Search NASA⌕ Search

SEARCH · Search NASA

Results for “solid solution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,099 records · Page 61

Effect of Strengthening Mechanism on Strain-Rate Related Tensile Properties of Low-Carbon Sheet Steels for Automotive Application

In order to ensure crash resistance of the steels used in automotive components, the ensile deformation behavior needs to be studied and predicted not only under quasi-static condition, but also under dynamic loading rates. In the present study, tensile tests have been performed on four different automobile grade sheet steels, namely interstitial free steel, dual-phase 600 and 800, and a carbon manganese steel over the strain rate regime of 0.001-800/s. Apart from the variation in strength (which always increased with strain rate), the effect of strengthening mechanism on strain rate sensitivity and strain hardening behavior has been evaluated. Strain rate sensitivity was found to increase at high-strain rate regime for all the steels. Contribution of solid solution hardening on strain rate sensitivity at lower plastic strains was found to be higher compared to dislocation strengthening and second-phase hardening. However, precipitation hardening coupled with solid solution hardening produced the highest strain rate sensitivity, in C-Mn-440 steel at high strain rates. Different strain-rate-sensitive models which take into account the change in yield stress and strain hardening behavior with strain rate for ductile materials were used to predict the flow behavior of these sheet steels at strain rates up to 800/s.

36 MATERIALS SCIENCE↗

Tribological Behavior of Structural Materials in High Temperature Helium Gas-Cooled Reactor Environments

The High-Temperature Gas-cooled Reactor (HTGR) is a Generation IV concept designed to produce electricity and hydrogen at high efficiencies via high operating temperatures (700 °C or higher). Helium, the primary coolant for HTGRs, contains impurities (e.g., CO, H2O and CH4) that can induce corrosion reactions at high temperatures such as oxidation and (de)carburization, which in turn can affect the tribological behavior of components. Incoloy® 800HT (Ni-Fe-Cr austenitic solid-solution alloy) and Inconel® 617 (Ni-Cr-Co-Mo solid-solution alloy) are two high-temperature superalloys currently selected as candidate structural materials for the HTGR. The objective of this study is to evaluate the high-temperature tribological performance of these two candidate alloys after conditioning them in HTGR environments. Four regimes of corrosion were considered: a non-conditioned regime (Regime I), an oxidizing regime (Regime II), a carburizing and oxidizing regime (Regime III), and a carburizing regime (Regime IV). To simulate oxidation in HTGR, samples were conditioned for 22 days at elevated temperatures in a once-through helium loop with 4 ppmv H2O. Carburization of the samples was achieved by the commercial process, Kolsterising®. In addition, two surface treatments – shot peening and aluminization – were considered as potential routes of improving the alloys’ wear resistance. Surface-treated samples were tested both before and after conditioning in Regime II. Tribological testing of the samples was performed via a pin-on-disk tribometer at elevated temperatures in ambient environment – 650 and 750°C for 800HT; 850 and 900°C for 617 – with applied loads of 1N, 2N and 5N. The wear behavior of the alloys was assessed via wear volume and friction coefficient measurements, supported by morphological, structural and compositional analyses of the wear tracks. Conditioning the samples in Regime II led to the formation of a chromium oxide on both alloys. This protective scale increased the wear resistance compared to that of as-received samples (Regime I) due to the formation of a compacted ‘glaze’ oxide layer during sliding, rendering the wear track nearly undistinguishable from the unworn background and resulting in wear volumes below the detection limits of the measurement technique. The variability of the friction coefficients of the conditioned samples was also considerably reduced compared to that of the as-received samples due to the glaze layer. Additionally, the initial friction coefficients of the samples conditioned in Regime II were reduced by 45% and 54% compared to those of as-received samples for alloys 800HT and 617, respectively. Carburizing the samples (Regime IV) hardened the surfaces of both alloys and promoted the formation of an iron oxide on 800HT during tribological testing, thereby increasing the wear resistance and decreasing the initial friction coefficient by a factor of two compared to those of as-received 800HT. Alloy 617 exhibited an enhanced wear resistance but similar initial friction coefficient compared to those of as-received samples due to the increased surface hardness. The Mn-Cr oxide developed during Regime III conditioning of 800HT did not develop a glaze layer during tribotesting, even at lower loads. Thus, it was not as protective as the oxide produced during conditioning of Regime II samples, leading to lower wear resistance of 800HT in Regime III compared to that measured in the Regime II condition. 800HT benefited from the aluminization surface treatment, particularly before conditioning in Regime II, due to the promotion of a wear-resistant aluminum oxide layer during testing and the increase in surface hardness due to the presence of a FeAl intermetallic phase. The presence of this phase caused an order-of-magnitude reduction in wear volumes compared to those of as-received 800HT. Aluminization of 617 decreased its wear resistance, particularly after conditioning in Regime II, due to significant wear of the aluminum oxide via a ceramic wear mechanism. This aluminum oxide was removed during sliding, causing the wear volumes to increase by a factor of five compared to those of 617 conditioned in Regime II. Shot-peened 800HT exhibited a tribological behavior similar to that of as-received 800HT, despite an enhancement in the rate of chromium oxide formation. Shot-peened 800HT conditioned in Regime II showed lower wear resistance compared to that of 800HT conditioned in Regime II due to the poor adhesion between the oxide and the underlying metal, preventing the formation of the glaze layer during sliding. Shot peening of 617 increased its wear resistance at higher load, reducing worn volumes by 60% compared to that measured with as-received 617. Tribotesting of shot-peened 617 in Regime II revealed that the glaze-oxide layer was formed at every load, resulting in negligible wear, similar to what was observed from testing 617 after conditioning in Regime II. Overall, alloy 617 exhibited tribologically superior behavior compared to that of alloy 800HT, as demonstrated by its lower friction coefficients and its order-of-magnitude lower wear volumes when measurable.

