At least 1,117 records · Page 62

Long-term superelastic cycling at nano-scale in Cu-Al-Ni shape memory alloy micropillars

Superelastic behavior at nano-scale has been studied along cycling in Cu-Al-Ni shape memory alloy micropillars. Arrays of square micropillars were produced by focused ion beam milling, on slides of [001] oriented Cu-Al-Ni single crystals. Superelastic behavior of micropillars, due to the stress-induced martensitic transformation, has been studied by nano-compression tests during thousand cycles, and its evolution has been followed along cycling. Each pillar has undergone more than thousand cycles without any detrimental evolution. Moreover, we demonstrate that after thousand cycles they exhibit a perfectly reproducible and completely recoverable superelastic behavior.

36 MATERIALS SCIENCE↗

The Effect of APS-HVOF Bond Coating Thickness Ratio on TBC Furnace Cycle Lifetime

In this work, combinations of NiCoCrAlY APS and high-velocity oxygen fuel (HVOF) bond coatings were deposited on alloy 247 disk substrates with APS yttria-stabilized zirconia (YSZ) top coatings to assess the benefit of air plasma sprayed (APS) ‘flash’ bond coatings. Using 1-h cycles at 1100 °C in air with 10% H 2 O and HVOF-only and APS-only bond coatings as a baseline, it was found that APS flash coatings extended the average coating lifetime by 16% to 35% with the thicker flash coating performing best. Principal component analysis and energy dispersive spectroscopy (EDS) compositional mapping on coatings characterized after 0, 100, 300 and 500 cycles and after failure showed that the Al in the bond coatings was depleted due to both oxidation and back diffusion into the substrate. The APS-only bond coating had significant oxidation throughout the bond coating and was so depleted in Al, that Al diffused from the substrate to the coating. Residual stress maps of the thermally-grown alumina scale were obtained every 100 cycles using photo-stimulated luminescence piezospectroscopy (PLPS) revealing that the Thick Flash coating had the slowest rate of damage accumulation in the oxide scale.

alumina scale↗

Life Prediction of Spent Fuel Storage Canister Material

The original purpose of this project was to develop a probabilistic model for SCC-induced failure of spent fuel storage canisters, exposed to a salt-air environment in the temperature range 30-70°C for periods up to and exceeding 100 years. The nature of this degradation process, which involves multiple degradation mechanisms, combined with variable and uncertain environmental conditions dictates a probabilistic approach to life prediction. A final report for the original portion of the project was submitted earlier. However, residual stress measurements for as-welded and repair welds could not be performed within the original time of the project. As a result of this, a no-cost extension was granted in order to complete these tests. In this report, we report on the results of residual stress measurements.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Impact of Powder Variability on the Microstructure and Mechanical Behavior of Selective Laser Melted Alloy 718

Powder-bed additive manufacturing processes use fine powders to build parts layer-by-layer. Alloy 718 powder feedstocks for selective laser melting (SLM) additive manufacturing are produced commercially by both gas and rotary atomization and are available typically in the 10-45 or 15-45 microns size ranges. A comprehensive investigation was conducted to understand the impact of powder variability on the microstructure and mechanical behavior of SLM 718 heat treated to Aerospace Material Specification (AMS) 5664. This study included sixteen virgin powders and three once-recycled powders within the 10-45 and 15-45 microns size ranges that were obtained from seven direct source suppliers and one reseller. Although alike as highly regular spheroids, these powders showed distinct differences in composition (especially Al, C and N contents), particle size distributions, and powder features such as degree of agglomeration, fusion and surface roughness. Compositional differences expectedly had the strongest impact on microstructure. High N and C contents formed TiN-nitrides and/or (Nb,Ti,Mo)-C carbides on the grain boundaries, prevented recrystallization during heat treatment, and resulted in retained (001)-scalloped shaped grains that ranged from 19 to 41 microns in average size. In the absence of this particle pinning, the average grain size of the heat treated SLM 718 ranged from 51 microns to 90 microns. Room temperature tensile and high cycle fatigue (HCF) testing compared as-fabricated (AF) and low stress ground (LSG) surface conditions. Tensile testing revealed consistent behavior between the two surface conditions and amongst the powder lots. The finer grained SLM 718 builds displayed the lowest tensile properties. A SLM 718 build fabricated from a powder with eight times lower C content showed statistically better tensile properties presumably due to enhanced coarsening of (delta)-Ni3Nb precipitates. The specimens from once-recycled powders had slightly higher tensile strengths and slightly higher ductility compared to their virgin equivalents; once-recycling also did not substantially degrade the mean HCF life. The LSG fatigue lives agreed with conventionally manufactured 718 data, while AF lives exhibited a knock-down due to surface roughness. The fatigue lives of AF specimens were statistically equivalent across powder lots except for one and failures typically initiated at stress concentrators associated with SLM surface asperities. Fatigue testing of low stress ground specimens result in both transgranular and within facet crack initiations. More than half of the cracks initiated from these facets for the machined condition; however, these facets appeared to be within grains that were larger-than-average in size. A nitrogen-atomized powder with fine prior particles of TiN-nitrides and M(Ti,Nb,Mo)C carbides from atomization on powder surfaces resulted in the best fatigue performance with segregation of these particles to the SLM 718 grain boundaries leading to higher resistance to early-stage crack propagation. Typically the fine-grained builds with minor phases along the grain boundaries did not perform well in fatigue, whereas a larger-grain build with lower carbon content and coarser delta-Ni3Nb precipitates showed the next best HCF response. Further details of the build microstructure and its impact on tensile and fatigue behavior was considered.

