At least 1,081 records · Page 60

Benchmarking a 9Cr-2WVTa Reduced Activation Ferritic Martensitic Steel Fabricated via Additive Manufacturing

Reduced activation ferritic (RAF) martensitic steels are promising candidates for the first wall of fusion reactors. However, current manufacturing capabilities call for these components to be made by welding wrought plates. This limits design freedom and necessitates the use of post-weld heat treatments (PWHT) in accordance with the boiler and pressure vessel code. Additive manufacturing (AM) can offer a unique solution to solve this challenge by leveraging the layer-wise deposition strategy to come up with temper bead deposition techniques to eliminate post-processing heat treatments (PPHT). However, it is necessary to benchmark the properties of RAF steels fabricated by AM with their wrought counterparts to identify the process-structure-property correlation, which is the goal of this study. The study demonstrates that while tensile properties at room temperature and high temperatures are satisfactory, the as fabricated and samples after PPHT have significant heterogeneity in tensile elongation. This has been attributed to the presence of discontinuities in the build. The as-fabricated samples have an average tensile strength of 1190 + 12 MPa and an average elongation of 15 + 5% at room temperature and 658 ± 20 MPa ultimate tensile strength (UTS) and 14 ± 7% at 600 °C. After the post-weld heat treatment, mechanical properties decrease to around 600–650 MPa and an elongation between 20–25% at room temperature to 300 MPa UTS and 25–28% elongation at 600 °C. The characterization of microstructures at various length scales demonstrates that the as-fabricated structure has a significant fraction of delta ferrite in a lath martensitic matrix. No precipitates could be identified in the as-fabricated structure. PPHT led to a decrease in the area fraction of delta ferrite and precipitation of M 23 C 6 and MX. Detailed characterization clearly demonstrates that the lack of precipitates in the as-fabricated structure could be due to the slow tempering response of the alloy. Finally, the needs to develop new alloys to achieve the objectives stated above are articulated.

36 MATERIALS SCIENCE↗

Thermal stability of the microstructure of an aged Nb-Zr-C alloy

The effects of thermal aging with and without an applied stress on the microstructure of a Nb-Zr-C alloy containing 0.9 wt percent Zr and 0.06 percent C were studied. Chemical analysis, metallographic examination, energy dispersive X-ray spectra of the bulk material, and chemical and X-ray analyses of the phase-extracted residue were used to characterize the microstructure. The samples examined were from a creep strength study involving hot and cold working, and various combinations of exposure to temperatures ranging from 1350 to 1755 K with and without applied load times as long as 34,000 plus hours. The results showed that the initial microstructure consisted primarily of orthorombic precipitates of Nb sub C which were partially or completely transformed to face-centered cubic carbides of Nb and Zr, (Zr, Nb)C, upon prolonged exposure to elevated temperatures. Furthermore, it was found that the microstructure of the alloy is extremely stable owing to the very finely distributed precipitates throughout its matrix and along the grain boundaries. The lattice parameters of the cubic carbides were determined to vary from 0.458 to 0.465 nm as the Zr/Nb ratio varied from 38/62 to 75/25.

Uz, Mehmet↗

Thermal stability of the microstructure of an aged Nb-Zr-C alloy

The effects of thermal aging with and without an applied stress on the microstructure of a Nb-Zr-C alloy containing 0.9 wt percent Zr and 0.06 wt percent C were studied. Chemical analysis, metallographic examination, energy dispersive x-ray spectra of the bulk material, and chemical and x-ray analyses of the phase-extracted residue were used to characterize the microstructure. The samples examined were from a creep strength study involving hot and cold working, and various combinations of exposure to temperatures ranging from 1350 to 1755 K with and without applied load for times as long as 34,000 plus hours. The results showed that the initial microstructure consisted primarily of orthorombic precipitates of Nb sub 2 C which were partially or completely transformed to face-centered cubic carbides of nb and Zr, (Zr, Nb)C, upon prolonged exposure to elevated temperatures. Furthermore, it was found that the microstructure of the alloy is extremely stable owing to the very finely distributed precipitates throughout its matrix and along the grain boundaries. The lattice parameters of the cubic carbides were determed to vary from 0.458 to 0.465 nm as the Zr/Nb ratio varied from 38/62 to 75/25.