36 MATERIALS SCIENCE↗

Internal friction sensitivity to precipitation in Al-12 wt% Mg alloy

Highlights: • Internal friction is sensible to semi coherent and non-coherent phases (β′ and β). • Internal friction is not enough sensible to coherent GP zones formation in Al-12 wt% Mg. • Appearance of two IF peaks is due to β′ and β phases formation and dissolution. - Abstract: In order to improve the understanding of the sensibility of the internal friction phenomena to different stages of precipitation in Al-Mg alloys, the ageing effect of a supersaturated solid solution on the Temperature Dependent Internal Friction (TDIF) spectra has been studied. The research showed that the dissolution of the β phase and the transfer of Mg atoms to a solid solution and the formation of β′ metastable phase have an effect on internal friction. Thus, it was proved that the precipitation or the dissolution of β phase plays an important role in the anelasticity of Al-Mg alloys. A detailed TDIF analysis revealed the sensibility of the internal friction technique to the formation of semi-coherent and non-coherent phases (β′ and β) but it is not sensitive enough to the formation of coherent phases (GP zones). Several observations on the nature and the shape of the precipitates are also discussed.

36 MATERIALS SCIENCE↗

Iron in carbonate containing AFm phases

One of the AFm phases in hydrated Portland cement is Ca{sub 3}(Al{sub x}Fe{sub 2} {sub -} {sub x})O{sub 6}.CaCO{sub 3}.nH{sub 2}O. It is based on hexagonal and platey structural elements and the interlayer structure incorporates CO{sub 3}{sup 2-}. The solid phases were experimentally synthesized and characterized by different techniques including X-ray techniques (XRD and EXAFS) and vibrational spectroscopy techniques (IR, Raman). Fe-monocarbonate (Fe-Mc) and Al-monocarbonate (Al-Mc) were found to be stable up to 50 {sup o}C, while Fe-hemicarbonate (Fe-Hc) was unstable with respect to Fe-Mc in the presence of calcite. Fe-Mc has a rhombohedral R3-barc symmetry which is different from the triclinic of the Al analogue. Both XRD and thermodynamic modelling of the liquid compositions indicated that Al-Mc and the Fe-Mc phases do not form solid solution. The solubility products were calculated experimentally at 20 {sup o}C and 50 {sup o}C. Under standards condition the solubility products and other thermodynamic parameters were estimated using temperature-solubility product extrapolation and found to be logK{sub S0} (Fe-Mc) = -34.59 {+-} 0.50, logK{sub S0} (Fe-Hc) = -30.83 {+-} 0.50 and logK{sub S0}(Al-Mc) = -31.32 {+-} 0.50.