laser deposition↗

PIP-II cryoplant non thermal cycling updates

The Proton Improvement Plan-II (PIP-II) is a crucial upgrade to the Fermilab accelerator complex, featuring a new 800-MeV Superconducting Radio-Frequency (SRF) linear accelerator (LINAC) with 23 cryomodules operating at 2 K. The LINAC thermohydraulic conditions are satisfied by the cryogenic subsystems: Cryogenic Distribution System (CDS), a helium refrigerator cold box (CB), a warm compression station (WCS) and a helium recovery system (RSYS). The accelerator has a strict requirement of non-thermal cycling of the LINAC cryomodules during planned and unplanned subsystem outages. This paper presents an integrated reliability analysis of the PIPII cryoplant. The study evaluates both normal and abnormal operating modes, with a focus on identifying integrated scenarios that put subsystems components under stress. The conclusions of this study will help build redundancy to mitigate LINAC thermal cycling risks during planned and unplanned subsystem outages.

43 PARTICLE ACCELERATORS↗

Low-Temperature Plasticity in Olivine: Grain Size, Strain Hardening, and the Strength of the Lithosphere

Plastic deformation of olivine at relatively low temperatures (i.e., low-temperature plasticity) likely controls the strength of the lithospheric mantle in a variety of geodynamic contexts. Unfortunately, laboratory estimates of the strength of olivine deforming by low-temperature plasticity vary considerably from study to study, limiting confidence in extrapolation to geological conditions. Here we present the results of deformation experiments on olivine single crystals and aggregates conducted in a deformation-DIA at confining pressures of 5 to 9 GPa and temperatures of 298 to 1473 K. These results demonstrate that, under conditions in which low-temperature plasticity is the dominant deformation mechanism, fine-grained samples are stronger at yield than coarse-grained samples, and the yield stress decreases with increasing temperature. All samples exhibited significant strain hardening until an approximately constant flow stress was reached. The magnitude of the increase in stress from the yield stress to the flow stress was independent of grain size and temperature. Cyclical loading experiments revealed a Bauschinger effect, wherein the initial yield strength is higher than the yield strength during subsequent cycles. Both strain hardening and the Bauschinger effect are interpreted to result from the development of back stresses associated with long-range dislocation interactions. We calibrated a constitutive model based on these observations, and extrapolation of the model to geological conditions predicts that the strength of the lithosphere at yield is low compared to previous experimental predictions but increases significantly with increasing strain. Our results resolve apparent discrepancies in recent observational estimates of the strength of the oceanic lithosphere.

58 GEOSCIENCES↗

Analysis and Test of Deep Flaws in Thin Sheets of Aluminum and Titanium. Volume 2: Crack Opening Displacement and Stress-Strain Data

Static fracture tests were performed on surface flawed specimens of aluminum and titanium alloys. A simulated proof overload cycle was applied prior to all of the cyclic tests. Variables included in each test series were flaw shapes and thickness. Additionally, test temperature was a variable for the aluminum test series. The crack opening displacement and stress-strain data obtained are presented.

