Search NASA⌕ Search

SEARCH · Search NASA

Results for “interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,099 records · Page 61

The effect of water-containing electrolyte on lithium-sulfur batteries

Dissolved polysulfides, formed during Li-S battery operation, freely migrate and react with both the Li anode and the sulfur cathode. These soluble polysulfides shuttle between the anode and cathode – the so-called shuttle effect – resulting in an infinite recharge process and poor Columbic efficiency. We present that water present as an additive in the Li-S battery electrolyte is found to reduce the shuttle effect in Li-S batteries. Batteries where water content was below 50 ppm exhibited a substantial shuttle effect and low charge capacity. Alternatively, addition of 250 ppm water led to stable charge/discharge behavior with high Coulombic efficiency. XPS results show that H 2 O addition results in the formation of solid electrolyte interphase (SEI) film with more LiOH on Li anode which protects the Li anode from the polysulfides. Batteries cycled without water result in a SEI film with more Li 2 CO 3 likely formed by direct contact between the Li metal and the solvent. Intermediate quantities of H 2 O in the electrolyte result in high cycle efficiency for the first few cycles which then rapidly decays. Lastly, this suggests that H 2 O is consumed during battery cycling, likely by interaction with freshly exposed Li metal formed during Li deposition.

25 ENERGY STORAGE↗

Effect of overcharge on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 /graphite lithium ion cells with poly(vinylidene fluoride) binder. III — Chemical changes in the cathode

Here, 1.5 Ah pouch cells based on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 cathodes and graphite anodes, both containing poly (vinylidene fluoride) (PVDF) binders, were systematically overcharged to 100, 120, 140, 160, 180, and 250% state of charge (SOC), at which point they vented. The cells were subsequently discharged to 0% SOC and disassembled under an inert atmosphere for characterization. A combination of X-ray photoelectron spectroscopy (XPS), scanning-electron microscopy (SEM), energy-dispersive spectroscopy (EDS), 6 Li SSNMR, and X-ray diffraction (XRD) analysis of the NMC532 cathodes indicates the formation of a thin C- and O-rich cathode electrolyte interphase layer, progressive Li loss above 140% SOC, and retention of the bulk crystal structure at all states of charge.

25 ENERGY STORAGE↗

Electrochemical and Interfacial Behavior of All Solid State Batteries Using Li10SnP2S12 Solid Electrolyte

Thio-Lithium Superionic Conductor (Thio-LISICON) Li10GeP2S12 equivalent Li10SnP2S12 (LSPS) is comparable in ionic conductivity yet with a lower cost as an electrolyte for all solid-state batteries (ASSBs). ASSBs with LSPS solid electrolyte (SE), lithium-indium alloy anode, and LiCoO2 (LCO) cathode were successfully fabricated and their electrochemical performance at 60 °C was examined. Atomic layer deposition of Li3NbO4 on LCO was conducted to improve the interfacial stability. The Li3NbO4 coating significantly improves the cycle stability of the ASSB, which retains about 85% of the initial capacity after 70 cycles at a current density of 0.13 mA/cm2, while the ASSB with uncoated LCO retains ~ 60% of the initial capacity after 70 cycles. Electrochemical impedance spectroscopy tests indicate a rapid growth of charge transfer resistance upon cycling for the cell with the uncoated LCO, primarily due to the surface instability and build-up of a space charge layer between LSPS and LCO. However, the ASSBs with Li3NbO4 coated LCO show a more stable interface with a negligible impedance increase upon cycling, attributable to the buffering and passivating roles of the Li3NbO4 coating. The interfacial microstructure was analyzed to elucidate at the underlying reasons for the impedance increase and the pivotal role of the Li3NbO4 coating. Our study indicates that the surface coating significantly improves the cycle stability of the ASSBs with LSPS as the electrolyte, mostly due to an improvement of the charge transfer mechanism. The coating reduced the interphase thickness and the interfacial resistance to about a third of the uncoated one after 10 cycles.

