At least 1,081 records · Page 60

Characterization of Inclusions in 3rd Generation Advanced High-Strength Steels

Samples taken from laboratory-produced 3rd generation advanced high-strength steels, solidified at a low cooling rate, have been investigated to study the characteristics of non-metallic inclusions. Two steels, containing 2 and 5 pct Mn content, were produced for this purpose. A higher number of total inclusions were observed in 5 pct Mn steel. The four main types of inclusions observed were Al{sub 2}O{sub 3}, AlN, MnS, and AlSiMn-oxide. These classes were divided into subclasses according to variations in their chemistry. The major subclasses of AlN inclusions are either plate-like or regular in shape and have different size distributions. Thermodynamic calculations suggest that plate-like AlN inclusions are formed at the initial stage of solidification, while faceted/regular-shaped inclusions are precipitated toward the end of solidification. Moreover, it was found that the size of nitride inclusions is related to their N content. This phenomenon is discussed from the viewpoint of nucleation theory.

36 MATERIALS SCIENCE↗

Closure of Internal Porosity in Continuous Casting Bloom During Heavy Reduction Process

To investigate the closure behavior of internal porosity (also referred to as internal void) in continuous casting bloom during heavy reduction (HR) and thus provide theoretical guidance for minimizing this kind of internal defect more effectively with HR, a three-dimensional (3D) mechanical model was developed based on the predicted temperature field by a 2D heat transfer model. With this 3D mechanical model, closure behaviors of internal porosity in continuous casting bloom during HR at and after the strand solidification end under different process conditions were numerically studied. It was found that the void axis length decreased significantly along the bloom thickness direction and increased slightly along the casting and bloom width directions after HR, and the influence of the initial void size on the void closure was not obvious. With a decrease of temperature difference between the bloom surface and center, HR efficiency for minimizing internal void decreased, while the required reduction force significantly increased. Compared with blooms with a uniform temperature distribution of 1100 °C, the void closure index after HR implemented at the strand solidification end was increased by ~ 25 pct. Compared with a conventional flat roll, the application of a convex roll during HR could contribute to minimizing the internal porosity more effectively and significantly enhance the reduction capacity of the withdrawal and straightening units. The void closure index of η{sub s} and η{sub v} (where η{sub s} and η{sub v} were defined based on the variation of the void aspect ratio and the void volume, respectively) was closely related to the equivalent strain (ε{sub eq}) and the hydrostatic integration parameter (Q), respectively, and two mathematical equations were derived to quantitatively describe the relationship of η{sub s} − ε{sub eq} and η{sub v} − Q.

36 MATERIALS SCIENCE↗

Grain Refinement by Authigenic Inoculation Inherited from the Medium-Range Order Structure of Ni-Cr-W Superalloy

The combination of liquidus casting and thermal control solidification furnace was applied to obtain a fine-grained ingot. A rapid quenching method and x-ray diffraction measurement were used to investigate the effect of authigenic inoculation on grain refinement. The structure factor S(Q) of liquid Ni-Cr-W superalloy at 1400 °C (Liquidus temperature) and bright-field image of the microstructures quenched from 1400 °C have been measured by the high-temperature x-ray diffractometer and the transmission electron microscopy (TEM), respectively. The results show that a pre-peak exists on a S(Q) curve at the liquidus temperature. The clusters of atom in rapidly quenched microstructures obtained by isothermal heat treatment at 1400 °C were studied using TEM. Meanwhile, the effect of isothermal different temperatures on rapidly quenched microstructures was studied. The results also show that there are only the globular, equiaxed grains distributed in the solidification structure. These particles are inherited from the medium-range order structure, which is beneficial for grain refinement. The normalized work-hardening rate-strain curve indicates the work-hardening rate of fine grain is higher than that of conventional grain at the same temperature and the same deformation.

36 MATERIALS SCIENCE↗

Influence of Thermal History on the Hot Ductility of a Continuously Cast Low Alloyed Cr-Mo Steel

The hot ductility of a low alloyed Cr-Mo steel has been investigated to evaluate the surface cracking sensitivity within the straightening or unbending regime during the continuous casting process. Tensile samples were subjected to various thermal treatments, including melting and solidification, and were tested at deforming temperatures ranging between 600 and 1100 °C using a strain rate of 10{sup −3} s{sup −1}. Hot ductility was evaluated based on reduction in area measurement and metallographic investigations. The investigated steel exhibits a drop in ductility at around 800 °C due to intergranular cracking. Microstructural examinations and supplementary thermokinetic computer simulations were carried out to describe the evolution of the microstructure during solidification and cooling.

