrix at a relatively short sintering time. By using the Rietveld method the crystallite size and microstrain measurements were determined and correlated with the microhardness values. For the proper characterization of the nanoparticles present in the Al matrix, atomic force microscopy and high resolution electron microscopy were used. - Highlights: • Nanostructured Al{sub 4}C{sub 3} reinforcement was fabricated via mechanical milling and heat treatment. • We found a significant increase of the mechanical properties at short sintering times. • The formation of Al{sub 4}C{sub 3} with during sintering time restricted the excessive growth of the crystallite. • Al{sub 4}C{sub 3} located in the grain boundaries causes brittle fracture observed in compression tests. • There is a correlation between, crystallite size and microstrain values with microhardness.

36 MATERIALS SCIENCE↗

Interfacial characterization in carbon nanotube reinforced aluminum matrix composites

In this work, the effects of the sintering parameters, such as temperature and the techniques used (HP and SPS), on CNT/Al composite interfaces are studied. The major role of the native aluminum oxide (Al{sub 2}O{sub 3}) layer covering the aluminum grains is highlighted. It is shown that, for a sintering temperature below 620 °C, the amorphous Al{sub 2}O{sub 3} layer prevents the reaction between aluminum and carbon. For greater sintering temperatures, the breaking of the oxide layer due to its crystallization leads to the formation of aluminum carbide (Al{sub 4}C{sub 3}) by reaction between aluminum and the CNT. The Al{sub 4}C{sub 3} crystals grow perpendicularly to the matrix grain boundaries by thermally activated diffusion of the carbon atoms coming from the CNT. It is also demonstrated that, by limiting the sintering time, which is the case in SPS, it is possible to limit the growth of the Al{sub 4}C{sub 3} crystals and thus to preserve the CNT. - Highlights: • The high reactivity between CNT and Al matrix, resulting Al{sub 4}C{sub 3} formation during the sintering process is highlighted. • We demonstrate, thanks to in-situ TEM observations, that Al{sub 4}C{sub 3} crystals grow into aluminum grains by carbon diffusion. • The native aluminum oxide around the aluminum particles prevents the diffusion of carbon into the aluminum grains. • We show that the protective layer can be broken because of its crystallization, leading to the formation of Al{sub 4}C{sub 3}. • SPS, by limiting the sintering duration, is an interesting way for preparing CNT/Al composites without carbide formation.

36 MATERIALS SCIENCE↗

Chromium segregation at phase boundaries in Cr-doped WC-Co cemented carbides

Highlights: • Experimental evidence of a mixed (W,Cr) carbide layer on WC grain surfaces • Evidence of Cr segregation in the Co-rich binder phase in front of WC grain surfaces • Temperature dependent equilibrium segregation of Cr estimated from atom probe data • Experimental observations supported by predictions from thermodynamic modelling - Abstract: Atom probe tomography has shown (Cr,W)C to be present as a thin WC grain surface layer in an as-sintered Cr-doped WC-Co cemented carbide microstructure slowly cooled from the sintering temperature. The Co-rich binder phase contained a segregation of Cr in front of this surface layer. The mixed carbide layer was not observed when the as-sintered material had been heat treated at 1000 °C for 3000 s and then quickly cooled. A reduced amount of segregated Cr was, however, still present in the binder phase in front of the WC grain surface. These observations are supported by predictions from thermodynamic modelling; (Cr,W)C becomes stable at temperatures below 940 °C in the absence of other secondary carbides. The equilibrium segregation of Cr in the binder phase was estimated to 0.8 and 0.4 monolayer in the as-sintered and heat treated materials, respectively. The energy of segregation was calculated to 0.22 eV/Cr atom from the atom probe data. This value would result in a Cr segregation of 0.3 monolayer at the sintering temperature 1410 °C, provided that the energy of segregation in the Co-rich liquid phase sintering medium is the same as in the Co-rich binder phase. This Cr segregation may explain the WC grain growth inhibiting effect of Cr additions to WC-Co cemented carbide materials.

