Search NASA⌕ Search

SEARCH · Search NASA

Results for “cracking temperature”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,081 records · Page 60

Low cycle fatigue and creep-fatigue behavior of Ni-based alloy 230 at 850 C

Strain-controlled low cycle fatigue (LCF) and creep-fatigue testing of Ni-based alloy 230 were carried out at 850 C. The material creep-fatigue life decreased compared with its low cycle fatigue life at the same total strain range. Longer hold time at peak tensile strain further reduced the material creep-fatigue life. Based on the electron backscatter diffraction, a novel material deformation characterization method was applied, which revealed that in low cycle fatigue testing as the total strain range increased, the deformation was segregated to grain boundaries since the test temperature was higher than the material equicohesive temperature and grain boundaries became weaker regions compared with grains. Creep-fatigue tests enhanced the localized deformation, resulting in material interior intergranular cracking, and accelerated material damage. Precipitation in alloy 230 helped slip dispersion, favorable for fatigue property, but grain boundary cellular precipitates formed after material exposure to the elevated temperature had a deleterious effect on the material low cycle fatigue and creep-fatigue property.

Creep-fatigue↗

Development of joining technology using local heating for SiC fuel cladding

Silicon carbide (SiC) is an attractive material for an accident-tolerant fuel in light water reactors because of its lower hydrogen-generation rate and lower heat of reaction than conventional Zircaloy. On the other hand, practical application of SiC fuel cladding faces a lot of critical issues, one of which is end-plug joining. The objective of this study is to clarify the feasibility of end-plug joining by silicon brazing using local heating by evaluating the shear strength of joint specimens and producing a circumferential joint experimentally. Silicon is thought to be a compatible joining material with SiC because as well as being a constituent of SiC, its thermal-expansion coefficient is close to that of SiC. Local heating using processes such as laser irradiation and a resistance-heating element needs to be applied for end-plug joining. Brazing is expected to seal a cladding with an end plug by using brief heating without a strong compression force. Shear strength was evaluated using specimens with silicon-brazing joints processed using laser irradiation. The joint sections without defects showed shear strengths higher than or equal to 59 MPa at temperatures from normal room temperature to 1473 K. The average shear strength of the joint (99 MPa) is comparable to that of a diffusion-bonding joint using titanium or molybdenum foil. A tube and a plug were circumferentially joined with silicon brazing using laser irradiation or a graphite heating element. A defocused laser beam was effective for joining without cracking during laser irradiation. Although local heating using a resistance-heating element can more easily control the temperature of the joint, it took longer processing time than that using laser irradiation due to limited temperature-increase rate in order to avoid thermal shock damage. (authors)

36 MATERIALS SCIENCE↗

A summary of the Hanford single-shell tank structural analysis of record - 15526

Washington River Protection Solutions, LLC (WRPS), the US DOE Hanford Site tank contractor, developed an enhanced Single-Shell Tank Integrity Project (SSTIP) in 2009 to better understand the integrity of the single-shell tanks (SSTs). A panel of experts from industry and academia was created to recommend project activities in four main areas: structural integrity, liner degradation, leak integrity and prevention, and contamination migration. One of the panel's primary recommendations was to perform a detailed structural integrity analysis of the SSTs. WRPS and the U.S. Department of Energy, Office of River Protection commissioned the Pacific Northwest National Laboratory (PNNL) to perform this structural integrity analysis of record for the Hanford single shell tanks. This is one of seventeen panel recommendations that form the M-45-10-1 Change Package for the Hanford Federal Agreement and Compliance Order; also known as the Tri-Party Agreement. Finite element analysis was used to predict the structural response of the SSTs to the historical thermal and operating loads, plus design basis seismic loads. Bounding thermal histories were established from waste temperature records and applied to the model to include the thermal degradation of concrete modulus and strength, plus cracking due to differential thermal expansion while under in situ static loading conditions. PNNL contracted with Becht Engineering to evaluate the dynamic response of the tanks to a design basis earthquake. The degraded stiffness of the reinforced concrete was also incorporated in the seismic analysis. The combined response to static and seismic loads was then evaluated against the design requirements of the American Concrete Institute standard, ACI-349-06, for nuclear safety-related concrete structures. Specific analyses were performed for the four major tank designs.This paper presents an overview of the analysis methods used and it summarizes the major analytical findings that are common to the tanks and others that are specific to the individual tank designs. The analyses of record determined that including the bounding effects of their operating histories, each tank design currently satisfies the ACI-349-06 structural integrity design requirements. Although leak tightness is not directly addressed in the structural integrity analysis, this analysis will be a key input in the formal tank integrity assessment due in 2018. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Anaerobic polymers as high vacuum leak sealants