Vinado, Carolina↗

Understanding the trilemma of fast charging, energy density and cycle life of lithium-ion batteries

Increasing energy density of Li-ion batteries (LiBs) along with fast charging capability are two key approaches to eliminate range anxiety and boost mainstream adoption of electric vehicles (EVs). Either the increase of energy density or of charge rate, however, heightens the risk of lithium plating and thus deteriorates cell life. The trilemma of fast charging, energy density and cycle life are studied systematically in this work utilizing a physics-based aging model with incorporation of both lithium plating and solid-electrolyte-interphase (SEI) growth. The model is able to capture the key feature of temperature-dependent aging behavior of LiBs, or more specifically, the existence of an optimal temperature with the longest cycle life. We demonstrate that this optimal temperature is a result of competition between SEI growth and lithium plating. Further, it is revealed that either the increase of charge rate or of energy density accelerates lithium plating induced aging. As such, the optimal temperature for cell life increases from ~20 °C for a high-power cell at 1C charge to ~35–45 °C with the increase of charge rate and/or energy density. In conclusion, it would be beneficial to further increase the charge temperature in order to enable robust fast charging of high energy EV cells.

25 ENERGY STORAGE↗

Bis(trimethylsilyl) 2-fluoromalonate derivatives as electrolyte additives for high voltage lithium ion batteries

Three trimethylsilyl based malonate esters, bis(trimethylsilyl) 2-methyl-2-fluoromalonate (BTMSMFM), bis(trimethylsilyl) 2-ethyl-2-fluoromalonate (BTMSEFM) and bis(trimethylsilyl) 2-propyl-2-fluoromalonate (BTMSPFM), have been used as additives in 1.0 M LiPF 6 /ethylene carbonate (EC)-dimethyl carbonate (DMC)-diethyl carbonate (DEC) (1-1-1, by v) baseline electrolyte for LiNi 0.80 Co 0.15 Al 0.05 O 2 (NCA) based high voltage lithium ion batteries. The NCA half-cells with 5 wt% BTMSMFM exhibit higher capacity retention than that in the baseline electrolyte at different upper cut off voltages, that is, 4.2, 4.3, 4.4 and 4.5 V vs. Li/Li + . Scanning electron microscope (SEM) show that the additive successfully prevents the formation of thick solid electrolyte interphase (SEI) films on the surface of the NCA electrodes. X-ray diffraction (XRD) further reveals that the crystal structure of NCA is also maintained in the electrolyte with 5 wt% BTMSMFM at high cut off voltages. Finally, besides beneficial to NCA cathode, the BTMSMFM additive also ensures better cycling performance of the graphite based half-cells and NCA/graphite full-cells, and thus is a promising additive for application in rechargeable lithium ion batteries.

25 ENERGY STORAGE↗

Lithium–sulfur battery with partially fluorinated ether electrolytes: Interplay between capacity, coulombic efficiency and Li anode protection

Seven partially fluorinated ethers (PFE) were explored as co-solvents for lithium-sulfur battery with the goal to understand the interplay between the molecular structure and the electrochemical properties, including capacity, Coulombic efficiency and SEI formation on the Li anode. Electrochemical cycling suggests a loose correlation between the Coulombic efficiency observed over 200 cycles and the fluorination degree of the PFE, which correlates with the computed pKa of the C–H bond of the ethers. PFE with lower pKa (<36) tends to chemically react with lithium anode forming a solid-electrolyte-interphase (SEI) layer thus preventing the shuttling effect of the lithium polysulfides. The cycled lithium anodes with DOL/PFE electrolyte was discovered to produce a protective SEI analyzed by FT-IR and SEM/EDS. Computations of the interactions between the PFEs of interest and a lithium surface suggest the generation of LiF and unsaturated PFE derivatives which are easily reduced and polymerized on the Li surface. The PFE decomposition is more thermodynamically likely with increasing fluorination degree. This research sheds light on the role that fluorine substitution and structure play in the high Coulombic efficiencies observed for Li–S cells.

