Y{sub 2}O{sub 3}:Eu{sup 3+} (5 mol%) with Ag nanoparticles prepared by citrate precursor
Y{sub 2}O{sub 3}:Eu{sup 3+} (5 mol% Eu{sup 3+}) and Y{sub 2}O{sub 3}:Eu{sup 3+} (5 mol% Eu{sup 3+}) containing 1 mol% of Ag nanoparticles were prepared by heat treatment of a viscous resin obtained via citrate precursor. TEM and EDS analyses showed that Y{sub 2}O{sub 3}:Eu{sup 3+} (5 mol% Eu{sup 3+}) is formed by nanoparticles with an average size of 12 nm, which increases to 30 nm when Ag is present because the effect of metal induced crystallization occurs. Ag nanoparticles with a size of 9 nm dispersed in Y{sub 2}O{sub 3}:Eu{sup 3+} (5 mol% Eu{sup 3+}) were obtained and the surface plasmon effect on Ag nanoparticles was observed. The emission around 612 nm assigned to the Eu{sup 3+} ({sup 5}D{sub 0{yields}}{sup 7}F{sub 2}) transition enhanced when the Ag nanoparticles were present in the Y{sub 2}O{sub 3}:Eu{sup 3+} luminescent material. - Graphical abstract: The presence of Ag nanoparticles together Y{sub 2}O{sub 3}:Eu{sup 3+} 5 mol% phosphor showed to affect directly the optical and crystallinity of the material. Luminescence spectra show directly the effect observed.