Finger, R. W.↗

Deep flaws in weldments of aluminum and titanium

Surface flawed specimens of 2219-T87 and 6Al-4V STA titanium weldments were tested to determine static failure modes, failure strength, and fatigue flaw growth characteristics. Thicknesses selected for this study were purposely set at values where, for most test conditions, abrupt instability of the flaw at fracture would not be expected. Static tests for the aluminum weldments were performed at room, LN2 and LH2 temperatures. Titanium static tests for tests were performed at room and LH2 temperatures. Results of the static tests were used to plot curves relating initial flaw size to leakage- or failure-stresses (i.e. "failure" locus curves). Cyclic tests, for both materials, were then performed at room temperature, using initial flaws only slightly below the previously established failure locus for typical proof stress levels. Cyclic testing was performed on pairs of specimens, one with and one without a simulated proof test cycle. Comparisons were made then to determine the value and effect of proof testing as affected by the various variables of proof and operating stress, flaw shape, material thickness, and alloy.

Masters, J. N.↗

Microtructure and Low-Cycle Fatigue Behavior of Additively Manufactured 316L Stainless Steel at 300°C

Metal additive manufacturing (AM) or 3D printing has the potential to transform the nuclear industry by producing high quality components faster and cheaper, thus enhancing the operating performance of current plants and advanced reactors. Two AM 316L tubes - intended to act as surrogates for complex components where nuclear equipment vendors are more likely to consider AM technologies - were printed using a Renishaw AM400 Laser Powder Bed Fusion (L-PBF) system. The porosity of the as-built material was found to be small, 0.06%. In prior research, the fatigue and corrosion fatigue crack growth rate (CGR) response of the AM specimens in the as-built condition was found to be similar to that expected for conventional alloys, and extremely resistant to stress corrosion cracking (SCC). The present research demonstrates that the low-cycle fatigue behavior of the AM material in air is similar to that of wrought stainless steel at LWR temperature. The data suggest that low porosity levels do not have a significant effect on the fatigue performance of AM materials. Taken together, all data generated to date demonstrate that the use of AM alloys in a nuclear environment is plausible. Additional research on environmental fatigue, crack initiation, and SCC needs to be conducted to provide the performance information needed to qualify AM materials for LWR applications.

36 MATERIALS SCIENCE↗

Analysis of Global Gene Expression in Brachypodium distachyon Reveals Extensive Network Plasticity in Response to Abiotic Stress

Brachypodium distachyon is a close relative of many important cereal crops. Abiotic stress tolerance has a significant impact on productivity of agriculturally important food and feedstock crops. Analysis of the transcriptome of Brachypodium after chilling, high-salinity, drought, and heat stresses revealed diverse differential expression of many transcripts. Weighted Gene Co-Expression Network Analysis revealed 22 distinct gene modules with specific profiles of expression under each stress. Promoter analysis implicated short DNA sequences directly upstream of module members in the regulation of 21 of 22 modules. Functional analysis of module members revealed enrichment in functional terms for 10 of 22 network modules. Analysis of condition-specific correlations between differentially expressed gene pairs revealed extensive plasticity in the expression relationships of gene pairs. Photosynthesis, cell cycle, and cell wall expression modules were down-regulated by all abiotic stresses. Modules which were up-regulated by each abiotic stress fell into diverse and unique gene ontology GO categories. This study provides genomics resources and improves our understanding of abiotic stress responses of Brachypodium.

59 BASIC BIOLOGICAL SCIENCES↗

In-Plane Shear Testing of Medium and High Modulus Woven Graphite Fiber Reinforced/Polyimide Composites

Iosipescu shear tests were performed at room temperature and at 316 C (600 F) o woven composites with either M40J or M60J graphite fibers and PMR-II-50 polyimide resin matrix. The composites were tested as supplied and after thermo-cycling, with the thermo-cycled composites being tested under dry and wet conditions. Acoustic emission (AE) was monitored during the room and high temperature Iosipescu experiments. The shear stresses at the maximum loads and the shear stresses at the significant onset of AE were determined for the composites as function of temperature and conditioning. The combined effects of thermo-cycling and moisture on the strength and stiffness properties of the composites were evaluated. It was determined that the room and high temperature shear stresses at the maximum loads were unaffected by conditioning. However, at room temperature the significant onset of AE was affected by conditioning; the thermal conditioned wet specimens showed the highest shear stress at the onset of AE followed by thermal-conditioned and then as received specimens. Also, at igh temperature the significant onset of AE occurred in some specimens after the maximum load due to the viscoelastoplastic nature of the matrix material.

Gentz, M.↗

The role of creep in high temperature low cycle fatigue.