25 ENERGY STORAGE↗

High accuracy in-situ direct gas analysis of Li-ion batteries

Cycling of lithium-ion batteries containing Ni-rich NMC cathodes at high voltage involves intense gas generation. From the safety standpoint, it is critical to understand how different gas species respond to changes of upper cut-off voltages. In this manuscript, we introduce a novel experimental set up for real-time analysis of gas generation in prismatic pouch cells. In a typical experiment, a lithium-ion pouch cell is directly connected to a quadruple mass spectrometer by glass capillary. Pressure difference helps move the generated gases to the mass spectrometer column for full analysis. The gaseous species are probed during both formation cycle and aging cycles in Li-ion pouch cells comprising NMC811 cathode and graphite anode. The gases are generated upon the creation of the solid electrolyte interphase on graphite during the first formation charge. Besides ethylene gas, C 2 H 4 , whose occurrence is related to the decomposition of ethylene carbonate, a minor solvent decomposition happened at a lower voltage is demonstrated to be associated with residue water on the electrode. For aging cycles, three upper cut-off voltages have been selected to investigate the gas evolution behavior upon charging to 4.2, 4.4 and 4.6 V. Higher upper cut-off voltages do not affect the amount of O 2 measured as a part of the generated oxygen could have reacted with electrolytes. Quite similar and low amounts of O 2 remain in the cells upon charging to the selected cut-off voltages. On the other hand, the generation of CO 2 has been found to be very sensitive to upper cut-off voltage. During similar aging cycles, 6167 nmol $g_{NMC}^{-1}$ of CO 2 is generated at 4.6 V, versus 1650 nmol $g_{NMC}^{-1}$ of CO 2 at 4.4 V, versus 91 nmol $g_{NMC}^{-1}$ of CO 2 at 4.2 V.

25 ENERGY STORAGE↗

Effects of charged interfaces on electrolyte decomposition at the lithium metal anode

Lithium–Sulfur batteries are promising candidates to substitute conventional Li-ion batteries due to their higher energy density and reduced cost. However, several challenges related to the reactivity of the lithium metal anode have prevented this technology from becoming broadly commercialized. Lithium's high reactive nature leads to the continuous decomposition of the electrolyte and the formation of the solid-electrolyte interphase (SEI) layer. Thus, a comprehensive understanding of how the SEI film is formed is crucial to help elucidate improvements for this battery technology. In this work, we use density functional theory (DFT) based computational methods to investigate the effect of charged interfaces on the electrolyte degradation at the lithium anode. Here, several electrolyte mixtures were considered including 1,2-dimethoxyethane (DME) and 1,3-dioxolane (DOL) as solvents, and lithium bis(fluorosulfonyl)imide (LiFSI) and lithium bis(trifluoromethanesulfonyl)imide (LiTFSI) as salts. It is found that the extent of salt decomposition is higher when the interface is charged. In addition, two types of solvent reduction mechanisms are identified: C–O bond cleavage and radical attacks. Charge transfer and evolution analysis are characterized in detail. Finally, solvent decomposition reactions are found to become more thermodynamically favorable and their activation barriers to be diminished under the effect of constant potentials and electric fields.

25 ENERGY STORAGE↗

Effect of temperature on capacity fade in silicon-rich anodes

Coin half-cells containing 80 wt% silicon electrodes are assembled and cycled at the similar to C/10 rate in the temperature range of 25-55 degrees C. To the best of our knowledge, this is the first time that the effect of temperature is reported for such high-silicon-containing cells. Two different electrolytes are used in this study, a baseline electrolyte and the baseline electrolyte +10 wt% fluoroethylene carbonate (FEC). Analysis of the capacity vs. cycle count data by curve fitting reveals that the addition of FEC markedly affects the capacity loss mechanism. Without FEC, the kinetic rate law for the capacity loss mechanism can be described as the sum of two logistic growth models. With the addition of FEC, the rate law depends on ln(t). Clearly, the addition of FEC has a profound effect on the mechanism of capacity loss. Interestingly, X-ray photoelectron spectroscopy (XPS) shows that the composition of the solid electrolyte interphase (SEI) layer changes markedly from mostly organic to mostly inorganic in the presence of FEC and how it varies at the different temperatures tested, especially in the absence of FEC.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Diffusional lithium trapping as a failure mechanism of aluminum foil anodes in lithium-ion batteries

Aluminum foils are an appealing anode for lithium-ion batteries due to high capacity and low-cost, but their viability has been limited due to poor cyclability arising from pulverization and solid-electrolyte interphase growth. Here, we show that significant capacity degradation of aluminum foil anodes during electrochemical cycling also occurs due to diffusional lithium trapping. Scanning electron microscopy of cross-sectioned, cycled foils in the delithiated state reveals large regions of β-LiAl that are passivated by a surface layer of α-Al, which has poor Li + diffusivity. It is found that lithium diffusion occurs preferentially along the β-LiAl grain boundaries, so the grain structure after initial lithiation significantly affects the trapping behavior. Diffusional lithium trapping is exacerbated by both higher delithiation rates and higher areal capacity, presenting a challenge towards commercialization of aluminum foil anodes. We further demonstrate that diffusional trapping in aluminum foil anodes can be mitigated through alloy design, with the addition of 2–3 wt% Li yielding improved first cycle efficiency, and the addition of 1 wt% Si yielding improved cycle life. These results provide a mechanistic understanding of diffusional lithium trapping in aluminum foil anodes and highlight compositional design of alloys as a promising strategy to overcome it.