Anaerobic polymers are useful as solventless leak sealants with good vacuum properties at moderate temperatures. Loctite 290 can seal leaks in a range generally encountered in carefully constructed ultrahigh vacuum and high vacuum systems. It was found that small leaks are sealed best under vacuum, whereas large leaks should be sealed at atmospheric pressure. The high-temperature behavior of Loctite 290 is limited by its fast cure, which prevents deep penetration into small leaks; cracking eventually occurs at the entrance to the leak. Repeated thermal cycling to about 300 C is possible, however, provided viscosity, curing time, and leak size are properly matched to ensure penetration into the body of the leak. This may require special formulations for high temperature vacuum applications.

Kendall, B. R. F.↗

AlGaN/GaN heterostructure prepared on a Si (110) substrate via pulsed sputtering

GaN films were grown on Si (110) substrates using a low-temperature growth technique based on pulsed sputtering. Reduction of the growth temperature suppressed the strain in the GaN films, leading to an increase in the critical thickness for crack formation. In addition, an AlGaN/GaN heterostructure with a flat heterointerface was prepared using this technique. Furthermore, the existence of a two dimensional electron gas at the heterointerface with a mobility of 1360 cm{sup 2}/Vs and a sheet carrier density of 1.3 × 10{sup 13} cm{sup −2} was confirmed. Finally, the use of the AlGaN/GaN heterostructure in a high electron mobility transistor was demonstrated. These results indicate that low-temperature growth via pulsed sputtering is quite promising for the fabrication of GaN-based electronic devices.

36 MATERIALS SCIENCE↗

A Radiation Hard Multi-Channel Digitizer ASIC for Operation in the Harsh Jovian Environment

In 1995, the Galileo spacecraft arrived at Jupiter to conduct follow-up experiments on pathfinder Pioneer and key Voyager discoveries especially at Io, Europa, Ganymede and Callisto. These new observations helped expand our scientific knowledge of the prominent Galilean satellites; studies revealed diversity with respect to their geology, internal structure, evolution and degree of past and present activity. Jupiter's diverse Galilean satellites, of which three are believed to harbor internal oceans, are central to understanding the habitability of icy worlds. Galileo provided for the first time compelling evidence of a near-surface global ocean on Europa. Furthermore, by understanding the Jupiter system and unraveling the history of its evolution from initial formation to the emergence of possible habitats and life, gives insight into how giant planets and their satellite systems form and evolve. Most important, new light is shed on the potential for the emergence and existence of life in icy satellite oceans. In 2009, NASA released a detailed Jupiter Europa Mission Study (EJSM) that proposed an ambitious Flagship Mission to understand more fully the satellites Europa and Ganymede within the context of the Jovian system. Key to EJSM is the NASA led Jupiter Europa Orbiter (JEO) and the ESA led Jupiter Ganymede Orbiter (JGO). JEO and JGO would execute a choreographed exploration of the Jovian system before settling into orbit around Europa and Ganymede, respectively. The National Academies Planetary Decadal Survey, 2011 has listed the NASA-led JEO as the second highest priority mission for the decade 2013-2022, and if chosen it would be launched in 2020 with arrival at Jupiter in 2025. If the JEO mission is not chosen it is anticipated that there will be opportunities in future decadal cycles. Jupiter Orbit Insertion (JOI) begins a 30-month Jovian system tour followed by nine months of science mapping after Europa Orbit Insertion (EOI) in July 2028. The orbiter will ultimately impact the surface of Europa after the mission is completed. The current JEO mission concept includes a range of instruments on the payload, to monitor dynamic phenomena (such as Io's volcanoes and Jupiters atmosphere), map the Jovian magnetosphere and its interactions with the Galilean satellites, and characterize water oceans beneath the ice shells of Europa and Ganymede. The payload includes a low mass (3.7 Kg) and low power (< 5 W) Thermal Instrument (TI) concept for measuring possible warm thermal anomalies on Europa s cold surface caused by recent (< 10,000 years) eruptive activity. Regions of anomalously high heat flow will be identified by thermal mapping using a nadir pointing, push-broom filter radiometer that provides far-IR imagery in two broad band spectral wavelength regions, 8-20 m and 20-100 m, for surface temperature measurements with better than a 2 K accuracy and a spatial resolution of 250 m/pixel obtained from a 100 Km orbit. The temperature accuracy permits a search for elevated temperatures when combined with albedo information. The spatial resolution is sufficient to resolve Europa's larger cracks and ridge axial valleys. In order to accomplish the thermal mapping, the TI uses sensitive thermopile arrays that are readout by a custom designed low-noise Multi-Channel Digitizer (MCD) ASIC that resides very close to the thermopile linear array outputs. Both the thermopile array and the MCD ASIC will need to show full functionality within the harsh Jovian radiation environment, operating at cryogenic temperatures, typically 150 K to 170 K. In the following, a radiation mitigation strategy together with a low risk Radiation-Hardened-By-Design (RHBD) methodology using commercial foundry processes is given for the design and manufacture of a MCD ASIC that will meet this challenge.

