Search NASA⌕ Search

SEARCH · Search NASA

Results for “etch”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,117 records · Page 62

In situ photoacoustic characterization for porous silicon growing: Detection principles

There are a few methodologies for monitoring the in-situ formation of Porous Silicon (PS). One of the methodologies is photoacoustic. Previous works that reported the use of photoacoustic to study the PS formation do not provide the physical explanation of the origin of the signal. In this paper, a physical explanation of the origin of the photoacoustic signal during the PS etching is provided. The incident modulated radiation and changes in the reflectance are taken as thermal sources. In this paper, a useful methodology is proposed to determine the etching rate, porosity, and refractive index of a PS film by the determination of the sample thickness, using scanning electron microscopy images. This method was developed by carrying out two different experiments using the same anodization conditions. The first experiment consisted of growth of the samples with different etching times to prove the periodicity of the photoacoustic signal, while the second one considered the growth samples using three different wavelengths that are correlated with the period of the photoacoustic signal. The last experiment showed that the period of the photoacoustic signal is proportional to the laser wavelength.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

The impact of interfacial Si contamination on GaN-on-GaN regrowth for high power vertical devices

The development of gallium nitride (GaN) power devices requires a reliable selective-area doping process, which is difficult to achieve because of ongoing challenges associated with the required etch-then-regrow process. The presence of silicon (Si) impurities of unclear physical origin at the GaN regrowth interface has proven to be a major bottleneck. Furthermore, this paper investigates the origin of Si contamination at the epitaxial GaN-on-GaN interface and demonstrates an approach that markedly reduces its impact on device performance. An optimized dry-etching approach combined with UV-ozone and chemical etching is shown to greatly reduce the Si concentration levels at the regrowth interface, and a significant improvement in a reverse leakage current in vertical GaN-based p–n diodes is achieved.

36 MATERIALS SCIENCE↗

Restored Passivation after Complete Removal of Front Poly-Si Between the Grid in Poly-Si/SiO2 Front/Back Cells

This work explores the use of wet chemical etching to completely remove the front poly-Si layer between grid lines of a front/back poly-Si/SiO2 passivated contact device. The purpose of the work is to provide excellent passivation under the metal grid, but to also maximize Jsc by eliminating optical absorption in the front poly-Si. We show that after a high temperature anneal to distribute carriers in the poly-Si/SiO2/c-Si interface all of the poly-Si can be removed selectively with TMAH, using the SiO2 as an etch-stop layer. The etched surface can be repassivated back to its original level with the addition of a SiNx/Al2O3 stack grown on the preserved tunnelling oxide layer followed by a short forming gas anneal. Using symmetric 100 - 200 nm intrinsically doped poly-Si/SiO2 on textured n-type wafer templates we show absolute device efficiency enhancement from 15% to 21% by increasing the Jsc by 12 mA/cm2 after removing the front poly-Si and repassivating while effectively preserving the Voc, and FF of the device. IQE values are similar to PERC devices in the short wavelength range.

etching↗

Tin removal by an annular surface wave plasma antenna in an extreme ultraviolet lithography source

Tin contamination of the collector mirror surface remains one of the crucial issues of EUV (Extreme Ultraviolet) sources, directly impacting the availability of the tool. Hydrogen plasma-based tin removal processes employ hydrogen radicals and ions to interact with tin deposits to form gaseous tin hydride (SnH 4 ), which can be removed through pumping. An annular surface wave plasma (SWP) source developed at the University of Illinois—Urbana Champaign is integrated into the cone and perimeter of the collection mirror for in situ tin removal. The SWP is characterized by high ion and radical densities, low electron temperature, and local generation where etching is needed. This method has the potential to significantly reduce downtime and increase mirror lifetime. Radical probe measurements show hydrogen radical densities in the order of 10 19 m -3 , while Langmuir probe measurements show electron temperatures of up to 6 eV and plasma densities on the order of 10 17–18 m -3 . The generated ions are essential to the tin cleaning and have sufficiently low energy to cause no damage to the collector capping layer. Tin etch rates of up to 270 nm/min were observed in a variety of experimental conditions, including various powers, pressures, flowrates, and temperatures. In conclusion, the high etch rates demonstrated in this study exceed the expected contamination rate of the EUV source.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Effect of fabrication processes on BaTiO 3 capacitor properties