25 ENERGY STORAGE↗

SEI formation mechanisms and Li + dissolution in lithium metal anodes: Impact of the electrolyte composition and the electrolyte-to-anode ratio

The lithium metal battery is one of today's most promising high-energy-density storage devices. Its full-scale implementation depends on solving operational and safety issues intrinsic to the Li metal high reactivity leading to uncontrolled electrolyte decomposition and uneven Li deposition. In this work, we study the spontaneous formation of the solid electrolyte interphase (SEI) upon contact of Li metal with the electrolyte and describe the heterogeneous SEI morphological features. Multiple electrolyte formulations based on lithium bis(fluorosulfonyl)imide (LiFSI), dimethoxyethane (DME), dimethyl carbonate (DMC), 1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) and bis(2,2,2-trifluoroethyl) ether (BTFE) are used. Findings include the description of the SEI evolution from dispersed LiO, LiS, LiN, and LiF clusters to a continuous and compact inorganic phase in which the LiO and LiF content depend on the presence of fluorine diluents. Further, the role of the DME ether solvent helping the growth of a “wet-SEI” is compared to that of the highly unstable carbonate DMC, which decomposes into complex radical oligomers that might contribute to further electrolyte decomposition. The impact of the electrolyte-to-anode ratio on LiFSI decomposition is highlighted. Finally, we suggest the existence of a critical LiFSI concentration and electrolyte-to-anode ratio that could potentially balance the rate of electrolyte depletion and lithium consumption.

25 ENERGY STORAGE↗

Unravelling fast-charging degradation in NMC/Gr pouch cells: Lithium plating and SEI properties

As fast-charging technology expands across the electric vehicle and emerging energy-storage applications, understanding its impact on battery performance and longevity is critical. In this study, 1.8 Ah LiNi 0.6 Mn 0.2 Co 0.2 O 2 /graphite pouch cells were charged at various charging rates (0.5C, 2C, 4C, and 6C) to investigate the degradation mechanisms. Our results showed that well-designed NMC/Gr pouch cells could reach over 1000 cycles with a 2C charging rate, while only reaching around 500 cycles with 4C and 6C charging rates. Fast-charging effects on NMC and graphite electrodes were obtained through a series of post-mortem characterizations, including electrochemical impedance spectroscopy (EIS), Raman spectroscopy, X-ray photoelectron spectroscopy (XPS), and scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS). Although higher charging rates cause pulverization of NMC secondary particles, the dominant degradation mechanism driving the fading of fast-charging-related performance lies in the graphite anode, where lithium plating and LiF-rich solid electrolyte interphase (SEI) formation result in Li inventory loss and impedance growth. The postmortem results suggest that the formation of a LiF-rich SEI, which exacerbates anode impedance and some irreversible Li + ion loss, is likely driven by the substantial decomposition of PF 6 − during fast charging, an effect often overlooked in smaller laboratory-scale studies.

Luo, Mei [Argonne National Laboratory (ANL), Argon↗

Solvation-guided inhibition of manganese dissolution of lithium- and manganese- rich cathode via cyclic carbonate molecular engineering

Lithium and manganese-rich (LMR) layered oxides represent a leading class of high-energy cathode materials, but their practical realization is fundamentally limited by severe manganese (Mn) dissolution, a process that triggers structural degradation and rapid capacity fade. While mitigation efforts have predominantly focused on interfacial engineering, the intrinsic contribution of bulk electrolyte solvation to this degradation pathway remains largely unexplored, primarily due to the difficulty of deconvolving its effects from concurrent cathode-electrolyte interphase (CEI) formation. Here, we report an experimental design to isolate the role of solvation. We systematically varied the electrolyte solvent solvation power by substituting the strongly coordinating ethylene carbonate (EC) with its weaker coordinating fluorinated derivatives, fluoroethylene carbonate (FEC) and trans-4,5-Difluoro-1,3-dioxolan-2-one (DFEC), while maintaining a consistent interfacial chemistry. Remarkably, the electrolyte formulated with the weakest solvent, DFEC, exhibits superior cycling stability, suppressing Mn dissolution by up to 63% relative to the conventional EC-based system. Post-mortem analysis unequivocally attributes this performance enhancement to the preservation of the LMR cathode's structural integrity, a direct consequence of mitigated Mn dissolution. This work provides conclusive evidence that modulating bulk electrolyte solvation is a potent and direct strategy for stabilizing LMR cathodes, establishing a vital design principle for next-generation battery systems.