Aslam, Shahid↗

Thermal modulation of nonlinear ultrasonic waves for nondestructive evaluation of elastic materials

Temperature variation is often considered an undesirable factor in ultrasonic testing, as wave velocity is highly sensitive to thermal fluctuations. However, completely eliminating the temperature effect is difficult, particularly in tests requiring precise velocity measurements. Recently, a method called Thermal Modulation of Nonlinear Ultrasonics (TMNL) has been developed. Instead of eliminating the thermal effect, the TMNL method leverages the temperature variation as a driving force to stimulate the nonlinear response of the medium and modulate the ultrasonic waves propagating in it. These modulated waves can then be used to evaluate the nonlinear behaviours of the test medium. This paper presents a focused review of the TMNL technique, including its theoretical foundations, particularly the conceptual challenges in integrating thermal effects into classical acoustoelastic theory, and recent applications in non-destructive evaluation (NDE). Three case studies are presented to demonstrate TMNL’s application in detecting microcracking in concrete, assessing ageing in polymer materials, and enabling temperature compensation in acoustoelastic tests. In conclusion, the review also summarises related studies, including photothermal crack modulation, and discusses current limitations and future directions of TMNL in elastic media.

NDE↗

High temperature static strain gage development

Final results are presented from a program to develop a thin film static strain gage for use on the blades and vanes of running, test stand gas turbine engines with goals of an 3 x 3 mm gage area and total errors of less than 10 pct. of + or - 2,000 microstrain after 50 hrs at 1250 K. Pd containing 13 Wt. pct. Cr was previously identified as a new strain sensor alloy that appeared to be potentially usable to 1250 K. Subsequently, it was discovered, in contrast with its behavior in bulk, that Pd-13Cr suffered from oxidation attack when prepared as a 4.5 micron thick thin film. Continuing problems with electrical leakage to the substrate and the inability of sputtered alumina overcoats to prevent oxidation led to the discovery that sputtered alumina contains appreciable amounts of entrapped argon. After the argon has been exsolved by heating to elevated temperatures, the alumina films undergo a linear shrinkage of about 2 pct. resulting in formation of cracks. These problems can be largely overcome by sputtering the alumina with the substrate heated to 870 K. With 2 micron thick hot sputtered alumina insulation and overcoat films, total 50 hr drifts of about 100 microstrain (2 tests) and about 500 microstrain (1 test) were observed at 1000 and 1100 K, respectively. Results of tests on complete strain gage systems on constant moment bend bars with Pd temperature compensation grids revealed that oxidation of the Pd grid was a major problem even when the grid was overcoated with a hot or cold sputtered alumina overcoat.

Hulse, C. O.↗

Hydrothermal synthesis of {beta}-nickel hydroxide nanocrystalline thin film and growth of oriented carbon nanofibers

Novel well-crystallized {beta}-nickel hydroxide nanocrystalline thin films were successfully synthesized at low temperature on the quartz substrates by hydrothermal method, and the oriented carbon nanofibers (CNFs) were prepared by acetylene cracking at 750 deg. C on thin film as the catalyst precursor. High resolution transmission electron microscopy (HR-TEM) measurement shows that thin films were constructed mainly with hexagonal {beta}-nickel hydroxide nanosheets. The average diameter of the nanosheets was about 80 nm and thickness about 15 nm. Hydrothermal temperature played an important role in the film growth process, influencing the morphologies and catalytic activity of the Ni catalysts. Ni thin films with high catalytic activity were obtained by reduction of these Ni(OH){sub 2} nanocrystalline thin films synthesized at 170 deg. C for 2 h in hydrothermal condition. The highest carbon yield was 1182%, and was significantly higher than the value of the catalyst precursor which was previously reported as the carbon yield (398%) for Ni catalysts. The morphology and growth mechanism of oriented CNFs were also studied finally.