36 MATERIALS SCIENCE↗

Nonequilibrium alloy formation in the immiscible Cu-Mo system studied by thermodynamic calculation and ion beam mixing

For the equilibrium immiscible Cu-Mo system characterized by a positive heat of formation (+19 kJ mol{sup -1}), thermodynamic calculation showed that by adding an adequate interfacial free energy, the Gibbs free energy of the Cu-Mo multilayered films could be elevated up to a higher level than the convex-shaped free energy curve of the amorphous phase and supersaturated solid solutions. Accordingly, ion beam mixing of the Cu-Mo multilayered samples did result in forming a unique amorphous phase with an alloy composition around 80 at. % Mo and two supersaturated solid solutions of fcc and bcc structures at around 27 at. % and 90 at. % Mo, respectively, matching well with the thermodynamic calculation.

36 MATERIALS SCIENCE↗

The formation of the complex manganites LnSr{sub 2}Mn{sub 2}O{sub 7} (Ln = La, Nd, Gd)

Graphical abstract: Display Omitted Highlights: ► Formation of the LnSr{sub 2}Mn{sub 2}O{sub 7} phases proceeds according to two different pathways. ► Cationic composition of the obtained phase depends on the formation pathway. ► Step-by-step synthesis allows obtaining single-phase material. ► Structure and magnetic properties of the single-phase NdSr{sub 2}Mn{sub 2}O{sub 7} were investigated. -- Abstract: The process of formation of the Ruddlesden–Popper phases LnSr{sub 2}Mn{sub 2}O{sub 7} (Ln = La, Nd, Gd) was investigated by means of X-ray diffraction, thermal analysis and microprobe analysis. Two parallel pathways were found for the reaction. The first one includes the formation of the intermediate K{sub 2}NiF{sub 4}-type compound by interaction of Sr{sub 7}Mn{sub 4}O{sub 15} and perovskite-type solid solution (Ln,Sr)MnO{sub 3}, while in the second one the K{sub 2}NiF{sub 4}-type intermediate is formed during the reaction of the same perovskite-type solid solution with the corresponding rare earth oxide. This result gives an explanation for the formation of two phases with slightly different cationic compositions. The kinetics of the reaction was investigated for both mechanisms resulting in determination of their relative contribution to the final composition. Pure NdSr{sub 2}Mn{sub 2}O{sub 7} was obtained using a step-by-step process according to the first mechanism, and the magnetic properties of this phase were investigated.

36 MATERIALS SCIENCE↗

Phase transition behavior for ZrW{sub 2-x}Mo{sub x}O{sub 8} compositions at elevated temperatures

A systematical study on cubic ZrW{sub 2-x}Mo{sub x}O{sub 8} (x=0.73, 0.53, 0.33, 0.11) solid solutions reveals that their temperature-dependent phase transition behaviors are related to the Mo fraction x. A phase diagram of cubic ZrW{sub 2-x}Mo{sub x}O{sub 8} solid solutions has been drawn over a wide temperature range (298-1473 K) on the basis of the temperature-dependent phase transition behaviors observed.