25 ENERGY STORAGE↗

Cr{sub 2}O{sub 5} as new cathode for rechargeable sodium ion batteries

Chromium oxide, Cr{sub 2}O{sub 5}, was synthesized by pyrolyzing CrO{sub 3} at 350 °C and employed as a new cathode in rechargeable sodium ion batteries. Cr{sub 2}O{sub 5}/Na rechargeable batteries delivered high specific capacities up to 310 mAh/g at a current density of C/16 (or 20 mA/g). High-resolution solid-state {sup 23}Na NMR both qualitatively and quantitatively revealed the reversible intercalation of Na ions into the bulk electrode and participation of Na ions in the formation of the solid-electrolyte interphase largely at low potentials. Amorphization of the electrode structure occurred during the first discharge revealed by both NMR and X-ray diffraction data. CrO{sub 3}-catalyzed electrolyte degradation and loss in electronic conductivity led to gradual capacity fading. The specific capacity stabilized at >120 mAh/g after 50 charge-discharge cycles. Further improvement in electrochemical performance is possible via electrode surface modification, polymer binder incorporation, or designs of new morphologies. - Graphical abstract: Electrochemical profile of a Cr{sub 2}O{sub 5}/Na battery cell and high-resolution solid-state {sup 23}Na MAS NMR spectrum of a Cr{sub 2}O{sub 5} electrode discharged to 2 V. - Highlights: • Cr{sub 2}O{sub 5} was synthesized and used as a new cathode in rechargeable Na ion batteries. • A high capacity of 310 mAh/g and an energy density of 564 Wh/kg were achieved. • High-resolution solid-state {sup 23}Na NMR was employed to follow the reaction mechanisms.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructural characterization and strengthening behavior of nanometer sized carbides in Ti–Mo microalloyed steels during continuous cooling process

Nanometer-sized carbides that precipitated in a Ti–Mo bearing steel after interrupted continuous cooling in a temperature range of 620–700 °C with or without hot deformation were investigated by field-emission-gun transmission electron microscopy. The nanometer-sized carbides were identified as randomly homogeneous precipitation carbides and interphase precipitation carbides coexisting in the ferrite matrix. It is found that this dual precipitation morphology of carbides in the steel leads to the non-uniform mechanical properties of individual ferrite grains. Vickers hardness data mainly revealed that, in the specimens cooled at a rate of 0.5 °C/s without hot deformation, the range of Vickers hardness distribution was 230–340 HV 0.1 when cooling was interrupted at 680 °C, and 220–360 HV 0.1 when cooling was interrupted at 650 °C. For the specimens cooled at a rate of 0.5 °C/s with hot deformation, the range of Vickers hardness distribution was 290–360 HV 0.1 when cooling was interrupted at 680 °C, and 280–340 HV 0.1 when cooling was interrupted at 650 °C. Therefore, a narrower range of hardness distribution occurred in the specimens that underwent hot deformation and were then cooled with a lower interrupted cooling temperature. The uniform precipitation status in each ferrite grain can lead to ferrite grains with a narrower Vickers hardness distribution. On the other hand, interrupted cooling produced a maximum Vickers hardness of 320–330 HV 0.1 for the hot deformed specimens and 290–310 HV 0.1 for the non-deformed specimens with cooling interrupted in the temperature range of 660–670 °C. The maximum Vickers hardness obtained in such a temperature range can be ascribed to the full precipitation of the microalloying elements in the supersaturated ferrite matrix with a tiny size (~ 4–7 nm). - Highlight: • The interrupted continuous cooling temperatures were 620 °C to 700 °C. • Precipitation carbides with dual dispersed morphology coexisted in the matrix. • Heavy hot deformation narrowed the range of hardness distribution. • Full precipitation of nano-sized carbides achieved maximum hardening.