Uz, Mehmet↗

Physicochemical evolution of uranium nitride kernel microstructure with varying carbon distribution for advanced TRISO fuel forms

Uranium nitride (UN) has emerged as a fuel candidate for advanced nuclear reactor concepts due to its superior uranium density, thermal conductivity, and high melting temperature. However, the fabrication route for converting UO 2 to UN is complex and difficult to standardize. Although the chemistry of this conversion process is well-studied, more insight into the physicochemical dynamics of this conversion using advanced characterization techniques can help further our understanding of this material system. This work leveraged thermogravimetric analysis (TGA), X-ray diffraction (XRD), and nondestructive 3D X-ray computed tomography (XCT) to characterize dynamic microstructural changes in the UO 2 → UCO → UN fabrication pathway for two kernels with a varying carbon distribution in the starting composition. TGA and XRD were used to quantify changes in the mass, density, and chemical composition of the two kernels, while three-dimensional image processing and segmentation of XCT data were used to quantify the volume, surface area, and spatial distribution of features within each kernel for multiple steps along the fabrication pathway. The analysis indicates distinct differences between the two kernels that are correlated to downstream conversion efficiency. In conclusion, this work is among the first to perform 3D quantification of physicochemical evolution during UN conversion, providing quantitative correlation between processing, properties, and expected fuel performance.

Nuclear fuel↗

X-ray microtomography

In this tutorial, we describe X-ray microtomography as a technique to nondestructively characterize material microstructure in three dimensions at a micron level spatial resolution. While commercially available laboratory scale instrumentation is available, we focus our attention on synchrotron-based systems, where we can exploit a high flux, monochromatic X-ray beam to produce high fidelity three-dimensional images. A brief description of the physics and the mathematical analysis behind the technique is followed by example applications to specific materials characterization problems, with a particular focus on the utilization of three-dimensional image processing that can be used to extract a wide range of useful information.

36 MATERIALS SCIENCE↗

316L Stainless Steel Wire Arc Additive Manufacturing and Characterization for Potential SNF Canister Production

In this paper, 316L stainless steel (316L SS) straight walls, curved walls, and vessels were printed by wire arc additive manufacturing (WAAM) using the 316L SS welding wire, to demonstrate the feasibility of spent nuclear fuel (SNF) canisters using this advanced manufacturing technique. Helium leak test with leak tight criteria of 1 × 10-7 ref-cc/s were performed on printed vessels with various wall thickness, and testing pressures were from 0.345 MPa (50 psi) to 1.724 MPa (250 psi). Printed wall microstructures were characterized using optical microscopy (OM) and scanning electron microscopy (SEM). Tensile specimens were machined out from printed walls along the length, height, and thickness directions, respectively, and tested at different temperature conditions, room temperature, 80 °C, 150 °C and 250 °C, respectively. Results showed t hat, all five WAAM-printed canisters with different thickness passed the helium leaktight criteria of radioactive materials containers by the ANSI N14.5; Dispersed micrometer-level size inclusions/voids were observed at printed wall cross sections, dendritic microstructures were found with grain size variation through the welding torch shifting direction, and very small amount of δ-ferrite and σ-phase were also observed in those cross sections; The printed walls were ductile, all tensile specimens broke with large plastic deformation/elongation and without brittle failure, and printed specimens yield strengths and tensile strengths under room temperature and 80 °C conditions are higher than minimum values of 316L SS for pressure vessels and for general applications at room temperature required by the ASTM standard, respectively.