36 MATERIALS SCIENCE↗

Crystal Structure and Phase Relations of the R{sub 2}Fe{sub 14}B–Y{sub 2}Fe{sub 14}B (R = Nd and Pr) Systems

The phase relations in the R{sub 2}Fe{sub 14}B–Y{sub 2}Fe{sub 14}B (R = Nd and Pr) systems have been investigated by means of X-ray powder diffraction (XRD), differential thermal analysis (DTA), and scanning electron microscopy (SEM) equipped with energy-dispersive X-ray spectroscopy (EDS). Crystal structure parameters for all studied alloys (R{sub 1−x}Y{sub x}){sub 2}Fe{sub 14}B (R = Nd and Pr) have been determined by Rietveld refinements. Their structures are similar to that of the Nd{sub 2}Fe{sub 14}B phase with tetragonal structure (space group P4{sub 2}/mnm). The continuous solid solutions are formed in these systems. The lattice parameters and unit cell volumes of the (R{sub 1−x}Y{sub x}){sub 2}Fe{sub 14}B (R = Nd and Pr) solid solutions decrease gradually with increasing Y content. The DTA results present that the decomposition temperature of (R{sub 1−x}Y{sub x}){sub 2}Fe{sub 14}B (R = Nd and Pr) rises with x ranging from 0 to 1.0. The vertical sections of the R{sub 2}Fe{sub 14}B–Y{sub 2}Fe{sub 14}B (R = Nd and Pr) systems are presented in this work.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Critical Evaluation and Thermodynamic Optimization of the Li{sub 2}O-Al{sub 2}O{sub 3} and Li{sub 2}O-MgO-Al{sub 2}O{sub 3} Systems

The thermodynamic and phase diagram data of the Li{sub 2}O-Al{sub 2}O{sub 3} and Li{sub 2}O-MgO-Al{sub 2}O{sub 3} systems were critically evaluated and optimized to obtain a set of consistent Gibbs energy functions for all phases in the systems. The LiAl{sub 5}O{sub 8}-MgAl{sub 2}O{sub 4} spinel solid solution was modeled with the two-sublattice compound energy formalism by considering the cation distribution between the tetrahedral and octahedral sites and excess vacancy in octahedral sites. The liquid phase and monoxide solid solution were also described using the modified quasichemical model with pair approximation and the Bragg–Williams random mixing model, respectively. The thermodynamic models with optimized model parameters enable the reproduction of all reliable thermodynamic and phase diagram as well as spinel structural data in the system.

36 MATERIALS SCIENCE↗

The anion exchange properties of AFm (hydrocalumite-group) minerals defined from solubility experiments and crystallographic information

Solubility experiments with binary series of OH-, Cl-, SO{sub 4}- and CO{sub 3}-AFm were re-examined with a non-ideal, multicomponent solid solution model. The electrical double layer on the mineral's outer surface, which neutralizes about 5% of the anionic charge, can be included. The choice of the end-members in the solid solution and the reaction formulation can help to eliminate the ‘non-ideality’ for OH-SO{sub 4} and Cl-OH exchange. CO{sub 3}-Cl-OH exchange is not ideal in the solubility experiments, nor can it be, because the mineral volume is not a linear combination of the end-members. The solubilities of the end-members are related to the anion charge and inversely to the anion-layer thickness. OH is part of the anion-charge, even when a pure, other anion form is the target of the synthesis. Pure OH-AFm is unstable and converts into hydrogarnet and portlandite, depending on the precipitation rate of hydrogarnet.

36 MATERIALS SCIENCE↗

Structural, magnetic, and electrochemical properties of LiMn{sub 1−x}Ni{sub x}PO{sub 4}

Highlights: • LiMn{sub 1−x}Ni{sub x}PO{sub 4} nanomaterials were synthesised via a hydrothermal route up to x = 0.45. • Structure and elemental analyses show solid solution behaviour obeying Vegard's law. • Magnetic properties reflect the substitution of Mn{sup 2+} by Ni{sup 2+}. • Mn{sup 2+/3+} reduction potential rises with increasing nickel concentration. - Abstract: A solid solutions series of LiMn{sub 1−x}Ni{sub x}PO{sub 4} nanomaterials with 0 ≤ x ≤ 0.45 was produced by a low-temperature microwave-assisted hydrothermal process. The materials have been systematically studied regarding structure, morphology, magnetism, and electrochemical properties. The lattice parameters in the orthorhombic olivine structure obey Vegard's law and linearly depend on x. Similarly, the static magnetisation reflects the decrease of the transition metal paramagnetic moment upon substitution of Mn{sup 2+} by Ni{sup 2+}. At low temperatures, antiferromagnetic long range order appears for all Ni-concentrations. The potential of the Mn{sup 2+/3+} redox couple is found to linearly increase with x. This is explained by a larger electronegativity of Ni{sup 2+} as compared to Mn{sup 2+} and associated changes in the covalency of the Mn-O bond.