36 MATERIALS SCIENCE↗

Microstructural and Mechanical Characterization of Directionally Solidified Conventional and Nb-Modified Mar-M247 Superalloy

This study analyzes the effects of replacing Ta by Nb (at.% basis) in the phase transformation temperatures, Scheil solidification behavior, and microstructural mechanical features of a Nb-modified as well as conventional Mar-M247 superalloys. Both alloys were directionally solidified at a withdrawal rate of 18 cm/h under a thermal gradient of about 80 °C/cm. DSC results were compared to thermodynamic simulations of phase transformation temperatures and showed a good correlation. The replacement of Ta by Nb has not altered the solidification path of Mar-M247, keeping the sequence L → L + γ → L + γ + MC → L + γ + MC + γ/γ′ eutectic. Due to the segregation of Hf and Zr to the very last liquid to solidify, a low melting point γ/Ni{sub 5}(Hf,Zr) constituent was observed. The as-solidified microstructures of both Mar-M247(Nb) and Mar-M247 were constituted of columnar dendrites of gamma matrix (γ) phase with cuboidal gamma-prime (γ′) precipitates. In addition, γ/γ′-eutectic was observed in the interdendritic region along with MC carbides in blocky, script (blocky dendritic), needle-like and fine nodular morphologies. Both alloys contained about 1.5 vol.% of MC carbides. The MC carbides in Mar-M247(Nb) and Mar-M247 are, respectively, Nb-rich and Ta-rich, with only a limited amount of Hf being detected in the MC phase. The yield stress of Nb-modified Mar-M247 showed higher values up to 750 °C. For higher temperatures, above 800 °C, a conventional Mar-M247 presented a higher value of yield stress.

36 MATERIALS SCIENCE↗

Deformation Behavior of Pure Copper Castings with As-Cast Surfaces for Electrical Parts

Herein, the tensile deformation behavior of pure copper castings with as-cast surfaces was investigated. It was found that small and sufficiently large uniform elongation types corresponded, respectively, to the presence or absence of a Cu-Cu{sub 2}O eutectic phase in the microstructure. Fissure defects were observed near the as-cast surfaces when the eutectic phase was present, probably leading to stress concentration. On the other hand, surface pinholes were observed when the eutectic phase was absent, and these were not prevented by directional solidification. Although the as-cast specimens (non-directionally solidified) exhibited a slightly reduced uniform elongation compared to the machined specimens in the absence of the eutectic phase, the directionally solidified as-cast samples exhibited a uniform elongation that was similar to that of the machined specimens. In addition, micropore arrays were formed along the grain boundaries inside the castings when the eutectic phase was absent, whereas almost no micropores were observed inside the directionally solidified as-cast specimens because the solidification process involved a faster cooling rate and/or higher temperature gradient. These results do not only suggest the existence of surface pinholes but also indicate that microporosity can reduce the cross-sectional area of the specimens, thus, affecting their uniform elongation.

36 MATERIALS SCIENCE↗

A stochastic scan strategy for grain structure control in complex geometries using electron beam powder bed fusion

Spatial control of microstructure within a three-dimensional component has been a dream of materials scientists for centuries. However, limitations in traditional manufacturing processes prevent detailed control over the distribution of microstructures in a single part. Here, we demonstrate the ability to control grain structure and crystallographic texture during metal additive manufacturing for arbitrary cross-sections of a practical size, with profound implications for the design and optimization of next-generation products. The key to this advance is a new geometry agnostic scan path algorithm that manipulates the spatial distribution of solidification conditions. Utilizing a fundamental understanding of solidification dynamics and a model of the heat transfer during processing, we have designed this algorithm to manipulate the natural competition between epitaxial dendrite growth and grain nucleation. With this algorithm, we successfully controlled the grain structure of Ni-based superalloy IN718 in the shape of the Mona Lisa.