There is an increasing desire to utilize complex functional electronic materials such as ferroelectrics in next-generation microelectronics. As new materials are considered or introduced in this capacity, an understanding of how we can process these materials into those devices must be developed. Here, the effect of different fabrication processes on the ferroelectric and related properties of prototypical metal oxide (SrRuO 3 )/ferroelectric (BaTiO 3 )/metal oxide (SrRuO 3 ) heterostructures is explored. Two different types of etching processes are studied, namely, wet etching of the top SrRuO 3 using a NaIO 4 solution and dry etching using an Ar + -ion beam (i.e., ion milling). Polarization-electric-field hysteresis loops for capacitors produced using both methods are compared. For the ion-milling process, it is found that the Ar + beam can introduce defects into the SrRuO 3 /BaTiO 3 /SrRuO 3 devices and that the milling depth strongly influences the defect level and can induce a voltage imprint on the function. Realizing that such processing approaches may be necessary, work is performed to ameliorate the imprint of the hysteresis loops via ex situ “healing” of the process-induced defects by annealing the ferroelectric material in a barium-and-oxygen-rich environment via a chemical-vapor-deposition-style process. This work provides a pathway for the nanoscale fabrication of these candidate materials for next-generation memory and logic applications.

36 MATERIALS SCIENCE↗

Point defect distribution in high-mobility conductive SrTiO{sub 3} crystals

We have carried out positron-annihilation spectroscopy to characterize the spatial distribution and the nature of vacancy defects in insulating as-received as well as in reduced SrTiO{sub 3} substrates exhibiting high-mobility conduction. The substrates were reduced either by ion etching the substrate surfaces or by doping with vacancies during thin-film deposition at low pressure and high temperature. We show that Ti vacancies are native defects homogeneously distributed in as-received substrates. In contrast, the dominant vacancy defects are the same both in ion etched crystals and substrates reduced during the film growth, and they consist of nonhomogeneous distributions of cation-oxygen vacancy complexes. Their spatial extension is tuned from a few microns in ion-etched samples to the whole substrate in specimens reduced during film deposition. Our results shed light on the transport mechanisms of conductive SrTiO{sub 3} crystals and on strategies for defect-engineered oxide quantum wells, wires, and dots.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Pyramidal pits created by single highly charged ions in BaF{sub 2} single crystals

In various insulators, the impact of individual slow highly charged ions (eV-keV) creates surface nanostructures, whose size depends on the deposited potential energy. Here we report on the damage created on a cleaved BaF{sub 2} (111) surface by irradiation with 4.5xq keV highly charged xenon ions from a room-temperature electron-beam ion trap. Up to charge states q=36, no surface topographic changes on the BaF{sub 2} surface are observed by scanning force microscopy. The hidden stored damage, however, can be made visible using the technique of selective chemical etching. Each individual ion impact develops into a pyramidal etch pits, as can be concluded from a comparison of the areal density of observed etch pits with the applied ion fluence (typically 10{sup 8} ions/cm{sup 2}). The dimensional analysis of the measured pits reveals the significance of the deposited potential energy in the creation of lattice distortions/defects in BaF{sub 2}.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Comparison endpoint study of process plasma and secondary electron beam exciter optical emission spectroscopy