Tang, Wei↗

Advanced TEM characterization of oxide nanoparticles in ODS Fe–12Cr–5Al alloys

For oxide nanoparticles present in three oxide-dispersion-strengthened (ODS) Fe–12Cr–5Al alloys containing additions of (1) Y 2 O 3 (125Y), (2) Y 2 O 3 + ZrO 2 (125YZ), and (3) Y 2 O 3 + HfO 2 (125YH), were investigated using transmission and scanning transmission electron microscopy. Furthermore, in all three alloys nano-sized (<3.5 nm) oxide particles distributed uniformly throughout the microstructure were characterized using advanced electron microscopy techniques. In the 125Y alloy, mainly Al 2 O 3 and yttrium–aluminum garnet (YAG) phases (Y 3 Al 5 O 12 ) were present, while in the 125YZ alloy, additional Zr(C,N) precipitates were identified. The 125YH alloy had the most complex precipitation sequence whereby in addition to the YAG and Al 2 O 3 phases, Hf(C,N), Y 2 Hf 2 O 7 , and HfO 2 precipitates were also found. The presence of HfO 2 was mainly due to the incomplete incorporation of HfO 2 powder during mechanical alloying of the 125YH alloy. The alloy having the highest total number density of the oxides, the smallest grain size, and the highest Vickers hardness was the 125YZ alloy indicating, that Y 2 O 3 + ZrO 2 additions had the strongest effect on grain size and tensile properties. Finally, high-temperature mechanical testing will be addressed in the near future, while irradiation studies are underway to investigate the irradiation resistance of these new ODS FeCrAl alloys.

36 MATERIALS SCIENCE↗

Modeling and characterizing anisotropic inclusion orientation in heterogeneous material via directional cluster functions and stochastic microstructure reconstruction

We present a framework to model and characterize the microstructure of heterogeneous materials with anisotropic inclusions of secondary phases based on the directional correlation functions of the inclusions. Specifically, we have devised an efficient method to incorporate both directional two-point correlation functions S{sub 2} and directional two-point cluster functions C{sub 2} that contain non-trivial topological connectedness information into the simulated annealing microstructure reconstruction procedure. Our framework is applied to model an anisotropic aluminum alloy and the accuracy of the reconstructed structural models is assessed by quantitative comparison with the actual microstructure obtained via x-ray tomography. We show that incorporation of directional clustering information via C{sub 2} significantly improves the accuracy of the reconstruction. In addition, a set of analytical “basis” correlation functions are introduced to approximate the actual S{sub 2} and C{sub 2} of the material. With the proper choice of basis functions, the anisotropic microstructure can be represented by a handful of parameters including the effective linear sizes of the iron-rich and silicon-rich inclusions along three orthogonal directions. This provides a general and efficient means for heterogeneous material modeling that enables one to significantly reduce the data set required to characterize the anisotropic microstructure.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Self-assembled flower-like antimony trioxide microstructures with high infrared reflectance performance

A simple hydrothermal process was adopted to self-assembly prepare high infrared reflective antimony trioxide with three-dimensional flower-like microstructures. The morphologies of antimony trioxide microstructures were characterized by X-ray diffractometry (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and high resolution transmission electron microscopy (HRTEM) respectively. It is also found that experimental parameters, such as NaOH concentration, surfactant concentration and volume ratio of ethanol–water played crucial roles in controlling the morphologies of Sb{sub 2}O{sub 3} microstructures. A possible growth mechanism of flower-like Sb{sub 2}O{sub 3} microstructure was proposed based on the experimental data. UV–vis–NIR spectra verified that the near infrared reflectivity of the obtained flower-like microstructures could averagely achieve as 92% with maximum reflectivity of 98%, obviously higher than that of other different morphologies of antimony trioxide microstructures. It is expected that the flower-like Sb{sub 2}O{sub 3} nanostructures have some applications in optical materials and heat insulation coatings. - Graphical abstract: Flower-like Sb{sub 2}O{sub 3} microstructures that composed of nanosheets with thickness of ca. 100 nm exhibit high reflectivity under UV–vis–NIR spectra. Highlights: ► Uniform flower-like microstructures were synthesized via simple hydrothermal reaction. ► The flower-like Sb{sub 2}O{sub 3} microstructures exhibited higher reflectivity than other morphologies under the UV–vis–NIR light. ► Influencing parameters on the Sb{sub 2}O{sub 3} morphologies have been discussed in detail. ► Possible mechanism leading to flower-like microstructures was proposed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Heat Treatments on the Tensile Properties of Additively Manufactured 15-5 Ph Stainless Steel