36 MATERIALS SCIENCE↗

3D Printed eutectic aluminum alloy has facility for site-specific properties

Additive manufacturing (AM) has the ability to print structures with site-specific properties. Existing AM approaches for site-specific properties are, however, based on complex processing-microstructure relationships in conventional alloys that were not designed for this purpose. Here, in this work, we report a straightforward approach for achieving site-specific properties that takes advantage of eutectic solidification characteristics. We demonstrate that the yield strength of a eutectic Al-Cu-Ce-Zr alloy can be tuned by varying the laser scan speed in concert with hatch spacing in laser powder bed fusion AM. A faster speed increases solidification rate resulting in finer eutectic spacing and higher strength. The hatch spacing is reduced at faster speeds to ensure overlap between melt pools which become smaller with increasing scan speed. The yield strength and its anisotropy relative to build direction are further tunable with a heat treatment. The scan speed-eutectic spacing-strength relationship is successfully applied to print a complex pattern of site-specific hardness in the alloy. The generalized principle of using AM for a eutectic alloy to create site-specific properties and anisotropy in properties is demonstrated.

36 MATERIALS SCIENCE↗

Segmentation of tomography datasets using 3D convolutional neural networks

Dendritic microstructures are ubiquitous in nature and are the primary solidification morphologies in metallic materials. Techniques such as X-ray computed tomography (XCT) have provided new insights into dendritic phase transformation phenomena. However, manual identification of dendritic morphologies in microscopy data can be both labor intensive and potentially ambiguous. The analysis of 3D datasets is particularly challenging due to their large sizes (terabytes) and the presence of artifacts scattered within the imaged volumes. Here, in this study, we trained 3D convolutional neural networks (CNNs) to segment 3D datasets. Three CNN architectures were investigated, including a new version of FCDenseNet which we extended to 3D. We show that using hyperparameter optimization (HPO) and fine-tuning techniques, both 2D and 3D CNN architectures outperform the previous state of the art. The 3D U-Net architecture trained in this study produced the best segmentations according to quantitative metrics (intersection-over-union of 95.56% and a boundary displacement error of 0.58 pixels), while 3D FCDense produced the smoothest boundaries and best segmentations according to visual inspection. The trained 3D CNNs are able to segment entire 852 × 852 × 250 voxel 3D volumes in only ~60 s, thus hastening the progress towards a deeper understanding of phase transformation phenomena such as dendritic solidification.

36 MATERIALS SCIENCE↗

Massively parallel phase-field simulations targeting exascale

The interface thickness in the phase-field (PF) method limits its simulation scales. Consequently, large-scale PF simulations become prohibitively expensive for resolving the extremely fine microstructures that typically form during rapid solidification processing. This challenge is significant in predicting microstructure evolution in metal additive manufacturing and has been identified by the United States Department of Energy’s Exascale Computing Project. Here, to address this, we develop a multi-GPU and MPI-based massively parallel simulation code, utilizing state-of-the-art algorithms, software, and libraries, for large-scale three-dimensional (3D) PF simulations. We report the first GPU-parallel PF simulations on Frontier (currently the second TOP500 exascale cluster) and Summit machines, taking dendritic growth as an example problem. We evaluate the parallel performance of our implementation using scaling studies with more than 24 000 GPUs (among the largest known computations to date) and the acceleration performance using large-scale simulations of dendritic growth in 3D. Finally, massively parallel GPUs in these supercomputers enabled the first coupled multiscale simulations of laser melting and subsequent dendritic solidification on the scale of a full melt-pool, demonstrating the feasibility of performing PF simulations with a point total over 2 billion grid points within an acceptable time.

Exascale↗

Effect of Sb substitution on crystal structure, texture and hard magnetic properties of melt-spun MnBi alloys

Melt-spun Mn 50 Bi 50-x Sb x alloys with x ≤ 5 were prepared at different solidification rates and characterized both in the as-spun state and after annealing. In the as-spun alloys, the Sb substitution leads to the formation of a metastable phase, similar to the binary "quenched high-temperature phase" but without the superstructure of the latter and exhibiting a different – increasing – temperature dependence of coercivity. The new nanocrystalline metastable phase is not only itself characterized by a high room-temperature coercivity (in excess of 20 kOe), but upon annealing it transforms into a high-coercivity (up to 13.5 kOe) "low-temperature" α phase. However, the advantage of obtaining a high coercivity without the otherwise required milling made possible by the Sb substitution is undermined by the absence of a local crystallographic texture in the melt-spun alloys. The best combination of the isotropic hard magnetic properties realized for the Mn 55 Bi 43.5 Sb 1.5 composition is a remanence of 35.5 emu/g and a coercivity of 8.1 kOe. The annealed Sb-free Mn 50 Bi 50 alloys did possess a local crystallographic alignment and, for high solidification rates, a moderate coercivity up to 5.6 kOe; however, they had an inadequate "rectangularity" in the demagnetization curve. The orthorhombic compound known as MnBi 0.9 Sb 0.1 and described earlier as antiferromagnetic was obtained in the annealed ribbons with x ≈ 5. The compound was found to order ferromagnetically between 200 K and ≈250 K and to exhibit a significant coercivity, 14.3 kOe at 50 K. Here, it is suggested that the MnBi 0.9 Sb 0.1 may actually be a Sb-stabilized "new phase" observed earlier as metastable in the Bi–MnBi eutectic alloys.