Traditionally process plasmas are often studied and monitored by optical emission spectroscopy. Here, the authors compare experimental measurements from a secondary electron beam excitation and direct process plasma excitation to discuss and illustrate its distinctiveness in the study of process plasmas. They present results that show excitations of etch process effluents in a SF{sub 6} discharge and endpoint detection capabilities in dark plasma process conditions. In SF{sub 6} discharges, a band around 300 nm, not visible in process emission, is observed and it can serve as a good indicator of etch product emission during polysilicon etches. Based on prior work reported in literature the authors believe this band is due to SiF{sub 4} gas phase species.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Tailored ion energy distributions on plasma electrodes

As microelectronic device features continue to shrink approaching atomic dimensions, control of the ion energy distribution on the substrate during plasma etching and deposition becomes increasingly critical. The ion energy should be high enough to drive ion-assisted etching, but not too high to cause substrate damage or loss of selectivity. In many cases, a nearly monoenergetic ion energy distribution (IED) is desired to achieve highly selective etching. In this work, the author briefly reviews: (1) the fundamentals of development of the ion energy distribution in the sheath and (2) methods to control the IED on plasma electrodes. Such methods include the application of “tailored” voltage waveforms on an electrode in continuous wave plasmas, or the application of synchronous bias on a “boundary electrode” during a specified time window in the afterglow of pulsed plasmas.

36 MATERIALS SCIENCE↗

Repair of a mirror coating on a large optic for high laser damage applications using ion milling and over-coating methods

Here, when an optical coating is damaged, deposited incorrectly, or is otherwise unsuitable, the conventional method to restore the optic often entails repolishing the optic surface, which can incur a large cost and long lead time. We propose three alternative options to repolishing, including (i) burying the unsuitable coating under another optical coating, (ii) using ion milling to etch the unsuitable coating completely from the optic surface and then recoating the optic, and (iii) using ion milling to etch through a number of unsuitable layers, leaving the rest of the coating intact, and then recoating the layers that were etched. Repairs were made on test optics with dielectric mirror coatings according to the above three options. The mirror coatings to be repaired were quarter wave stacks of HfO 2 and SiO 2 layers for high reflection at 1054 nm at 45 deg incidence in P-polarization. One of the coating layers was purposely deposited incorrectly as Hf metal instead of HfO2 to evaluate the ability of each repair method to restore the coating’s high laser-induced damage threshold (LIDT) of 64.0 J/cm 2 . The repaired coating with the highest resistance to laser-induced damage was achieved using repair method (ii) with an LIDT of 49.0 to 61.0 J/cm 2 .

36 MATERIALS SCIENCE↗

Fabrication of a terahertz quantum-cascade laser with a double metal waveguide based on multilayer GaAs/AlGaAs heterostructures

The Postgrowth processing of GaAs/AlGaAs multilayer heterostructures for terahertz quantumcascade lasers (QCLs) are studied. This procedure includes the thermocompression bonding of In–Au multilayer heterostructures with a doped n{sup +}-GaAs substrate, mechanical grinding, and selective wet etching of the substrate, and dry etching of QCL ridge mesastripes through a Ti/Au metallization mask 50 and 100 μm wide. Reactive-ion-etching modes with an inductively coupled plasma source in a BCl{sub 3}/Ar gas mixture are selected to obtain vertical walls of the QCL ridge mesastripes with minimum Ti/Au mask sputtering.

36 MATERIALS SCIENCE↗

Investigation of Bearing Axial Cracking: Benchtop and Full-Scale Test Results

The most common failure mode in wind turbine gearboxes is axial cracking in intermediate and high-speed-stage bearings, also commonly called white-etching cracks (WECs). Although these types of cracks have been reported for over a decade, the conditions leading to WECs, the process by which this failure culminates, and the reasons for their apparent prevalence in wind turbine gearboxes are all highly debated. This paper summarizes the state of a multipronged research effort to examine the causes of WECs in wind turbine gearbox bearings. Recent efforts have recreated WECs on a benchtop test rig in highly loaded sliding conditions, wherein it was found that the formation of a dark etching microstructure precedes the formation of a crack, and a crack precedes the formation of white-etching microstructure. A cumulative frictional sliding energy criterion has been postulated to predict the presence of WECs. Bearing loads have also been measured and predicted in steady state and transient drivetrain operations in dynamometer testing. In addition, both loads and sliding at full scale will be measured in planned uptower drivetrain testing. If the cumulative frictional sliding energy is the dominant mechanism that causes WECs, understanding the amount of frictional sliding energy that wind turbine bearings are subjected to in typical operations is the next step in the investigation. If highly loaded sliding conditions are found uptower, similar to the examined benchtop levels, appropriate mitigation solutions can be examined, ranging from new bearing coatings and improved lubricants to changes in gearbox designs and turbine operations.