This study investigated the effect of post-manufacture heat treatments on the microstructure and mechanical properties of 15-5 PH stainless steel (SS) fabricated by laser powder-directed energy deposition (LP-DED). Various heat treatment procedures (CA-H900 and CA-H1150) were conducted to evaluate their effects on the tensile behavior of LP-DED 15-5 PH SS. Scanning electron microscopy was used to characterize the microstructural features and the fracture surfaces. Tensile tests were performed to evaluate the mechanical properties at cryogenic and room temperatures. Reduction in area of CA-H1150 treated specimens after tensile tests was significantly higher than CA-H900 ones, while the ultimate tensile and yield strengths of CA-H900 specimens were higher compared to the CA-H1150 ones. The mechanical behavior of the LP-DED 15-5 PH SS in various heat treatment conditions is discussed based on their microstructures and fracture surfaces.

Laser powder directed energy deposition (LP-DED)↗

Microstructure Evolution of Gas Atomized Iron Based ODS Alloys

In a simplified process to produce precursor powders for oxide dispersion-strengthened (ODS) alloys, gas-atomization reaction synthesis (GARS) was used to induce a surface oxide layer on molten droplets of three differing erritic stainless steel alloys during break-up and rapid solidification. The chemistry of the surface oxide was identified using auger electron spectroscopy (AES) and scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS). The precursor iron-base powders were consolidated at 850 C and 1,300 C using hot isostatic pressing (HIPing). Consolidation at the lower temperature resulted in a fully dense microstructure, while preventing substantial prior particle-boundary-oxide dissociation. Microstructural analysis of the alloys consolidated at the higher temperature confirmed a significant reduction in prior-particle-boundary-oxide volume fraction, in comparison with the lower-temperature-consolidated sample. This provided evidence that a high-temperature internal oxygen-exchange reaction occurred between the metastable prior particle-boundary-oxide phase (chromium oxide) and the yttrium contained within each prior particle. This internal oxygen-exchange reaction is shown to result in the formation of yttrium-enriched oxide dispersoids throughout the alloy microstructure. The evolving microstructure was characterized using transmission electron microscopy (TEM) and high-energy X-ray diffraction (HE-XRD).

36 MATERIALS SCIENCE↗

The effect of carbon on the microstructures, mechanical properties, and deformation mechanisms of thermo-mechanically treated Fe 40.4 Ni 11.3 Mn 34.8 Al 7.5 Cr 6 high entropy alloys

We investigated the effects of cold rolling followed by annealing on the mechanical properties and dislocation substructure evolution of undoped and 1.1 at. % carbon-doped Fe 40.4 Ni 11.3 Mn 34.8 Al 7.5 Cr 6 high entropy alloys (HEAs). X-ray diffraction, scanning electron microscopy (SEM), transmission electron microscopy (TEM) and atom probe tomography (APT) were employed to characterize the microstructures. The as-cast HEAs were coarse-grained and single phase f.c.c., whereas the thermo-mechanical treatment caused recrystallization (to fine grain sizes) and precipitation (a B2 phase for the undoped HEA; and a B2 phase, and M 23 C 6 and M 7 C 3 carbides for the C-doped HEA). Carbon, which was found to have segregated to the grain boundaries using APT, retarded recrystallization. The reduction in grain size resulted in a sharp increase in strength, while the precipitation, which produced only a small increase in strength, probably accounted for the small decrease in ductility for both undoped and C-doped HEAs. For both undoped and C-doped HEAs, the smaller grain-sized material initially exhibited higher strain hardening than the coarse-grained material but showed a much lower strain hardening at large tensile strains. Wavy slip in the undoped HEAs and planar slip in C-doped HEAs were found at the early stages of deformation irrespective of grain size. At higher strains, dislocation cell structures formed in the 19 μm grain-sized undoped HEA, while microbands formed in the 23 μm grain-sized C-doped HEA. Conversely, localized dislocation clusters were found in both HEAs at the finest grain sizes (5 μm). The inhibition of grain subdivision by the grain boundaries and precipitates lead to the transformation from regular dislocation configurations consisting of dislocation-cells and microbands to irregular dislocation configurations consisting of localized dislocation clusters, which further account for the decrease in ductility. Our investigation of the formation mechanism and strain hardening of dislocation cells and microbands could benefit future structural material design.