36 MATERIALS SCIENCE↗

Investigation of ion irradiation effects on mineral analogues of concrete aggregates

Irradiation can cause prominent damage to reactor concrete aggregates leading to amorphization, strength and modulus decrease, radiation induced volume expansion (RIVE) and micro-cracking, which limits their long-term performance. Here, to develop an improved understanding of irradiation effects in concrete, three mineral analogues of concrete aggregates (limestone, marble and quartzite) were irradiated by 5.5 MeV He ions and 13 MeV Ni ions to surface doses of 0.011 displacements per atom (dpa) and 0.23 dpa, respectively, at room temperature. The two different ion species allow irradiation spectrum effects (ionizing and displacive) to be examined. Irradiation induced cracks were observed in He irradiated limestone and marble, and Ni irradiated quartzite. Full amorphization was observed in Ni irradiated quartzite with 14.3 % RIVE, and ∼25 % hardness and modulus decrease, while almost no change was observed in He irradiated quartzite except 4.35 % RIVE, revealing a possible ionization enhanced diffusion effect for high energy light ions. Furthermore, partial amorphization was observed in Ni irradiated marble and limestone matrix with a 12 % hardness decrease in marble while no amorphization was observed for He irradiation with a 20 % hardness increase in limestone matrix. The role of knock-on damage and irradiation spectrum on amorphization, volumetric expansion and mechanical property changes are discussed. Moreover, the onset and critical doses for amorphization and RIVE in quartz are obtained for ion irradiations at room temperature. The dose dependence of RIVE exhibits a delay compared to the amorphization behavior. The superior irradiation resistance of calcite phase compared to quartz phase implies there could be advantages to using calcareous aggregates and lowering the usage of siliceous aggregates for concrete in nuclear power plants for extended operation beyond 60 years. However, other effects such as corrosion, aging and reactions during severe accidents should also be considered, and further investigations are needed.

Amorphous↗

Qualitative and quantitative analysis of neutron irradiation effects in SiC/SiC composites using X-ray computed tomography

Silicon carbide fiber-reinforced silicon carbide matrix (SiC/SiC) composites are candidate materials for cladding of light water reactor (LWR) fuels. Loss of fission product gas retention due to the formation of microcrack networks is considered a potential failure mechanism for SiC/SiC-cladded fuels. In this work, a variety of SiC/SiC composite tubes were irradiated with and without an LWR-relevant radial heat flux in the High Flux Isotope Reactor, followed by detailed characterization with X-ray computed tomography (XCT). This first set of XCT data for neutron-irradiated samples confirmed that the internal stresses arising from a combination of temperature gradients and irradiation-induced swelling act as the primary driver for cracking. Consequently, while the observed cracking patterns varied depending on the tube architectures, the sharp edges of relatively large pores were found to be the common stress concentrator. These findings are useful to help improve the design and manufacturing of SiC/SiC fuel claddings for reduced failure probability.

42 ENGINEERING↗

Additively manufactured β-Ti5553 with laser powder bed fusion: Microstructures and mechanical properties of bulk and lattice parts

Ti5553 (Ti-5Al-5Mo-5V-3Cr wt%) is a titanium alloy widely used for its high strength-to-weight ratio and good formability at elevated temperatures. Unlike Ti-6Al-4V, Ti5553 does not undergo martensitic transformation, preventing cracking of brittle martensite upon rapid cooling. This makes it a strong candidate for additive manufacturing (AM), particularly laser powder bed fusion (L-PBF). L-PBF offers the unique opportunity to make fine lattice structures to reduce component weight. Despite the growing field of AM, there have been limited studies on L-PBF Ti5553 lattices and how their properties differ from the bulk. Here the present work addresses this knowledge gap by investigating microstructures and properties of L-PBF bulk and lattice parts and the effect of post L-PBF heat treatments. Electron microscopy and mechanical testing show that the high dislocation density formed during L-PBF increases bulk part’s yield strength by approximately 100 MPa compared to the conventional alloy. Digital image correlation during compression testing of octet truss lattices reveals a layer-by-layer failure mode. Compared to the bulk, the lattice contains copious ω nanoprecipitation, weaker <001> texture, smaller average grain sizes, and larger content of high-angle grain boundaries. These features elicit differences in Taylor factor distributions for the lattice depending on load direction, underlining challenges in predicting lattice mechanical response based on bulk properties. By examining the processing-structure-property relationships in the bulk and lattice, the present results delineate their microstructural and mechanical differences and establish a benchmark for the future design applications of L-PBF Ti5553.