36 MATERIALS SCIENCE↗

Interfacial morphology evolution in directionally solidified FeCrAl alloys

Highlights: • The variations of cellular/dendritic spacing with different Al contents and velocities were studied by experiments. • The experimental data were compared with the Hunt-Lu model. • The effect of Al content on the interfacial morphology evolution was discussed for the directional solidified FeCrAl alloys. - Abstract: Interfacial morphology evolution in FeCrAl alloys with varying Al content has been investigated by conducting a series of directional solidification experiments. A comparison between the experimental data and the Hunt-Lu model confirms that cellular spacing widens while dendritic spacing narrows as Al content of the alloy increases. The ratio of upper and lower limit cellular/dendritic spacing λ{sub max}/λ{sub min} is only weakly dependent on growth velocity and Al content. Under the experimental conditions in the present study, cell to dendrite transition (CDT) occurs at a growth velocity between 25 μm/s and 50 μm/s, and dendrite to cell transition (DCT) is observed at a growth velocity less than 100 μm/s. Critical spacing of CDT λ{sub cd} and local solidification time (LST) t{sub f} are used to discuss the influence of Al content on CDT and DCT respectively. The transition between non-planar and planar interface of the alloy is investigated based on the interface stabilization theory of Mullins and Sekerka.

36 MATERIALS SCIENCE↗

On the formation mechanism of the ring-like microstructure of high-pressure die-cast A390 alloy

Highlights: • High-pressure die casting A390 alloy exhibited ring-like microstructure consisted of PSPs-free and PSPs-rich zones. • With 3D data, the size and morphology distribution of PSPs showed similar tendency regardless of the location. • The latent heat released from the PSPs led to the formation of ring-like band. • Widely observed defect band was inhibited because of the precipitation and growth of PSPs during solidification. - Abstract: The microstructure of the A390 alloy during high pressure die casting (HPDC), including pores, primary silicon particles (PSPs) and Cu-rich phases was characterized using synchrotron X-ray tomography. On the cross section of the sample exhibited ring-like or band microstructure, which comprised multiple PSPs-free and PSPs-rich zones. The PSPs distributed evenly in both size and morphology regardless of the ring-like microstructure. The size of aluminum dendrites changed according to the location of the ring-like microstructure, and was highly dependent on the local latent heat released from the PSPs as well as the distribution of the ‘net’ Cu-rich phases. Along the radial direction of the sample exhibited an abrupt increase of pores, indicating a tendency for forming a defect band in but such tendency was inhibited because of the huge amount of latent heat released by the PSPs during solidification, which was quite different from that of either magnesium alloys or hypoeutectic aluminum alloys.

36 MATERIALS SCIENCE↗

Formation of intermetallic structures at the interface of steel-to-aluminium explosive welds

Highlights: • The interface of Fe-Al explosive welds was characterised by SEM/EDS and EBSD. • The intermetallics formed at the weld interface are rich in Al (Fe{sub 4}Al{sub 13}, Fe{sub 2}Al{sub 5}). • The presence of intermetallic phases on the interface deeply affects the weldability. • Al-rich intermetallics increase the solidification time of the weld interface. - Abstract: The formation of intermetallic structures at the interface of carbon steel to 6082 aluminium alloy explosive welds and their influence on the weldability of these two materials were studied. The morphology, the microstructure, the chemical and phase compositions of the welds were characterised by several types of microscopy techniques. The interface characterisation proved that explosive mixtures with a lower detonation velocity were revealed as being more suitable for achieving consistent welds since jet entrapment was prevented and continuous molten layers were not formed at the weld interface. It was also found that the physical properties of the intermetallic phases generated at the weld interface have a strong influence on the weldability of steel-to-aluminium explosive welds. Specifically, it was shown that the formation of aluminium-rich intermetallic phases at the weld interface increases the solidification time of the interfacial molten material, decreasing the weldability of these two materials. The formation of these intermetallic compounds should be avoided by reducing the interaction between the flyer and the baseplate as well as by avoiding excessive molten layers.