36 MATERIALS SCIENCE↗

Analytical ultrasonics for structural materials

The application of ultrasonic velocity and attenuation measurements to characterize the microstructure of structural materials is discussed. Velocity measurements in cast stainless steel are correlated with microstructural variations ranging from equiaxed (elastically isotropic) to columnar (elastically anisotropic) grain structure. The effect of the anisotropic grain structure on the deviation of ultrasonic waves in cast stainless steel is also reported. Field-implementable techniques for distinguishing equiaxed from columnar grain structures in cast strainless steel structural members are presented. The application of ultrasonic velocity measurements to characterize structural ceramics in the green state is also discussed.

Kupperman, D. S.↗

Microstructure of Friction Stir Welded AlSi9Mg Cast with 5083 and 2017A Wrought Aluminum Alloys

Wrought aluminum alloys 5083 and 2017A were each joined with cast aluminum alloy AlSi9Mg through friction stir welding in butt weld configurations. For each material system, the wrought and cast alloy positions, i.e., the advancing side or the retreating side, were exchanged between welding trials. The produced weldments were free from cracks and discontinuities. For each alloy configuration, a well-defined nugget comprised of alternating bands of the welded alloys characterized the microstructure. The degree of mixing, however, strongly depended on which wrought alloy was present and on its position during processing. In all cases, the cast AlSi9Mg alloy dominated the weld center regardless of its position during welding. Electron backscattered diffraction analysis showed that the grain size in both alloys (bands) constituting the nugget was similar and that the majority of grain boundaries exhibited a high angle character (20°-60°). Regardless of the alloy, however, all grains were elongated along the direction of the material plastic flow during welding. A numerical simulation of the joining process visualized the material flow patterns and temperature distribution and helped to rationalize the microstructural observations. The hardness profiles across the weld reflected the microstructure formed during welding and correlated well with the temperature changes predicted by the numerical model. Tensile specimens consistently fractured in the cast alloy near the weld nugget.

36 MATERIALS SCIENCE↗

Microstructure-Based Estimation of Strength and Ductility Distributions for \(\alpha +\beta \) Titanium Alloys

Titanium alloys are processed to develop a wide range of microstructure configurations and therefore material properties. While these properties are typically measured experimentally, a framework for property prediction could greatly enhance alloy design and manufacturing. In this work, a microstructure-sensitive framework is presented for the prediction of strength and ductility as well as estimates of the bounds in variability for these properties. The framework explicitly considers distributions of microstructure via new approaches for instantiation of structure in synthetic samples. The parametric evaluation strategy, including the finite element simulation package FEpX, is used to create and test virtual polycrystalline samples to evaluate the variability bounds of mechanical properties in Ti-6Al-4V. Critical parameters for the property evaluation framework are provided by measurements of single crystal properties and advanced characterization of microstructure and slip system strengths in 2D and 3D. Property distributions for yield strength and ductility are presented, along with the validation and verification steps undertaken. Comparisons between strain localization and slip activity in virtual samples and in experimental grain-scale strain measurements are also discussed.