36 MATERIALS SCIENCE↗

Characterization of high-temperature mechanical properties of plasma-cladded coatings with thermo-mechanical coupling

High temperature mechanical properties was detected here to study the failure and strengthening mechanism of the coating-substrate (cobalt-based coatings were fabricated on FV520B substrate) integral structure with thermo-mechanical coupling effects. Microstructure, phase composition, element distribution of the coatings was characterized by optical microscopy (OM), scanning electron microscopy (SEM), transmission electron microscope (TEM), electron back scattering diffraction (EBSD), X-ray diffraction (XRD), electron probe microanalysis (EPMA) and energy dispersive X-ray analysis (EDS). Results elucidate that fracture occurs in the coating for Co50 coating-substrate structure from 300 °C to 700 °C, but failure position transfer to substrate from coating at elevated temperatures with the addition of niobium and cerium oxide. Throughout, there is no crack originated from the interface. Fracture mechanism: the dislocation pile-up causes great stress concentration in the grain boundary, which results in the nucleation of the crack, and then the crack extends along the hard brittle Fe-Cr phase until the material fails. HRTEM shows the high density dislocation and the severe lattice distortion was formed during tensile deformation. On the macro level, the fracture tends to occur in the coarse dendrites region.

36 MATERIALS SCIENCE↗

Elucidating microstructural evolution and hardness variation across friction self-piercing riveted Al-7055 using synchrotron X-ray scattering and advanced microscopy techniques

Friction self-piercing riveting (FSPR) is a unique hybrid joining technique that combines the advantages of mechanical interlocking, frictional heat, and solid-state joining (if metallurgically compatible) to produce crack free joints in high strength and/or low-ductility alloys at room temperature. Here, in the current study, Al-7055 sheets were joined using FSPR for lightweight automotive applications and significant microhardness variations were observed across the joint cross-section. A detailed microstructural characterization at multiple length scales was carried out using advanced electron microscopy and X-ray scattering techniques to provide a fundamental understanding of the process-structure-property relationships. The relative contributions of microstructural characteristics at various length scales (i.e., grain size, dislocation density, solute concentration, precipitate nature) to strengthening were estimated using existent formulations (i.e., Hall-Petch, Taylor, precipitate bypass/shear equations) and correlated to the observed microhardness values across different regions. Small-angle X-ray scattering and scanning transmission electron microscopy revealed significant changes in the size and volume fraction of precipitate species, i.e., GP-I Zones, η′, and Mg/Zn solute co-clusters, depending on the process region. It was observed that the dissolution of the small η′/GP-I zones (T ∼ 150–200 °C) in the heat-affected zone were the key reason for the hardness drop. Further, it was shown that solid-solution, dislocation, grain size and solute co-cluster strengthening played a key role in the thermo-mechanically affected zone and grain-refined zone (GRZ). Finally, these observations were leveraged along with the Zener-Holloman relationship and grain size in the GRZ to estimate the peak joining temperature of the GRZ (∼ 350 °C) near the steel rivet.

aluminum 7xxx alloy↗

Establishment of new design criteria for GlidCop ® X-ray absorbers

Here, an engineering research program has been conducted at the Advanced Photon Source (APS) in order to determine the thermomechanical conditions that lead to crack formation in GlidCop ® , a material commonly used to fabricate X-ray absorbers at X-ray synchrotron facilities. This dispersion-strengthened copper alloy is a proprietary material and detailed technical data of interest to the synchrotron community is limited. The results from the research program have allowed new design criteria to be established for GlidCop ® X-ray absorbers based upon the thermomechanically induced fatigue behavior of the material. X-ray power from APS insertion devices was used to expose 30 GlidCop ® samples to 10000 thermal loading cycles each under various beam power conditions, and all of the samples were metallurgically examined for crack presence/geometry. In addition, an independent testing facility was hired to measure temperature-dependent mechanical data and uniaxial mechanical fatigue data for numerous GlidCop ® samples. Data from these studies support finite element analysis (FEA) simulation and parametric models, allowing the development of a thermal fatigue model and the establishment of new design criteria so that the thermomechanically induced fatigue life of X-ray absorbers may be predicted. It is also demonstrated how the thermal fatigue model can be used as a tool to geometrically optimize X-ray absorber designs.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Fundamental Impact of Humidity on SOFC Cathode ORR

