Search NASA⌕ Search

SEARCH · Search NASA

Results for “Synthesis and processing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,135 records · Page 63

The Effects of Oxide Supports on the Low Temperature Hydrogenation Activity of Acetone over Pt/Ni Bimetallic Catalysts on SiO2 gamma-Al2O3 and TiO2

Low temperature (308 K) hydrogenation of acetone was used as a probe reaction to investigate the support effect on the hydrogenation activity of Pt/Ni bimetallic catalysts supported on TiO{sub 2}, SiO{sub 2} and {gamma}-Al{sub 2}O{sub 3}. The oxide supports significantly affected the catalytic properties of Pt/Ni catalysts, in which Pt/Ni/SiO2 bimetallic catalysts exhibited significantly higher activity than the other two bimetallic catalysts. TEM measurements revealed that the three supported Pt/Ni bimetallic catalysts have similar particle size distribution, while CO chemisorption measurements showed very different chemisorption capacity. Extended X-Ray absorption fine structure (EXAFS) measurements of the Pt L{sub III}-edge indicated that Pt atoms were fully reduced and the Pt-Ni bimetallic bonds were formed on all three catalysts. The extent of Pt-Ni bond formation followed the trend of SiO{sub 2} > {gamma}-Al{sub 2}O{sub 3} > TiO{sub 2}, which correlated very well with the hydrogenation activity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Comparison of HMF hydrodeoxygenation over different metal catalysts in a continuous flow reactor

The three-phase hydrodeoxygenation (HDO) of 5-hydroxymethylfurfural (HMF) and hydrogenation of 2,5-dimethylfuran (DMF) were studied over six carbon-supported metal catalysts (Pt, Pd, Ir, Ru, Ni, and Co) using a tubular flow reactor with 1-propanol solvent, at 180 °C and 33 bar. By varying the space time in the reactor, the reaction of HMF is shown to be sequential, with HMF reacting first to furfuryl ethers and other partially hydrogenated products, which then form 2,5-dimethylfuran (DMF). Ring-opened products and 2,5-dimethyltetrahydrofuran (DMTHF) were produced only from reaction of DMF. Rate constants for the pseudo-first-order sequential reactions were obtained for each of the metals. The selectivities for the reaction of DMF varied with the metal catalyst, with Pd forming primarily DMTHF, Ir forming a mixture of DMTHF and open-ring products, and the other metals forming primarily open-ring products. Catalyst stabilities followed the order Pt ~ Ir > Pd > Ni > Co > Ru. Since the stability order correlated with carbon balances in the product (>93% for Pt; <75% for Ru), deactivation appears to be caused by deposition of humins on the catalyst.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Poisoning of Ru/C by homogeneous Brønsted acids in hydrodeoxygenation of 2,5-dimethylfuran via catalytic transfer hydrogenation

It has been proposed that the combination of metal and acid sites is critical for effective ring opening of biomass-derived furans to linear molecules, a reaction that holds promise for the production of renewable polymer precursors and alkanes. As such, in this work, we use 2,5-dimethylfuran (DMF) as a model compound to investigate hydrogenolysis and hydrogenation pathways using a combination of H 2 SO 4 and Ru-mediated catalytic transfer hydrogenation in 2-propanol. Acid-catalyzed hydrolytic ring opening of DMF to 2,5-hexanedione (HDN) occurs readily at 80 °C with a selectivity of 89% in 2-propanol. Over Ru/C, HDN is fully converted after only 2 h at 80 °C, forming a mixture of both ring-closed products (~68% total yield), i.e., 2,5-dimethyltetrahydrofuran (DMTHF) and 2,5-dimethyl-2,3-dihydrofuran (DMDHF), as well as ring opened products (~28% total yield), i.e., 2,5-hexanediol (2,5-HDL) and 2-hexanol (HOL). Rather than observing sequential hydrolysis/hydrogenation reactions, we observe severe suppression of metal chemistry when having both Ru/C and H 2 SO 4 in the reaction system. While minor leaching of Ru occurs in the presence of mineral acids, X-ray photoelectron spectroscopy coupled with CO chemisorption studies suggest that the primary cause of the lack of Ru-mediated chemistry is poisoning by strongly adsorbed sulfate species. This hypothesis is supported by the observation of Ru-catalyzed chemistry when replacing H 2 SO 4 with Nafion, a solid Brønsted acid, as sulfonic acid groups tethered to the polymer backbone cannot adsorb on the metal sites.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