36 MATERIALS SCIENCE↗

Comparison of Commonly-Used Microwave Radiative Transfer Models for Snow Remote Sensing

This paper reviews four commonly-used microwave radiative transfer models that take different electromagnetic approaches to simulate snow brightness temperature (T(sub B)): the Dense Media Radiative Transfer - Multi-Layer model (DMRT-ML), the Dense Media Radiative Transfer - Quasi-Crystalline Approximation Mie scattering of Sticky spheres (DMRT-QMS), the Helsinki University of Technology n-Layers model (HUT-nlayers) and the Microwave Emission Model of Layered Snowpacks (MEMLS). Using the same extensively measured physical snowpack properties, we compared the simulated T(sub B) at 11, 19 and 37 GHz from these four models. The analysis focuses on the impact of using different types of measured snow microstructure metrics in the simulations. In addition to density, snow microstructure is defined for each snow layer by grain optical diameter (Do) and stickiness for DMRT-ML and DMRT-QMS, mean grain geometrical maximum extent (D(sub max)) for HUT n-layers and the exponential correlation length for MEMLS. These metrics were derived from either in-situ measurements of snow specific surface area (SSA) or macrophotos of grain sizes (D(sub max)), assuming non-sticky spheres for the DMRT models. Simulated T(sub B) sensitivity analysis using the same inputs shows relatively consistent T(sub B) behavior as a function of Do and density variations for the vertical polarization (maximum deviation of 18 K and 27 K, respectively), while some divergences appear in simulated variations for the polarization ratio (PR). Comparisons with ground based radiometric measurements show that the simulations based on snow SSA measurements have to be scaled with a model-specific factor of Do in order to minimize the root mean square error (RMSE) between measured and simulated T(sub B). Results using in-situ grain size measurements (SSA or D(sub max), depending on the model) give a mean T(sub B) RMSE (19 and 37 GHz) of the order of 16-26 K, which is similar for all models when the snow microstructure metrics are scaled. However, the MEMLS model converges to better results when driven by the correlation length estimated from in-situ SSA measurements rather than D(sub max) measurements. On a practical level, this paper shows that the SSA parameter, a snow property that is easy to retrieve in-situ, appears to be the most relevant parameter for characterizing snow microstructure, despite the need for a scaling factor.

Snow↗

An EBSD Evaluation of the Microstructure of Crept Nimonic 101 for the Validation of a Polycrystal–Plasticity Model

Nimonic 101 is one of the early nickel-based superalloys developed for the use in gas turbines. In such environments, the material is exposed to a combination of both high temperatures and mechanical loads for a long duration. Hence, thermal creep is of the utmost concern as it often limits service life. This study focuses on creep tests, carried out on Nimonic 101 at different temperatures under a constant tensile load of 735 MPa. To characterize the microstructural evolution, electron backscatter diffraction (EBSD) measurements were employed before and after loading. At higher temperatures, a significant change of the microstructure was observed. The grains elongated and aligned their orientation along the load axis. In parallel, a crystal plasticity material model has been set up in the classical large deformation framework. Modeling results are compared to the acquired EBSD data.

36 MATERIALS SCIENCE↗

Systematic discovery of new nano-scale metastable intermetallic eutectic phases in laser rapid solidified Aluminum-Germanium alloy

Laser surface remelting of as-cast Al-Ge eutectic alloy is shown to produce ultrafine lamellar eutectic morphology with interlamellar spacing refined up to ∼60 nm and composed of FCC Al solid solution and unusual Al x Ge y intermetallic phases that do not form during near-equilibrium solidification. The microstructures are characterized and analyzed using a combination of selected area electron diffraction, high-resolution scanning transmission electron microscopy, energy dispersive X-ray spectroscopy to obtain high-resolution elemental maps, and atomistic modeling using density functional theory followed by atomic-scale image simulation. Depending on the local solidification conditions, the crystallography of the Al x Ge y intermetallic phases in the eutectic microstructure is either monoclinic (C 2/c) or monoclinic (P 2 1 ), with high densities of defects in both cases. This is in sharp contrast to the as-cast alloys that showed nominally pure Al and Ge phases with significant solute partitioning and equilibrium FCC and diamond cubic crystal structures, respectively. Corresponding kinetic phase diagrams are proposed to interpret the evolution of nano-lamellar eutectic morphologies with equilibrium Al and metastable Al x Ge y phases, and to explain increased solid solubility in the Al phases manifested by precipitation of ultrafine clusters of Ge. Furthermore, the reasons for the formation of these metastable eutectics under laser rapid solidification are discussed from the perspective of the competitive growth criterion.

Al-Ge eutectic↗