36 MATERIALS SCIENCE↗

Improvement microstructural and damage characterization of ceramic composites Y{sub 2}O{sub 3} – V{sub 2}O{sub 5} with MgO nano particles

Compacted samples of Y{sub 2}O{sub 3}-V{sub 2}O{sub 5} – MgO Nano – particles wt. % sintered at different sintering temperature (700, 900, 1100, 1300) ) C° for 2 hours under static air were investigated by x-ray diffraction and differential thermal analysis(DTA), to identify the phase present .Microstructure examination achieved by scanning electron microscopy .Sintered density and porosity were measured for all sintered samples .Compression was tested too and the Brake down voltage and dielectric strength were measure for all sintered samples .The clear improvement were noticed in both microstructure and damage characterization respectively after existing the MgO Nano-particles, by increasing in about 30% in sintered density and 25% for the compressive strength .The improvement also noticed on both brake down voltage and dielectric strength.

36 MATERIALS SCIENCE↗

Effect of thermal treatments on electrochemical behavior of binder jetted 17-4 PH stainless steel

Binder jetted 17–4 PH stainless steel was post-processed to relate heat treatment, microstructure, and corrosion in 3.5 wt% NaCl. Specimens were sintered at 1380 or 1400 °C, solution-annealed at 1055 °C for 1 h, and aged at 482 °C for 1 h. Here, as-sintered parts showed α′-martensitic matrix with a δ-ferrite network and Cu-rich precipitates in ferrite; inclusions (MnS, NbC) promoted localized attack. solutionizing redistributed elements and reduced ferrite, while aging generated coherent Cu nano-precipitates. Corrosion resistance was highly sensitive to post-processing in which aged specimens exhibited the lowest corrosion current density and formed a thicker, stable Cr 2 O 3 -rich passive film, whereas sintered specimens degraded most. Pitting potential depended on sintering temperature and microstructure, with 1400 °C sintering yielding more positive pitting potentials and the best overall performance after aging. Although the 1400-solutionized condition showed a relatively noble pitting response versus 1380-solutionized, it displayed unstable corrosion kinetics attributed to an imperfect passive film linked to higher NbC density. XPS depth profiles corroborated these trends, showing thicker, more continuous Cr 2 O 3 in aged states and discontinuous/thinning oxides in less resistant conditions. Practically, high-temperature sintering (∼1400 °C) followed by solutionizing and aging is recommended, with further gains expected from reducing NbC/MnS populations and porosity via powder and process control.

36 MATERIALS SCIENCE↗

Development of direct ink write radially graded alumina/zirconia

Functionally graded materials (FGMs) are of interest in multiple fields, yet many materials combinations are limited by coefficient of thermal expansion (CTE) mismatch. Here, a radially graded alumina/yttria-doped zirconia (Al 2 O 3 /8YZ) FGM is used to demonstrate processing strategies to mitigate CTE and sintering behavior differences between these oxides. FGM materials are especially sensitive to ink stability during printing, as all components (in this case, Al 2 O 3 and 8YZ) must be stabilized in the same dispersant or additive solution. Thus, this system is also ideal to demonstrate ink optimization best practices. Materials were characterized throughout processing to correlate the effects of common additives on both the ceramic particle suspensions and final sintered components. Aggregation observed in the initial additive-containing suspensions were present in the sintered component. The differences in sintering onset temperature and shrinkage rate resulted in internal stresses within the sintered component, which ultimately caused mechanical failure of the component under low stress. In conclusion, a processing strategy was recommended to mitigate the sintering behavior mismatch of alumina and 8 wt% yttria-stabilized zirconia.