36 MATERIALS SCIENCE↗

Influence of alloying element Zn on the microstructural, mechanical and corrosion properties of binary Mg-Zn alloys after severe plastic deformation

Highlights: • Mg-Zn alloys are processed by equal channel angular pressing with back-pressure. • The α-Mg matrix consists of highly deformed and partially recrystallized areas. • Zn concentration varies in the α-Mg matrix by up to 2 at.%. • The alloys exhibit mechanical anisotropy and a significant increase in strength. • Equal channel angular pressing increases corrosion rate of Mg-Zn alloys. - Abstract: This work presents an analysis of the microstructural, mechanical and corrosion properties of two binary Mg-Zn alloys. Mg-6 wt%Zn and Mg-12 wt%Zn cast alloys were subjected to annealing followed by quenching and processed via equal channel angular pressing with applied back-pressure (ECAP-BP). After ECAP-BP, both alloys were thoroughly examined and showed partially recrystallized and highly deformed areas. High-angle annular dark-field imaging revealed a difference in Zn content across the α-Mg matrix of the Mg-12 wt%Zn after ECAP-BP due to the growth of MgZn{sub 2} nanoparticles. Electron energy-loss spectroscopy (EELS) was carried out to qualify an average Zn content in these areas, and a variation in Zn content up to 2 at.% was found. Compression tests revealed mechanical anisotropy and a significant increase in the strength of both alloys after ECAP-BP. The yield strength, σ{sub 02}, was in the range from 269 to 385 MPa depending on the composition and compression axis. The initial state alloys showed yield strengths, σ{sub 02}, of only 75–150 MPa but improved ductility. The corrosion rates of the Mg-Zn alloys in the initial state, evaluated using a hydrogen evolution method in NaCl solution, were higher for Mg-12 wt%Zn. The corrosion rates of both alloys after ECAP-BP were higher than those of the initial state. Light microscopy observations did not reveal any preference for corrosion propagation, including transcrystalline, intercrystalline or interphase corrosion, in any of the materials.

36 MATERIALS SCIENCE↗

Coarsening of nanoscale (Ti,Mo)C precipitates in different ferritic matrixes

Coarsening of nanoscale (Ti,Mo)C precipitates within quasi-polygonal ferritic (QPF) matrix and polygonal ferritic (PF) matrix is studied via HRTEM and In-situ heating TEM. Influenced by different nucleation processes, inverse coarsening process showing dissolution of large clustered precipitates and growth of small interphase precipitates is directly observed in the PF matrix. However, due to the evolution of high-density subboundaries, coarsening of precipitates in QPF matrix is mainly characterized by the subboundary migration assisted coarsening process, during which arch-like coarsened precipitates form after the sweeping of subboundaries. Analysis of atomic structure clarify that “imposts” of the arch-like coarsened precipitates are established by the re-precipitation of solute atoms from movable subboundary to the close packed planes {111} of (Ti,Mo)C precipitates, and that the “key stones” are constructed due to the change of re-precipitation planes to {200}. Geometric phase analysis (GPA) illustrates that not only the change of re-precipitation direction during the formation of arch-like precipitates, but also the selective coarsening of clustered precipitates in PF matrix, is caused by the highly anisotropic strain field around (Ti,Mo)C precipitates.

36 MATERIALS SCIENCE↗

Materials science applications of Neutron Depth Profiling at the PGAA facility of Heinz Maier-Leibnitz Zentrum

Highlights: • Exploiting the range of NDP from thin films to electrodes for Li-ion batteries • Adopting an analytical method to probe undisturbed depth profiles from thick films • Revealing depth-dependent lithium immobilization in Li-ion battery electrodes Neutron depth profiling (NDP) is a non-destructive, isotope-sensitive profiling technique to monitor concentration profiles in almost any material matrix. Since NDP is sensitive to {sup 6}Li and lithium is widely used for different material science applications such as ceramics, optical waveguides or energy-storage systems, NDP offers answers to a broad spectrum of research questions. In the present work, the recently developed instrument N4DP at MLZ is used to address two research questions which are hardly accessible by conventional analytical techniques. First, the homogeneity of lithium formations within lithium niobate thin films for optical waveguide applications is investigated. Afterwards, the accumulation of inactive lithium in the solid-electrolyte-interphase (SEI) of silicon-graphite electrodes for lithium-ion batteries is studied ex situ. Since the material mass loading differs considerably between the two applications, a new analytical technique is introduced which mathematically separates the different particle signals and thus allows to investigate samples with high mass loadings.

36 MATERIALS SCIENCE↗