Although solid oxide fuel cells (SOFC) have demonstrated excellent performance, the durability of SOFCs under real working conditions is still an issue for commercial deployment. In particular cathode exposure to atmospheric air contaminants, such as humidity, can result in long-term performance degradation issues. Therefore, a fundamental understanding of the interaction between water molecules and cathodes is essential to resolve this issue and further enhance cathode durability. In order to study the effects of humidity on the oxygen reduction reaction (ORR), we used in-situ 18 O isotope exchange techniques to probe the exchange of water with two of themost common SOFC cathode materials, (La 0.8 Sr 0.2 ) 0.95 MnO 3±δ (LSM) and La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ (LSCF). In this experiment, heavy water, D 2 O (with a mass/charge ratio of m/z = 20), is used to avoid the overlapping of H 2 O and the 18 O 2 cracking fraction, which both provide a peak at m/z = 18. A series of temperature programmed isotope exchange measurements were performed to comprehensively study the interaction of water with the cathode surface as a function of temperature, oxygen partial pressure, and water vapor concentration. The results suggest that water and O 2 share the same surface exchange sites, leading to competitive adsorption. Our findings show that water prefers to exchange with LSCF at lower temperatures, around 300–450°C. For LSM, O 2 is more favorable than water to be adsorbed on the surface and the presence of O 2 limits water exchange. The experimental data are summarized in a Temperature-PO 2 diagram to help visualize how the exchange of water on each material depends on the operating conditions.

30 DIRECT ENERGY CONVERSION↗

Self-healable Copolymer Composites for Extended Service H 2 Dispensing Hoses

In this project, we designed, synthesized and fabricated using X-winder technologies precommercialized novel, self-healingable commodity copolymer fiber-reinforced composites to extend the H 2 hose service life beyond the current target of 1000 fills. These studies demonstrated that these composites are able to withstand over 25,000 damage-repair cycles, which was the main objective of the proposed project, in the temperature range of -40 to +80 °C under variable pressures. When micro-cracks are formed after about 1,000 cycles/fueling per hose in the inner composite layer, these micro-cracks self-heal, thus extending the lifetime of a prototype inner layer of the hose. These composites were tested by exposure to H 2 fuel and demonstrated the ability to recover from mechanical damage. Thermomechanical testing combined with analysis of the stress and strain fields across the cross-section of the inner layer composite hoses also identified the ring-like stresses on the edge of inner layers arising from changes of the fiber winding angle directions from +45° to -45°. The developed novel concept that self-healing commodity copolymers can be used in the development of prototype composites for the extended service of H 2 dispensing hoses will have major implications for other energy-related technologies, where the extended service life in harsh environments is expected. In this project, we optimized, validated, and demonstrated novel copolymer fiber-reinforced composites for H 2 dispensing hose applications, which can be utilized in future manufacturing using commodity materials. The estimated cost of materials (exluding labor) is in the range of < $1.0/ft.

08 HYDROGEN↗

Comparison of experimental and theoretical thermal fatigue lives for five nickel base alloys

The alloys Nimonic 90, IN 100, coated IN 100, B 1900, coated B 1900, MAR M200, and MAR M200DS (directionally solidified) were studied. Maximum temperatures ranged from 770 C to 1120 C (1420 F to 2050 F). Specimen geometries included tapered disks, double-edged wedges, and cambered airfoils. The disks and wedges were heated and cooled in fluidized beds. The airfoil specimens were heated by a Mach 1 natural gas burner and rapid-air-cooled, with and without spanwise loading. Life calculations included two distinct failure modes: conventional low cycle fatigue and cyclic creep. Required material properties were limited to conventional thermal, tensile, and creep rupture data. The complete life calculation system included the calculation of transient temperature distributions, thermal strains, stresses, creep damage, fatigue damage, and cycles to first crack. Calculated lives were within a factor of two for 76 of the 86 data points analyzed. Cyclic creep accounted for 81% of all the calculated damage.

Spera, D. A.↗