17 WIND ENERGY↗

Rethinking surface reactions in nanoscale dry processes toward atomic precision and beyond: a physics and chemistry perspective

In this review, we discuss the progress of emerging dry processes with atomic precision. Researchers in the field of plasma processing and surface science have addressed the increasingly challenging demands of material selectivity by utilization of synergistic enhancement of etching or deposition. The discussion encompasses major challenges in the plasma science and technology community. Here, the focus of the review is advances in atomic layer etching and area-selective deposition with activation or deactivation, especially in terms of materials scaling and variety. Control of high-aspect-ratio feature fabrication in semiconductor manufacturing and etched shapes of interior features at the nanoscale are needed. Issues related to profile distortion have received much attention. State-of-the-art techniques used in semiconductor manufacturing are reviewed and future challenges are outlined.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Compact Submillimeter-Wave Receivers Made with Semiconductor Nano-Fabrication Technologies

Advanced semiconductor nanofabrication techniques are utilized to design, fabricate and demonstrate a super-compact, low-mass (<10 grams) submillimeter-wave heterodyne front-end. RF elements such as waveguides and channels are fabricated in a silicon wafer substrate using deep-reactive ion etching (DRIE). Etched patterns with sidewalls angles controlled with 1 deg precision are reported, while maintaining a surface roughness of better than 20 nm rms for the etched structures. This approach is being developed to build compact 2-D imaging arrays in the THz frequency range.

Silicon micromachining↗

Black-silicon as a Wideband Infrared Absorber for the Space Instruments: Fabrication, Modeling, and Characterization

The uniform black silicon (BSI) cryogenically etched has been demonstrated as a superior absorber in par with other ultra-absorbers such as carbon nano tubes in the visible and near-infrared spectrum. In this work, we discuss the fabrication, modeling, and characterization of the BSI aiming at the 2.5-5 microns range. We investigated a series of cryogenic parameters such as temperature, pressure, oxygen flowrate, power, and etching duration and fabricated a series of uniformly etched wafers. Additionally, we established at hree-dimensional mathematical model of a unit cell and manipulated the silicon needle geometry and shape. Our preliminary fabrication results show silicon needles of 8 micron height have five orders of magnitude specular reflectance in the infrared region. The modeling efforts how longer pillar heights could be better absorbers as the wavelength increases.

Wideband absorber↗

Plasma Treatment of Single-Cell Niobium SRF Cavities

Superconducting radio frequency cavities of bulk Niobium are integral components of particle accelerators based on superconducting technology. Wet chemical processing is the commonly used procedure for impurities and surface defects removal and surface roughness improvement , both required to improve the RF performance of the cavity. We are studying plasma etching as an alternate technique to process these cavities. The uniformity of the plasma sheath at the inner wall of the cavity is one prerequisite for its uniform etching. We are developing electro-optic diagnostic techniques to assess the plasma uniformity. Multiple electro-optical probes are placed at different locations of the single cell cavity to diagnose the electrical and optical properties of the plasma. The electrical parameters are required to understand the kinetic nature of the plasma and the optical emission spectroscopy provides the spatial distribution of radicals in the plasma. The spatial variation of the plasma parameters inside the cavity and their effect on the etching of niobium samples placed at different locations in the cavity will be presented.