36 MATERIALS SCIENCE↗

Precipitation in a Cu–Cr–Zr–Mg alloy during aging

The precipitation processes in a Cu-0.69Cr-0.10Zr-0.02Mg alloy aged at 450 °C and 550 °C have been investigated by transmission electron microscopy and high resolution transmission electron microscopy. The precipitation sequence in this alloy aged at 450 °C is: supersaturated solid solution → Guinier–Preston zone (fcc Cr-rich phase) → ordered fcc Cr-rich phase → ordered bcc Cr-rich phase. The precipitation sequence in this alloy aged at 550 °C is: supersaturated solid solution → ordered fcc Cr-rich phase → ordered bcc Cr-rich phase. In the evolution of decomposition, the orientation relationship between the precipitates and the Cu matrix changes from cube-on-cube to Nishiyama–Wassermann orientation. The ordering of Cr-rich precipitates facilitates the formation of the bcc precipitates and promotes the development of Nishiyama–Wassermann orientation. - Highlights: • Two different precipitation sequences in the Cu–Cr–Zr–Mg alloy are proposed. • The changes in orientation relationship of the precipitates are presented. • The roles of ordering and coherent interface of the precipitates are discussed.

36 MATERIALS SCIENCE↗

Reactive flash sintering of TiZrN and TiAlN ternary metal nitrides

Here, this study demonstrated the reactive flash sintering (RFS) for two powder mixtures: TiN-ZrN (both conducting) and AlN-TiN (TiN conducting but AlN insulating), targeting ternary metal nitrides (TMN) of Ti 0.5 Zr 0.5 N and Ti 0.5 Al 0.5 N, respectively. A constant volage and pressure (e.g., 8 V DC, ∼15 MPa) at room temperature triggered the flash (current density up to 27 A/mm 2 ) without pre-heating, and the entire RFS process finished in a few minutes. For TiZrN, the flash was instantaneous whereas for TiAlN, there was a long incubation before the flash followed by a quick and dramatic flash. Both conventional ex situ XRD and in situ synchrotron study had been carried out. They showed a uniform Ti 0.57 Zr 0.43 N solution formed in RFS and persisted upon cooling, while (Ti, Al) N solid solution formed at high temperature was not stable and likely went through a very quick phase separation in the cooling process. The final products from RFS had been characterized using SEM/EDS for microstructure. Both TiZrN and TiAlN were dense. Distribution of Ti, Zr, and N was uniform for TiZrN; for TiAlN, Ti and N distribution was uniform, while association of Al with oxygen was observed. TGA-DSC revealed the onset oxidation temperature for TiZrN was comparable to TiN and ZrN, while it was higher by ∼200 °C for TiAlN, likely due to the formation of Al 2 O 3 . In terms of mechanical properties such as hardness or fracture toughness, forming a single-phase solid solution (like TiZrN) does not offer obvious benefits. while large grain size from RFS seemed to be unfavorable. Future optimization of RFS condition and in-depth study by both experiments and simulation are needed to fully understand the composition-processing-structure-property relationships for such TMN from the reactive flash sintering process.