The significance of the role that creep can play in governing high-temperature, low-cycle fatigue resistance is investigated by conducting strain cycling tests on two high-temperature stainless steel alloys and making concurrent measurements of stress, temperature, and strain at various frequencies. The results are then analyzed in terms of damage imposed by creep and fatigue components. It is shown that creep can play an important and sometimes dominant role in low cycle fatigue at high temperatures. The results of the study include the findings that: (1) the simple life-fraction theory described is adequate for calculating creep damage when the cyclic creep rupture curve is used as a basis for analysis; (2) a method of universal slopes originally developed for room temperature use is sufficiently accurate at high temperature to be used to calculate pure fatigue damage; and (3) a linear creep-fatigue damage rule can explain the transitions observed from one failure mode to another.

Manson, S. S.↗

Temperature dependence of the biaxial modulus, intrinsic stress and composition of plasma deposited silicon oxynitride films

Silicon oxynitride films were deposited by plasma-enhanced chemical-vapor deposition. The elemental composition was varied between silicon nitride and silicon dioxide: SiO(0.3)N(1.0), SiO(0.7)N(1.6), SiO(0.7)N(1.1), and SiO(1.7)N(0.%). These films were annealed in air, at temperatures of 40-240 C above the deposition temperature (260 C), to determine the stability and behavior or each composition. the biaxial modulus, biaxial intrinsic stress, and elemental composition were measured at discrete intervals within the annealing cycle. Films deposited from primarily ammonia possessed considerable hydrogen (up to 38 at.%) and lost nitrogen and hydrogen at anneal temperatures (260-300 C) only marginally higher than the deposition temperature. As the initial oxygen content increased a different mechanism controlled the behavior or the film: The temperature threshold for change rose to approximately equal to 350 C and the loss of nitrogen was compensated by an equivalent rise in the oxygen content. The transformation from silicon oxynitride to silica was completed after 50 h at 400 C. The initial biaxial modulus of all compositions was 21-3- GPa and the intrinsic stress was -30 to 85 MPa. Increasing the oxygen content raised the temperature threshold where cracking first occurred; the two film compositions with the highest initial oxygen content did not crack, even at the highest temperature (450 C) investigated. At 450 C the biaxial modulus increased to approximately equal to 100 GPa and the intrinsic stress was approximately equal to 200 MPa. These increases could be correlated with the observed change in the film's composition. When nitrogen was replaced by oxygen, the induced stress remained lower than the biaxial strength of the material, but, when nitrogen and hydrogen were lost, stress-relieving microcracking occurred.

Harding, David R.↗

Assessing pellet-clad interaction with VERA: WBN1, cycles 6-7

The Consortium for Advanced Simulation of Light Water Reactors (CASL) aims to provide high fidelity simulations of nuclear reactors through the development of the Virtual Environment for Reactor Applications (VERA). One of the primary goals of CASL is to estimate local cladding failure through pellet-clad interaction (PCI). While this capability is being pursued through several different approaches, the procedure presented here focuses on running independent fuel performance calculations with the BISON fuel performance code being developed by Idaho National Laboratory using the multicycle output data from coupled neutron transport/thermal-hydraulics simulations generated by MPACT, CTF, and MAMBA. This type of approach is consistent with traditional fuel performance analysis methods, where the fuel performance analyses are typically separate from core simulation analyses. Recent work simulating 12 cycles of Watts Bar Unit 1 (WBN1) with VERA are capitalized upon, and stand-alone quarter-core BISON results can be obtained for several cycles, assessing parameters of interest to PCI (e.g., maximum centerline fuel temperature, maximum clad hoop stress, minimum gap thickness, and cumulative damage index). This is accomplished by using the coupled neutronics/thermal-hydraulics output power and temperature distributions as inputs for each BISON fuel rod case. Building on previous work which demonstrated this capability for Cycles 1 through 3, this paper presents the results for Cycles 6 and 7. Cycle 7 is of particular interest because significant CRUD-induced power shift was observed. While the current results do not immediately indicate that any rods are at an extreme risk of failure, further analysis on rods highlighted by this work may shed additional light on the likelihood of failure. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A path-dependent fatigue crack propagation model under non-proportional modes I and III loading conditions