36 MATERIALS SCIENCE↗

Microstructural evolution of rapidly solidified hypoeutectic Al 10Cu alloy during non-isothermal annealing transients induced by nano-second laser pulses

The evolution of characteristic nonequilibrium features presenting in morphologically distinct regions of rapid solidification (RS) microstructures in a hypoeutectic Al—10Cu (atomic %) in response to non-isothermal annealing transients has been studied by transmission electron microscopy (TEM). The capabilities of the Movie-Mode Dynamic TEM (MM-DTEM) instrument were used to expose select regions of the RS microstructure to sequences of rapid heating and cooling transients induced by nanosecond laser pulses while permitting in-situ observation. Partial melting, microstructural scale coarsening, morphological changes of the nonequilibrium features in the multi-phase RS microstructure, and solid-state phase transformation were observed. Heterogeneous nucleation of nanoscale θ-Al 2 Cu phase involved metastable supersaturated α-Al and the θ'-Al 2 Cu phases, establishing different sets of orientation relationships for the stable θ-Al 2 Cu and α-Al phases. Replacement of banded morphology grains that formed under conditions driven farthest from equilibrium by an equiaxed nanocrystalline structure comprised of α-Al phase, the primary solidification product, and an intergranular network of Al 2 Cu crystals has been attributed to local remelting. Here the experimental approach explored, permitted discovery of mechanistic details of location-specific transformation pathways activated in the multi-phase RS microstructure of hypoeutectic Al—Cu during subsequent nonisothermal transients.

36 MATERIALS SCIENCE↗

Microstructure and mechanical behavior of laser remelted amorphous Al-Ni-La welds

To explore the feasibility of using laser powder bed fusion systems to print bulk amorphous Al alloys, a single autogenous weld produced by laser remelting on a cast Al-5La-9Ni (at.%) alloy was studied for its microstructure and mechanical behavior. The solidification rates experienced by material within the welds were high enough to produce entirely amorphous regions within the welds. Welds were characterized using SEM, STEM, and APT and were found to contain Ni-rich amorphous clusters. Micropillar compression tests were used to assess mechanical properties of the welds and found that all of the amorphous regions exhibited yield strengths around 1 GPa. In conclusion, these results are discussed in the context of diffusivity of Ni and rare earth elements in liquid, glass forming ability, thermodynamic driving force for phase formation during solidification, free volume concentrations in bulk metallic glasses, and cluster-related softening.

APT↗

Cooling dynamics of two titanium alloys during laser powder bed fusion probed with in situ X-ray imaging and diffraction

Metal parts produced by laser powder bed fusion (LPBF) additive manufacturing exhibit characteristic microstructures comparable to those observed in laser welding. The primary cause of this characteristic microstructure is rapid, localized heating and cooling cycles, which result in extreme thermal gradients where material solidification is followed by fast cooling in the solid state. The final microstructure and mechanical performance are also influenced by pore formation caused by melt pool fluid dynamics. Here, we use high speed, in situ X-ray diffraction to probe the kinetics of cooling and solid-solid phase transitions after laser melting in two aerospace titanium alloys: Ti-6Al-4V, an α + β alloy; and Ti-5Al-5V-5Mo-3Cr, a near-β alloy. We complement these diffraction studies with in situ X-ray imaging to probe melt pool dynamics and pore formation. From these two complementary probes, we quantify pore formation during melting and the subsequent microstructural evolution as the material rapidly cools after solidification. These results are critical for understanding defect formation and residual stress development in different titanium alloys under LPBF conditions and can help inform process models to predict final part performance.

36 MATERIALS SCIENCE↗

Disorder trapping and formation of antiphase nanodomains in Ni 3 Sn: in situ observation and high resolution characterization

Rapid solidification of the intermetallic Ni 3 Sn compound from an undercooled liquid was investigated using time-resolved synchrotron X-ray diffraction. Primary growth of an ordered and a disordered cubic solid was observed in situ at a low and a high undercooling, respectively. The disordered cubic solid was reordered after rapid solidification and experienced a solid-state transformation in cooling. A HRTEM study revealed high density of crystal defects and nanodomains in the transformed matrix. A HAADFSTEM study determined that the nanodomains are antiphase domains with chemical disorder. These observations indicated a possibility of online control of mechanical properties in additively manufactured intermetallics.