Lamm, Benjamin W. [Oak Ridge National Laboratory (↗

Preparation and characterization of novel foamed porous glass-ceramics

Foamed glass-ceramics without using foaming agent have been synthesized in a novel glass system of SrO-CaO-Al{sub 2}O{sub 3}-TiO{sub 2}-B{sub 2}O{sub 3}-SiO{sub 2}-P{sub 2}O{sub 5}-M{sub x}O{sub y} (where M = Ba, Mg, La, Ce and Ni) by a simple process of powder sintering. The glass and glass-ceramics are characterized by dilatometry, differential scanning calorimetry (DSC), heating stage microscopy (HSM), X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), optical microscopy and Fourier transformed infrared spectroscopy (FTIR). All the glasses formed are amorphous and the glass transition temperature and dilatometric softening temperature of these glasses are found to be in the range 673–678 °C and 706–728 °C respectively. The glasses are highly stable as indicated by the DSC evaluated glass stability parameters of the range 195–240 °C. Quantitative sintering study of glass powder compacts revealed swelling in the samples with NiO and CeO{sub 2} corresponding to a geometry change of 75 and 108% around 900 °C respectively. With reference to this finding the glass powder compacts are heated to 900 °C and the foamed glass-ceramics are obtained. Characteristic crystalline silicate phases have been identified in the XRD studies and their microstructures are recorded by FESEM. Optical microscope study of the foamed samples revealed formation of bigger foamed cavity with residual pores in samples with NiO and CeO{sub 2} in comparison to samples with BaO, MgO and La{sub 2}O{sub 3}. The mean pore diameters of the samples with NiO and CeO{sub 2} are determined to be 43 and 32 μm, and their respective porosities are 2.34 and 1.82 cm{sup 3}/g respectively. Thus NiO and CeO{sub 2} are found to be very effective to obtain foamed glass-ceramics without using foaming agent by the viscous flow sintering of fine glass powder compacts along with the reduction of the respective polyvalent ions. - Highlights: • Synthesis of foamed porous glass-ceramics without foaming agent by sintering method • Only powder compact yielded foamed porous glass-ceramics but bulk glass did not. • Glasses containing NiO and CeO{sub 2} exhibited significant foaming efficiency. • Bloating of entrapped gas during viscous flow sintering is the origin of foaming. • Residual void created pores in the sintered glass-ceramics as evidenced in FESEM.

36 MATERIALS SCIENCE↗

Synthesis and characterization of nanocrystalline Nd{sup 3+}-doped gadolinium scandium aluminum garnet powders by a gel-combustion method

Graphical abstract: The graph shows the emission spectra (λ{sub ex} = 808 nm) of 1 at.% Nd:GSAG powders sintered at different temperatures for 3 h. Compared with the powder sintered at 900 °C, the PL intensity of the powder sintered at 1000 °C decreased significantly. The changes in the PL intensity should mainly due to the crystallinity and dispersion of the powders. Highlights: ► We synthesized Nd:GSAG nano-powders by gel-combustion method successfully. ► We analyzed the structure and the morphology of the heat-treated products. ► We studied the optical characteristics of Nd:GSAG nano-powders. -- Abstract: Nd{sup 3+}-doped gadolinium scandium aluminum garnet (Nd:GSAG) precursor was synthesized by a gel combustion method using metal nitrates and citric acid as raw materials. The structure and morphology of the precursor and the sintered powders were studied by means of X-ray diffraction (XRD), infrared spectroscopy (IR) and transmission electron microscopy (TEM). The results showed that the precursor transformed into pure GSAG polycrystalline phase at about 800 °C, and the powders sintered at 800–1000 °C were well-dispersed with average particle sizes in the range of 30–80 nm. Optical properties of Nd:GSAG nano-powders were characterized by using photoluminescence spectroscopy. The highest photoluminescence intensity was achieved for the powder sintered at 900 °C.

36 MATERIALS SCIENCE↗

Understanding the effects of fabrication process on BaZr 0.9 Y 0.1 O 3– δ grain-boundary chemistry using atom probe tomography

Proton-conducting oxides, such as BaZr 0.9 Y 0.1 O 3–δ (BZY10), are receiving significant scientific attention for application in a variety of electrochemical applications. It has been shown that the synthesis route has a significant effect on the ionic behavior of these materials, especially the grain boundaries (GB). In this study, laser-pulsed atom probe tomography (APT) is used to characterize the GB chemistry of BZY10 samples prepared by four different methods: (1) spark plasma sintering (SPS), (2) conventional sintering followed by high-temperature annealing (HT), (3) conventional sintering with NiO used as a sintering aid (SSR-Ni), and (4) solid-state reactive sintering of oxide precursor powders with NiO as a reactive sintering aid (SSRS-Ni). Oxygen depletion (corresponding to oxygen vacancy accumulation) was observed at every GB in this study, consistent with the positive space-charge GB region commonly assigned to these materials. In contrast to the consistent trends associated with oxygen depletion, cation constituents showed varying segregation/depletion behaviors. The samples that used NiO revealed Ni preferentially segregating to the GB. The most common impurities in BZY10 are Al, Fe, Mg, Si, and Sr, all of which generally accumulate at GBs. In order to quantify these chemical trends, the APT method was optimized for this material supplemented with understanding from density functional theory (DFT). Finally, this APT study reveals the complexity of BZY10 GB chemistry and shows that even adjacent GBs in the same material can sometimes show surprisingly different GB chemistry.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Magnetic behavior of Ni and Co doped CuMn2O4 spinels