It has been well established that fatigue damage process is load-path dependent under non-proportional multi-axial loading conditions. Most of studies to date have been focusing on interpretation of S-N based test data by constructing a path-dependent fatigue damage model. Our paper presents a two-parameter mixed-mode fatigue crack growth model which takes into account of crack growth dependency on both load path traversed and a maximum effective stress intensity attained in a stress intensity factor plane (e.g.,KI-KIII plane). Furthermore, by taking advantage of a path-dependent maximum range (PDMR) cycle definition (Dong et al., 2010; Wei and Dong, 2010), the two parameters are formulated by introducing a moment of load path (MLP) based equivalent stress intensity factor range (ΔKNP) and a maximum effective stress intensity parameter KMax incorporating an interaction term KI·KIII. To examine the effectiveness of the proposed model, two sets of crack growth rate test data are considered. The first set is obtained as a part of this study using 304 stainless steel disk specimens subjected to three combined non-proportional modes I and III loading conditions (i.e., with a phase angle of 0°, 90°, and 180°). The second set was obtained by Feng et al. (2007) using 1070 steel disk specimens subjected to similar types of non-proportional mixed-mode conditions. Once the proposed two-parameter non-proportional mixed-mode crack growth model is used, it is shown that a good correlation can be achieved for both sets of the crack growth rate test data.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Simulated Bladed MMC Disk LCF Validation

The goal of this program was to evaluate the low cycle fatigue behavior of an SCS-6/Ti-6Al-4V sub-component under bi-axial loading conditions at 316 C(600 F). A simulated bladed TMC disk was designed having thirty four blades representing the number that would be used in Allied Signal's JTAGG II impeller. The outer diameter of the bladed ring was 254 mm (10.0 inch) and the inner diameter 114.3 mm (4.50 inch). The outer and inner diameter of the composite zone was 177.8 mm (7.00 inch) and 127.O mm(5.00 inch) respectively. Stress analysis showed that the fatigue life of the bladed composite ring would be about 12000 cycles for the test conditions applied. A modal analysis was conducted which showed that the blades would have sufficient life margin from dynamic excitation. The arbor design was the same as that employed in the spin-to burst test of NAS3-27027. A systematic stress analysis of each part making up the arbor was undertaken to assure the design would meet the low cycle fatigue requirements of the program. The Textron Systems grooved foil-fiber process was chosen to make the SCS-6/Ti-6Al-4V core ring based on the success they had in contract NAS3-27027. Fiber buckling, however, was observed at several locations in the first ring made which rendered it unsuitable for spin testing. The fiber buckling was attributed to cracking of the graphite tooling during the consolidation process. On this basis a second ring was made but it too contained fiber buckling defects. Analysis by Textron indicated that the fiber buckling was most likely due to poor placement of the SCS-6 fiber in the etched grooves of the Ti-6Al-4V foil. This was also a contributor to the defects in the first ring. Since there was little indication of control in the process to manufacture a quality ring a third attempt at making a ring was not undertaken.

Merrick, H. F.↗

Coefficient of Thermal Expansion Evolution during Ratchet Growth of PBX 9502 and Neat TATB

The Plastic-Bonded Explosive (PBX) 9502 is comprised of the insensitive high explosive TATB (triamino trinitrobenzine) crystals coated in FK-800 polymer binder and isostatically pressed. The TATB crystals have a graphitic, plate-like morphology and possess significant thermal and mechanical anisotropy. Compactions of neat TATB or TATB-based composites (like PBX 9502) have been shown to have TATB crystals that are oriented during the pressing process giving rise to TATB texture and resulting in micro- and macro-scale anisotropy of the compaction. Thermal cycling of the compactions results in irreversible volume expansion (or ratchet growth) likely by creating stress points on the microscale. However, the actual mechanism behind this expansion is not fully understood. Previous characterization of the ratchet growth phenomenon has focused on the magnitude of the irreversible strain as measured before and after a thermal cycle. In the work presented here, we analyze the evolving thermal expansion behavior during the ascending and descending temperature ramps and compare differences observed due to the presence/absence of binder in the compaction.

45 MILITARY TECHNOLOGY, WEAPONRY, AND NATIONAL DEF↗

Temperature distributions and thermal stresses in a graded zirconia/metal gas path seal system for aircraft gas turbine engines

A ceramic/metallic aircraft gas turbine outer gas path seal designed for improved engine performance was studied. Transient temperature and stress profiles in a test seal geometry were determined by numerical analysis. During a simulated engine deceleration cycle from sea-level takeoff to idle conditions, the maximum seal temperature occurred below the seal surface, therefore the top layer of the seal was probably subjected to tensile stresses exceeding the modulus of rupture. In the stress analysis both two- and three-dimensional finite element computer programs were used. Predicted trends of the simpler and more easily usable two-dimensional element programs were borne out by the three-dimensional finite element program results.

Taylor, C. M.↗