43 PARTICLE ACCELERATORS↗

Advancing Core Safety of Gen IV and Gen IV + Reactors by Encompassing High-Temperature Resistant Materials - 18673

The paper focuses on the development of materials for Gen IV/IV+ reactor core. It discusses the advancement of materials studied and their application in different components of the reactor core and other auxiliary components which will help in the development of future generation reactors. The paper summarizes the material study showing the characteristic behavior of different materials (coated with FeB and FeB{sub 2}), towards irradiation at near high temperatures and high energy neutron flux condition. The project includes different materials which are coated on the boundaries with varied thickness of FeB and FeB{sub 2}. The samples included Carbon steel, Stainless steel 310, Stainless steel 316, Inconel 718. All above-mentioned samples were received by Prof. J. Szpunar, through an industry with coatings of FeB and FeB{sub 2} with varied thickness along with a bare sample of each material. The samples were irradiated at the University of Saskatchewan reactor, with fast neutron flux of 1.1x10{sup 11} n.cm{sup -2}.sec{sup -1}. I worked on all the samples but the paper particularly focuses on, two carbon steel samples results, received so far. The methodology for the project been followed for all the samples is as follow: 1. Received samples were first polished. 2. Vickers Hardness Test. 3. Mirror polished. 4. Etched with the appropriate etchant for the material. 5. Microscopic study of the etched surface. 6. SEM imaging. 7. Sent for irradiation. 8. The same set of material testing done after irradiation, with an EBSD run on the boundary and main surface. The two Carbon Steel samples (sample 21 and 19) analyzed, were irradiated for 14 hrs. Sample 21 was a bare sample and sample 19 had a coating of FeB, FeB{sub 2} with a ∼0.0010'' thickness. The methodology was followed for material testing before and after the irradiation. The advantage of FeB and FeB{sub 2} coatings are: 1. Higher hardness - 10 times (FeB-1775 and FeB{sub 2}-1450), 2. High-stress capacity, 3. Lower abrasion, 4. Low corrosion. Through the test results obtained before and after the irradiation, I was able to get a view of coating damage at the boundaries of sample 19. The bare sample don't show any difference after irradiation but the coated sample do show cracks in the FeB layer. Which can be seen in the SEM images of sample 19. The hardness results are promising, as hardness didn't change significantly. The hardness test was done on the substrate as the coating was significantly narrow to perform the test. Though the hardness test on coatings was performed by the possessor company which show hardness higher by a factor of 10 when compared to uncoated surfaces. The XRD results, reveal irradiation effect on the crystal lattice, making it deformed, which though is usual during irradiation. The overall analysis along with EBSD done on the two samples are favorable and promising. Though it still needs to be cleared out, whether the cracks on the coating were due to irradiation or due to etching after the samples were irradiated.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

A Reactive Inkjet Printing Process for Fabricating Biodegradable Conductive Zinc Structures

A novel reactive inkjet printing (RIJ) process for fabricating environmentally benign, conductive zinc structures on biodegradable substrates is reported. A precursor consisting of oxidized zinc microparticles is formulated into a viscous ink for high‐resolution, high‐repeatability screen printing. A single RIJ process is performed to selectively dispense an acid‐based oxide etching agent onto the screen‐printed zinc ink to significantly improve its electrical conductivity, up to 4 × 10 4 S m −1 . The RIJ process enables precise control of the amount of deposited etching agent, allowing control of conductivity and avoiding damage caused by excessive acid exposure. The RIJ process deposits the etching agent selectively on the screen‐printed, water‐soluble zinc patterns, thus preserving the print fidelity by avoiding ink smearing that can occur when using a blanket treatment such as submersion. A printed biodegradable antenna with a minimum feature size of 500 μm for use with a batteryless radio frequency identification (RFID) chip is fabricated as demonstration. Due to the higher ink conductivity and improved pattern fidelity, the antenna fabricated by the RIJ process shows a ≈2.2× increase in reading distance compared with a similar antenna that is screen printed and activated using a drop‐casting process.

Sui, Yongkun↗