Mn1.68Co0.24Ni0.48Cu0.6O4 was produced by slip casting and sintering of spray-pyrolysis produced powders. Magnetic properties of this composition were measured for the first time, as a function of processing temperature (900 or 1000°C sintering), to study the effects of Cu and Mn valence and site preference. Quantitative x-ray photoelectron spectroscopy showed that Cu+ site occupancy changed from tetrahedral to a mix of tetrahedral and octahedral with increasing sintering temperature. X-ray diffraction demonstrated that the materials had a cubic spinel structure devoid of tetragonal Jahn-Teller distortion. AC magnetic susceptibility indicated ferrimagnetic behavior below ~109 K and spin glass behavior below ~66-74 K depending on measurement frequency. Magnitudes of the AC magnetic susceptibility, DC magnetization, and Curie-Weiss temperature were lower for samples sintered at 1000°C than for those sintered at 900°C. AC susceptibility freezing temperatures were modeled with the Vogel-Fulcher law and showed characteristics intermediate between canonical spin glasses and cluster glasses. For the sample sintered at 1000°C, the activation energy for magnetic relaxation was decreased and the interaction parameter temperature was increased compared to the 900°C sample. These materials show promise for advancing fundamental understanding of consequences of multivalent, mixed site occupancy cations on magnetic properties.

Environmental Molecular Sciences Laboratory↗

An Assessment of Additively Manufactured Bonded Permanent Magnets for a Distributed Wind Generator

In this paper, we examine and compare the performance of a generator design optimized using additively manufactured NdFeB-SmFeN in nylon-polymer-bonded permanent magnets (PMs) against a generator design with conventional NdFeB sintered PMs. To realize this, a commercially available 15-kW wind generator's rotor is re-optimized using both additively manufactured and sintered NdFeB magnets using simple geometric parameterization that allowed for two specific magnet shapes, namely, arc-shaped and crown-shaped designs. Results showed that for a similar generator performance, the designs with additively manufactured bonded PMs are more cost-competitive in terms of the estimated PM material cost and also have negligible eddy current magnet losses.

additive manufacturing↗

VTO FY20Q4 quarterly report

Project Objective.This project has three objectives: (1) tuning microstructures of 3D-printed SSE separators,(2) determining material and processing compatibilities with cathode printing,and (3)3D printing of sintering-free SSE separators.Project Impact.All-solid-state lithium batteries are difficult to process due to the brittleness of ceramic materials, poor solid-solid contact, and electrolyte-electrode stability issues. As a result, the energy and power density and also cycling stability are far from satisfying. This project will address fabrication difficulties by using state-of-the-art 3D-printing techniques that can introduce 3D interfaces and architectures to enhance solid-solid contact and reduce charge transfer resistance. Success will benefit the DOE by establishing the best manufacturing methods for ASSBsto achieve VTO goals on the performance of beyond Li-ion batteries. Approach.The project employs 3D-printing techniques to manufacture SSEs and related components for ASSBs. The team starts with direct ink writing (DIW) to develop ink recipes with desired rheological properties and explore post-sintering approaches to achieve high densification. In parallel with DIW3D printing, the team also explores other 3D printing options, such as projection microstereolithography (PuSL). Both sintering and sintering-free approaches can gain benefit from 3D printing and therefore will be investigated.Out-Year Goals.The team will determine particle sizes and morphologies as well as post-processing conditions that deliver good ionic conductivity and charge transfer properties of LLZTO separators. They will examine co-sintering of LLZTO/cathode and determine the effects of material, particle size, surface coating, and sintering conditions.Collaborations.Microstructures, ionic conductivities, and mechanical properties will be provided to the LLNL simulation team, led by PI B. Wood, for establishing and validating phase-field modeling methods.