Flash Sintering↗

Change in the Magnetocapacity in the Paramagnetic Region in a Cation-Substituted Manganese Selenide

The capacity and the dielectric loss tangent of a Gd{sub x}Mn{sub 1–x}Se (x ≤ 0.2) solid solution have been measured in the frequency range 1–300 kHz without a magnetic field and in a magnetic field of 8 kOe in the temperature range 100–450 K, and the magnetic moment of the solid solution has been measured in a field of 8.6 kOe. The magnetocapacity effect and the change in the magnetocapacity sign have been observed in room temperature in the paramagnetic region. A correlation of the changes in the dielectric permittivity and the magnetic susceptibility with temperature has been revealed. The magnetocapacity is described using the model with orbital electron ordering and the Maxwell–Wagner model.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Phase relationships and crystallography of annealed alloys in the Ce5Si4-Ce5Ge4 pseudobinary system

The phase relationships of annealed alloys in the Ce{sub 5}Si{sub 4-x}Ge{sub x} system were determined by X-ray powder diffraction (XRD). Two structurally distinct terminal phase regions were observed in this system: the Ce{sub 5}Si{sub 4}-based solid solution (0 {le} x < 2.85) crystallizing in the Zr{sub 5}Si{sub 4}-type tetragonal structure with space group P4{sub 1}2{sub 1}2, and the Ce{sub 5}Ge{sub 4}-based solid solution (3.35 < x {le} 4) crystallizing in the Sm{sub 5}Ge{sub 4}-type orthorhombic structure with space group Pnma. An intermediate phase, which has a narrow composition range with the monoclinic Gd{sub 5}Si{sub 2}Ge{sub 2}-type structure, space group P112{sub 1}/a, was found to exist at x = 2.95 {+-} 0.05. The Rietveld powder diffraction profile fitting technique was used to refine the crystal structures, lattice parameters, and the atomic positions. The phase relationships of the Ce{sub 5}Si{sub 4-x}Ge{sub x} pseudobinary system after heat treatment were established from these data.

36 MATERIALS SCIENCE↗

Geochemical modeling of leaching of Ca, Mg, Al, and Pb from cementitious waste forms

Results from extraction tests on cement-waste samples were simulated with a thermodynamic equilibrium model using a consistent database, to which lead data were added. Subsequent diffusion tests were modeled by means of a 3D diffusive transport model combined with the geochemical model derived from the extraction tests. Modeling results of the leached major element concentrations for both uncarbonated and (partially) carbonated samples agreed well with the extraction test using the set of pure minerals and solid solutions present in the database. The observed decrease in Ca leaching with increasing carbonation level was qualitatively predicted. Simulations also revealed that Pb leaching is not controlled by dissolution/precipitation only. The addition of the calcite-cerrusite solid solution and adsorption reactions on amorphous Fe- and Al-oxides improved the predictions and are considered to control the Pb leaching during the extractions tests. The dynamic diffusive leaching tests were appropriately modeled for Na, K, Ca and Pb.

36 MATERIALS SCIENCE↗

Magnetic and structural properties of nanostructured Fe–20Al–2Cr powder mixtures

Nanostructured Fe–20Al–2Cr (wt.%) powders have been prepared using high energy planetary ball-mill. Changes in structural, morphological and magnetic properties of the powders during mechanical alloying (MA) and during subsequent annealing have been examined by X-ray diffraction, scanning electron microscopy (SEM) and vibrating sample magnetometer (VSM). The observed structural and microstructural changes have been related to several processes occurring during MA. After MA, the material becomes significantly disordered and refines to nanoscale grain sizes (~ 14 nm). The obtained bcc α-Fe(Al,Cr) solid solution shows a ferromagnetic behavior. Upon subsequent annealing at 400 °C, α-Fe{sub 2}O{sub 3} and spinel oxides are formed at the surface of particles, while structural defects disappeared as Fe(Al,Cr) solid solution becomes more ordered and grain growth occurs. The saturation magnetization (Ms) shows lower values after annealing, attributed to the formation of metal oxides with low magnetic moment. - Graphical abstract: Display Omitted - Highlights: • Nanostructured Fe–Al–Cr powders were prepared by MA. • Careful analysis of the XRD patterns by using the Rietveld refinement • The lattice distortion is evidenced by the increase of both the lattice parameter and the static Debye Waller parameter. • Annealing at 400 °C stabilizes the microstructure at the nanometer range and leads to the formation of Fe{sub 3}O{sub 4} and Fe{sub 2}O{sub 3} oxides. • Both the milled and annealed samples are ferromagnetic.

36 MATERIALS SCIENCE↗