36 MATERIALS SCIENCE↗

Tape casting and characterizations of MgO ceramics

Herein we report a high density MgO ceramic substrate produced by the tape casting technology. The tape casting formulation and process produced a uniform tape free of cracking. Y 2 O 3 and SiO 2 were used as the sintering aid for the pressureless sintering of the green tape. X-ray diffraction phase identification indicates that MgO is the main phase, while both Y 2 O 3 and SiO 2 sintering aids react with MgO to form MgY 4 Si 3 O 13 as the second phase. Liquid phase sintering occurs in the temperature range from 1030°C to ~1500°C, which is confirmed by the simultaneous Thermal Gravitation Analysis/ Differential Scanning Calorimeter (TGA/DSC) and the percent linear shrinkage and densification. A 96.5% theoretical density was achieved by presureless sintering at 1650°C for 2 hours, which was further increased to a fully dense structure using hotisostatic- pressing(HIP) at 1650°C and 207 MPa in argon. Scanning electron microscopy (SEM) and energy dispersive(EDS) spectroscopic analysis on the HIP’ed sample show that MgY 4 Si 3 O 13 is located at the MgO grain boundary and the sample has a fully dense structure. The refractive indices and extinction coefficient were measured on the HIP’ed sample along with thermal properties and dielectric properties. Thermal diffusivity and heat capacity were measured to calculate the thermal conductivity.

36 MATERIALS SCIENCE↗

PRELIMINARY STUDY OF CERAMICS FOR IMMOBILIZATION OF ADVANCED FUEL CYCLE REPROCESSING WASTES

The Savannah River National Laboratory (SRNL) developed a series of ceramic waste forms for the immobilization of Cesium/Lanthanide (CS/LN) and Cesium/Lanthanide/Transition Metal (CS/LN/TM) waste streams anticipated to result from nuclear fuel reprocessing. Simple raw materials, including Al{sub 2}O{sub 3}, CaO, and TiO{sub 2} were combined with simulated waste components to produce multiphase ceramics containing hollandite-type phases, perovskites (particularly BaTiO{sub 3}), pyrochlores, zirconolite, and other minor metal titanate phases. Identification of excess Al{sub 2}O{sub 3} via X-ray Diffraction (XRD) and Scanning Electron Microscopy with Energy Dispersive Spectroscopy (SEM/EDS) in the first series of compositions led to a Phase II study, with significantly reduced Al{sub 2}O{sub 3} concentrations and increased waste loadings. Three fabrication methodologies were used, including melting and crystallizing, pressing and sintering, and Spark Plasma Sintering (SPS), with the intent of studying phase evolution under various sintering conditions. XRD and SEM/EDS results showed that the partitioning of the waste elements in the sintered materials was very similar, despite varying stoichiometry of the phases formed. The Phase II compositions generally contained a reduced amount of unreacted Al{sub 2}O{sub 3} as identified by XRD, and had phase assemblages that were closer to the initial targets. Chemical composition measurements showed no significant issues with meeting the target compositions. However, volatilization of Cs and Mo was identified, particularly during melting, since sintering of the pressed pellets and SPS were performed at lower temperatures. Partitioning of some of the waste components was difficult to determine via XRD. SEM/EDS mapping showed that those elements, which were generally present in small concentrations, were well distributed throughout the waste forms. Initial studies of radiation damage tolerance using ion beam irradiation at Los Alamos National Laboratory (LANL) showed little if any modification of the material after irradiation. Additional study in this area is needed. Chemical durability was briefly studied using the Product Consistency Test (PCT). Most of the elements measured were retained by the ceramic waste forms, indicating good chemical durability. Cs, Mo, and Rb were released at somewhat higher rates as compared to the matrix components, although benchmark compositions and additional characterization are needed in order to qualify the PCT results.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

DEVELOPMENT OF CERAMIC WASTE FORMS FOR AN ADVANCED NUCLEAR FUEL CYCLE

A series of ceramic waste forms were developed and characterized for the immobilization of a Cesium/Lanthanide (CS/LN) waste stream anticipated to result from nuclear fuel reprocessing. Simple raw materials, including Al{sub 2}O{sub 3} and TiO{sub 2} were combined with simulated waste components to produce multiphase ceramics containing hollandite-type phases, perovskites (particularly BaTiO{sub 3}), pyrochlores and other minor metal titanate phases. Three fabrication methodologies were used, including melting and crystallizing, pressing and sintering, and Spark Plasma Sintering (SPS), with the intent of studying phase evolution under various sintering conditions. X-Ray Diffraction (XRD) and Scanning Electron Microscopy coupled with Energy Dispersive Spectroscopy (SEM/EDS) results showed that the partitioning of the waste elements in the sintered materials was very similar, despite varying stoichiometry of the phases formed. Identification of excess Al{sub 2}O{sub 3} via XRD and SEM/EDS in the first series of compositions led to a Phase II study, with significantly reduced Al{sub 2}O{sub 3} concentrations and increased waste loadings. The Phase II compositions generally contained a reduced amount of unreacted Al{sub 2}O{sub 3} as identified by XRD. Chemical composition measurements showed no significant issues with meeting the target compositions. However, volatilization of Cs and Mo was identified, particularly during melting, since sintering of the pressed pellets and SPS were performed at lower temperatures. Partitioning of some of the waste components was difficult to determine via XRD. SEM/EDS mapping showed that those elements, which were generally present in small concentrations, were well distributed throughout the waste forms.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

THE EFFECT OF TEMPERATURE AND UNIAXIAL PRESSURE ON THE DENSIFICATION BEHAVIOR OF SILICA AEROGEL GRANULES

Materials are being developed in U.S. for the removal and immobilization of iodine from gaseous products of nuclear fuel reprocessing in support of the Fuel Cycle Technology Separations and Waste Forms Campaign. The silver-functionalized silica aerogel proved to be an excellent candidate for this treatment because of its high selectivity and sorption capacity for radioiodine and its possible conversion to a durable silica-based waste form. The present study investigated with nitrogen sorption and helium pycnometry the effect of pressureless isothermal sintering at temperatures of 900-1400°C for 2.5-90 min or isothermal hot-pressing at 1200°C for 2.5 min on densification of raw and silver-functionalized silica aerogel granules. Rapid sintering was observed at 1050 and 1200°C. Only 15 min of pressureless sintering at 1200°C resulted in almost complete densification. The macropores disappeared, surface area decreased from 1114 m2/g to 25 m2/g, pore volume from 7.41 cm3/g to 0.09 cm3/g, and adsorption pore size from 18.7 to 7 nm. The skeletal density of sintered granules was similar to the bulk density of amorphous silica (2.2 g/cm3). The hot-pressing accelerated the sintering process, decreasing significantly the pore size and volume.

BET↗

Influence of Ba Substitutions on Microstructure and Magnetic Properties of La–Ca–Co System Permanent Ferrite

La{sub 0.6}Ca{sub 0.4−x}Ba{sub x}O⋅n/2(Fe{sub 1−y}Co{sub y}){sub 2}O{sub 3}(x = 0, 0.05, 0.1, 0.15 and 0.2) permanent ferrite materials were prepared by ceramic technique. The topography and the structure were characterized by scanning electron microscopy (SEM) and x-ray diffraction (XRD), respectively. The magnetic properties were measured using vibrating sample magnetometer (VSM) and digital magnetometer. Single M-phase and flake-like grains were obtained for samples without Ba substitution(x = 0), and the magnetic properties of the pre-sintering La–Ca–Co ferrite were as follows: B{sub r} = 440 mT, H{sub cb} = 296 kA/m, H{sub cj} = 426 kA/m, (BH){sub max} = 36.6 kJ/m{sup 3} and H{sub k}/H{sub cj} = 0.83. When Ca was substituted by Ba, pre-sintered powder presents single M-phase structure and close three-dimensional size of grains, resulting in an improved rectangle ratio of sintered magnet. The rectangle ratio of sintered magnet reaches a maximum of 0.93 when x = 0.1. By optimizing process parameters, M-type La–Ca–Ba–Co sintered magnet was prepared with B{sub r} = 445 mT, H{sub cb} = 337 kA/m, H{sub cj} = 420 kA/m, (BH){sub max} = 38.6 kJ/m{sup 3} and H{sub k}/H{sub cj} = 0.95.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure evolution during binder jet additive manufacturing of H13 tool steel

H13 is one of the most used tool steels for both hot and cold work tooling applications. Binder jet additive manufacturing offers the potential to deposit complex tools at scale due to larger powder bed sizes and faster deposition rates. However, to date there is no published literature on the sintering of H13 to full densification. Here, we discuss the pressureless sintering of binder jet AM H13 steel to full densification via supersolidus liquid phase sintering (SLPS) while presenting appropriate process windows (1360 °C – 1380 °C) for densification without distortion. The process windows have been rationalized based on thermodynamic calculations of liquid volume fractions with temperature. We show that higher binder saturation results in higher carbon retention and subsequently early liquid formation that can initiate the sintering process at lower temperatures. We report abnormal grain growth during sintering and found that the solidification phase transformations play a critical role on microstructural evolution and must be considered to accurately model the kinetics of SLPS.

36 MATERIALS SCIENCE↗